Sinopec Fujian Hdpe Fl8920

Sinopec Fujian HDPE FL8920

    • Product Name: Sinopec Fujian HDPE FL8920
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 456704
    Density 0.949 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.08 g/10 min
    Tensile Strength At Yield 25 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 600 %
    Flexural Modulus 1100 MPa
    Vicat Softening Temperature 124 °C
    Brittleness Temperature ≤ -70 °C
    Environmental Stress Cracking Resistance > 1000 h
    Shore D Hardness 62
    Melting Point 131 °C
    Crystallinity 75 %
    Water Absorption < 0.01 %
    Dielectric Constant 2.3
    Volume Resistivity > 10^16 Ω·cm
    Film Haze 12 %
    Film Gloss 50 %
    Dart Impact Strength 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g

    As an accredited Sinopec Fujian HDPE FL8920 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Fujian HDPE FL8920 is packaged in 25 kg polyethylene-lined woven bags, stacked on pallets for secure shipping.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Sinopec Fujian HDPE FL8920 in 25 kg bags, palletized, shrink-wrapped, evenly distributed and securely lashed for ocean transport.
    Shipping Sinopec Fujian HDPE FL8920 is a non-hazardous high-density polyethylene resin. Ship as general cargo in 25 kg bags on shrink-wrapped pallets. No UN number or hazard class required. Keep dry, clean, and away from direct sunlight/heat. Store cool and ventilated. Avoid bag damage during handling.
    Storage Store Sinopec Fujian HDPE FL8920 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags sealed and palletized; protect from moisture, dust, UV exposure, and contamination. Avoid excessive stacking to prevent deformation. Rotate stock and use within recommended shelf life. Keep away from incompatible materials and ensure good ventilation.
    Shelf Life Sinopec Fujian HDPE FL8920 shelf life: typically 12 months in original, unopened packaging, stored dry, cool, ventilated, away from direct sunlight.
    Application of Sinopec Fujian HDPE FL8920

    What Limits Sheet Flatness in HDPE Geomembrane Extrusion?

    For flat-die geomembrane production, Sinopec Fujian HDPE FL8920 targets 1.0–2.5 mm smooth or textured sheet for landfill caps, heap-leach pads, and agricultural water reservoirs. The sector compliance framework is defined by GRI-GM13 and GB/T 17643; lot-release testing includes density per ASTM D1505-18, melt mass-flow rate per ISO 1133-1:2022 at 190°C/2.16 kg, tensile yield and break per ASTM D638-14, environmental stress cracking in 10% Igepal CO-630 per ASTM D1693-15e1, and oxidative induction time per ASTM D3895-19. A typical letdown ratio is 96.5–97.8 wt% FL8920, 2.0–2.5 wt% carbon black supplied as a 40% carbon black HDPE masterbatch, and 0.15–0.30 wt% phenolic/phosphite stabilizer masterbatch; actual carbon black dispersion is inspected to ISO 18553:2002 or ASTM D5596. Extrusion on production lines with single-screw extruders of L/D ≥ 30 and Maddock mixing sections uses feed-zone temperatures of 170–190°C, metering-zone temperatures of 190–215°C, and die temperatures of 210–225°C; melt temperature is maintained at 214–228°C. Thickness uniformity is controlled with gravimetric mass-flow closed-loop feed and actuator-driven die bolts; line speeds for 2.0 mm sheet typically range from 0.8–2.5 m/min. Terminal product types are landfill basal liner, slope liner, heap-leach pad liner, canal liner, stormwater containment liner, and fish farm liner. A process conflict occurs when melt-index drift exceeds 0.25 g/10 min: flat-die sheet sag increases and edge-bead correction becomes continuous, while high backpressure shear can raise gel counts in the finished sheet. Published data for FL8920-specific output rates is limited, but comparable bimodal HDPE film grades in the 0.20–0.35 g/10 min band are processed in the same window.

    Compliance parameterTest designationExpected lot-release band for HDPE geomembrane-grade resins
    DensityASTM D1505-180.948–0.956 g/cm³
    Melt mass-flow rateISO 1133-1:20220.18–0.25 g/10 min at 190°C/2.16 kg
    Tensile yield stressASTM D638-1422–28 MPa
    Elongation at breakASTM D638-14>600%
    ESCR F50ASTM D1693-15e1>500 h in 10% Igepal at 50°C
    Carbon black contentASTM D16032.0–2.5 wt%
    Oxidative induction timeASTM D3895-19≥100 min at 200°C
    Carbon black dispersionISO 18553:2002≤ 3 category

    Lot-specific values in the certificate of analysis for Sinopec Fujian HDPE FL8920 govern final acceptance; the table lists expected lot-release bands for high-molecular-weight HDPE film grades in this sector, not a substitute for the producer’s certificate.

    For thin high-stiffness carrier bag film, FL8920 is blended at 88–95 wt% with 5–12 wt% LLDPE to improve tear initiation at the handle cut-out, while pigment masterbatch is added at 2–5 wt% and slip/antiblock masterbatch at 0.4–1.0 wt%. Food-contact produce bags follow FDA 21 CFR 177.1520(c), EU 10/2011, and GB 9685-2016; mechanical testing uses ASTM D882-18 for tensile, ASTM D1709-16a for dart drop, ASTM D1922-15 for tear, and ASTM D1894-14 for blocking. Production occurs on single-layer high-stalk blown-film lines with die diameters 80–200 mm, die gaps 0.9–1.6 mm, melt temperatures 190–215°C, and blow-up ratios 3.5–5.0; the high-stalk bubble is extended to 5–8 times die diameter to develop machine-direction strength and downgauging capability. Final film thickness ranges 10–30 µm, and output per die circumference typically reaches 0.8–1.5 kg/(h·mm) depending on cooling air and stabilization cage design. Terminal products are T-shirt carrier sacks, produce roll bags, bakery bags, and point-of-sale handle bags. A processing constraint in high-stalk production is that excessive frost-line height beyond 8 die diameters can draw the film too far into the crystalline phase before orientation is released, producing intermittent bubble oscillation; operators correct this by adjusting cooling air velocity and cage height.

    Dart Integrity and Seal Initiation in Heavy-Duty Industrial Sack Film

    The production of heavy-duty industrial sack film from FL8920 requires 80–90 wt% FL8920, 10–20 wt% LLDPE or plastomer, 2–4 wt% white or neutral color masterbatch, 0.5–1.0 wt% slip/antiblock masterbatch, and 0.02–0.08 wt% fluoropolymer processing aid when die-lip build-up appears. Dart drop resistance is tested per ASTM D1709-16a method A or B, seal strength per ASTM F88/F88M-21, tear propagation per ASTM D1938-19, and film blocking per ASTM D1894-14; industrial packaging compliance follows ISO 21898:2019 for flexible intermediate bulk containers and UN 6.1.3 dangerous-goods packaging clauses when used as an inner liner. Three-layer coextrusion blown-film lines with extruder diameters of 55–75 mm, L/D 28–32, and die diameters of 200–400 mm run outer layers rich in FL8920, a core layer containing up to 35 wt% reprocessed edge trim, and a seal layer with 15–20 wt% lower-density material for hot-tack performance. Melt temperatures are held at 200–220°C, blow-up ratio at 3.0–4.2, and film thickness at 80–180 µm. Terminal products are heavy-duty sacks, FIBC inner liners, cement bag liners, fertilizer bag liners, and valve sacks. If melt temperatures exceed 230°C for more than 180 s during purging or shutdown, bimodal HDPE forms gel particles that appear as specks in thin sack walls; transition purging with an LLDPE grade is used to reduce thermal history.

    In under-slab and wall moisture-control assemblies, HDPE-based vapor control layers are specified where low water-vapor transmission, high tensile strength, and nail-sealability around penetrations are required. For this use, FL8920 is compounded at 87–93 wt% with 7–13 wt% LLDPE or polyethylene elastomer to improve low-temperature puncture resistance, plus 1.0–2.5 wt% carbon black masterbatch for UV exposure beyond 60 days and 0.3–0.8 wt% processing stabilizer masterbatch. Compliance is evaluated under EN 13984:2013 for flexible sheets for waterproofing-vapor control layers, EN 13859-1:2014 for underlays and vapour control layers in walls, ASTM E96/E96M-22 for water vapor transmission, ASTM D882-18 for thin-sheet tensile, and ASTM D1709-16a for impact. Production is carried out on cast film lines or three-layer blown-film lines; cast film runs at 240–270°C melt temperature for higher output but can increase odor in confined indoor use, therefore blown film at 205–215°C is preferred for low-emission building certification projects. When blown film is selected, the die gap is 1.8–2.5 mm, BUR 2.5–3.5, and final film thickness 150–500 µm. Water vapor transmission depends on thickness and barrier design; for 200 µm film, published data for equivalent HDPE films ranges from 1.0–2.5 g/(m²·day) under 38°C/90% RH cup conditions. Terminal product types include under-slab vapor barrier, wall vapor retarder, crawl-space liner, and temporary construction enclosure film. A limitation is that FL8920-based films cannot be used where direct contact with bituminous waterproofing membranes occurs, because plasticizer and oil migration from bitumen may accelerate stress cracking; in those configurations a polyester or glass-fiber carrier is interposed.

    When HDPE Film Replaces LDPE in Dry-Food Liner Structures

    Dry-food liner replacement of LDPE with HDPE FL8920 is evaluated in cereal box liners, cracker pouches, dry-mix pouches, and frozen vegetable bags where downgauging and stiffness are required. The blend ratio is set at 90–96 wt% FL8920 with 4–10 wt% LLDPE for seal reliability, 0.3–0.8 wt% silica-based antiblock masterbatch, 0.2–0.6 wt% erucamide slip masterbatch, and 0.02–0.05 wt% fluoropolymer processing aid. Compliance is governed by FDA 21 CFR 177.1520(c) 3.2a for olefin polymers, EU 10/2011 with overall migration limits below 10 mg/dm², and GB 9685-2016 for additives; sensory checks are carried out per ASTM E460-20 or internal panel protocols. Production is performed on single or three-layer blown-film lines with die diameters 100–250 mm, die gaps 0.8–1.5 mm, melt temperatures 190–215°C, and BUR 2.0–3.0. Because HDPE has a higher crystallization rate than LDPE, bubble stability in the low-stalk pocket requires the frost-line height to be kept at 3–5 die diameters; if the frost line rises beyond this, film haze increases above 20% and heat-seal initiation rises by 5–10°C. Terminal products include box liners for breakfast cereal, dry-mix pouches, cookie and cracker bags, frozen vegetable films, and secondary liners for paper bags. A limitation in direct substitution is that HDPE has lower heat-seal strength than LDPE at temperatures below 120°C; converters compensating with higher seal-bar settings must monitor for burn-through at 130–150°C on high-speed vertical form-fill-seal equipment running 60–90 bags/min.

    When liquid household and agricultural chemical packaging requires ESCR-resistant structural film, FL8920 is formulated at 72–82 wt% as the middle and outer structural layers, with 10–18 wt% LLDPE or metallocene polyethylene in skin layers for strong seal seams, 0.3–0.8 wt% slip/antiblock, and 0.2–0.5 wt% processing stabilizer. If high-pH agricultural formulations are packed, the outer layer may include 1.0–2.0 wt% UV stabilizer masterbatch. Compliance for dangerous-goods flexible packagings is evaluated under UN 6.1.3 and ADR/RID/IMDG packaging instructions; stress cracking resistance is tested by ASTM D1693-15e1 in 10% Igepal CO-630 at 50°C, seal strength per ASTM F88/F88M-21, and filled drop resistance per ISTA 3A or ASTM D5276-19. Production is carried out on high-barrier coextrusion lines with 3–5 layers; the HDPE layers are extruded at 200–220°C, while tie and barrier layers are matched to the materials selected. BUR is set at 2.0–3.5, die gaps 1.5–2.2 mm, and final thickness 120–200 µm. Terminal products are inner liners for liquid detergent cartons, agrochemical pouch film, spouted pouches for refill packs, and flexible packagings for oil-based additives. The critical processing boundary is the restriction on EVOH or PA barrier layers that require extrusion above 230°C; FL8920 should not be run at these temperatures for extended periods because of film gel formation. Published data for FL8920 in tandem with EVOH at high output is limited, and trials are required to define the exact temperature trade-off between barrier adhesion and gel dispersion.

    Free Quote

    Competitive Sinopec Fujian HDPE FL8920 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Fujian HDPE FL8920 is a high-density polyethylene film resin supplied by Fujian Refining & Petrochemical Co., Ltd. for blown film conversion. The grade is specified with a density of 0.954–0.958 g/cm³ according to ISO 1183-1:2019 and a melt mass-flow rate of 0.75–0.85 g/10 min under 190 °C/2.16 kg according to ISO 1133-1:2022. It is classified as a high-molecular-weight, medium-broad molecular weight distribution resin with a peak melting temperature of approximately 132–135 °C when measured by differential scanning calorimetry under ISO 11357-3:2018. The product is supplied as free-flowing pellets with a bulk density generally in the range of 0.55–0.60 g/cm³. Typical conversion targets include lightweight carrier bags, thin-gauge industrial liners, hygiene overwrap, and laminated film base webs. The grade is positioned for stiffness-driven films where down-gauging and controlled melt strength are more important than elastomeric puncture behaviour.

    What Limits Melt Strength and Bubble Stability in FL8920 Blown Film?

    Blown film behaviour is governed by extensional viscosity near the die and the resin’s ability to resist bubble deformation under cooling air. At melt temperatures of 195–215 °C, FL8920 exhibits pronounced shear thinning. Capillary rheometry under ISO 11443:2021 typically places apparent viscosity at 900–1300 Pa·s at 100 s⁻¹, which supports bubble stability at blow-up ratios from 1.8:1 to 3.5:1. A robust processing window requires frost-line height to be held between 600–900 mm on a 200 mm circular die with a die gap of 1.2–1.8 mm. Bubble instability is observed when melt pressure exceeds approximately 40 MPa at the breaker plate or when the web is drawn below 10 µm without corrective neck-height adjustment. FL8920 does not rely on deliberate long-chain branching for melt strength; its bubble integrity is derived from high molecular weight and polydispersity. Compared with heavily strain-hardening resins, the grade may show earlier bubble flutter when the frost line is too high or when draw-down ratios are excessive. Where an existing line differs from the above configuration, published data for that specific configuration is limited, and start-up evaluations should establish the stable operating envelope.

    Molecular architecture in this density class controls die swell, back-pressure, and melt fracture limits. The low melt mass-flow rate and measurable die swell relative to injection-grade HDPE indicate a high weight-average molecular weight and a polydispersity index above 4, although a full GPC trace is not always published in the certificate of analysis. The resin should be processed after storage at or below 50 °C and 60% RH to avoid surface moisture pickup. If ambient relative humidity exceeds 60%, hopper drying at 80 °C for 4 h in a hot-air or desiccant dryer is recommended to prevent bubble defects caused by steam formation. Sieve-pack design should account for the resin’s viscosity; 80/100/80 mesh screen combinations are common on production lines running film grades in this melt-flow class.

    Density, Comonomer Length, and the Flexural Modulus Differential

    At 0.954–0.958 g/cm³ density, the flexural modulus of FL8920 typically falls between 950–1150 MPa under ISO 178:2019. This is significantly higher than a linear low-density polyethylene film resin at 0.918 g/cm³, which usually exhibits a flexural modulus of 250–450 MPa. The higher modulus allows converters to reduce film gauge while retaining secant stiffness in the converted article. Short-chain branching introduced by butene-1 comonomer reduces crystalline fraction relative to a homopolymer HDPE of equivalent density. In comparison with hexene-1 or octene-1 copolymer film grades, the butene-based structure typically produces a lower tie-chain fraction in the amorphous region. That structural difference reduces dart impact strength at equivalent melt index and density. The practical consequence is that FL8920 competes in applications where stiffness, tensile yield stress, and gauge consistency dominate over extreme puncture or slow crack resistance. The tensile yield stress of the film under ISO 527-3:2018 is generally 25–30 MPa in the machine direction and 23–28 MPa in the transverse direction. Elongation at break is typically 500–700%, although actual values vary with film gauge, frost-line height, and draw ratio.

    Typical property profile of Sinopec Fujian HDPE FL8920
    PropertyTest methodTypical range
    Density at 23 °CISO 1183-1:20190.954–0.958 g/cm³
    Melt mass-flow rateISO 1133-1:2022, 190 °C/2.16 kg0.75–0.85 g/10 min
    Tensile yield stress, MDISO 527-3:201825–30 MPa
    Tensile yield stress, TDISO 527-3:201823–28 MPa
    Elongation at break, MD/TDISO 527-3:2018500–700%
    Dart impact resistance, F50, 38 mm dart, 25 µmISO 7765-1:2017110–150 g
    Elmendorf tear resistance, MD/TDISO 6383-2:20198–14 N/mm MD / 10–16 N/mm TD
    Flexural modulusISO 178:2019950–1150 MPa
    Vicat softening temperature, A50ISO 306:2022123–127 °C

    If Higher Dart Impact Is Required, Compare Against Hexene-Copolymer Film Grades

    FL8920 is positioned for applications in which stiffness and down-gauging potential are the deciding factors. Where a converter requires dart impact values above 150 g at 25 µm, a hexene- or octene-copolymer HDPE film grade of similar density may be more suitable. Under ASTM D1709-15, FL8920 generally exhibits a lower F50 impact value than high-performance octene-modified film resins because shorter butene branches are less effective in generating tie molecules. The lower tie-chain fraction also influences environmental stress-cracking resistance. For films exposed to wetting agents, detergents, or polar chemical formulations, ESCR should be evaluated according to ASTM D1693-15, condition B, in 10% Igepal CO-630 at 50 °C. The base resin is expected to withstand dry packaging and limited wet-contact service, but published data for chemical-containing formulations is limited and must be validated on the specific film structure. By contrast, a hexene-copolymer film resin may show higher ESCR at equivalent density and melt index because the longer comonomer promotes more effective tie-chain connectivity.

    On production-scale equipment, FL8920 has been processed on a 55 mm grooved-feed extruder with an L/D ratio of 30:1, a 200 mm die, and a dual-lip air ring. Barrel settings from 180 °C to 210 °C and die settings from 200 °C to 220 °C produce stable bubble formation. Output rates of 90–120 kg/h are attainable without melt fracture when the die gap is maintained between 1.2–1.8 mm. Converted films in the 8–50 µm range are used in carrier bags, trash liners, and laminate base webs. The stiffness permits gauge reduction of 10–15% compared with LLDPE carrier film at equivalent secant modulus, provided downstream sealing and tear requirements are also satisfied. In film conversion, the grade shows characteristic high-density polyethylene seal initiation behaviour; heat-seal temperature is typically higher than for LLDPE, so sealing schedules under ASTM F2029 or equivalent should be adjusted accordingly.

    Die Pressure and Frost-Line Control Govern the Stable Operating Window

    Grooved-feed extruders are preferred for this melt-flow class because high-molecular-weight HDPE with melt mass-flow rate below 1 g/10 min can slip unpredictably on smooth-bore barrel walls. The grooved feed section should extend over 3–5 D of barrel length to suppress feed-zone slip and to build pressure consistently. A pressure profile of 350–450 bar at the breaker plate is typical for stable output. Die size selection is matched to layflat and blow-up ratio: for a 600 mm layflat, a 200 mm die and blow-up ratio of 1.9:1 are commonly used. Neck height should be held at 6–8 times die diameter to avoid excessive molecular orientation before the frost line. Air-ring cooling should maintain a frost-line height of 600–900 mm. If the frost line is allowed to rise above that range, bubble flutter and film thickness variation increase. If it is forced too low, freezeline quenching can reduce transverse direction tear resistance and increase film curl. These process boundaries are not unique to FL8920, but they are particularly relevant because of its high melt viscosity and density-driven crystallization rate.

    Regulatory verification checklist for Sinopec Fujian HDPE FL8920
    Standard or regulationMethod or criterionStatus expected in supplier documentation
    EU Regulation (EU) No 10/2011Overall migration by EN 1186-1:2002Compliance declared for final food-contact articles; converter verification required
    FDA 21 CFR 177.1520Olefin polymer requirements under 177.1520(c)Compliance subject to additive restrictions and end-use condition
    China GB 4806.6-2016Food-contact plastic resin and article requirementsSupplier declaration provided; migration limits apply after conversion
    REACH Annex XVII / SVHCSVHC content below 0.1% w/w as of production dateCompliance declared by manufacturer
    RoHS 2011/65/EUPb, Cd, Hg, Cr(VI), PBB, PBDE content limitsCompliant for plastic components in electrical and electronic equipment

    Storage above 30 °C or prolonged exposure to ultraviolet light can increase surface oxidation and gel-particle formation during subsequent extrusion. The resin should be stored in closed silos or sealed bulk bags and kept away from direct sunlight. In high-humidity environments above 60% RH, surface water can generate bubble instability and film defects; pre-drying at 80 °C for 4 h is recommended before processing. FL8920 should not be blended with polypropylene or EVOH without a compatibilizer because phase separation and interfacial instability can reduce film properties. Additive packages containing unsaturated amides or strong oxidizers should be screened for melt-processing compatibility. Published data for antimicrobial masterbatch interactions with this specific grade is limited, and any such formulation should be evaluated by capillary rheometry and film property testing before full-scale production.

    Top