Sinopec Fujian Hdpe Dmda6200

Sinopec Fujian HDPE DMDA6200

    • Product Name: Sinopec Fujian HDPE DMDA6200
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 354487
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.953 g/cm³
    Melt Flow Rate 0.35 g/10 min (190°C/2.16 kg)
    Melt Flow Ratio 100
    Tensile Yield Strength 24 MPa
    Tensile Break Strength 30 MPa
    Elongation At Break >500%
    Flexural Modulus 1000 MPa
    Vicat Softening Temperature 125°C
    Brittleness Temperature -70°C
    Environmental Stress Cracking Resistance >1000 h
    Shore D Hardness 60
    Water Absorption <0.01%

    As an accredited Sinopec Fujian HDPE DMDA6200 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Fujian HDPE DMDA6200 is packed in 25 kg woven polypropylene bags, 40 bags (1,000 kg) per pallet, stretch-wrapped.
    Container Loading (20′ FCL) Container loading (20′ FCL): Sinopec Fujian HDPE DMDA6200, 25 kg bags; 25 MT net unpalletized or 20 MT palletized.
    Shipping Sinopec Fujian HDPE DMDA6200 is shipped as a non-hazardous thermoplastic resin, typically in 25 kg woven bags or jumbo bags, palletized and stretch-wrapped. Store cool, dry, ventilated, away from sunlight, heat, and moisture. Standard 20'/40' containers or truckload.
    Storage Store Sinopec Fujian HDPE DMDA6200 in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, heat, and ignition sources. Keep original bags sealed and palletized; avoid crushing or damage. Separate from strong oxidizers. Observe stack-height limits and use first-in, first-out rotation. Keep storage area clean, dry, and free of spilled pellets. Follow the supplier SDS and local regulations.
    Shelf Life Sinopec Fujian HDPE DMDA6200 has a shelf life of 24 months if stored cool, dry, and away from direct sunlight.
    Application of Sinopec Fujian HDPE DMDA6200

    In extrusion blow molding lines producing rigid containers for household cleaning formulations, Sinopec Fujian HDPE DMDA6200 is processed as a virgin polyolefin base with a melt-flow rate at 190 °C/2.16 kg reported as approximately 0.20 g/10 min under ISO 1133-1:2022 and a density of 956 kg/m³ under ISO 1183-1:2019. The relevant compliance framework for non-food household cleaning bottles includes the EU Packaging and Packaging Waste Directive 94/62/EC heavy-metal limit, which restricts the sum of cadmium, lead, mercury and hexavalent chromium to ≤100 mg/kg, and, where the filled product is classified as dangerous goods under the UN Model Regulations Rev. 23, 2023, the pack must additionally satisfy UN 6.1.5.3 drop-test and leakproofness requirements for the assigned packaging group. The charge basis on a single-station shuttle blow molding machine is typically 100 parts by weight of DMDA6200, with closed-loop clean regrind from the same bottle line held at ≤20 wt% of total charge, white or colored masterbatch added at 0.8–1.5 wt%, and optional HDPE-based UV stabilizer masterbatch added at 0.3–0.8 wt% when storage in outdoor-adjacent retail environments is specified. The melt is plasticated through a 65 mm single-screw extruder with an L/D of 24:1 and a five-zone barrel profile from 180 °C to 205 °C, then shaped into a parison through a diverging die head with a programmable die gap; the parison is transferred to a split blow mold at a clamp force of 15–40 t, inflated with dry air at 0.6 MPa, and contact-cooled against a mold surface held at 8–15 °C. Finished monolayer containers in this segment are typically 0.5 L to 5 L bottles or handleware for bleach, liquid detergent, hard-surface cleaner, and fabric softener formulations; wall-thickness profiling at the handle pinch-off and shoulder regions is adjusted to maintain a minimum sidewall thickness of 0.45 mm and to avoid fold-over thinning that reduces environmental stress-crack resistance.

    A persistent production constraint in this segment is that regrind loading above 20 wt% or any inclusion of post-consumer recyclate of unverified provenance raises the probability of gel-induced parison puncture and lowers ASTM D1693-15 condition B failure time in 10% Igepal CO-630 at 50 °C below a qualified baseline. When the bottle is intended for chlorine bleach, contact with the filled product generates oxidative cleavage at the inner surface, so ESCR validation must be conducted at the specified sodium hypochlorite concentration and storage temperature rather than inferred from generic high-density polyethylene ratings.

    Why Are Migration Limits, Not Melt Flow, Decisive for Dairy and Juice Blow Molding?

    The compliance pathway for milk, juice, and drinking-yogurt packs built from DMDA6200 begins with the regulatory clearance of the olefin polymer rather than with its flow properties. The base resin must meet 21 CFR §177.1520 for food-contact olefin polymers in the United States, EU Regulation (EU) No 10/2011 with the overall migration limit of 10 mg/dm² for plastic materials in contact with aqueous and acidic food simulants, and, for China-bound applications, GB 4806.7-2023 for food-contact plastic resins. The compounding formulation for milk jugs and juice bottles uses 100 parts by weight DMDA6200, closed-loop regrind from the same food-contact production lot held to ≤15 wt%, food-grade white masterbatch at 0.5–1.0 wt%, and no external slip agents or antistatic agents unless separately cleared under Regulation (EU) No 10/2011 positive-list requirements. Downstream production is performed on a two-station shuttle extrusion blow molding line with an accumulator head or a continuous parison discharge, barrel temperature settings ranging from 190 °C to 210 °C, die-head temperature at 195 °C, and treated chilled water at 10 °C circulated through the mold base; after demolding, containers pass through a leak tester with a differential pressure setpoint of 0.03 MPa and a fill-volume check. Terminal finished products include 250 mL to 2 L high-density polyethylene bottles for pasteurized milk, chilled juice, drinking yogurt, and ambient aseptic fruit drinks.

    Operational boundaries in this segment include the requirement that regrind must be generated only from the same food-contact grade and must be traceable under EC 2023/2006 good manufacturing practice; recycled material from external sources is not acceptable without specific migration testing because unknown antioxidants or slip additives may alter organoleptic transfer into high-fat dairy phases. Melt-temperature excursions above 230 °C or barrel residence times beyond 4 min produce oxidative species that can be detected as off-taste in low-flavor foods, so startup and short-run purge procedures are applied before food-contact production restarts.

    When primary pharmaceutical bottles are formed from DMDA6200, the resin selection logic shifts from mechanical property alone to extractables control, biological reactivity testing, and cleanroom documentation. The compliance framework for these packages is governed by USP <661.1> for plastic materials of construction, with physicochemical testing under USP <661.2>, biological reactivity testing under USP <87> and <88>, Ph. Eur. 3.1.3 for polyethylene, and ICH Q3D elemental-impurity risk assessment when potential metal residues from polymerization catalysts are considered. The formulation is restricted to 100 parts by weight of virgin DMDA6200; regrind introduction is typically avoided in primary packaging, and where a validated closed-loop regrind stream is used it is held at ≤10 wt% of the same lot with documented traceability under 21 CFR Part 211 production controls. Production is carried out on extrusion blow molding machines installed in an ISO 8 cleanroom environment, with blow air filtered through 0.2 µm membrane, mold cooling water at 12 °C, and cycle parameters controlled so that parison fall time remains under 0.5 s to avoid sag-induced wall-thickness variation exceeding ±0.1 mm at the bottle shoulder. Terminal pharmaceutical package types include 20 mL to 250 mL round or square high-density polyethylene bottles for oral solid dosage forms, liquid multivitamin preparations, and effervescent tablets with desiccant-loaded closure systems.

    A critical limitation is that terminal sterilization by gamma irradiation above 25 kGy can cause measurable oxidative embrittlement in HDPE, and steam autoclaving at 121 °C is not applicable because the temperature approaches the softening range of the bottle wall. Published data for DMDA6200-specific post-irradiation physical property retention under dose rates above 25 kGy is limited, so each radiation dose must be validated on the finished bottle and closure system rather than extrapolated from unpigmented resin data.

    UN-Certified Industrial Jerrycan Production and Low-Temperature Drop-Test Boundaries

    Industrial jerrican production using DMDA6200 is typically executed on accumulator blow molding machines with hydraulic clamp forces between 120 t and 250 t because the large parison mass and thick pinch-off weld demand high tonnage without mold deformation. The regulatory compliance path for UN-certified industrial containers falls under the UN Model Regulations Rev. 23, 2023 Chapter 6.1 for non-removable-head plastics jerricans, with drop testing conducted at 1.2 m for packaging group II liquids after conditioning at −18 °C, leakproofness testing at 30 kPa over 10 minutes, and hydrostatic pressure testing at 250 kPa for 30 minutes where prescribed. The compounding charge for a 20 L jerrican is 100 parts by weight DMDA6200, carbon black or gray UV masterbatch at 1.0–2.0 wt%, antistatic masterbatch at 0.5–1.0 wt% for lubricating-oil containers, and zero external regrind or PCR unless the molder re-qualifies the entire packaging design under a new UN certification. Melt is prepared in a 90 mm single-screw extruder with an L/D of 28:1 and a grooved feed zone, with barrel temperatures set from 185 °C to 210 °C, an accumulator shot size of 1.5–3.0 L, and a profiled die gap from 2.5 mm to 5.0 mm to compensate for parison swell and localized thinning at the handle pinch-off. Terminal products include 5 L, 10 L, 15 L, 20 L, and 25 L monolayer UN 3H1 jerricans for lubricating oils, fuel additives, antifreeze formulations, and non-classified industrial fluids.

    Pinch-weld integrity, rather than sidewall ductility, is the dominant failure mode in this segment. When mold closing speed is too high or melt temperature falls below 185 °C, the pinch weld can retain micro-voids that open under impact; batch-to-batch variation in die swell also shifts pinch-weld thickness unless parison weight is kept within ±1.5% of the qualified target. ESCR loss in the pinch zone, measured according to ASTM D1693-15 condition B, is the most common root cause of low-temperature drop-test failure in this geometry.

    Across cosmetic and personal-care packaging lines, the controlling material property for DMDA6200 is not tensile yield but environmental stress-crack resistance against emulsified lipid systems, silicone oils, and ester-based fragrance carriers that are common in shampoo and body wash formulations. The relevant packaging compliance framework is EC Regulation No 1223/2009 Article 17 on packaging-material safety, under which the packaging must not cause cosmetic product deterioration or release substances in quantities that exceed the cosmetic safety assessment limits; additionally, heavy-metal limits from 94/62/EC apply to the packaging article. The formulation basis for high-gloss monolayer bottles is 100 parts by weight DMDA6200, pearlescent masterbatch at 1.0–3.0 wt%, translucent color masterbatch at 0.3–1.0 wt%, and clean closed-loop regrind at ≤20 wt% from the same bottle stock, with no silicone oil added to the melt because surface streaks can transfer to the mold and alter gloss retention. Processing is performed on a single-station or double-station shuttle blow molding machine with a 50 mm screw diameter and L/D 24:1, melt temperature controlled between 185 °C and 205 °C, mold temperature held at 12–18 °C, and blow air pressure at 0.5 MPa; the mold cavity is polished to at least SPI A2 finish to reproduce pearlescent flow lines demanded in retail personal-care packaging. Terminal finished parts are 50 mL to 1 L bottles for shampoo, conditioner, body wash, hand soap, and skin lotions, often with matching overcaps that may be compression-molded from a different HDPE grade.

    Fragrance loading imposes another constraint: high levels of limonene or linalool can act as stress-cracking agents in the wall layer, so ESCR validation according to ASTM D1693-15 is required with the final fragrance concentration rather than with an inert simulant. Wall thickness below 0.35 mm in thin-walled personal-care bottles is not recommended with aggressive fragrance systems because the reduced stress-crack resistance shortens shelf life in contact with surfactant-rich formulations.

    When Agricultural Fluid Packaging Requires Barrier Treatment of Monolayer HDPE

    If non-dangerous liquid fertilizer or agricultural adjuvant formulations are filled below 5 L, monolayer HDPE containers based on DMDA6200 can be considered provided the solvent load contains no more than trace xylene, cyclohexanone, or dimethylformamide; otherwise, wall permeability exceeds the shelf-life retention specification and a barrier treatment or co-extruded structure becomes mandatory. The applicable compliance framework for agricultural liquid packaging includes the UN Model Regulations Rev. 23, 2023 for dangerous goods where the formulation is classified, and FAO/WHO pesticide storage and packaging guidance for crop-protection product containers, with drop and permeation testing aligned to the assigned packaging group. The compound charge for a 1 L to 5 L agrochemical bottle is 100 parts by weight DMDA6200, carbon black masterbatch at 1.5–2.5 wt%, HDPE-based UV stabilizer masterbatch at 0.5–1.5 wt%, and high-viscosity blowing aid at 0.02–0.05 parts by weight when thicker parison sections are needed; external regrind is excluded, and internal regrind is limited to ≤10 wt% because the aggressive filled product magnifies stress-crack propagation from regrind-induced gel defects. Production of monolayer containers uses a shuttle blow molding machine with a 60 mm extruder, L/D 24:1, barrel temperatures from 190 °C to 210 °C, mold cooling at 8 °C, and a post-molding leak test at 0.02 MPa; when permeation limits cannot be met in monolayer, the DMDA6200 layer is used as the structural back layer in a co-extruded structure or the formed container is surface-fluorinated in-line under controlled fluorine/nitrogen ratios. Terminal products include 0.5 L to 10 L containers for non-classified liquid foliar fertilizers, soil adjuvants, water-soluble fertilizer concentrates, and certain low-solvent crop protection formulations.

    Fluorination treatment changes the surface polarity and extractables profile of the container, and published data for DMDA6200-specific fluorinated barrier performance under multi-year tropical storage is limited. Permeation validation must therefore be conducted on filled containers with the exact formulation, and monolayer structures without barrier treatment should not be qualified for aromatic or ketonic solvent systems exceeding trace levels.

    Free Quote

    Competitive Sinopec Fujian HDPE DMDA6200 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Fujian HDPE DMDA6200 is specified as a high-molecular-weight, high-density polyethylene extrusion blow moulding resin for large-volume rigid packaging. The product is supplied in pellet form and is normally processed on accumulator-head blow moulding machines or high-output shuttle presses; it is not intended for injection moulding or rotational moulding. The design focus is a combination of high flexural stiffness, controlled melt strength for extended parison hang times, and resistance to environmental stress cracking in industrial and mild chemical service. These properties are not assessed by a single test; they are evaluated through a matrix of resin-level and container-level qualification methods.

    Certifiable values for this exact grade are controlled by the producer’s certificate of analysis and lot-release documentation. Published independent data for Sinopec Fujian HDPE DMDA6200 is limited; therefore the compliance matrix in the following table presents the inspection window for high-molecular-weight HDPE large-part blow moulding feedstocks. The table is not a substitute for the producer’s current technical data sheet or lot-specific values.

    Property or verification requirementStandard or test methodTypical inspection windowUsual verification point
    Melt flow rate, 190 °C, 2.16 kgISO 1133-1:20220.18–0.30 g/10 minIncoming lot QA
    Density at 23 °CISO 1183-1:20190.950–0.956 g/cm³Incoming lot QA
    Tensile stress at yieldISO 527-2:2012, type 1A, 50 mm/min23.0–28.0 MPaPeriodic type test
    Flexural modulusISO 178:2019, 2 mm/min850–1,050 MPaPeriodic type test
    Elongation at breakISO 527-2:2012>400% typical; lower in thick-section skin layersPeriodic type test
    Environmental stress-crack resistance, F50ASTM D1693, condition B, 10% Igepal CO-630, 50 °C>150 h common acceptance floor; some end-user specifications require >600 hPeriodic type test and lot verification for critical packaging
    Notched Charpy impact at 23 °CISO 179-1:2010≥20 kJ/m² or no break; ductile-brittle transition must be verified below -30 °CPeriodic type test
    Vicat softening temperature, A50ISO 306:2022122–128 °CPeriodic type test

    Material Identification and Production-Grade Filing

    The grade designation DMDA6200 is classified in Sinopec Fujian commercial documentation as a virgin high-density polyethylene blow moulding grade. The suffix places it within a high-molecular-weight large-part blow moulding series rather than an injection moulding, film, or pipe extrusion series. The producer does not fully disclose molecular weight distribution, catalyst residue data, or comonomer placement in all markets. When a converter builds an incoming raw-material specification, the normal practise is to take the producer’s lot-specific values for melt flow rate, density, tensile yield stress, flexural modulus and environmental stress-crack resistance and apply an internal trending chart rather than relying on a single published nominal data sheet. The finished container may additionally be filed under packaging codes such as 1H2 non-removable-head plastics drums when the full article is qualified under the UN Recommendations on the Transport of Dangerous Goods, Model Regulations.

    What Rheological Constraints Govern the Use of DMDA6200 in Accumulator-Head Blow Moulding?

    The processing window for DMDA6200 is dominated by a low melt flow rate in the 0.18–0.30 g/10 min range when tested under ISO 1133-1:2022 at 190 °C and 2.16 kg. A melt flow rate in this range indicates a high-molecular-weight resin with high zero-shear viscosity and a relatively long relaxation time. These rheological features increase die swell and parison wall uniformity at long hang times but also raise extruder torque demand. The die gap is usually started at 2.0–3.5 mm for large-part tooling; narrower gaps can increase melt fracture risk at the die lips, while wider gaps can produce visible die lines and a thicker weld-line region. The die melt temperature should be maintained between 190 °C and 210 °C. A measured melt stream below 175 °C is associated with elevated viscosity, localised melt fracture, and increased screw drive load. Sustained melt temperatures above 220 °C are not recommended because long residence time at high temperature can shift the melt flow rate, increase odour potential, and consume the primary antioxidant package.

    On a 90 mm single-screw extruder with 30:1 L/D barrier screw and grooved feed section, comparable high-molecular-weight HDPE blow moulding grades in this MFR band typically produce head pressures of 18–35 MPa at screw speeds from 55 rpm to 75 rpm. This pressure range is a diagnostic starting window, not a certified property of DMDA6200. If the extruder drive approaches its ampere limit before the target plastication rate is reached, the preferred corrective action is to reduce screw speed or increase feed stability; raising barrel set points above 220 °C to lower viscosity is not a safe substitute because it can alter the melt flow rate and reduce stress-crack resistance. During changeover from a lower-viscosity HDPE, the accumulator head and adaptor should be purged until the melt pressure stabilises. Short purging can leave low-viscosity residual material in the head, causing variable parison sag and inconsistent wall distribution on the first production cycles.

    On accumulator-head lines producing 200 L tight-head drums, parison programming is used to compensate for sag when unprogrammed hang time exceeds 10–15 s. The upper section of the parison generally requires 5–10% additional wall thickness relative to the lower section. A circumferential melt temperature variation greater than 5 °C across the die can produce parison curl and wall-thickness asymmetry. Clamp force for such drum tooling is typically specified in the 600–1,200 kN class, although the exact value depends on the number of cavities, part geometry and cooling configuration. Weld-line strength at the pinch-off must be verified on the finished container by drop impact or hydrostatic pressure testing; a resin-level tensile test under ISO 527-2:2012 does not quantify pinch-off fusion quality or weld-line contamination.

    Resin-level lot-to-lot variation also affects large-part processing. When the melt flow rate shifts within the 0.18–0.30 g/10 min window, part weight and parison length can change; therefore incoming lots are trended against accumulated head pressure and cycle time. A shift of 0.02 g/10 min within the specification band is often visible as a part-weight change on a 200 L drum line even though it is not a certificate-level failure. Field reports from large-part lines indicate that the dominant processing defects are parison curl due to die temperature asymmetry, weld-line cracking from low pinch pressure, and inner surface roughness from moisture. None of these defects is caused by melt flow rate alone.

    Large-Volume Containers and Industrial Packaging Stress-Cracking Resistance

    When the material is used in 200 L non-removable-head drums, environmental stress cracking is the main long-term failure mode under stack load and chemical exposure. The typical ESCR acceptance floor is F50 > 150 h under ASTM D1693 condition B, 10% Igepal CO-630, at 50 °C; more demanding end-user specifications may set F50 > 600 h. These values are container-lot acceptance thresholds, not universal producer guarantees. For drop impact, filled drum qualification is commonly performed after conditioning at -18 °C for 24 h using a drop height of 1.2 m or 1.5 m depending on the packaging group. The test is a container-level assessment and cannot be replaced by resin-level Charpy impact or tensile data.

    In intermediate bulk container inner bottles, weld-line integrity at the top and bottom pinch-off is often more important than the tensile yield stress of the resin. A feedstock with acceptable ESCR can still fail in service if the pinch-off is cold or contaminated; therefore incoming resin is not qualified by melt flow rate and density alone. Coupon immersion under ASTM D543 provides a comparative chemical resistance ranking for screening, but final approval for aggressive fillings requires warehouse-scale storage in the actual container at 40 °C for at least 21 days. Strong oxidising acids and surfactant/oxygenate mixtures can shorten stress-crack life; such fillings require container-level chemical compatibility testing before field release.

    Food-contact use of DMDA6200 must be confirmed in the finished article rather than the pellet alone. Polyethylene produced under appropriate good manufacturing practise may be evaluated against FDA 21 CFR 177.1520 and EU 10/2011/EC; migration testing is required with the actual filling and temperature because the pellet may comply while the finished container additive package, regrind content, or colour masterbatch does not.

    When the Grade Is Compared Against General-Purpose HDPE Extrusion Materials

    Compared with a general-purpose injection moulding HDPE having an MFR of 6–20 g/10 min, DMDA6200 is not a flow-optimised grade. The low MFR reduces spiral flow length and increases injection pressure requirement; injection moulding is not a specified use. In extrusion blow moulding, the same high-molecular-weight architecture reduces parison sag across the extended hang times associated with 200 L drums and large industrial containers. A converter moving from a conventional 0.4 g/10 min blow moulding grade to DMDA6200 should expect higher extruder torque demand or a 5–15% reduction in screw speed for the same plastication rate. This is a rheological difference rather than a density-driven effect.

    Relative to high-density polyethylene grades designed for thin-wall consumer bottles, DMDA6200 is positioned for large-part tooling where the ratio of wall thickness to part length is higher and the critical weld-line stress is driven by low-speed drop impact and hydrostatic pressure rather than high-speed tensile failure. Differences in additive package also matter. If masterbatch addition exceeds 2.0%, the converter should re-verify ESCR under ASTM D1693 and weld-line impact at production wall thickness, because carrier resins and pigments can reduce stress-crack resistance or shift the density outside the specified 0.950–0.956 g/cm³ window.

    Storage and handling boundaries follow standard high-density polyethylene pellet practise. The material should be kept in a closed silo or hopper at ambient temperature below 50 °C and protected from prolonged ultraviolet exposure, which can reduce the surface stress-crack resistance of the finished container. When pellets are transferred from cold storage and the ambient relative humidity exceeds 60%, condensation drying at 70–80 °C for 2 h is used to prevent surface moisture defects. Regrind use in large-part blow moulding is common, but regrind levels above 20% should be tested for ESCR retention under ASTM D1693 and for density shift beyond 0.956 g/cm³. The resin should not be blended with incompatible polypropylene regrind or with unapproved amine-based additive concentrates unless the final container qualification demonstrates no loss in weld-line toughness or stress-crack resistance.

    Top