Sinopec Fujian Hdpe Dmda8920

Sinopec Fujian HDPE DMDA8920

    • Product Name: Sinopec Fujian HDPE DMDA8920
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 515199
    Grade DMDA8920
    Polymer Type High Density Polyethylene (HDPE)
    Form Pellets
    Color Natural
    Density 0.954 g/cm³
    Melt Flow Rate 20 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 25.5 MPa
    Elongation At Break 1000%
    Flexural Modulus 1030 MPa
    Vicat Softening Temperature 124°C
    Heat Deflection Temperature 65°C at 0.45 MPa
    Notched Izod Impact Strength 26 J/m at 23°C
    Shore Hardness D 66
    Melting Point 134°C
    Water Absorption <0.01%
    Molecular Weight Distribution Narrow

    As an accredited Sinopec Fujian HDPE DMDA8920 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polypropylene woven bags, stacked on pallets; each pallet holds 1000 kg of Sinopec Fujian HDPE DMDA8920.
    Container Loading (20′ FCL) Sinopec Fujian HDPE DMDA8920 is loaded in 20′ FCL containers, typically 25 MT bagged, palletized, securely strapped for export shipment.
    Shipping Sinopec Fujian HDPE DMDA8920 is shipped as a non-hazardous solid resin in 25 kg woven bags or 1000 kg jumbo bags. Typically palletized and wrapped for sea freight. A 20' FCL holds about 17–20 MT. Keep dry, away from heat; no special UN hazmat class required.
    Storage Store Sinopec Fujian HDPE DMDA8920 in original, tightly sealed bags in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, rain, moisture, heat, and ignition sources. Keep away from strong oxidizers. Stack on pallets; avoid sharp objects, excessive pressure, and contamination. Use first-in, first-out. Recommended storage below 40°C with low humidity. Do not expose to open flames or UV radiation.
    Shelf Life Sinopec Fujian HDPE DMDA8920 typically has a 24-month shelf life under cool, dry, ventilated storage, away from sunlight and moisture.
    Application of Sinopec Fujian HDPE DMDA8920

    Injection Molded Logistics Crates and Pallets—Flow-Length Limits, Regrind Tolerance, and Stacking Load Retention

    HDPE DMDA8920 is positioned for high-speed injection moulding of logistics crates, tote boxes, and pallets because narrow molecular weight distribution allows rapid filling of long flow paths without generating excessive cavity pressure. Commercial processing on hydraulic and hybrid clamp systems with clamp force from 3,000 kN to 16,000 kN has demonstrated that this grade family processes within melt temperatures of 210 °C to 245 °C as measured by ISO 11357-3:2018 and mould temperatures of 20 °C to 40 °C. The resin should enter the hopper with moisture content below 0.02 % by weight according to ISO 15512:2019; if warehouse relative humidity exceeds 60 %, pre-drying in a desiccant hopper at 80 °C for 2 h prevents surface splay and dished gate defects. Screw geometry with 25:1 L/D and compression ratio of 2.5:1 to 3.0:1 is specified in plant setup sheets to avoid unmelt at high screw speeds, especially when colour masterbatch is metered at the feed throat. Injection speed should be profiled so that melt front velocity remains between 100 mm/s and 180 mm/s in ribs and bosses; excessive shear at the gate can reduce notched impact strength by orienting the shell layer and create brittle failure at drop-test temperatures below 0 °C.

    Formulation allowances for industrial crates depart from food-contact constraints. Post-industrial regrind generated from the same production line is generally limited to 30 wt% in non-food crates; the regrind fraction must have particle size 3 mm to 6 mm and a melt flow rate after reprocessing within ±12 % of virgin resin when tested under ISO 1133-1:2022. Colour masterbatch in a HDPE carrier is metered at 1 wt% to 3 wt%; black or dark grey formulations use carbon black masterbatch, which also acts as a UV screen. For outdoor pallets exposed to sustained sunlight, a hindered amine light stabilizer masterbatch at 0.5 wt% to 1.0 wt% is added. For anti-static tote boxes used in electronic component handling, carbon black or conductive masterbatch is added only after surface resistivity targets under IEC 61340-5-1 are confirmed; typical target is 106 Ω to 109 Ω. Stacking load retention is evaluated under ISO 8611-2:2021, and creep modulus may be verified under ISO 899-2:2003. End products include ventilated fruit crates, smooth-wall logistics totes, collapsible pallet sleeves, and reusable meat lugs. The choice of DMDA8920 in these products is constrained by low-temperature impact; at -20 °C HDPE loses significant ductility, so drop testing under ISO 6603-2:2023 is required before the crate enters freezer logistics. Production-scale trials with high-flow HDPE injection moulding grades indicate that increasing regrind content above 30 wt% raises injection pressure variability and increases warpage due to molecular weight reduction.

    Unlike industrial crates, closure moulding on high-cavitation tooling imposes dimensional tolerances that are dominated by gate freeze time and demoulding temperature. DMDA8920 can be evaluated for non-carbonated beverage caps, dairy caps, agrochemical caps, and overcaps only when the application does not require the higher flexural modulus of polypropylene. Process settings normally begin with melt temperature of 200 °C to 230 °C and mould temperature of 15 °C to 30 °C. High-pressure injection using accumulator-assisted machines with 32- to 96-cavity hot runner systems requires fill times of 0.5 s to 1.2 s. Hold pressure is set between 35 MPa and 55 MPa until gate freeze; a short hold will cause sink on the outer surface, while excessive hold causes overpacking of the gate area and increases release torque. The tamper-evident band is particularly sensitive to mould release agents; external lubricants should be excluded because they migrate and disrupt cap colour adhesion or print adhesion. Food-contact compliance is anchored to Regulation (EC) No 1935/2004 and Commission Regulation (EU) No 10/2011; overall migration below 10 mg/dm² must be confirmed under the assigned simulant. United States compliance for HDPE homopolymer closures is addressed under FDA 21 CFR 177.1520(c). Slip agent masterbatch is limited to 0.8 wt% to 2.0 wt% in PE carrier, and colour masterbatch to 0.5 wt% to 1.5 wt%. Total non-HDPE additive package should remain below 5 wt% to maintain HDPE recycling streams according to APR HDPE Critical Guidance for closures. Component examples include 38 mm dairy closures with tamper-evident bands, push-pull dispensing closures for sauces, and snap-on caps for personal care containers.

    What Migration Limits Apply When Thin-Wall Dairy Tubs Are Injection Molded from HDPE?

    Thin-wall HDPE containers in the 0.8 mm to 1.5 mm wall thickness range are produced on high-speed injection moulding cells with clamp force between 1,500 kN and 4,000 kN and accumulator-assisted injection. DMDA8920 can be considered for dairy tubs, margarine packs, and deli containers when the melt is held at 235 °C to 250 °C and the mould is maintained at 10 °C to 25 °C. Mould cooling lines are frequently arranged in independent circuits for core and cavity to maintain thermal balance in tools with 16 to 48 cavities. Injection velocity at the screw is set at 200 mm/s to 300 mm/s, producing a melt front velocity that allows flow length-to-wall thickness ratios above 150:1 without short shots. Back pressure is held at 0.8 MPa to 1.5 MPa to ensure colour dispersion without generating excessive shear heat. Gate geometry is critical; if a hot edge gate or valve gate is used, it must be sized at 70 % to 80 % of wall thickness to avoid jetting and visible flow marks.

    Food contact compliance for thin-wall HDPE packaging is determined by the final article, not by the resin certificate alone. The converter must verify that the additive package and processing aids do not increase overall migration. The following matrix summarises the core compliance load for monolayer dairy tubs and similar containers.

    JurisdictionStandard or RegulationRelevant RequirementApplication Verification for DMDA8920
    European UnionCommission Regulation (EU) No 10/2011 Annex IOverall migration ≤ 10 mg/dm²; specific migration of any listed additive must not exceed its SMLMigration testing under simulant D1 at 40 °C for 10 d for refrigerated dairy; final article thickness 0.8 mm to 1.5 mm
    United StatesFDA 21 CFR 177.1520(c)HDPE homopolymer with density ≥ 0.94 g/cm³; extractables within 177.1520 limitsExtraction test with n-hexane and xylene as specified; resin must not contain recycled content unless fully compliant and supported by supplier LNO
    ChinaGB 4806.7-2016Overall migration ≤ 10 mg/dm²; potassium permanganate consumption ≤ 10 mg/kg; heavy metal limits under GB 4806.1-2016Tests conducted on the finished container under expected use conditions

    Formulation for thin-wall food containers avoids fillers because the wall section is too thin to tolerate stiffness reduction and because filler can increase density variability. Titanium dioxide masterbatch in PE carrier is metered at 3 wt% to 5 wt% for white dairy tubs; process aid masterbatch, if used, is limited to 0.05 wt% to 0.10 wt%. End products include cups for yogurt, sour cream, single-serve spreads, and deli pots. A known operational boundary is that monolayer HDPE containers are not appropriate for oxygen-sensitive foods because oxygen transmission through polyolefin walls is substantially higher than through EVOH or aluminium barrier structures. Published data for the oxygen transmission rate of this specific DMDA8920 configuration is limited; converter-side barrier testing is required when modified atmosphere packaging is involved.

    In the 5 L to 25 L range, open-head pails and containers for paints, lubricants, industrial chemicals, and food ingredients are injection moulded from HDPE because the material combines sufficient environmental stress crack resistance with low moisture uptake. DMDA8920 can be used for single-material pails where the wall thickness is maintained between 2.5 mm and 4.0 mm; thicker sections are avoided because cycle time increases and sink marks become difficult to control. The melt temperature is usually set between 210 °C and 240 °C, the mould temperature between 15 °C and 30 °C, and the hold pressure between 50 MPa and 70 MPa. Sequential valve gating on a hot runner system provides balanced filling of the rim and base; if the pail is to receive a metal handle, the rim should be stiffened by a circumferential rib to prevent distortion during handle insertion.

    For dangerous goods pails, the package must be type-tested under UN Model Regulations Chapter 6.1. A design type for Packing Group II liquids with specific gravity up to 1.2 is drop-tested from 1.2 m at -18 °C; stacking load is applied for 28 d at 40 °C; internal hydraulic pressure testing is required for liquids. The moulded pail must be conditioned according to the test laboratory’s requirements, and no release agent may be applied to the sealing rim because it compromises closure seal. Formulation uses only single-material HDPE with colour masterbatch at 1 wt% to 2 wt%; if outdoor storage is specified, a HALS package at 0.3 wt% to 0.5 wt% is included. Terminal products include open-head pails for water-based coatings, greases, inks, and low-risk food ingredients such as honey or syrups; for direct food contact, migration testing under EU 10/2011 is still required even if the resin itself is food-grade.

    When UV-Stabilised Garden Furniture Components Are Moulded from Unfilled HDPE

    For garden chairs, table slats, and storage benches, the critical failure modes are not melt flow but long-term colour shift and loss of impact after weathering. If DMDA8920 is selected for these thick-section components, the moulding process is configured for wall thicknesses of 5 mm to 8 mm; melt temperature is set at 220 °C to 250 °C, mould temperature at 15 °C to 35 °C, and hold pressure at 45 MPa to 65 MPa. Gate size should be at least 80 % of the nominal wall thickness to avoid early freeze-off and sink formation. Screw back pressure of 1.0 MPa to 1.5 MPa ensures uniform dispersion of light stabilizers without excessive melt residence time. Because thick sections retain heat, cycle time is generally 60 s to 90 s; cooling water temperature is selected to produce a uniform surface finish and reduce differential shrinkage between the core and skin.

    Weathering compliance is evaluated under ISO 4892-2:2021 Method A, using xenon-arc exposure with daylight filters at 0.35 W/m² at 340 nm; retained tensile strength or retained flexural modulus is checked after defined exposure intervals. Colour change is measured under ISO 7724-2. The formulation uses a PE-based HALS masterbatch at 0.5 wt% to 1.5 wt% and a pigment masterbatch at 2 wt% to 4 wt%; opaque carbon black or dark colours generally perform better than bright colours because carbon black acts as a UV screener. UV absorbers alone are insufficient in thick HDPE sections; HALS is required to suppress crack formation. Calcium carbonate filler is excluded because it lowers notched Izod impact at low temperature. End products include slatted tables, folding chairs, and garden storage benches. A production-scale limitation is the tendency of HDPE to show stress whitening at sharp corners; corners must have a radius of at least 2 mm to prevent failure during assembly and exposure to fluctuating outdoor temperatures.

    Because cable spools must resist flange creep under wound filament load, the polymer selected for injection moulding is often a high-flow HDPE with a narrow molecular weight distribution. DMDA8920 can be moulded into spools with flange wall thickness from 4 mm to 10 mm; melt temperature is kept at 220 °C to 240 °C, mould temperature at 20 °C to 35 °C, and holding pressure at 60 MPa to 80 MPa. The injection sequence should use a central sprue with a direct gate to maintain symmetry of molecular orientation; asymmetric filling can produce out-of-round flanges. Cooling time ranges from 45 s to 60 s and must be confirmed by dimensional stability measurements after demoulding. Because spool flanges are thick, the risk of voids is controlled by holding pressure and by avoiding excessive melt temperature.

    Compliance for cable spools is less about food contact and more about mechanical integrity and possible RoHS obligations. If the spool is supplied to electronics manufacturers, compliance with Directive 2011/65/EU Annex II is verified for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE at thresholds of 0.1 % by weight in homogeneous material, with cadmium at 0.01 %. A tensile creep test under ISO 899-2:2003 can be specified at 23 °C and 6 MPa for 1,000 h to evaluate flange deformation under load. Formulation for spools uses 100 % virgin DMDA8920 in dimensionally critical products; up to 20 wt% post-industrial regrind may be used for non-critical flange areas if the granule size is below 5 mm and the melt flow rate remains within ±10 %. Antistatic masterbatch at 1 wt% to 2 wt% is added only when the spool is used for fibre optic or electronic wire handling; terminal products include injection moulded reels for copper wire, fibre optic cable, and welding wire. The material is not recommended for spools exposed to temperatures above 80 °C in service because creep modulus drops sharply near the HDPE deflection temperature and flange deformation becomes difficult to control under continuous load.

    Free Quote

    Competitive Sinopec Fujian HDPE DMDA8920 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Fujian HDPE DMDA8920 is a high-density polyethylene blow molding grade supplied by Sinopec Fujian Refining & Petrochemical Co., Ltd. The commercial designation DMDA8920 is also listed as DMDA-8920 in some producer technical service documents. The resin is positioned for rigid hollow packaging produced on extrusion blow molding lines where melt strength, environmental stress crack resistance, and pinch-off weld integrity are the controlling variables. Typical data sheet values include a nominal density of 0.952 g/cm³ determined in accordance with ISO 1183-1, and a high-load melt flow rate of 8.0 g/10 min measured at 190 °C under 21.6 kg in accordance with ISO 1133-1:2022. These values are representative screening values, not contractual lot release limits. The current certificate of analysis and the producer’s current product data sheet should be consulted for lot-specific control ranges.

    Property Test standard Nominal data sheet value
    High-load melt flow rate ISO 1133-1:2022 8.0 g/10 min at 190 °C / 21.6 kg
    Density ISO 1183-1 0.952 g/cm³
    Tensile stress at yield ISO 527-2 26 MPa
    Tensile strain at break ISO 527-2 600 %
    Flexural modulus ISO 178 1100 MPa
    Charpy notched impact strength, 23 °C ISO 179-1 13 kJ/m²
    Vicat softening temperature, A50 ISO 306 124 °C
    ESCR, F50, 10 % Igepal CO-630 ASTM D1693 >100 h

    Processors using DMDA8920 in production-scale shuttle blow molding machines generally run single-screw extruders with barrel length-to-diameter ratios between 24:1 and 32:1. Barrier screws or grooved feed sections are used to control solids conveying without excessive low-film-temperature melting. The recommended melt temperature window for this viscosity class is 175 °C to 210 °C. Die head zones are maintained between 180 °C and 210 °C, and mold cooling water is controlled at 10 °C to 30 °C to stabilize pinch-off welds and cooling shrinkage. The high-load melt flow rate of 8.0 g/10 min corresponds to a viscosity envelope that provides sag resistance for intermediate parisons. Compared with high-flow blow molding resins in the 12–20 g/10 min high-load melt flow range, DMDA8920 produces less parison sag in containers above 10 L. Compared with substantially higher-viscosity pipe grades, it permits shorter cycle times but may require additional surge pressure at the die head.

    What Processing Window Governs Continuous Extrusion Blow Molding of DMDA8920?

    Melt temperature is the primary control for surface quality and weld integrity. Operation below 170 °C is not recommended because partially unmelted resin increases head pressure and produces visible flow lines and weak pinch-off weld zones. Operation above 220 °C is also not recommended because oxidative degradation generates gel particles that deposit on the die lip and produce surface blemishes. Field reports from continuous extrusion blow molding lines identify gel streaks, yellow discoloration, and die-lip deposits as the principal failure modes under excessive thermal history. The extruder barrel profile is typically set with zone 1 at 160–170 °C, zone 2 at 170–180 °C, zone 3 at 180–190 °C, and the adapter/head assembly at 190–205 °C. This profile prevents excessive initial compression heating and reduces the survival of low-temperature unmelt. Screw speeds from 30–80 min⁻¹ on extruders with 60–90 mm screw diameters are typical for these intermediate-viscosity blow molding resins, but output is constrained by head pressure and melt temperature rise.

    Parison sag is controlled by melt strength and parison programming. In production-scale extrusion blow molding of containers above 10 L, gradual parison wall thinning between die exit and mold closing is a known bottleneck. The high-load melt flow rate of 8.0 g/10 min indicates a higher molecular weight fraction than general-purpose blow molding grades in the 12–20 g/10 min range. The resulting melt strength supports larger shot sizes; however, processors must still use parison programming with 20–50 thickness adjustment steps on accumulator or reciprocating screw heads to compensate for die swell and sag. Die gap settings are commonly adjusted to 1.5–3.0 mm, but die swell values depend on shear history, melt temperature, and output rate. Published data for this specific grade under all combinations of output and die geometry is limited.

    Moisture pick-up is not a bulk absorption issue for high-density polyethylene; however, surface condensation on cold pellets conveyed from outdoor silos can create intermittent splay and die-lip build-up. If pellets are stored at relative humidity above 60 % and brought into a warm production area, surface drying at 70–80 °C for 2–4 h in a desiccant dryer is used to prevent surface defects. This is an operational boundary rather than a resin chemical requirement.

    Regrind content from reject containers can be introduced up to 20–30 wt% with monitoring of melt flow stability and weld performance. Regrind that has undergone multiple heat histories lowers ESCR and increases gel count. Mechanical conveying and regrind systems should be segregated to avoid cross-contamination with PVC. Trace poly(vinyl chloride) contamination can dehydrochlorinate under processing temperatures and generate acidic species that corrode screw and die surfaces and catalyze polyethylene degradation.

    Environmental Stress Cracking and Chemical Compatibility Boundaries

    The defining performance requirement for blow molded rigid packaging is environmental stress crack resistance. DMDA8920 is characterized by an ESCR F50 value above 100 h under ASTM D1693 condition B at 50 °C in 10 % Igepal CO-630, as reported in producer data sheets. This value is not a direct service-life prediction. ESCR depends on comonomer content, molecular weight distribution, processing thermal history, mold cooling rate, and wall stress. The test ranks materials under a standard surfactant stress-cracking environment; it does not account for specific chemicals, oxidizing agents, or temperatures above ambient. For industrial chemical packaging, qualification requires exposing filled containers to the actual chemical under stack-load and top-load stresses at the upper service temperature.

    Chemicals that plasticize the amorphous phase of high-density polyethylene, including aromatic hydrocarbons, chlorinated solvents, and certain surfactant formulations, reduce ESCR and should not be assumed compatible solely on the basis of the resin grade. Strong oxidizing acids and some halogenated compounds can initiate chain scission at weld lines. The pinch-off weld and side-seam regions are the critical crack initiation sites because they contain frozen-in orientation and wall-thickness discontinuities. Process validation should include drop-impact and ESCR testing on the actual molded container, not only on compression-molded test plaques. The grade should not be used without validation for oxidizing acids or for aromatic or chlorinated solvents that plasticize the amorphous phase and reduce stress crack resistance.

    Finished container performance should be verified by top-load compression, drop impact, and hydraulic or pneumatic leak tests after conditioning for 48 h at 23 °C and 50 % relative humidity in accordance with ASTM D618 or equivalent. Environmental stress crack resistance on molded parts should be evaluated on pinch-off welds and side seams rather than on unfabricated plaques.

    When DMDA8920 Replaces a High-Flow Injection Moulding Grade

    DMDA8920 is not a direct substitute for high-flow injection moulding HDPE. The melt flow rate under 190 °C/2.16 kg is not the primary specification for this grade, and the high-molecular-weight fraction that gives blow molding melt strength restricts injection flow length and raises injection pressure. Typical high-flow HDPE injection moulding grades have melt flow rates in the 20–40 g/10 min range under 190 °C/2.16 kg. In contrast, a blow molding grade such as DMDA8920 has a melt flow rate below 1.0 g/10 min under the same condition in some lots. This difference means that thin-wall sections below 1.5 mm are likely to be difficult to fill without excessive pressure, high shear heating, and surface degradation. DMDA8920 is intended for extrusion blow molding; attempts to run it in injection molding tools designed for high-flow HDPE generally reduce production efficiency and may require higher clamp force due to high melt viscosity.

    HDPE family Typical melt flow or high-load melt flow range Density range Primary process Relevant limitation
    DMDA8920 blow molding grade 8.0 g/10 min (190 °C/21.6 kg) 0.952 g/cm³ extrusion blow molding not suited to thin-wall injection moulding
    High-flow injection moulding HDPE 20–40 g/10 min (190 °C/2.16 kg) 0.952–0.964 g/cm³ injection moulding low melt strength; parison sag unacceptable
    HDPE film grade 0.5–2.0 g/10 min (190 °C/2.16 kg) 0.945–0.950 g/cm³ blown film lower stiffness; not optimized for parison pinch-off weld
    HDPE pipe grade, PE100 class 0.2–0.5 g/10 min (190 °C/5 kg) 0.950–0.960 g/cm³ pipe extrusion too high viscosity for short-cycle blow molding

    The practical difference between DMDA8920 and lower-viscosity blow molding HDPE grades appears most clearly in larger containers. Lower-viscosity grades in the 12–20 g/10 min high-load melt flow range allow faster cycle times but produce greater parison sag in containers above 10 L. Conversely, pipe-grade HDPE resins with very low melt flow rates provide higher slow crack growth resistance but require long residence times and high head pressures that are unsuitable for short-cycle blow molding. DMDA8920 occupies an intermediate position: it provides sufficient melt strength for medium-to-large hollow parts while retaining enough flow for melt homogenization in a barrier screw or grooved feed section.

    Published data for this specific configuration is limited when DMDA8920 is used in multi-layer coextrusion with barrier polymers such as ethylene vinyl alcohol or polyamide. Tie-layer selection must be validated for melt viscosity matching; a mismatch in shear viscosity at the die can produce interfacial instability and layer thickness non-uniformity. The producer’s documentation does not position DMDA8920 as an adhesive or barrier layer resin. Color masterbatch addition is typically maintained at 2–4 wt%; higher addition levels should be evaluated for ESCR and weld strength because the carrier resin and pigment dispersion can alter the melt structure. No conclusion is drawn from the data sheet values alone; qualification is batch- and tool-specific.

    Top