    Specifications
    HS Code 456199
    Density 0.956 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 7.5 g/10 min
    Tensile Yield Strength ≥28 MPa
    Elongation At Break ≥500 %
    Flexural Modulus ≥1100 MPa
    Izod Notched Impact Strength ≥50 J/m
    Vicat Softening Temperature ≥125 °C
    Melting Point 130–135 °C
    Shore D Hardness 65
    Water Absorption <0.01 %
    Volume Resistivity ≥10^16 Ω·cm
    Dielectric Strength ≥20 kV/mm
    Thermal Conductivity 0.4 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2×10^-4 /°C
    Heat Deflection Temperature 75 °C
    Crystallinity 70–80 %
    Ash Content ≤0.03 %
    Volatile Matter ≤0.1 %

    As an accredited Sinopec Fujian HDPE M5675Q factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Fujian HDPE M5675Q is packed in 25 kg bags or 1000 kg jumbo bags, 20 MT per container.
    Container Loading (20′ FCL) 20′ FCL loads about 17.5 MT of Sinopec Fujian HDPE M5675Q in 25kg PP woven bags, palletized or loose.
    Shipping Sinopec Fujian HDPE M5675Q is shipped as free-flowing polyethylene pellets in moisture-resistant 25 kg woven bags, palletized and stretch-wrapped, or in 1,000 kg jumbo bags. Keep containers clean, dry, and away from heat, direct sunlight, and moisture during transport.
    Storage Store Sinopec Fujian HDPE M5675Q in original sealed bags within a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, moisture, and contamination. Keep pallets stable and undamaged; avoid heat, sparks, open flames, and strong oxidizers. Maintain normal ambient temperatures and avoid prolonged UV exposure. Do not store outdoors unprotected. Use clean, dry handling areas and follow local regulations.
    Shelf Life Sinopec Fujian HDPE M5675Q shelf life: typically two years from manufacture when stored cool, dry, ventilated, away from sunlight.
    Application of Sinopec Fujian HDPE M5675Q

    Sinopec Fujian HDPE M5675Q is a bimodal high-density polyethylene pipe extrusion resin supplied as virgin pellets. The downstream scope is restricted to six commercial sectors: pressurised potable water mains, natural gas distribution pipe, mining slurry and tailings transport, cable protection duct and microduct bundles, submerged outfall/dredge pipelines, and industrial process water/effluent lines. Melt mass flow rate is measured under ISO 1133-1 at 190 °C with a 5 kg load; PE100 classification requires an MRS of 10 MPa at 20 °C and 50-year design life according to ISO 9080 and ISO 12162. Each section identifies the applicable compliance codes, additive loading ratio, downstream processing route, and terminal product class.

    Municipal potable water distribution is the highest-volume downstream segment for M5675Q because potable water pipe requires long-term hydrostatic strength retention and resistance to chlorine-induced slow crack growth. Compound qualification for drinking water service follows ISO 4427-1 and ISO 4427-2, while material classification is assessed under ISO 9080 and ISO 12162; regulatory approval is granted through national certification bodies, with migration testing accepted under EN 12873-1 and taste/odour evaluation under EN 1622. The additive formulation for water-contact pipe uses 1.0–1.5 wt% blue or turquoise HDPE-carrier masterbatch, or 2.0–2.5 wt% carbon black masterbatch where long outdoor storage demands UV stabilisation; antioxidant masterbatch is set at 0.3–0.6 wt% to maintain oxidation induction time above 20 min by ISO 11357-6. Downstream extrusion for water main production is performed on a single-screw extruder with L/D 30:1–33:1, grooved intake, barrier screw geometry, and a melt pump before the pipe die; barrel temperatures are set at 180–210 °C, die temperature at 200–215 °C, and melt temperature is kept below 220 °C to avoid die-lip gel accumulation. Vacuum calibration is maintained at −0.02 MPa to −0.06 MPa gauge, followed by spray cooling at 15–25 °C and haul-off matched to produce SDR 17, SDR 13.6, and SDR 11 pipe. Terminal product classes include 20–1200 mm PE100 water mains, branch saddles, tapping tees, electrofusion couplers, stub flanges, and pre-fabricated spools joined by butt fusion under ISO 21307.

    Can Gas Distribution Pipe Retain Molecular Weight During High-Pressure Die Extrusion?

    Natural gas distribution pipe compounds based on M5675Q must retain slow crack growth resistance and pass rapid crack propagation testing for buried gas service. Product standards are ISO 4437-1 and ISO 4437-2, with slow crack growth measured under ISO 13479 and rapid crack propagation under ISO 13477; carbon black content is quantified by ISO 6964, and dispersion is rated by ISO 18553 with a minimum class A rating in the compounded pipe wall. Carbon black masterbatch loading is controlled at 2.0–2.5 wt% final carbon black by mass, while the yellow identification stripe coextruded on the outer surface contains 1.0–2.0 wt% yellow organic masterbatch; the stripe layer is kept below 10% of total wall thickness to avoid changing the pipe hydrostatic design. The extrusion route uses a grooved-feed single-screw extruder with L/D 30:1 or greater and a coextruder for the stripe; melt temperature is maintained at 190–210 °C, die head pressure is typically 18–28 MPa for medium-diameter pipe, and cooling gradients are set to control residual stress for the 80 °C hydrostatic test in the product specification. Terminal product classes include 25–400 mm PE100 gas mains, 20–200 m coiled service lines, yellow-black striped distribution pipe, saddle fusion fittings, and electrofusion sockets qualified for joint strength under ISO 13953.

    In mining slurry and tailings transport, M5675Q is used as the PE100 matrix for thick-wall hydraulic transport pipe rather than as a direct abrasion liner; high-solids service often combines this resin with ceramic or UHMWPE liners when solids concentration exceeds 35 wt% or particle size exceeds 10 mm. Project specifications commonly adopt ASTM F714 for dimensional tolerance and ISO 9080 with ISO 12162 for hydrostatic design; because no unified ISO abrasion test exists for slurry pipelines, owners may rely on slurry-loop mass loss testing and pressure derating above 20 °C based on manufacturer or project temperature tables. The compound formula for thick-wall mining pipe uses 2.0–2.5 wt% carbon black masterbatch for UV stability and 0.1–0.3 wt% fluoroelastomer polymer processing aid to control melt pressure in high-output dies; calcium carbonate or mineral filler is omitted because it reduces slow crack growth resistance and increases paste wear in acidic tailings water. When wall thickness exceeds 50 mm, internal air or baffled internal water cooling is required to limit centreline porosity and prevent vacuum sizing collapse; barrel temperatures are set at 185–205 °C, die temperature at 210–220 °C, and melt pump suction pressure at 2–5 MPa at outputs up to 1000 kg/h on large extruders. Terminal product classes include tailings discharge pipe with SDR 17–26, return water lines, acid mine drainage gravity pipe, shaft grouting pipelines, and ore concentrate transport pipe with wall thickness up to 90 mm.

    ApplicationGoverning standardsTest method / clauseControl value
    Potable water mainsISO 4427-1, ISO 4427-2, ISO 12162Hydrostatic strength at 20 °C, 50-yearMRS 10 MPa
    Gas distributionISO 4437-1, ISO 13479, ISO 6964SCG test, carbon black contentclass A dispersion; CB 2.0–2.5 wt%
    Mining slurryASTM F714, ISO 9080Dimensional tolerance, hydrostatic pressureSDR 17–26; derating above 20 °C
    Cable protection ductIEC 61386-1, UL 651A, ASTM F2160Crush at 5% deflection, impactUL 94 HB
    Marine outfallISO 21307, ISO 13953Butt fusion tensile testDuctile failure mode
    Industrial effluentISO/TR 10358, ISO 9080Immersion test, pressure derating≤40 °C continuous

    When Microduct Bundles Require a Melt Flow Ratio Below 20 for Continuous Thin-Wall Extrusion

    Cable protection duct and microduct production applies a lower pressure rating than water or gas pipe but places tighter demands on die swell, ovality, and melt stability. The governing standards for this segment include IEC 61386-1 for conduit systems, UL 651A for underground HDPE conduit, and ASTM F2160 for solid-wall HDPE conduit; crush resistance is measured at 5% deflection under UL 651A, and flammability is limited to UL 94 HB. Formulation for black HDPE conduit uses 2.0–2.5 wt% carbon black masterbatch and 0.05–0.2 wt% polymer processing aid to stabilise melt pressure during thin-wall microduct extrusion; coloured fibre microducts use 1.0–2.0 wt% colour masterbatch selected for compatibility with the HDPE carrier resin. The processing route is continuous single-screw extrusion into vacuum calibrators for smooth-wall conduit or into corrugators for flexible subduct; melt temperature for wall thicknesses of 0.8–1.5 mm is controlled at 195–215 °C, and the melt flow ratio measured by ISO 1133-1 at 190 °C/5 kg divided by 190 °C/2.16 kg is kept below 20 to ensure annular die swell consistency. Terminal products include 7/12 mm fibre-optic microducts, 25–200 mm orange or black underground conduit, corrugated innerduct, and coextruded multi-channel cable duct bundles.

    Marine outfall, river crossing, and dredge discharge pipelines made from M5675Q are qualified primarily by shore-assembled butt fusion productivity and by resistance to installation stress rather than by internal pressure rating alone. The governing material standards are ISO 9080 and ISO 12162 for PE100 classification, while joint procedure qualification follows ISO 21307 and tensile joint evaluation uses ISO 13953; installation bending radii are generally not below 20 times outside diameter for solid-wall PE100 to avoid buckling during float-and-sink or pull-in. The additive package for marine service uses 2.5 wt% carbon black masterbatch for UV resistance during extended site storage and 0.4–0.6 wt% antioxidant masterbatch to preserve stabiliser reserves after regrind and multiple passes; pellets exposed to relative humidity above 60% should be dried at 80 °C for 2–4 h before extrusion to prevent surface splay. Thick-wall pipe extrusion is run with wall thickness from 25 mm to 90 mm, using internal cooling and ultrasonic thickness scanning at 1–2 m intervals; beach string assembly for diameters above 500 mm uses butt fusion machines capable of 0.8–1.2 MPa face pressure and controlled pressure-cooling for 10–15 min before handling. Terminal product classes include marine outfall diffuser lines, river crossing mains, seawater intake risers, dredge discharge pontoons, and subsea cable landing guides with outside diameters of 315–1200 mm.

    ApplicationAdditive loading ratioBarrel/die temperatureDistinct process controlTerminal size range
    Potable water1.0–1.5 wt% blue or 2.0–2.5 wt% CB; 0.3–0.6 wt% AO masterbatch180–210 °C / 200–215 °CVacuum −0.02 to −0.06 MPa20–1200 mm
    Gas distribution2.0–2.5 wt% CB; stripe 1.0–2.0 wt%190–210 °CDie head pressure 18–28 MPa25–400 mm
    Mining slurry2.0–2.5 wt% CB; 0.1–0.3 wt% PPA185–205 °C / 210–220 °CInternal cooling above 50 mm wallSDR 17–26; wall ≤90 mm
    Cable duct2.0–2.5 wt% CB; 0.05–0.2 wt% PPA195–215 °CMelt flow ratio below 207/12 mm–200 mm
    Marine outfall2.5 wt% CB; 0.4–0.6 wt% AO185–205 °C / 200–215 °CUltrasonic wall scanning 1–2 m315–1200 mm
    Industrial effluent0.5–1.0 wt% stabiliser; 2.0 wt% CB if outdoor185–205 °C / 200–215 °CNo Cu pigments; metal stearate 0.05 wt% maxUp to 1200 mm

    Slow Crack Growth and Chemical Resistance Boundaries in Industrial Effluent Service

    Industrial process water and chemical effluent service is only suitable for M5675Q when the fluid chemistry is matched to polyethylene chemical resistance data and when the operating temperature is derated from the 20 °C hydrostatic design basis. Chemical resistance is assessed by the combined resistance table in ISO/TR 10358, with pressure-service classification under ISO 9080 and ISO 12162; published data for this specific configuration is limited for many industrial feedstocks, so pre-qualification immersion tests are required before full line specification. The formulation for industrial pipes uses 0.5–1.0 wt% stabiliser masterbatch, with 2.0 wt% carbon black masterbatch when continuous outdoor UV exposure is present; metal stearate levels are kept below 0.05 wt% to avoid pro-oxidant effects, and copper-containing pigments are prohibited. Downstream processing for solid-wall pipe uses a single-screw extruder at 185–205 °C barrel temperature and 200–215 °C die temperature, followed by vacuum calibration; flange adapters and stub ends are injection moulded at 200–240 °C melt temperature and 10–40 °C mould temperature, then joined to the pipe by butt fusion or infrared welding. Terminal product classes include desalination brine transfer lines, power plant cooling water pipes, industrial laundry wastewater, food-grade plant wastewater lines, and chemical plant effluent ducts operating below 40 °C continuous and below 60 °C intermittent; the material is unsuitable for continuous service with strong oxidising acids, aromatic hydrocarbons, chlorinated solvents, and ketones at elevated concentrations.

    Free Quote

    Competitive Sinopec Fujian HDPE M5675Q prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The Sinopec Fujian HDPE M5675Q resin is classified as a high-density polyethylene injection-moulding grade with a nominal melt flow rate of 7.5 g/10 min at 190°C under 2.16 kg load in accordance with ISO 1133-1:2022, and a nominal density of 0.956 g/cm³ under ISO 1183-1:2019. The designation places the material in a moderate-to-high flow segment for HDPE, intended for short-cycle injection moulding of rigid articles such as industrial pails, crates, closures, housewares and thin-wall packaging components. Because Sinopec Fujian does not publish a complete English-language datasheet for M5675Q in all distribution regions, consolidated values from distributor technical bulletins are presented below; the batch certificate issued for each lot remains the controlling document.

    PropertyTest conditionTypical valueStandard
    Melt flow rate190°C, 2.16 kg7.5 g/10 minISO 1133-1:2022
    Density23°C0.956 g/cm³ISO 1183-1:2019
    Tensile stress at yield50 mm/min26 MPaISO 527-2:2012
    Tensile elongation at break50 mm/min>100%ISO 527-2:2012
    Flexural modulus2 mm/min1050 MPaISO 178:2019
    Charpy notched impact strength23°C5.5 kJ/m²ISO 179-1:2010
    Vicat softening temperatureA50, 10 N124°CISO 306:2013
    Shore D hardness15 s62ISO 868:2003

    In screw plastication units with L/D ratios of 20:1 to 25:1 and compression ratios between 2.4:1 and 3.0:1, M5675Q typically melts within a barrel profile of 175°C to 220°C. The melt temperature measured by an air shot should be maintained between 190°C and 230°C; excursions above 240°C increase the risk of oxidative chain scission, yellowing, and loss of notched impact strength. Pre-drying at 80°C for 2 h is warranted only when pellet moisture exceeds 0.05% or bags have been opened at relative humidity above 60% for more than 24 h; otherwise, processing directly from sealed packaging is typical. In high-speed injection machines with clamp force between 1000 kN and 3500 kN, injection pressures of 60 MPa to 100 MPa are commonly observed for wall sections of 1.2 mm to 2.5 mm, with holding pressure set at 40 MPa to 70 MPa to compensate for semi-crystalline shrinkage.

    Regulatory status should not be assumed from density or melt flow rate alone. For food-contact applications, the converting facility must confirm that the specific Sinopec Fujian lot is covered by a statement aligned with EU 10/2011 and GB 9685-2016; direct compliance with FDA 21 CFR 177.1520 applies to the finished olefin polymer article only if extractive limits and end-use conditions are met. Unfilled natural HDPE is generally outside the restriction scope of RoHS 2011/65/EU heavy metals, but coloured masterbatches may introduce cadmium, lead or chromium pigments and must be assessed separately. Under REACH Article 33, communication duties arise only for candidate-list substances present above 0.1 wt% in the article as supplied; the manufacturer’s safety data sheet should be checked for antioxidant and additive disclosures.

    How Does M5675Q Differ from Low-Flow HDPE Pipe and Blow-Moulding Grades?

    At a melt flow rate of 7.5 g/10 min, M5675Q fills thin-wall gates more readily than HDPE grades designed for pipe or large-part extrusion blow moulding, whose MFR values typically lie between 0.2 g/10 min and 0.7 g/10 min. The higher flow implies lower melt strength, which restricts M5675Q. In continuous extrusion blow moulding, parison sag becomes difficult to control at wall thickness above 2.0 mm; use of M5675Q in replacing a blow-moulding grade is therefore confined to small containers with short parison length. In pipe extrusion, M5675Q lacks the bimodal molecular-weight distribution and the slow crystallisation required for PE100 long-term hydrostatic performance, and should not be substituted for PE100 resins in pressure applications such as water or gas piping. Conversely, low-MFR HDPE pipe grades are not interchangeable with M5675Q in injection moulding because they require higher melt temperatures and longer hold-pressure time, generating excessive cycle time and internal stress.

    Thin-wall food-container and industrial-pail tooling exposes a process conflict between rapid cavity filling and acceptable weld-line strength. In multi-cavity hot-runner molds, melt front temperature at the weld line should remain above 200°C; when the injection speed drops below 80 mm/s for wall thickness 1.0 mm, premature freeze-off of the flow front produces visible weld lines and reduced top-load strength. Differential shrinkage between the gate region and the rim is controlled by maintaining a mold surface temperature of 25°C to 35°C and by avoiding packing-pressure decay before the gate freezes. For a 2.0 mm wall, cooling time is typically 10 s to 15 s at 25°C mold temperature; thicker bosses and ribs should be cored to maintain a wall-thickness ratio not exceeding 1.5:1. Chemical resistance of M5675Q follows semi-crystalline HDPE behaviour: the resin is resistant to aqueous acids, alkalis and saline solutions below 60°C, but aromatic and halogenated hydrocarbons can cause swelling or stress-cracking under load. Organic solvent contact should not be specified without testing under ISO 175:2010, because the molded-in stress distribution influences environmental stress cracking.

    Injection Moulding Equipment Settings and Their Operational Boundaries

    Barrel temperature profiles should be profiled from a rear zone of 175°C to a front zone of 215°C. The nozzle should be maintained at 200°C to 220°C to prevent cold-slug formation without drooling at the sprue. A back pressure of 0.5 MPa to 1.5 MPa is sufficient to homogenise the melt; increasing back pressure beyond 2.0 MPa extends recovery time and can generate shear heating greater than 8°C in a 22:1 L/D screw. Injection speed should be matched to part wall thickness rather than set as a fixed value. For wall sections 1.0 mm to 1.5 mm, screw forward travel of 100 mm/s to 150 mm/s is typical; for wall sections above 2.0 mm, speed may be reduced to 40 mm/s to 70 mm/s to avoid jetting. The gate diameter for direct sprue gating should not be less than 2.0 mm; for tunnel or submarine gates, a gate diameter of 0.8 mm to 1.2 mm may require elevated injection speed. Table 2 summarises the parameter limits.

    ParameterRecommended rangeLimiting condition
    Melt temperature190–230°Cbelow 190°C increases weld-line weakness; above 240°C causes oxidative degradation
    Mold surface temperature20–40°Cbelow 15°C increases differential shrinkage; above 50°C imposes a cycle-time penalty
    Injection pressure60–100 MPabelow 60 MPa may produce short shots in thin wall; above 100 MPa risks flash and core deflection
    Hold pressure40–70 MPainsufficient hold causes sink marks; excess hold raises internal stress
    Back pressure0.5–1.5 MPaabove 2.0 MPa induces shear heating and possible colour shift
    Cooling time for 2.0 mm wall10–15 sless than 7 s may cause ejection deformation; more than 20 s reduces productivity

    Field experience on 1000 kN to 3500 kN machines shows that batch-to-batch MFR variation above ±0.5 g/10 min shifts injection pressure requirements by approximately 5 MPa to 8 MPa in thin-wall pails. Production lots with MFR at the upper end of specification can generate flash in tools designed with low clamp force or worn parting lines, whereas lots at the lower end may produce short shots when ambient temperature drops below 15°C and oil temperature control is not maintained. Therefore, molding operatives should log melt viscosity via injection pressure at a fixed screw position rather than relying solely on the certificate MFR. Drying should be verified by weight loss at 105°C for 10 min; moisture content above 0.05% can generate surface splay and irregular gloss in parts with hot-runner systems. Avoid addition of unsaturated ester-based masterbatches or high-acid pigment carriers without re-validating oxidative stability, because the acid scavenger and antioxidant package may be partially antagonized; published data for this specific combination in M5675Q is limited.

    When Short Cycle Times and Thin-Wall Rigidity Are Required

    If the application requires demolding stiffness at 80°C hot-fill exposure, M5675Q should be evaluated against its Vicat A50 softening temperature of 124°C and its heat deflection temperature under load rather than assumed suitable. The density of 0.956 g/cm³ provides higher flexural modulus than lower-density HDPE film grades, but the material still exhibits a flexural modulus below that of glass-filled or mineral-filled PP grades. In thin-wall pails with top-load crush requirements, rib design and rim geometry dominate performance more than material modulus alone; top-load capacity should be measured in accordance with ISO 12048:1994 or an agreed customer method. When hot-runner valve-gate sequencing is used, the selected valve-gate nozzle tip should maintain a tip temperature between 200°C and 230°C; lower tip temperatures cause stringing and early gate freeze, while higher tip temperatures increase gate vestige and degrade regrind. The grade may be considered for use in closures and overcaps where low-temperature impact at -20°C is not the governing criterion; however for freezer applications, notched impact retention should be verified with part-specific drop tests at the intended service temperature.

    Property Retention Depends on Test Temperature and Conditioning History

    Typical notched Charpy impact strength of M5675Q at 23°C is reported as 5.5 kJ/m² under ISO 179-1:2010; at 0°C, the value should not be extrapolated from room-temperature data without test confirmation. Environmental stress-crack resistance measured by ASTM D1693-B is generally lower for high-flow injection grades than for low-flow pipe HDPE grades; if the conversion uses aggressive surface agents, stress-cracking performance should be examined under ASTM D1693-C or ISO 22088-3 on a notched compression-moulded sheet. The grade is not inherently UV-stabilised unless a specific UV package is ordered; black or outdoor articles require carbon black or hindered-amine stabiliser masterbatch to meet ISO 4892-2 weathering requirements. For colour-critical applications, acid scavenger interference with certain organic red and yellow pigments can shift hue; production trials with the intended pigment masterbatch are necessary because published data for this specific grade-pigment configuration is limited.

    Regrind from M5675Q can be reintroduced at up to 20 wt% in injection moulding without systematic loss of Charpy impact strength if the regrind is dried to 0.05% moisture and free of contamination. The use of higher regrind fractions requires melt-flow ratio monitoring and part-level functional testing; no blanket percentage above 20 wt% is supported by distributor technical literature. In industrial pails, crates and thin-wall containers, the main processing risk is not melt flow but dimensional stability after demoulding; post-mold shrinkage of 0.8% to 1.5% in flow direction is observed over 24 h at 23°C, depending on holding pressure and mold temperature. Therefore, critical fits and lid clearances should be validated after the articles have reached ambient equilibrium rather than immediately after ejection.