Sinopec Fujian Hdpe Dmda8007

Sinopec Fujian HDPE DMDA8007

    • Product Name: Sinopec Fujian HDPE DMDA8007
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 512944
    Product Name Sinopec Fujian HDPE DMDA8007
    Manufacturer Sinopec Fujian
    Polymer Type High Density Polyethylene (HDPE)
    Grade DMDA8007
    Density 0.956 g/cm3
    Melt Flow Rate 8.0 g/10 min at 190°C/2.16 kg
    Tensile Strength At Yield 25 MPa
    Elongation At Break 500 %
    Flexural Modulus 1000 MPa
    Notched Izod Impact Strength 50 J/m at 23°C
    Vicat Softening Temperature 125 °C
    Melting Temperature 130 °C
    Thermal Deflection Temperature 75 °C
    Hardness 65 Shore D
    Mold Shrinkage 1.5-3.0 %
    Water Absorption <0.01 %
    Color Natural
    Form Pellet
    Processing Method Injection Molding

    As an accredited Sinopec Fujian HDPE DMDA8007 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Fujian HDPE DMDA8007 is packaged in 25 kg bags, palletized; 1,000 kg jumbo bags available.
    Container Loading (20′ FCL) Sinopec Fujian HDPE DMDA8007 is loaded in 20′ FCL as 25 kg bags, normally 25 MT (1,000 bags) per container.
    Shipping Sinopec Fujian HDPE DMDA8007 is a non-hazardous high-density polyethylene resin, not classified as dangerous goods for transport. Typically shipped in 25 kg woven bags or jumbo bags, palletized and stretch-wrapped. Store in a cool, dry, ventilated area; avoid moisture, direct sunlight, heat, and handle with care.
    Storage Store Sinopec Fujian HDPE DMDA8007 in a cool, dry, well-ventilated warehouse away from ignition sources, direct sunlight, heat, moisture, and UV radiation. Keep original bags or containers sealed and palletized off the floor. Avoid contact with strong oxidizers, acids, and open flames. Maintain good housekeeping to prevent dust and contamination. Follow local regulations and the supplier’s SDS.
    Shelf Life Typically 12 months under recommended storage conditions: original unopened packaging, cool, dry, ventilated area, away from direct sunlight and heat.
    Application of Sinopec Fujian HDPE DMDA8007

    Sinopec Fujian HDPE DMDA8007 is a blow-moulding-grade high-density polyethylene with a melt index of 0.8 g/10 min measured at 190 °C under 2.16 kg load in accordance with ASTM D1238 and a density of 0.956 g/cm³ determined by ASTM D792. On continuous shuttle extrusion blow moulding lines with single-screw extruders of 24:1 to 30:1 L/D and barrier screws, the resin is processed into monolayer containers for household detergents, hard-surface cleaners, laundry products and institutional cleaning chemicals. Typical bottle sizes range from 500 mL to 2 L, with sidewall thickness of 0.8–1.2 mm. Formulation involves a virgin resin stream blended with a polyethylene-carrier colour masterbatch at 2–3 wt%; masterbatches based on EVA or excessive wax carriers should be excluded unless qualified by ASTM D1693 Condition B on the finished bottle because they can lower environmental stress crack resistance and contribute to die-lip deposit. For hypochlorite bleach and detergent bottles, the filled container is screened through accelerated storage at 60 °C for 21 days followed by ESCR evaluation per ASTM D1693 Condition B. The selected closure system is typically a 28-410 or 33-400 threaded neck; top load acceptance for an empty 500 mL bottle is generally set above 100 N when measured at 23 °C in accordance with ASTM D2659. Pre-drying is not required for pellets stored below 60% RH; if surface condensation occurs after outdoor silo storage, a hopper dryer at 70–80 °C for 2–4 h prevents splay. Melt temperature should remain between 190 °C and 205 °C; sustained operation above 220 °C increases thermal oxidative degradation and generates gels that appear as pinholes or local thin spots at the parison wall.

    Starting parameters for a shuttle-machine monolayer bottle are provisional and require line-specific optimisation against machine clamp stroke, accumulator head pressure and mould venting.

    Extrusion blow moulding parameterStarting range for DMDA8007 monolayer bottles
    Feed zone165–175 °C
    Compression/barrier zone185–195 °C
    Metering zone190–200 °C
    Head and die195–205 °C
    Melt temperature190–205 °C
    Mould temperature15–25 °C
    Blow pressure0.6–0.8 MPa
    Die swell allowance30–50%

    What Process Adjustments Control Die Swell and Surface Gloss in Personal Care Bottles?

    In personal care bottle manufacture, the primary limitation is parison diameter stability over a drop length of 250–450 mm before mould close. DMDA8007 exhibits a die swell range of 30–50% depending on die gap, shear rate and melt temperature; the die gap for a 500 mL bottle is therefore set at 40–60% of the desired final wall thickness rather than at the final wall thickness itself. For high-gloss shampoo and conditioner bottles, mould temperature is held at 20–30 °C; lower mould temperatures produce matte surfaces and increase frozen-in stress near the parting line. The resin is blended with a pearlescent or opaque colour masterbatch at 1–2 wt%; pearlescent loadings above 2 wt% can reduce pinch-off weld integrity and should be re-qualified by a filled drop test at 4 °C. Surfactant-containing formulations, including sodium laureth sulfate and cocamidopropyl betaine, create stress cracking conditions; candidate bottles are tested with the market formula at 50 °C for 14–28 days and then subjected to ESCR measurement by ASTM D1693 Condition B. Blow pressure is set at 0.6–0.8 MPa, and blow time is adjusted so that the frost line reaches the lower pinch-off zone before ejection. The terminal article is typically a 250 mL to 1 L bottle with body wall thickness of 0.7–1.1 mm and a neck finish of 24-410 or 28-410. If silk-screen or pressure-sensitive labelling is specified, the container surface should be corona-treated within 24–48 h post-moulding to a wetting tension of 42–48 mN/m measured by ASTM D2578; untreated HDPE surface energy decays rapidly and ink adhesion becomes inconsistent.

    In tablet and capsule packaging, DMDA8007 is processed into monolayer HDPE pharmaceutical bottles with 33 mm and 38 mm neck finishes that receive child-resistant closures. The application is governed by USP <661.1> physicochemical testing and is supported by resin compliance with FDA 21 CFR 177.1520 for olefin polymers when the final article is tested for total nonvolatile residue and specific migration. In clean-room blow moulding, the extruder hopper and mould area are separated from printing and trimming equipment to prevent particulate contamination; no mould-release spray may be used because the resulting extractables can alter USP test outcomes. For pharmaceutical bottles from 30 mL to 250 mL, wall thickness is generally 0.8–1.5 mm to maintain closure torque retention after repeated opening. The moisture vapour transmission rate of HDPE is often reported in the range of 0.2–0.5 g·mm/(m²·day) under 38 °C and 90% RH when tested by ASTM F1249, but published data for this specific grade in finished bottle geometry is limited; desiccant-filled closures and induction seals are specified when the drug product has a release specification for moisture gain. Drop testing is performed at 4 °C using filled bottles conditioned for 24 h; acceptance is usually no rupture and no closure detachment after 1.2 m drops onto concrete. The grade is not tested in this context as an oxygen barrier; products requiring low oxygen ingress should use a coextruded EVOH structure or an aluminium foil induction seal.

    When ESCR Thresholds Control 5-L Agrochemical Jerrycan Qualification

    The qualification of a 5-L agrochemical jerrycan made from DMDA8007 begins with classification of the filled container under the UN performance packaging code 3H1 for plastics jerricans with a non-removable head. In this application the resin is processed on accumulator-head blow moulding machines with parison programmers configured for 8–12 profile points. The typical jerrycan mass for 5 L is 180–220 g; wall thickness is programmed between 0.8 mm and 1.8 mm, with thicker distribution at the pinch-off, handle bridge and base corners. A programmed parison wall profile of 20–30% base-heavy and 10–15% top-heavy relative to the centre section prevents thin-out in the flush corners. Pinch-off weld thickness must be at least 1.2× the adjacent sidewall thickness; if the flash is trimmed too aggressively to below this ratio, the drop impact failure mode shifts from ductile deflection to brittle cleavage along the parting line.

    Environmental stress crack resistance is the controlling material property. The resin should be evaluated with ASTM D1693 Condition B in 10% Igepal CO-630 at 50 °C; for agrochemical formulations containing aromatic solvents or cyclohexanone, the F50 value should be qualified against an internal specification of at least 150 h. Actual product compatibility must be verified by storing filled jerrycans at 50 °C and 80% RH for 28 days followed by drop, stack and leak testing as prescribed for UN packaging. The UN classification requires hydraulic pressure testing at 100 kPa for 5 min, drop testing from 1.2 m for packing group II, and stacking under load at 40 °C for 28 days. Additive selection for outdoor agricultural use includes 0.2–0.5 wt% HALS and 0.1–0.2 wt% UV absorber in a PE carrier masterbatch; the base resin must not be blended with more than 5 wt% polypropylene or low-molecular-weight LDPE, as both lower ESCR and reduce pinch-off weld toughness. When a colour masterbatch is loaded above 3 wt%, Charpy notched impact strength measured by ISO 179-1:2010 should be re-confirmed because pigments can act as stress concentrators.

    Compliance verification matrix for DMDA8007 downstream packaging segments.

    SegmentRegulatory instrumentVerification/test condition
    Household detergent bottlesEU Packaging Directive 94/62/EC; REACH Regulation (EC) No 1907/2006Packaging heavy metals sum below 100 ppm; SVHC content communication
    Pharmaceutical bottlesUSP <661.1>; FDA 21 CFR 177.1520(c)Physicochemical battery; extraction and total nonvolatile residue
    Agrochemical jerrycanUN 3H1; ADR/RID/IMDGDrop 1.2 m; hydraulic 100 kPa; stack 40 °C for 28 days
    Food barrier bottleFDA 21 CFR 177.1360; EU Regulation (EC) No 10/2011Overall migration limit below 10 mg/dm²; specific migration for EVOH
    Personal care bottleREACH Regulation (EC) No 1907/2006; EU Regulation (EC) No 1223/2009Packaging must not release substances that alter the cosmetic product

    Coextruded HDPE-Tie-EVOH Barrier Structures for Oxygen-Sensitive Food Sauces

    Six-layer coextrusion blow moulding of DMDA8007 as the structural HDPE layer is used for squeezable barrier bottles for ketchup, mayonnaise and edible oil packaging. The layer sequence is typically HDPE outer / tie / EVOH / tie / regrind / HDPE inner, with the two HDPE layers together contributing 60–75 wt% of total wall thickness and the EVOH layer contributing 3–5 wt%. EVOH grades with ethylene content of 27–32 mol% are selected because at this composition the oxygen barrier under 23 °C and 50% RH can be maintained while retaining coextrusion processability. DMDA8007 is used in the outer and inner HDPE layers, but the regrind layer must be limited to 25–30 wt% because the oriented EVOH domains in regrind increase viscosity and create interfacial streaks. Viscosity matching is critical at the HDPE/tie interface; if the melt temperature difference between adjacent layers exceeds 10 °C, interfacial instability appears as parabolic weld lines. The oxygen transmission rate of the finished barrier bottle should be measured by ASTM D3985 and is typically specified below 0.5 cm³/(m²·day·bar) at 23 °C and 50% RH; by comparison, monolayer HDPE of 0.7 mm wall thickness will transmit above 150 cm³/(m²·day·bar) under the same conditions. Food-contact compliance is evaluated under FDA 21 CFR 177.1360 for the EVOH layer and FDA 21 CFR 177.1520 for HDPE, with migration testing performed on the final article under Commission Regulation (EU) No 10/2011. The terminal container is typically 300–750 mL with body wall thickness of 0.6–1.0 mm; the HDPE inner layer prevents direct contact between the EVOH barrier and water-based food contents, which would otherwise plasticise the EVOH and increase oxygen transmission.

    Three-station injection blow moulding of DMDA8007 differs from extrusion blow moulding in that a precision preform is injection moulded around a core pin before blowing. The process is used for small-mouth containers from 10 mL to 100 mL such as travel-size lotion bottles, eye-wash bottles and cosmetic samplers. The injection station is operated with a melt temperature of 190–210 °C, an injection pressure of 60–100 MPa, and a core-pin temperature of 10–20 °C to prevent preform sagging. The blow station uses air at 0.7–0.9 MPa and a blow-mould temperature of 15–25 °C. Because the neck finish is formed in the preform mould rather than trimmed from the blow-moulded parison, the internal bore tolerance can be held within ±0.05 mm; this is critical for dropper tips and child-resistant closures that require a stable insertion force. Published data for this specific DMDA8007 configuration is limited; process qualification should therefore include a short-shot study on the injection core pin and a preform temperature map before full production. The grade is not recommended for continuous extrusion blow moulding of large flat panels or for rotational moulding, because the melt index of 0.8 g/10 min and molecular weight distribution are tuned for high melt strength under parison draw rather than for powder flow in rotational moulds.

    Free Quote

    Competitive Sinopec Fujian HDPE DMDA8007 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    For blow-moulded rigid packaging in the 20 L to 200 L range, Sinopec Fujian HDPE DMDA8007 is supplied as a high-density polyethylene extrusion blow-moulding grade with a typical density of 0.956 g/cm³ measured to ISO 1183-1 and a melt flow rate of 0.80 g/10 min at 190°C under 2.16 kg load per ISO 1133-1:2022. The grade is used in monolayer extrusion blow moulding of tight-head drums, open-top pails, jerry cans, and industrial packaging requiring melt strength, stiffness, and environmental stress-crack resistance. The low melt flow rate indicates a high-molecular-weight backbone, which increases parison hang strength on reciprocating screw blow moulders with 24:1 to 30:1 L/D extruders. Against injection-grade HDPE with melt flow rates above 10 g/10 min, DMDA8007 retains significantly higher elongational viscosity and resists thinning at the flash pinch-off and across unsupported parison lengths.

    Mechanical values reported in supplier grade documentation are typical, not lot-release limits. Tensile stress at yield is approximately 27 MPa to ISO 527-2, tensile elongation at break exceeds 600%, and flexural modulus is approximately 1100 MPa to ISO 178. Environmental stress-crack resistance determined under ASTM D1693, condition B at 50°C in 10% Igepal CO-630, is reported above 200 h F50. Vicat softening temperature is approximately 126°C under ISO 306 method A120. The combination of density and molecular weight yields higher slow-crack resistance than lower-molecular-weight blow moulding or injection grades of similar density.

    The following table consolidates grade-identification data and the test methods used to resolve batch disputes.

    PropertyTypical valueTest method
    Density0.956 g/cm³ISO 1183-1
    Melt flow rate0.80 g/10 minISO 1133-1:2022, 190°C, 2.16 kg
    Tensile stress at yield27 MPaISO 527-2
    Tensile elongation at break>600%ISO 527-2
    Flexural modulus1100 MPaISO 178
    ESCR, F50>200 hASTM D1693, condition B
    Vicat softening temperature126°CISO 306/A120

    Food-contact acceptability is generally supported when the finished article meets the olefin polymer requirements of FDA 21 CFR 177.1520(c) paragraphs 3.1a and 3.2a and the migration restrictions of EU 10/2011. Compliance is not conferred by the resin alone; additives, colorants, and process residues require evaluation under the final packaging geometry and filling conditions. For hazardous-goods packaging, DMDA8007 is commonly evaluated within UN performance tests for top load, drop impact, stacking, and leakproofness under UN Model Regulations Chapter 6.1. The resin contributes to top-load retention after ageing but is not a substitute for structural design verification or appropriate wall-thickness distribution.

    What Distinguishes DMDA8007 from High-MFI Blow Moulding and Injection HDPE Grades?

    The primary distinction is rheological. A melt flow rate of 0.80 g/10 min is roughly one-half to one-third of the value used in thin-wall blow moulding grades for bottles under 1 L. Those high-MFI grades, typically between 1.5 g/10 min and 2.5 g/10 min, permit faster parison extrusion and shorter cycle times but usually show lower environmental stress-crack resistance and lower hoop-stress capacity in large-format containers. DMDA8007 trades some throughput for higher molecular weight, greater melt extensibility, and improved resistance to aggressive fill products such as surfactants, detergents, and oxidising liquids. Compared with injection-grade HDPE having melt flow rates between 10 g/10 min and 30 g/10 min, the difference is more pronounced: injection grades are optimized for high-shear mould filling and spiral-flow length, whereas DMDA8007 is formulated for sag resistance and parison wall-thickness uniformity in extrusion blow moulding, not for high-speed injection.

    The difference also appears in slow-crack growth. Resins of similar density but lower molecular weight often match short-term tensile stiffness yet fail earlier under constant stress below the yield point. DMDA8007’s density of 0.956 g/cm³ and melt flow rate of 0.80 g/10 min yield higher F50 ESCR than comparable-density injection grades and many thin-wall blow grades. In production, this distinction appears as reduced parison draw-down, better wall-thickness control in long parison profiles, and more stable top-load performance after drop-impact conditioning.

    Representative comparison of DMDA8007 with typical industrial HDPE classes is shown below; the comparative ranges are general process-selection values, not supplier specifications.

    Material classMelt flow rateDensityESCR F50Primary process
    Sinopec Fujian HDPE DMDA80070.80 g/10 min0.956 g/cm³>200 hExtrusion blow moulding
    High-MFI blow moulding HDPE1.5–2.5 g/10 min0.950–0.960 g/cm³50–150 hExtrusion blow moulding
    Injection-grade HDPE10–30 g/10 min0.950–0.965 g/cm³<50 hInjection moulding

    Thermal Processing Window, Screw Configuration, and Die Head Settings

    Extrusion blow moulding of DMDA8007 is typically initiated at a melt temperature between 180°C and 210°C. The lower bound is driven by melt homogeneity and prevention of unmelted gels; the upper bound is driven by thermal degradation and viscosity reduction that can impair parison integrity. Die head temperatures are normally maintained between 190°C and 210°C. Mould temperatures of 10°C to 30°C are used to freeze part surfaces and control shrinkage. Pre-drying is not normally required at ambient relative humidity below 60%. At higher humidity or after condensation, a desiccant dryer set at 80°C for 2 h reduces surface moisture and minimises cosmetic defects from steam. Barrier screws with compression ratios of 2.2:1 to 3.0:1 and L/D of 24:1 to 30:1 are standard on production lines. Melt temperature should be confirmed with a needle pyrometer at the die exit rather than inferred from barrel set points.

    Processing limitations are specific. The grade is not intended for injection moulding; filling thin-wall moulds under high injection pressure can produce short shots and flash because the viscosity remains elevated. For parts below 2 mm wall thickness, a higher-MFR blow moulding or injection-grade HDPE should be selected. Conversely, for long parison hang times or large open diameters, DMDA8007’s low MFR is advantageous. In commercial blow moulding, parison tears at pinch-off often originate from melt temperature below 180°C or insufficient die gap. On shuttle machines, wall-thickness controls should be programmed to compensate for parison sag; although the high molecular weight reduces sag, it does not eliminate it at unsupported lengths above 1 m. Converters should monitor melt pressure and parison length after grade changes because batch-to-batch variance in MFR and density, while controlled within supplier release limits, can shift the optimum die gap.

    At the molecular level, slow crack growth in HDPE is governed by tie-molecule concentration and lamellar structure. A density of 0.956 g/cm³ is above the region where low-density copolymers give very high ESCR but lower stiffness; DMDA8007 balances crystalline stiffness with sufficient tie molecules to resist crack advance under constant stress. During blow moulding, rapid cooling at the mould surface creates a skin-core morphology with orientation. Excessive melt temperature can reduce orientation and lower ESCR; too-low melt temperature can create flow-induced defects that act as crack initiation sites. The practical melt-temperature window is therefore narrow in demanding applications, and production trials at 185°C, 195°C, and 205°C are used to locate the best balance of surface finish, top load, and ESCR.

    Screw selection for DMDA8007 should prioritise distributive mixing and temperature homogeneity over high-shear dispersive mixing. High-shear mixers can impose excessive viscous heating and reduce effective molecular weight at the die. Barrier screws with shear rates kept below 1000 s−1 in the metering section are preferred; grooved-barrel extruders are generally not required. Back pressure should be set to the minimum needed to maintain melt homogeneity, because additional shear work raises melt temperature and increases the risk of parison sag. Hopper drying at 80°C is the only pre-processing step commonly required, except where high levels of regrind are used.

    In industrial container production, DMDA8007 is used in extrusion blow moulding of 20 L to 120 L open-head and tight-head containers, agricultural-chemical packaging, and closures requiring high ESCR. Accumulator-head machines are often selected where unsupported parison lengths exceed 600 mm; the resin is also run on continuous shuttle machines with radial wall-thickness programming. For aggressive solvent mixtures, published data for this specific configuration is limited, and compatibility testing at the container level is required before commercial filling. Food-contact articles should be tested for overall migration and specific migration under the intended food simulant, because additives and colorants can alter compliance independent of the base resin.

    When ESCR Validation Moves to the Finished Container

    Environmental stress-crack resistance is a material property measured under a defined stress and environment, but field performance depends on container geometry, residual stress from processing, and fill-formulation aggressiveness. A resin F50 above 200 h under ASTM D1693 does not guarantee compatibility with every filling medium or every top-load condition. In filled-container tests, failures frequently initiate at pinch-off scars, mould parting lines, or sharp corner transitions where frozen-in stress concentrates. For UN-certified 1H1 closed-head drums, drop-impact and stacking sequences are performed after filling with water or test liquids; the result depends on the container’s wall-thickness distribution as much as on the ESCR of the base resin.

    Converters evaluating DMDA8007 against lower-MFI HDPE grades should compare not only F50 ESCR but also top-load retention after exposure to surfactants at elevated temperature, typically 40°C to 60°C. Where hopper-loading or regrind levels exceed 20%, ESCR and melt viscosity may shift; controlled regrind incorporation and property verification are required. The grade is not precompounded with UV stabilisers, so outdoor service in direct sunlight requires a well-dispersed UV masterbatch and relevant accelerated weathering validation.

    For outdoor or long-life industrial packaging, the absence of pre-added UV stabilizer differentiates DMDA8007 from compounded HDPE grades containing carbon black or hindered-amine light stabilisers. In such applications, a masterbatch is required, and the converter must re-verify tensile impact strength and ESCR because additive masterbatches can reduce melt strength if added at high levels. The base resin is typically supplied as natural pellets; colouring is performed at the machine feed throat using proportional dosing at levels specified by the masterbatch supplier.

    The product is not intended for blown film or pipe extrusion. In blown film, melt flow rates below 1 g/10 min can create high head pressure and unstable bubble cooling at standard die gaps; film-grade HDPE formulations are usually selected for web uniformity. In pipe extrusion, long-term hydrostatic strength is governed by different melt index and density targets under ISO 9080; using a blow moulding grade in pipe is not appropriate without complete long-term pressure regression testing. This narrows the application window to extrusion blow moulding and some sheet or profile uses where melt strength is valued.

    From a regulatory standpoint, converters may request letters confirming that the neat resin is within the concentration limits for lead, cadmium, mercury, hexavalent chromium, PBB and PBDE under RoHS Directive 2011/65/EU at the homogeneous material level. Under REACH Regulation (EC) No 1907/2006, the supplier is obliged to communicate safe-use information and, where relevant, candidate-list SVHCs. Such statements are lot and formulation specific; they are not part of the standard data sheet unless separately issued.

    Where a high-burden industrial container must combine top load above 1.0 MPa compressive stress, drop-impact performance at -18°C, and slow-crack resistance in the presence of fatty acid derivatives, DMDA8007 is commonly shortlisted for trial runs on accumulator-head lines with 80 mm to 120 mm screw diameters. Published data for this specific configuration is limited; converters typically generate in-house data by moulding 20 L pails and performing top-load tests to ASTM D2659 with inspection at yield or buckling. Such trials establish whether the grade’s higher melt strength justifies the longer cooling time required relative to lower-molecular-weight HDPE alternatives.

    Top