Sinopec Fujian Hdpe Fta 001

Sinopec Fujian HDPE FTA-001

    • Product Name: Sinopec Fujian HDPE FTA-001
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 555758
    Density 0.954 g/cm³
    Melt Flow Rate 0.05 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield ≥25 MPa
    Tensile Strength At Break ≥30 MPa
    Elongation At Break ≥500%
    Dart Impact Strength ≥200 g
    Vicat Softening Temperature ≥120 °C
    Melting Temperature 135 °C
    Environmental Stress Cracking Resistance ≥1000 h
    Haze ≤12%
    Bulk Density ≥0.50 g/cm³
    Moisture Content ≤0.1%

    As an accredited Sinopec Fujian HDPE FTA-001 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Fujian HDPE FTA-001 is packaged in standard 25 kg woven polypropylene bags, each palletized for industrial shipment.
    Container Loading (20′ FCL) 20′ FCL container loading of Sinopec Fujian HDPE FTA-001: 25 kg bags, 25 MT net, palletized, shrink-wrapped, and securely stowed.
    Shipping Sinopec Fujian HDPE FTA-001 is a non-hazardous thermoplastic resin, typically shipped in 25 kg PE-lined woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport by sea/land in clean, dry containers; keep away from moisture, sunlight, and heat. No special dangerous goods handling required.
    Storage Store Sinopec Fujian HDPE FTA-001 in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, moisture, heat, sparks, flames, and strong oxidizers. Keep original bags sealed, palletized, and off the floor. Avoid contamination, crushing, and prolonged UV exposure. Do not store near food, feed, or incompatible materials. Follow local fire regulations; control dust and ensure safe stacking.
    Shelf Life Sinopec Fujian HDPE FTA-001 shelf life is typically 24 months stored cool, dry, ventilated, away from direct sunlight in sealed packaging.
    Application of Sinopec Fujian HDPE FTA-001

    Sinopec Fujian HDPE FTA-001 enters blown film conversion for retail T-shirt sack production at die gaps of 0.8–1.2 mm, bubble blow-up ratios of 3:1 to 4:1, and frost line heights of 6–8 times die diameter. The resin is dry-blended with a linear low-density polyethylene at 10–25 wt% when gauge uniformity below 15 µm is specified, because the added linear component raises bubble stability and reduces splitty tear propagation. Film produced at 12–20 µm nominal thickness is tested for dart drop impact under ASTM D1709-16a and tensile yield under ISO 527-3:2018; the high-density fraction contributes machine-direction modulus, while the low-density fraction preserves puncture resistance. On production-scale lines with 40–65 mm screw diameter and L/D 25–30, barrel temperatures are set from 180°C to 210°C in the feed zone and 200°C to 220°C in the metering zone, with die temperature held at 210°C to 230°C to suppress melt fracture. Roll-stock film is converted into T-shirt bags by side-seal or bottom-seal machines; finished bag widths of 300–550 mm and lengths of 450–700 mm are common for grocery and convenience-store sacks. The grade should not be processed without internal bubble cooling when film below 10 µm is targeted, because oscillation of the frost line may create gauge bands outside ±0.5 µm. Color masterbatch addition is limited to 2–5 wt%; higher loading can lower melt strength and generate visible sharkskin on the film surface. If regrind is incorporated above 30 wt%, pre-drying at 80°C for 2 h is recommended to reduce gel particles from oxidized trim. Finished sacks are tested for seal strength, elongation, and load retention; no direct food-contact certification is implied unless the converter verifies finished-article compliance with FDA 21 CFR 177.1520 and EU 10/2011 migration limits.

    What Governs Melt Fracture and Gauge Spread in Thin-Gauge Industrial Liner Films?

    Thin-gauge industrial liner conversion from HDPE FTA-001 is constrained by melt fracture onset and bubble stability rather than by melt temperature alone. On three-layer blown film lines with 50 mm extruder diameter and L/D 30, a die gap of 1.0–1.4 mm and blow-up ratio of 2.5:1 to 3.5:1 are used to produce film at 8–15 µm. The formulation commonly blends FTA-001 with a metallocene linear low-density polyethylene at 20–30 wt%; the metallocene component depresses the onset of sharkskin and increases dart drop resistance, but reduces machine-direction modulus. Slip and antiblock masterbatch is dosed at 1,000–1,500 ppm active silica or erucamide content, verified by supplier certificate, to prevent roll blocking. Frost line height is maintained at 4–6 die diameters above the die face; excessive cooling air velocity above 35 m/s destabilizes the bubble and creates gauge oscillation. Barrel temperature profile is 190°C/200°C/205°C/210°C from feed to die, with screen pack 20/40/60/80 mesh to remove gel particles above 100 µm. The resulting liners are converted into can liners and drum liners at thicknesses of 8–25 µm, with tensile strength at break measured by ASTM D882-18 and Elmendorf tear measured by ASTM D1922-09(2015). A production bottleneck observed on high-output lines occurs when internal bubble cooling air temperature exceeds 35°C; this lifts the frost line and reduces transverse direction tensile strength. Pre-drying of virgin resin is normally not required if silo storage relative humidity is below 60%, but regrind above 20 wt% increases gel frequency unless the trim is ground with a 5 mm screen and dried at 70°C for 2 h. Finished industrial liners must meet REACH and RoHS heavy-metal restrictions, but no food-contact claim applies to this conversion unless separately certified.

    Geomembrane Flat Die Extrusion and ESCR-Dominated Formulation Checks

    HDPE FTA-001 can be considered for geomembrane sheet extrusion only after finished-sheet environmental stress crack resistance screening is conducted, because liner-grade HDPE requires high resistance to stress cracking under long-term wetting with surfactants. Flat die extrusion at sheet thickness 1.0–2.5 mm and die width up to 4,500 mm is carried out on single-screw extruders with 90–150 mm screw diameter and L/D 30–36. Melt temperature at the die entry is held between 220°C and 240°C to avoid unmelts and to keep head pressure below 250 bar. Chill roll temperatures are set at 60–90°C on a three-roll stack, because rapid quenching below 40°C reduces stress crack resistance and creates residual stress. Finished sheet is tested according to ASTM D1693-15 condition B with 10% Igepal CO-630 at 50°C; a failure time above 300 h is generally required for landfill lining specifications, although project-specific values may exceed 1,000 h. Tensile properties are measured by ISO 527-3:2018 or ASTM D638-14, with yield strength typically in the 22–28 MPa range for HDPE sheet of 0.950 g/cm³ density class. Puncture resistance is evaluated with ASTM D4833-07(2024); a finished 1.5 mm HDPE geomembrane commonly shows puncture resistance above 400 N, but the lot certificate for FTA-001 must be reviewed because additive packages differ between film and geomembrane grades. Oxidative induction time by ASTM D3895-14 at 200°C is a batch-release criterion for exposed geomembrane installations; values below 100 min suggest inadequate antioxidant loading for long-term UV exposure. Carbon black masterbatch is added at 2–3 wt% with particle size below 25 nm to achieve 2.0–2.5% carbon black content in the finished sheet, as required in many environmental lining specifications.

    Control PropertyTest StandardIndicative HDPE Geomembrane Window
    Melt flow rateISO 1133-1:20220.5–1.0 g/10 min at 190°C/2.16 kg
    DensityISO 1183-1:20190.948–0.956 g/cm³
    Environmental stress crack resistanceASTM D1693-15>300 h, condition B, F50
    Carbon black contentASTM D1603-122.0–2.5%
    Oxidative induction timeASTM D3895-14>100 min at 200°C

    When HDPE FTA-001 is coextruded as a stiffness core ply in multi-layer retail packaging, the converter must separate viscosity matching from sealant compatibility. In a five-layer line with die gap 0.8–1.2 mm, the core layer containing FTA-001 is run at 30–50% of total film thickness, while skin layers of metallocene linear low-density polyethylene or plastomer provide heat sealing below 110°C. The HDPE core raises bending stiffness and deadfold compared with all-LLDPE structures at equal thickness, but it also increases seal initiation temperature; therefore the sealant skin thickness is maintained above 7 µm per side. Layer ratio is controlled by gravimetric feeders with accuracy ±0.3% of setpoint, and the extruders are profiled from 190°C to 220°C for the HDPE core to maintain viscosity ratio against LLDPE skins at 0.8–1.2. Melt temperature at the feedblock is held at 220°C ± 5°C to avoid interfacial flow instabilities. Film gauge is typically 30–70 µm, with tensile modulus in the machine direction measured by ASTM D882-18 and tear propagation resistance by ASTM D1922-09(2015). The finished film is converted into stand-up pouches, side-gusset bags, and heavy-duty retail packaging. Silo storage above 60% relative humidity requires pre-drying at 80°C for 2 h before extrusion because surface moisture can create bubbles at the die lip. This structure is not suitable for retort or high-temperature sterilization above 110°C unless the entire structure is revalidated for seal strength and migration under EU 10/2011 or FDA 21 CFR 177.1520.

    If the Grade Is Drawn into Raffia Tape After Water-Bath Orientation

    HDPE FTA-001 may be evaluated for raffia tape extrusion only when the converter’s line uses a water-bath orientation unit that can maintain a stretch ratio of 6:1 to 8:1 without fibrillation. Tape lines with 65–90 mm extruder screw diameter and L/D 28–32 are operated at 220–250°C melt temperature, with a flat die gap of 0.8–1.2 mm and chill bath temperature of 30–45°C. The extruded film is slit into tapes of 2–4 mm width and drawn in a hot-air oven at 120–150°C; final tape denier is controlled between 800 and 1,200 denier. A masterbatch of UV stabilizer is added at 2–3 wt% to meet outdoor sack requirements. Tensile tenacity of drawn tape is measured by ISO 2060:2015 for linear density and ISO 13934-1:2013 for breaking strength; a well-oriented HDPE tape typically shows tenacity above 0.35 N/tex, but grade-specific validation is required. Woven fabric is produced on circular looms with 10–12 tapes per inch in warp and weft, and sacks are coated or laminated with linear low-density polyethylene at 15–25 g/m² if moisture barrier is required. The primary limitation of using a film-grade HDPE in raffia is lower melt strength than dedicated raffia grades; web sag between die and chill bath may require a lower melt temperature of 200°C and reduced drawdown. Published data for FTA-001 in this specific configuration is limited, so trial runs with fabric tensile testing by ISO 13934-1:2013 and tear testing by ASTM D2261-13 are required before commercial conversion.

    Parison Swell and Top Load Are Decisive in Non-Food Blow Molded Containers

    For extrusion blow molding of non-food rigid containers, HDPE FTA-001 raises specific considerations around parison swell and melt fracture when validated on shuttle blow molders with clamp force above 50 kN. The extruder is profiled from 180°C to 210°C, with die head temperature at 200–220°C and mold temperature at 15–30°C. Parison swell is measured as weight swell and diameter swell; a swing of more than ±3% in parison diameter produces wall-thickness variation outside acceptable top-load limits. Blow air pressure is set at 6–8 bar, and blow-up ratio is kept between 2:1 and 3:1. Containers of 250 mL to 2 L are tested for drop impact at -20°C after conditioning for 24 h, with pass criteria defined by the customer. Top load strength of finished bottles is measured by ASTM D2659-16 at 23°C; a 1 L container in HDPE of 0.950 g/cm³ density class often requires top load above 250 N, but grade-specific lot data must be confirmed. Stress crack resistance of the molded article is evaluated by ASTM D1693-15 condition A or B because non-food household chemical containers may contact surfactants. The grade should not be used for food-contact blow molded containers unless the converter verifies finished-article migration under FDA 21 CFR 177.1520 and EU 10/2011; antioxidant and catalyst residues must be below the applicable specific migration limits. Dimensional stability of the molded part is improved by allowing 24 h post-mold conditioning before top load and volume shrinkage testing. Published data for FTA-001 in extrusion blow molding is more limited than for blown film; therefore production-scale trials should include drop impact, ESCR, and top load measurements before fixed tooling is approved.

    Free Quote

    Competitive Sinopec Fujian HDPE FTA-001 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Fujian HDPE FTA-001 is a high-density polyethylene copolymer supplied in pellet form for blown film extrusion. The product code is assigned by Sinopec Fujian Refining & Chemical Company Limited and belongs to the high-molecular-weight HDPE film class, in which melt flow rate at 190 °C/2.16 kg is maintained below 0.10 g/10 min to preserve melt strength during bubble expansion. Independent published data for this exact product configuration are limited; therefore, the numerical bands in this technical profile are reference data for high-molecular-weight HDPE blown film extrusion resins tested under the stated methods and should be replaced by lot-specific values from the manufacturer’s certificate of analysis.

    Reference characterization matrix for HMW-HDPE blown film resins
    PropertyTest procedureReference band
    DensityISO 1183-10.948–0.952 g/cm³
    Melt flow rate, 190 °C/2.16 kgISO 1133-10.04–0.08 g/10 min
    DSC melting peak temperatureISO 11357-3132–138 °C
    Vicat softening temperature A50ISO 306122–128 °C
    Tensile yield stress, 50 mm/minISO 527-224–30 MPa
    Flexural modulus, 2 mm/minISO 178900–1200 MPa

    The above matrix is not a specification. Comonomer distribution, molecular weight broadening, and additive loading shift values within the HMW-HDPE family, so the supplier’s lot-specific certificate of analysis is the controlling document for density, melt flow rate, and thermal transitions.

    What Rheological Conditions Govern Bubble Stability in FTA-001 Extrusion?

    High-molecular-weight HDPE film extrusion requires a melt temperature at the die lip high enough to reduce viscoelastic defects but low enough to avoid thermal oxidation. On a grooved-feed single-screw extruder with an L/D ratio of 30:1 to 33:1 and a 100 mm to 160 mm spiral mandrel die, barrel set points from 170 °C to 210 °C are commonly used for this resin class. The die gap is typically set at 0.8 mm to 1.2 mm; larger die gaps reduce shear heating and melt fracture but increase the requirement for precise gauge control. Bubble stability derives from the strain-hardening behaviour of the high-molecular-weight chains, which resists neck-in and bubble sag under blown film draw. Throughput must be balanced against frost-line height: if the frost line is set below 2 die diameters, the bubble may quench too rapidly and generate blocking; if set above 6 die diameters, bubble oscillation can create gauge bands.

    Pellet conditioning before extrusion is governed by transport moisture and ambient humidity. HDPE is hydrophobic, but surface condensation from warehouse temperature swings can produce pinholes during extrusion; pre-drying at 70–80 °C for 2–4 h is applied only when storage humidity exceeds 60% RH. The grade should not be blended with calcium carbonate masterbatch above 15 wt% without adjusting bubble cooling because filler reduces melt strength and tear resistance. Regrind levels above 30% may require additional processing stabilizer, although the producer already incorporates an antioxidant package. For food-contact applications, converters should verify compliance with FDA 21 CFR 177.1520, EU Regulation No 10/2011 including overall migration limit 10 mg/dm², and applicable REACH SVHC declarations before use.

    Blown Film Mechanical Properties and Barrier Function

    Film converted from FTA-001-class HMW-HDPE is characterized by high tensile yield stress and high modulus, enabling down-gauging in merchandise bags, refuse sacks, and industrial liners. Tensile properties measured according to ISO 527-3 on 25 µm film typically give a yield stress of 22–28 MPa and a break strain above 500%; secant modulus can exceed 700 MPa in the machine direction. Water vapour transmission rate measured by ASTM F1249 at 38 °C/90% RH for 50 µm film is typically in the range 3–6 g/m²·day, positioning HDPE film as a moisture barrier but not an oxygen barrier. Puncture resistance measured by ASTM D5748 is lower than LLDPE at equal thickness, but the higher modulus of HDPE means that a thinner gauge can support the same load-bearing stiffness.

    The conversion window is strongly influenced by the high melt viscosity. Screw speeds on a 55 mm grooved-feed extruder processing this class are often limited by motor amperage rather than plastication capacity. Die pressure before the screen changer can reach 25–35 MPa, and screen packs should be specified for high differential pressure. Melt temperature overshoot at the die lip should be kept below 230 °C to avoid gel formation and oxidative odour. A dual-lip air ring operated at 300–600 m³/h and internal bubble cooling are commonly used to stabilize thin-gauge bubbles. Without internal bubble cooling, gauge variation at 10 µm may exceed ±8%.

    Differential Profile Against Commodity HDPE and LLDPE Film Resins

    This grade differs from lower-viscosity commodity HDPE film resins primarily in melt viscosity and bubble stability. A direct comparison with a conventional medium-molecular-weight HDPE film resin with melt flow rate near 0.2–0.5 g/10 min shows that the FTA-001 class requires higher extruder torque and lower screw speed for equivalent output. The higher melt strength permits a wider blow-up ratio range from 2:1 to 5:1 and supports lower gauge variation. Against butene-LLDPE film resins, the HDPE class provides higher modulus but lower extensional toughness; dart drop impact of HDPE film at 25 µm may be 100–160 g measured by ASTM D1709A, while LLDPE of the same thickness can exceed 300 g.

    Comparative reference bands at 25 µm film thickness
    Property / methodFTA-001 class HMW-HDPECommodity HDPEButene-LLDPE
    Dart drop impact ASTM D1709A100–160 g50–90 g300–600 g
    MD secant modulus ISO 527-3700–950 MPa650–850 MPa200–350 MPa
    TD Elmendorf tear ISO 6383-21.0–2.0 N0.5–1.0 N3.0–6.0 N
    WVTR, 50 µm, 38 °C/90% RH ASTM F12493–6 g/m²·day3–6 g/m²·day2–5 g/m²·day

    The difference in extensional toughness is offset by thickness reduction. Because stiffness scales with the cube of thickness, a 15 µm HMW-HDPE film can provide equivalent bending resistance to a thicker lower-modulus LLDPE film in many applications. Tear anisotropy is also affected by blow-up ratio; low blow-up ratios increase machine-direction orientation and lower transverse tear strength.

    When the Grade Is Used for Downgauged High-Stiffness Film

    Processors using FTA-001-class resin for downgauged high-stiffness film should limit melt temperature overshoot because high viscosity increases shear heating in the die. An adapter set point of 200 °C can produce a die-lip melt temperature 5–10 °C higher, so thermocouple placement and melt-temperature profiling are necessary. With a dual-lip air ring and internal bubble cooling, bubble diameter at 10 µm can be stabilized within ±5% gauge variation if the frost line is held at 2–3 die diameters. Film blocking is controlled with slip and antiblock masterbatch at 0.5–2.0 wt%, although the exact dosage depends on final gauge, winding tension, and storage temperature. Converters should verify that the masterbatch carrier is compatible with high-molecular-weight HDPE and does not reduce bubble stability through viscosity dilution.