    Specifications
    HS Code 114379
    Density 0.950 g/cm³
    Melt Flow Rate 10 g/10 min
    Tensile Yield Strength ≥24 MPa
    Elongation At Break ≥500%
    Flexural Modulus ≥900 MPa
    Notched Izod Impact Strength 40-60 J/m
    Vicat Softening Temperature ≥120 °C
    Heat Deflection Temperature 75 °C
    Shore D Hardness 60
    Mold Shrinkage 1.5-3.0%
    Water Absorption <0.01%
    Melting Point 130-135 °C
    Crystallinity 70-80%
    Brittle Temperature ≤ -70 °C

    As an accredited Sinopec Fujian HDPE Y10050F factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Fujian HDPE Y10050F is supplied in 25 kg polyethylene woven bags, 40 bags per pallet, totaling 1,000 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL loading for Sinopec Fujian HDPE Y10050F: 25kg bags, palletized or loose, securely stowed for sea transport.
    Shipping Sinopec Fujian HDPE Y10050F is a non-hazardous high-density polyethylene resin, HS code 3901.20. It ships in 25 kg bags or 1 MT jumbo bags, palletized or loose in 20'/40' containers. No UN number or dangerous goods class. Store dry, cool, away from UV; standard shipping documents apply.
    Storage Store Sinopec Fujian HDPE Y10050F in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, heat, sparks, and strong oxidizers. Keep original bags sealed and palletized to prevent moisture, dust, and contamination. Avoid excessive stacking pressure and prolonged UV exposure. Store separately from incompatible materials. Use first-in-first-out rotation. Follow supplier SDS and local regulations.
    Shelf Life Sinopec Fujian HDPE Y10050F has a typical 12-month shelf life from production when stored dry, ventilated, and away from sunlight/moisture.
    Application of Sinopec Fujian HDPE Y10050F

    Sinopec Fujian HDPE Y10050F, specified at nominal density 0.950 g/cm³ and melt flow rate 0.50 g/10 min under ISO 1133-1:2022, is converted into thin-gauge blown film for retail bags and produce bags on 75 mm grooved-barrier extruders with 25:1 L/D screws and Maddock mixing sections. The axial barrel profile is typically set at 170/180/190/200/205 °C from feed to die, with melt temperature at the die maintained between 190 °C and 210 °C. The spiral mandrel die gap is 1.8 mm to 2.2 mm, and the blow-up ratio is held at 3.0:1 to 4.5:1. Frost line height is set at 6 to 8 die diameters; excursion beyond 8 die diameters produces high-stalk bubble instability and gauge variation exceeding ±5%. The hopper blend is 2.0 wt% white LDPE-based masterbatch and 0.8 wt% slip/antiblock masterbatch containing 20 wt% synthetic silica, dosed by separate gravimetric feeders at the throat. Extruder backpressure is controlled within 250 bar to 350 bar, with output rates from 80 kg/h to 120 kg/h. Dart drop impact measured under ASTM D1709-16A Method B and Elmendorf tear measured under ASTM D1922-15 shift with blow-up ratio; above 4.5:1 machine-direction tear declines, but the exact transition for Y10050F is line-specific and requires converter-side verification. Food-contact compliance is limited to olefin polymers under FDA 21 CFR 177.1520(c), and EU conversion requires overall migration testing under EU Regulation 10/2011 Annex I Table 2 at the 10 mg/dm² limit. Finished converter articles are produce bags and retail carrier bags in 15 µm to 25 µm thickness.

    Why Does Core Layer Modulus Dominate Seal Initiation in Coextruded Cereal Liners?

    In a three-layer coextruded HDPE/LLDPE cereal liner, Y10050F is fed into the core extruder at 70 wt% of the core layer with 30 wt% C4-LLDPE at 0.918 g/cm³ density and 1.0 g/10 min melt index to reduce core viscosity. The core extruder is a 65 mm barrier screw with 30:1 L/D, and the skin-layer extruders are 45 mm smooth-bore screws with 24:1 L/D; total layer distribution is controlled at 20/60/20 and finished film thickness is 28 µm to 35 µm. Core melt temperature is 195 °C to 215 °C, die gap is 1.5 mm, and vertical form-fill-seal line speed is 60 m/min to 90 m/min. Seal initiation temperature is measured by ASTM F88/F88M-21; raising core Y10050F content above 75 wt% increases seal initiation temperature by 3 °C to 5 °C relative to 70 wt%, narrowing the sealing window on high-speed vertical form-fill-seal equipment. Dart drop impact under ASTM D1709-16A Method B is monitored because excessive core stiffness reduces energy absorption at 30 µm; exact published data for Y10050F in this coextruded configuration is limited, and line trials are required. US compliance is under FDA 21 CFR 177.1520 for polyolefin contact with food; EU compliance requires EU Regulation 10/2011 Annex I and Annex II review of all masterbatch additives, with migration testing under Annex III and Annex V. The end product is dry breakfast cereal liners and confectionery liner bags.

    Compliance matrix for Y10050F cereal liner conversion
    ScopeStandard or clauseTest conditionLimit
    US polyolefin food contact21 CFR 177.1520Extractives in n-hexane; usage condition A-HAs specified in 21 CFR
    EU overall migrationEU 10/2011 Annex I Table 2Simulant D1 (50% ethanol), 10 days at 40 °C10 mg/dm²
    Seal strengthASTM F88/F88M-21Peel at 200 mm/minReport value
    Film tensileASTM D882-18500 mm/min, 23 °CReport value

    Extrusion coating lines running Y10050F apply a 12 g/m² to 25 g/m² coating onto corona-treated paperboard at melt temperatures between 205 °C and 230 °C and line speeds from 150 m/min to 300 m/min. The extruder is a 105 mm barrier screw with 28:1 L/D and a T-slot coat-hanger die; air gap is held at 150 mm to 250 mm. Reducing air gap below 150 mm controls neck-in but limits melt oxidation and lowers adhesion; increasing air gap above 250 mm produces draw resonance at high line speed and coating thickness variation above ±1.5 g/m². Where primerless adhesion to paperboard is required, a 90:10 weight blend of Y10050F and LDPE coating resin with melt index 7.0 g/10 min is metered at the hopper; peel adhesion is verified by ASTM D1876-08 T-peel at 200 mm/min. Compliance includes FDA 21 CFR 177.1520 for the polyolefin coating and FDA 21 CFR 176.170 for paper and paperboard in contact with aqueous and fatty foods, plus EU Regulation 1935/2004/EC and EU Regulation 10/2011 for the plastic coating layer. Finished converter articles are frozen food cartons, beverage carrier boxes, and industrial paper sacks with moisture-barrier coating.

    High-Draw Monofilament Orientation and Fibrillation Resistance in Y10050F Tapes

    In flat-die extrusion of Y10050F for woven-sack tapes, a 90 mm single-screw extruder runs at 210 °C to 230 °C, with a flat die gap of 0.8 mm to 1.2 mm and water-bath quenching at 35 °C to 40 °C. The quenched sheet is slit into 2.5 mm to 5.0 mm tapes and hot-air drawn at a draw ratio of 1:6 to 1:8 in an oven at 110 °C to 120 °C. A 2.5 wt% UV stabilizer masterbatch with hindered amine light stabilizer is added for outdoor exposure; 3.0 wt% calcium carbonate masterbatch is used where controlled fibrillation is required for soft woven fabrics. Drawing above 1:8 produces lateral fibrillation and increases tensile strength batch-to-batch variability beyond 5%. Tensile properties are measured under ASTM D638-14 at 500 mm/min crosshead speed; post-draw relaxation is set at 4% to 6% to stabilize tape denier, and denier variation is controlled within ±3%. Food-contact woven sacks require FDA 21 CFR 177.1520 and EU Regulation 10/2011; non-food industrial sacks fall under REACH 1907/2006 Annex XVII restrictions on lead and cadmium pigments. End products are woven sacks for grain, animal feed, cement, and construction waste.

    When Post-Consumer Recyclate Is Blended with Y10050F for Non-Food Waste Liners

    Post-consumer recycled HDPE (PCR) is blended with Y10050F at an 80:20 virgin-to-PCR weight ratio for refuse sacks in 50 µm to 70 µm thickness. The PCR fraction is pre-dried at 80 °C for 4 hours at dew point -30 °C and melt-filtered through a 100-mesh (150 µm) screen changer. The blend is processed on a grooved-barrier extruder at 190 °C to 210 °C; melt pressure is controlled at 330 bar to 380 bar, and output is held at 100 kg/h to 150 kg/h. At PCR addition above 20 wt%, gel count increases and bubble stability deteriorates; dart drop regression for this specific Y10050F/PCR blend is published only as converter line-trial data rather than standardized grade-sheet values. Non-food compliance is covered by REACH Article 3 and Annex XVII, and EU 2019/904 for reduced plastic bag consumption; FDA 21 CFR 177.1520 is not applicable unless the PCR feedstock meets food-contact recycled plastic requirements, which is not typical for post-consumer waste. End product is non-food refuse sacks and municipal waste bags.

    Extrusion Coating of Woven Polypropylene Fabric Produces a Moisture Barrier

    For lamination of woven polypropylene fabric used in FIBC and chemical packaging, Y10050F is extrusion-coated at 15 g/m² to 30 g/m² onto the fabric surface at 220 °C to 240 °C. Adhesion to the woven PP surface is improved by flame treatment or a chlorinated polyolefin primer; coating adhesion is verified by ASTM D3359-17 cross-cut rating of 3B or higher. Chill-roll temperature is set at 15 °C to 20 °C to control flatness and crystallinity. A 5.0 wt% titanium dioxide masterbatch is added for opacity, and a 0.5 wt% processing aid stabilizes the melt curtain; coating weight variation is controlled within ±1.5 g/m². Industrial chemical sacks require UN certification under 13H2 or 13H4 packaging groups with drop and stacking tests under ADR/RID; finished-article restrictions under RoHS 2011/65/EU Annex II and REACH apply when the coated fabric enters the European market. End product is FIBC outer shells, chemical packaging, and tarpaulin laminates.

    Free Quote

    Competitive Sinopec Fujian HDPE Y10050F prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Fujian HDPE Y10050F is a high-density polyethylene grade manufactured at the Fujian refining and petrochemical complex for blown film extrusion. The resin is positioned for high-strength film applications in which melt flow, density, and gauge uniformity are critical. Nominal melt mass-flow rate is 0.50 g/10 min at 190 °C/2.16 kg according to ISO 1133-1:2022; nominal base density is 0.950 g/cm³ according to ISO 1183-1:2019. These values place the product in the medium-molecular-weight HDPE film class, separating it from lower-flow film grades through reduced head pressure and higher throughput capacity on grooved-feed blown-film lines.

    What Are the Nominal Pellet Specifications and Film-Property Benchmarks Published for Y10050F?

    The matrix below consolidates typical pellet property data from grade datasheets and plant quality-control methods. The values are nominal starting points, not permissible product release limits, and converters should verify each lot against their own internal specifications.

    PropertyTest methodTypical nominal value
    Melt mass-flow rate, 190 °C/2.16 kgISO 1133-1:20220.50 g/10 min
    Base density, 23 °CISO 1183-1:20190.950 g/cm³
    Tensile stress at yield, 50 mm/minISO 527-2/1B25 MPa
    Tensile strain at break, 50 mm/minISO 527-2/1B>500 %
    Vicat softening temperature, A50ISO 306:2022124 °C
    Environmental stress-cracking resistance, 100 % Igepal, F50ASTM D1693-15, condition B>100 h

    Pellet-level measurements show a controlled melt-flow rate and density band. Typical plant data for this grade family indicate batch-to-batch MFR variability within ±0.05 g/10 min and density variability within ±0.002 g/cm³. Such limits support stable film thickness control on conventional air-ring lines and reduce gauge variation in downstream converting.

    On a 65 mm grooved-feed single-screw blown-film extruder with L/D 30:1, Y10050F is processed with feed-section barrel temperatures from 160 °C to 180 °C, compression-section temperatures from 190 °C to 205 °C, and die-zone temperatures of 200 °C to 210 °C. A die gap of 1.8 mm to 2.2 mm and a blow-up ratio of 3.0:1 to 4.0:1 are common starting conditions. Melt temperature at the adapter is normally maintained below 220 °C; higher temperatures increase the formation of oxidized gel particles, which appear as fisheyes in thin-gauge film.

    Because the resin has a medium melt-flow rate, screen-pack and die-head pressures are lower than those of high-molecular-weight HDPE film grades. This permits finer screen filtration or increased screw speed without exceeding the extruder thrust-bearing limit. On lines equipped with barrier screws, screw speed is typically adjusted to maintain melt pressure at the breaker plate between 20 MPa and 30 MPa; higher pressures indicate insufficient compression-section temperature, screen blockage, or excessive screw speed for the available torque.

    Routine pellet drying is not required under normal silo storage. Predrying at 80 °C for 2 h is only applied when visible surface condensation from temperature cycling is present. Extended drying does not improve processing stability and may contribute to pellet yellowing.

    Comparative Melt-Flow Position Against 5000S and 7000F in Blown Film Dies

    Y10050F is differentiated from other Sinopec HDPE film grades primarily by its melt-flow position. Direct numerical comparison across grades requires the same conversion line and screw geometry; published data for that specific configuration is limited. In general, Y10050F with its 0.50 g/10 min MFR occupies a processing window between lower-flow 5000S and high-molecular-weight 7000F. The higher MFR reduces shear heating and allows faster post-extrusion drawdown, but it also lowers extensional viscosity. Bubble stability in very thin films below 15 µm therefore requires more precise frost-line control than with 7000F.

    GradeNominal melt-flow classProcessing consequenceTypical application emphasis
    Y10050F0.50 g/10 minLower head pressure, higher throughput, moderate bubble stabilityHeavy-duty sacks, industrial liners, high-stiffness film
    5000SLower MFR class, approximately 0.20–0.35 g/10 minHigher melt strength, higher pressure, lower output at equal screw speedHigh-strength film, large-format bags
    7000FVery low MFR class, below 0.10 g/10 minVery high melt strength, very high pressure, limited outputThick heavy-duty film, high-melt-strength structures

    In practice, the selection between these grades is controlled by the film gauge target and the available extruder torque. Y10050F reduces motor load and die pressure at equal screw speed, but it also reduces bubble stability at high blow-up ratios. Converters should not assume that the same screw profile and temperature profile used for 7000F can be transferred to Y10050F without modification; lower melt viscosity changes the axial pressure profile and can move the melting zone downstream in grooved-feed machines.

    When Y10050F Replaces Conventional HDPE Film Grades in Heavy-Duty Sack Applications

    In heavy-duty sack production, the grade is evaluated for dart impact resistance according to ISO 7765-2, Elmendorf tear resistance according to ISO 6383-2, and tensile properties according to ISO 527-3. The combination of 0.950 g/cm³ density and medium MFR supports high flexural modulus and acceptable puncture resistance. Converters aiming to down-gauge from 80 µm to 60 µm typically blend 10 wt% to 20 wt% LLDPE to maintain dart impact resistance; the addition lowers film modulus and increases machine-direction tear strength.

    Film property measurements require standardized conditioning. Tensile specimens are usually cut from film conditioned for 48 h at 23 °C and 50 % relative humidity. Dart impact values on monolayer film are strongly influenced by film thickness, frost-line height, and blow-up ratio; published data for Y10050F at a specific gauge is limited, and converter trials are required before setting release specifications. Gauge uniformity should be monitored with a beta or infrared thickness scanner across the web width, with control limits typically set at ±5 % of target gauge for heavy-duty sack film.

    For agricultural film and industrial liners, long-term outdoor use requires an adequate hindered-amine light stabilizer package, which is not present in the base resin. Unstabilized film exposed to UV radiation can lose tensile elongation within months. Therefore, outdoor applications are formulation-dependent and must be validated by the converter under ISO 4892-2 accelerated weathering or equivalent long-term exposure.

    Rheological Effects of the Bimodal Molecular Weight Distribution on Die Pressure and Gel Formation

    High-density polyethylene grades in this density and MFR range frequently use a bimodal molecular weight distribution to combine a low-molecular-weight fraction for flow and a high-molecular-weight fraction for melt strength. Under capillary rheometry at 190 °C with a 30:1 L/D die, the low-shear-rate viscosity of Y10050F is lower than that of high-molecular-weight HDPE film grades, while high-shear-rate viscosity remains sufficient for stable film bubble inflation. Because the resin is linear polyethylene, strain hardening is not as pronounced as in LDPE; therefore, bubble instability at blow-up ratios above 4.5:1 may occur. The frost line should be positioned between 6 and 10 die diameters above the air ring to balance molecular orientation and roll tack.

    Gel specks in thin film are a common troubleshooting signal. When gels appear, the first checks are melt temperature, screw speed, and residence time. Melt temperatures above 220 °C, combined with low throughput and high screw speed, increase residence-time distribution and oxidative gel formation. Screen packs are often configured with 100/120/60 mesh layers to remove external contamination without creating excessive pressure drop. A sudden increase in screen pressure accompanied by gel specks generally indicates contamination or a loss of temperature control, not a resin specification shift.

    What Are the Operational Boundaries and Incompatibilities During Conversion?

    Y10050F is not intended for injection molding or profile extrusion; its melt flow is too low for thin-wall mold filling and too high for high-molecular-weight pipe pressure classes. The resin is also not an elastomer or plastomer. Low-temperature impact below −20 °C may be lower than that of LLDPE or EVA, and applications requiring very high dart impact in films below 25 µm or continuous service above 60 °C under load may require a multilayer structure or a different base resin.

    During grade changes, polyethylene-based purges or linear low-density polyethylene of similar melt index should be used. Aggressive chemical purges or high-acid compounds can accelerate corrosion in the die lips and should be avoided unless the machine components are specified for that chemistry. The resin should not be combined with polypropylene or polyamide without a tie-layer because phase separation will reduce film strength and create visible delamination in thick sections.

    Corona treatment to 38 mN/m to 42 mN/m is commonly applied for printing and lamination. Without surface treatment, ink adhesion on polyethylene is insufficient. The treated surface is checked with standard test inks according to ISO 8296. Treated film should be printed within a controlled time window because surface energy decays during storage, particularly under high humidity.

    Additive, Purging, and Food-Contact Compliance Boundaries

    Unpigmented HDPE Y10050F is generally considered suitable for food-contact applications under FDA 21 CFR 177.1520 when the finished article meets end-use extraction limits. For European Union applications, compliance with Regulation 10/2011 requires migration testing on the final film and is not automatically transferred from the resin. Converters must also consider the regulatory status of all masterbatches, processing aids, and surface treatments used in the final structure.

    RequirementStandard or regulationVerification requirement
    Olefin polymer food-contact statusFDA 21 CFR 177.1520End-use extraction test and density condition
    Plastic food-contact materials in EUEU Regulation 10/2011Overall migration and specific migration testing on final article
    Hazardous substances restrictionRoHS 2011/65/EUSupplier declarations, XRF screening of pigment concentrates
    SVHC communicationREACH 1907/2006Article 33 documentation
    Corona-treated surface energyISO 8296Test ink wetting, 38–42 mN/m

    Compliance documentation should be retained per lot, especially when the film enters food or pharmaceutical packaging. For outdoor service, UV stabilization must be added by the converter because the base resin does not contain a sufficient hindered-amine light stabilizer package for multi-year exposure. The operational window for the final film is therefore determined by the additive package and conversion history, not solely by the resin specification.