Sinopec Fujian Hdpe M200054f

Sinopec Fujian HDPE M200054F

    • Product Name: Sinopec Fujian HDPE M200054F
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 498007
    Productname Sinopec Fujian HDPE M200054F
    Manufacturer Sinopec Fujian Refining & Chemical Co., Ltd.
    Grade M200054F
    Polymertype High-Density Polyethylene (HDPE)
    Density 0.954 g/cm³
    Meltflowrate 20 g/10 min (190°C, 2.16 kg)
    Tensileyieldstrength 24 MPa
    Elongationatbreak 500%
    Flexuralmodulus 1000 MPa
    Vicatsofteningtemperature 124°C
    Heatdeflectiontemperature 75°C
    Hardness 65 Shore D
    Notchedizodimpactstrength 50 J/m
    Meltingpoint 130°C
    Moldshrinkage 2.0-3.0%
    Form Pellets
    Color Natural
    Application Injection molding

    As an accredited Sinopec Fujian HDPE M200054F factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Fujian HDPE M200054F is supplied in 25 kg polyethylene-lined woven bags, with 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL loading: Sinopec Fujian HDPE M200054F in 25 kg woven bags, loose-loaded, approximately 18–20 MT net per container.
    Shipping Sinopec Fujian HDPE M200054F ships as a non-hazardous thermoplastic resin in 25 kg PP woven bags, jumbo bags, or bulk bags, palletized and shrink-wrapped. Transport in dry, clean containers or trucks at ambient temperature; keep away from moisture, direct sunlight, and ignition sources. Typically 17–20 metric tons per 20-foot FCL.
    Storage Store Sinopec Fujian HDPE M200054F in a cool, dry, well-ventilated warehouse. Keep original bags sealed and palletized, away from direct sunlight, moisture, heat, sparks, and flames. Avoid contamination with oils, chemicals, or strong oxidizers. Maintain stable ambient temperature, use first-in, first-out stock rotation, stack securely, and protect from UV radiation and physical damage.
    Shelf Life Shelf life is approximately 12 months in unopened original packaging under cool, dry, ventilated storage, away from sunlight and moisture.
    Application of Sinopec Fujian HDPE M200054F

    Processing of Sinopec Fujian HDPE M200054F in thin-gauge retail carrier film begins with a grooved-feed single-screw extruder rather than a smooth-bore cylinder, because the viscosity of this film-grade HDPE at typical film extrusion throughput produces high back pressure and limits feed-zone melting. Extruders with barrel diameters from 45 mm to 75 mm and length-to-diameter ratios from 30:1 to 33:1 are specified. Screw architecture includes a barrier flight section, a spiral Maddock or dispersive mixer, and a low-compression metering section to prevent temperature peaks. Melt temperature is maintained between 190 °C and 220 °C; melt pressure ahead of the screen changer is typically observed in the 25 MPa to 45 MPa range under stable output. Die gap is set at 1.0 mm to 1.5 mm, and blow-up ratio is held between 3.0:1 and 4.5:1 for retail bag gauge bands from 10 μm to 25 μm. Frost line height is controlled between 6 and 8 die diameters. Finished film is evaluated under ASTM D882 for tensile properties, ASTM D1922 for Elmendorf tear, ASTM D1709 Method A for dart drop impact, and ASTM D1004 for slow tear. Downgauging from 20 μm to 12 μm is controlled by machine-direction tear resistance and by dart impact failure mode on high-speed conversion, not by tensile yield alone. Product-specific data for M200054F at gauges below 15 μm is limited in public documentation; pilot-line qualification on the actual bag machine is therefore required before commercial downgauging.

    Conversion of thin high-molecular-weight HDPE film into T-shirt bags introduces secondary processing requirements. Bag-machine sealing jaws operating at 120 °C to 150 °C produce acceptable seal strength only if the film has adequate anti-block and slip additive distribution; otherwise, drag and wrinkling occur at sealing stations. Seal strength is tested by ASTM F88, and coefficient of friction by ISO 8295. Print adhesion on high-speed flexographic lines is measured using tape peel tests in accordance with ASTM F2252 or an equivalent method, with surface treatment held at 38 mN/m to 42 mN/m as determined by ASTM D2578. The terminal product is a high-stiffness retail T-shirt bag with downgauged side walls and a reinforced bottom gusset.

    Which Frost Line Height Preserves Produce Bag Roll Release Without Compromising MD Tear Resistance?

    Produce bag rollstock made from M200054F depends on a high-stalk blown-film geometry to satisfy both tear resistance and roll release at the filling station. The film is produced with a blow-up ratio from 2.8:1 to 3.5:1; the bubble neck is held above the die for a distance of 6 to 8 die diameters before radial expansion begins. This high-stalk configuration reduces the critical machine-direction orientation that otherwise produces low MD tear values measured by ASTM D1922. Raising the frost line to 8 to 10 die diameters is the primary process adjustment; however, a frost line above 10 die diameters introduces bubble oscillation and gauge bands that exceed ±8% of nominal thickness. Internal bubble cooling is recommended when output exceeds the line’s air-ring-only cooling capacity; the IBC exhaust must be balanced to avoid condensation on the internal bubble surface. Anti-block inorganic additives at 1000 ppm to 2500 ppm based on film mass and slip additive at 300 ppm to 800 ppm are used to prevent roll blocking; blocking force is measured by ASTM D3354. The terminal product is a perforated roll of produce bags that opens cleanly on a dispensing rack at ambient storage temperatures from 5 °C to 35 °C. Published product-specific data for high-stalk M200054F processing are limited; therefore, the exact frost line height must be mapped on the target line because die diameter, air-ring design, and cooling-air temperature shift the stable window.

    Dart impact of produce bag film is assessed under ASTM D1709 Method A for thicknesses below 25 μm, and tensile elongation at break is measured by ASTM D882. The film must maintain sufficient elongation at break to survive the perforation step on the bag machine, where blade pressure and film tension can initiate micro-cracks at the perforation root. A minimum elongation at break in machine direction of 400% is commonly required, but the exact acceptance limit is set by the bag-machine maker or packer specification.

    Coextruded cereal liners use M200054F in the core layer of three-layer structures to provide stiffness and moisture vapor resistance while avoiding direct exposure of the high-density polyethylene to the sealing jaw. A typical structure is a skin/core/skin layering with M200054F at 50 wt% to 70 wt% of the film and LLDPE or metallocene LLDPE skins at the balance. The high-density core reduces water vapor transmission rate measured by ASTM F1249 at 37.8 °C and 90% RH, and the LLDPE skins provide seal initiation temperature and hot-tack strength. Seal strength is measured by ASTM F88, hot tack by ASTM F1921, and oxygen transmission rate by ASTM D3985 at 23 °C and 0% RH. Coextrusion lines use spiral mandrel dies with diameters from 150 mm to 250 mm and die gaps from 1.8 mm to 2.4 mm. The terminal product is a breakfast cereal liner with improved shelf-life barrier performance at reduced total film thickness. If the core layer exceeds 70 wt%, interfacial instability between the high-viscosity HDPE and the LLDPE skins may create visible flow lines; layer-profile validation by pilot-line optical inspection is required.

    Use of M200054F in cereal liners intended for food contact requires compliance with 21 CFR 177.1520(c) for the U.S., Regulation (EU) No 10/2011 for Europe, and GB 4806.7-2023 for China, provided the resin lot is covered by the supplier’s food-contact declaration. Overall migration is tested on the finished laminate with food simulants according to EN 1186 series, and the limit is 10 mg/dm² or 60 mg/kg depending on the stated conversion. The terminal product is a dry-food cereal liner that must meet organoleptic neutrality in addition to migration compliance.

    M200054F Serves as a High-Viscosity Virgin Diluent in Recycled-Content Retail Bag Film

    Post-consumer HDPE film regrind collected from commercial bag streams has reduced melt strength and lower environmental stress crack resistance after repeated thermal and oxidative histories. Incorporating M200054F at 20 wt% to 40 wt% into washed regrind restores bubble stability and increases film toughness in the resulting recycled-content retail bag film. The blend is compounded on a co-rotating twin-screw extruder with screw diameter from 40 mm to 60 mm and L/D ratio of 40:1, followed by strand pelletization. Melt-flow rate is measured by ISO 1133-1:2022 at 190 °C and 5 kg load; the virgin resin amount is adjusted so that the blend remains within the processable range for the existing blown-film extruder. Tensile properties are tested under ASTM D638-14 on compression-molded sheets, and ESCR is tested by ASTM D1693 Method B in Igepal CO-630 solution. The main processing constraint is particulate contamination in post-consumer regrind; continuous screen changers with layered mesh packs from 40/80/120 are used to prevent melt pressure above 45 MPa. Without adequate filtration, screen-pack leakage and melt-temperature spikes occur. The terminal product is a retail bag containing 20% to 40% post-consumer recycled HDPE and meeting the retailer’s film durability specification. Published data for the specific M200054F/PCR blend ratio is limited, so lot-by-lot characterization is required.

    Regulatory compliance for recycled-content retail bags includes REACH SVHC screening at 0.1 wt% and heavy-metal limits under Directive 94/62/EC at 100 mg/kg for the sum of lead, cadmium, mercury, and chromium VI in packaging. The film is also tested for odor and residual contaminants using the packer’s internal sensory procedure, because post-consumer feedstocks can carry degradation by-products that affect roll presentation.

    Dry Food Pouch HDPE Film Laminates and the Associated Compliance Burden

    Dry food pouches can use M200054F as the sealant web or as an internal lamination layer when the primary sealant is a lower-melting polyolefin. The resin’s function in this structure is to provide stiffness and puncture resistance at reduced thickness while maintaining compatibility with adhesive lamination and flexographic printing. Film is produced on blown-film equipment with a die gap of 1.0 mm to 1.4 mm, a blow-up ratio of 2.5:1 to 3.5:1, and a frost line height of 6 to 9 die diameters. Puncture resistance is tested by ASTM D5748 or a specified internal probe method; tensile properties are measured by ASTM D882; and haze is determined by ASTM D1003. The terminal product is a flat-bottom pouch or side-gusset pouch for dry mixes, grains, or sugar-based products, where HDPE contributes to product protection and reduces packaging weight. Total film thickness for this application is typically 40 μm to 80 μm in the lamination web, with the final laminate thickness controlled by the converter.

    JurisdictionRegulationRelevant Provision/TestTypical Limit
    United States21 CFR 177.1520(c)Olefin polymer specification and optional extractables for food contact typesCompare with extraction limits in the regulation for the intended food type
    European UnionRegulation (EU) No 10/2011Overall migration via EN 1186 series10 mg/dm²
    ChinaGB 4806.7-2023Overall migration for plastics10 mg/dm²
    EU packagingDirective 94/62/ECSum of lead, cadmium, mercury, chromium VI100 mg/kg

    For heavy-duty industrial liners and construction waste sacks, M200054F is processed at higher thicknesses to exploit its high-molecular-weight structure and slow crack resistance. Film thicknesses from 50 μm to 150 μm are produced on blown-film lines with blow-up ratios of 2.0:1 to 3.0:1 and die gaps of 1.2 mm to 1.8 mm. Dart drop impact is tested by ASTM D1709 Method B for films above 50 μm, Elmendorf tear by ASTM D1922, and slow puncture resistance by ASTM D5748 where specified. Carbon black masterbatch is added at 2.0 wt% to 2.5 wt% for UV stabilization when bags are stored outdoors; dispersion is checked by optical microscopy or ASTM D5596. The terminal product is a heavy-gauge construction waste liner or agricultural sack with high resistance to tear propagation during loading and transport. Gauge control on thick HDPE film is less demanding than thin-gauge packaging, and this scenario requires only standard blown-film extrusion practice once the die gap and air-ring settings are established.

    Free Quote

    Competitive Sinopec Fujian HDPE M200054F prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    HDPE M200054F, marketed by Fujian Refining & Chemical Co., Ltd. within the Sinopec portfolio, is a high-density polyethylene grade designed for blown-film extrusion of thin-gauge packaging structures. The resin is supplied as pellets and is used in vest-style carrier bags, bin liners, and high-stiffness overwrap. Its nominal density of 0.954 g/cm³ measured according to ISO 1183-1:2019 and nominal melt flow rate of 0.05 g/10 min at 190 °C under 2.16 kg load measured according to ISO 1133-1:2022 place the grade in the high-molecular-weight HDPE film class. The grade-code suffix “F” indicates film extrusion. Compared with injection-molding HDPE grades of 5–20 g/10 min, the lower melt index of M200054F increases melt strength and bubble stability. Compared with medium-flow HDPE film grades of 0.20–0.70 g/10 min, the resin provides stronger thin-gauge film and higher melt tension, but increases extruder back pressure and may require wider die gaps. Published release values should be confirmed against the manufacturer’s certificate of analysis, because resin lots may vary within the specification band.

    On conventional HDPE film lines fitted with 45–90 mm single-screw extruders and 24:1–30:1 L/D barrier screws, barrel profiles are usually set from 170 °C in the feed section to 200 °C in the metering section, with adapter and die zones held at 190–210 °C. A screen pack of 40/60/80 mesh protects the die from carbonized resin and metal fines. Start-up with a 1.2–2.0 mm die gap and a blow-up ratio of 3:1–5:1 establishes a stable frost line before automatic gauge control is activated. For high-molecular-weight HDPE film, die-gap adjustments of 0.05 mm can produce disproportionately large changes in die-head pressure and bubble curvature; therefore small geometry changes are preferred over large melting-profile shifts.

    What Limits Melt Pressure and Bubble Stability on High-Density Film Lines?

    Extrusion back pressure depends on melt viscosity at the die-land shear rate, die land length, and screw speed. For a resin with 0.05 g/10 min melt flow rate and 0.954 g/cm³ density, apparent shear viscosity at 100 s−1 is expected in the range of 5,000–8,000 Pa·s; product-specific published data is limited, so this band is inferred from HDPE film grades of similar molecular weight and density. Melt pressure above 50 MPa at the breaker plate usually indicates screen blockage, insufficient metering-zone temperature, or an excessively narrow die-lip gap. Processing at melt temperature above 225 °C lowers extensional viscosity and can induce bubble sag, gauge variation, and edge folds. In coextruded structures, the M200054F skin layer is often run at 10–15 °C below the adjacent LLDPE core to preserve layer geometry and reduce die-lip oxidation. Long-chain branching is not deliberately introduced; the grade relies on high molecular weight and density for melt strength.

    Extensional deformation in the bubble is dominated by the high-molecular-weight fraction. In linear polyethylenes, strain hardening is weaker than in metallocene LLDPE, so bubble stability is controlled mainly by cooling rate and frost-line geometry. The ratio of melt flow rate under 21.6 kg to 2.16 kg is used as an indirect indicator of molecular weight distribution; high-molecular-weight HDPE film grades in the 0.05 g/10 min class typically show flow rate ratios of 100–160. A lower ratio indicates a narrower distribution and less shear thinning; a higher ratio can improve processing at high output but may promote melt fracture. Sharkskin on the bubble exterior is generally observed when die wall shear stress exceeds approximately 0.14–0.18 MPa for linear HDPE. M200054F is positioned to operate below this shear-stress threshold on polished dies, but die-temperature uniformity and die-lip surface condition remain critical at high output rates.

    Because M200054F is linear and lacks the long-chain branching of high-pressure LDPE, its melt elasticity is lower. High-pressure LDPE grades typically exhibit greater shear thinning and extensional viscosity at low melt temperature, which can stabilize the bubble during high-stalk extrusion. In blends, additions of 10–30 wt% M200054F to LDPE or LLDPE increase film modulus; the main operational limits are die-lip buildup and melt fracture caused by the viscosity mismatch between the linear HDPE and the more elastic branch-containing material.

    In coextruded three-layer film structures, M200054F is typically assigned to the outer skins to increase flexural stiffness and moisture barrier, while LLDPE occupies the core for dart impact and seal-initiation behavior. Layer thickness ratios of 10/80/10 or 20/60/20 by volume are common starting points. The melt temperature of the HDPE skin is held 10–15 °C lower than the LLDPE core to prevent layer intermixing at the die land and to preserve barrier geometry. If layer encapsulation is observed, the die-body temperature gradient should be reduced by 5 °C intervals rather than altering the resin ratio, because viscosity matching is more controllable than throughput ratio changes.

    The M200054F grade occupies a specific position within the Sinopec Fujian HDPE film portfolio. Lower-flow film grades are usually selected for very thin high-strength bags where bubble stability and melt strength are the bottleneck; higher-flow film grades are selected for thick sheet or cast-film lines where heat removal and output limit productivity. M200054F is intended for blown-film lines that need a balance between extrusion pressure, bubble stability, and film stiffness. In thin-gauge grocery sacks, it can replace a medium-flow HDPE grade when dart impact and melt strength are limiting; the trade-off is increased back pressure and lower throughput on the same die gap.

    Film Stiffness, Moisture Barrier, and Tear Propagation in M200054F

    At a density of 0.954 g/cm³, the resin provides higher secant modulus than LLDPE and LDPE film grades. For HDPE film in this density range, secant modulus at 1% strain is generally reported from 800 MPa to 1,100 MPa under ISO 527-2, while a butene-LLDPE film grade of 0.920 g/cm³ density typically exhibits 180–280 MPa. This stiffness permits down-gauging from 25 µm LLDPE to 18 µm HDPE in carrier-bag side walls without unacceptable collapse under load. The compromise is lower dart impact and lower machine-direction tear strength; M200054F is therefore not a direct replacement for LLDPE in high-puncture or high-stretch service. Water vapor transmission rate for high-density film of this density at 25 µm is typically 4–7 g·m−2·day−1 at 38 °C and 90% RH under ASTM E96/E96M, while LLDPE of the same gauge is often 12–18 g·m−2·day−1. Product-specific WVTR data for M200054F is limited.

    The following typical lot data are provided for initial engineering calculations. They are not specification limits and are not design allowables.

    PropertyTest MethodUnitTypical Value
    Melt flow rate, 190 °C, 2.16 kgISO 1133-1:2022 / ASTM D1238-23g/10 min0.05
    Density, 23 °CISO 1183-1:2019 / ASTM D1505-18g/cm³0.954
    Tensile yield stressISO 527-2/1BMPa27
    Tensile strain at breakISO 527-2/1B%600
    Secant modulus at 1% strainISO 527-2/1BMPa900
    Dart impact, Method AASTM D1709-16ag160
    Vicat softening temperature A120ISO 306°C124

    These values indicate a material that is stiff, with moderate impact resistance. The dart impact value is highly dependent on film gauge, die gap, frost-line height, and regrind content; published data for this specific grade under all combinations is limited, so converters should generate internal process capability data before setting specification limits. In practice, the resin’s density is the main variable governing film stiffness, while the melt flow rate governs extruder output and bubble tension. A density shift of 0.001 g/cm³ can alter secant modulus by approximately 20–40 MPa in high-density film grades, making reactor density control critical.

    Differences from other film resin classes are summarized below. The ranges are general process-engineering comparisons, not grade-specific certifications.

    Resin ClassMelt Flow RateDensityTypical Secant ModulusPrimary Drawback in Thin Film
    M200054F HDPE0.05 g/10 min0.954 g/cm³800–1,100 MPaHigher back pressure than medium-flow HDPE
    Medium-flow HDPE film grade0.20–0.70 g/10 min0.953–0.956 g/cm³800–1,000 MPaLower melt strength and lower dart impact
    Butene-LLDPE film grade0.8–1.2 g/10 min0.918–0.922 g/cm³180–280 MPaLower stiffness and lower moisture barrier

    Fluoropolymer processing aids in the range of 200–500 ppm are sometimes added to reduce die-lip buildup and delay the onset of melt fracture. If the film is printed, surface treatment should achieve a wetting tension of at least 42 mN/m measured by ISO 8296 or ASTM D2578. HDPE tends to retain surface oxidation more slowly than polypropylene, but treated film should still be converted within a defined inventory window because dyne level decays with time, humidity, and slip-migration to the surface.

    When Gauge Uniformity and Frost-Line Positioning Are Used as Quality Gates

    After film is collapsed, heat sealing is usually performed at jaw temperatures of 125–135 °C. Hot-tack strength of high-density film in this density class is lower than that of LLDPE, so high-speed bag machines may require an antiblock masterbatch addition of 2,000–5,000 ppm synthetic silica and a slip masterbatch addition of 300–800 ppm erucamide depending on unwind and print requirements. Without such additives, blocking force can exceed 0.5 coefficient of friction and cause film-web transfer failure. Product-specific data for M200054F is limited; these ranges are derived from general HDPE blown-film practice.

    Gauge profile on thin HDPE film is monitored with capacitance or beta gauges after the collapsing frame. For a resin of 0.954 g/cm³ density and 0.05 g/10 min melt flow rate, frost-line height is the primary thermal variable controlling orientation balance and tear anisotropy. A frost line set too close to the die freezes molecular orientation before stress relaxation, yielding high machine-direction shrinkage and low machine-direction tear. On conventional lines with a blow-up ratio near 4:1, frost-line heights of 6–8 times die diameter are used as initial quality gates. Die-lip and air-ring adjustments are made only after the bubble has been stable for at least 10 min at a constant melt temperature. Heat-sealing surfaces are influenced by additive plate-out and by low-molecular-weight degradation products. Visual inspection of die lips at 8 h intervals and gel analysis under ASTM D7310 can detect oxidative gels before they become sealing defects. In commercial film production, reclaim addition up to 20 wt% is common, but each 10 wt% increment of trim scrap can shift melt flow rate by 0.01–0.03 g/10 min upward and reduce dart impact by 5–15%; the exact shift depends on scrap thermal history and contamination level.

    Film breakage on the tower is commonly caused by excessive frost-line height, unbalanced air-ring velocity, or a die lip contaminated with degraded resin. Low-molecular-weight degradation products can appear as yellow-brown specking at die edges and then transfer to the film as gel streaks. The corrective action is usually to purge the die with a lower-MI HDPE or a commercial purging compound, then reset the temperature profile from the die backward rather than increasing all zones simultaneously.

    Mechanical recycling of edge trim and rejected film is possible because the matrix is a linear polyethylene. Reclaim should be free of adhesive labels, polypropylene contamination, and paper fibers; polypropylene contamination above 2 wt% can promote localized gels and reduce tear strength. Flake bulk density after grinding is generally 250–450 kg/m³, and feeding systems should be designed to prevent bridging. Converters should monitor gel counts after regrind introduction because oxidative gels from multiple heat histories can raise the coefficient of friction and degrade heat-seal performance.

    Food-contact declarations for HDPE M200054F require finished-article compliance with FDA 21 CFR 177.1520 and, in the European Union, EU Regulation (EU) No 10/2011. Overall migration testing in 10 days at 40 °C with aqueous food simulants and specific migration testing for any added masterbatch components remain the converter’s responsibility. The grade is not rated for pressure pipe or structural injection molding. It should not be combined with high levels of oxidizing or pro-degradant masterbatch because oxidative chain scission can shift melt flow rate and reduce impact. HDPE is not hygroscopic, but pellet sweating during transfer from cold silos to heated machine hoppers can introduce surface moisture. If condensation is present, pre-drying at 60 °C for 2 h in a hot-air or desiccant hopper is a common corrective action. Halogenated flame-retardant additives are not recommended for this matrix unless specific compatibilization and thermal stabilization have been validated under ISO 11358-1 thermal decomposition screening.

    Top