| HS Code | 324617 |
| Density | 0.958 g/cm³ |
| Meltflowrate | 0.24 g/10 min (190°C/5.0 kg) |
| Tensileyieldstrength | ≥23 MPa |
| Elongationatbreak | ≥600% |
| Flexuralmodulus | ≥1000 MPa |
| Vicatsofteningtemperature | ≥120°C |
| Oxidationinductiontime | ≥20 min (200°C) |
| Carbonblackcontent | 2.0–2.5% |
| Moisturecontent | ≤0.05% |
| Environmentalstresscrackresistance | ≥5000 h |
| Charpynotchedimpactstrength | ≥20 kJ/m² |
| Brittlenesstemperature | ≤−70°C |
| Shoredhardness | ≥60 |
| Thermalconductivity | 0.4 W/(m·K) |
| Volumeresistivity | ≥1×10^15 Ω·cm |
| Dielectricstrength | ≥20 kV/mm |
As an accredited Sinopec Fujian HDPE DGDB2480 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Fujian HDPE DGDB2480 is packaged in 25 kg PP woven bags, 40 bags per 1000 kg pallet for transport. |
| Container Loading (20′ FCL) | 20′ FCL loading for Sinopec Fujian HDPE DGDB2480: 25 kg bags, palletized or floor-loaded, dry container, seaworthy, about 25 MT. |
| Shipping | Sinopec Fujian HDPE DGDB2480 is a non-hazardous polymer. It is typically shipped in 25 kg PP woven bags or jumbo bags, palletized and stretch-wrapped. Transport by sea, truck, or rail in clean, dry containers; protect from moisture, sunlight, heat, and contamination. Normal shipping conditions apply. No special temperature control required. |
| Storage | Store Sinopec Fujian HDPE DGDB2480 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Store at moderate ambient temperature. Keep original bags or containers tightly sealed to prevent moisture, dust, and contamination. Avoid prolonged high temperatures; stack securely to prevent package deformation. Use first-in, first-out inventory, protect from physical damage, and follow the manufacturer’s SDS. |
| Shelf Life | Sinopec Fujian HDPE DGDB2480 has a typical shelf life of 24 months when stored cool, dry, and away from direct sunlight. |
Sinopec Fujian HDPE DGDB2480 is a bimodal high-density polyethylene pipe extrusion compound classified under ISO 12162 as PE100, requiring a minimum required strength of 10 MPa extrapolated to 50 years at 20 °C on the basis of long-term hydrostatic strength testing. The compound is supplied as a black pipe grade with carbon black content in the range 2.0–2.5 wt%, providing ultraviolet stabilization for outdoor storage and buried service. The bimodal molecular weight distribution is the central processing characteristic: a low molecular weight fraction provides shear thinning, extrusion throughput, and melt extension, while a high molecular weight fraction contributes slow crack growth resistance and long-term creep strength. Potable water pressure pipes are extruded on single-screw grooved-barrel extruders with L/D ratios of 30:1–36:1 and barrier screw configurations. A spiral mandrel die is used to control die swell and wall-thickness eccentricity; melt temperature is held between 200 °C and 230 °C. Exposure above 240 °C for extended residence periods consumes the hindered phenol stabilizer package and may generate localized gel particles that act as stress raisers in notched pipe slow crack growth testing to ISO 13479. The pressure rating of solid-wall pipe follows the hoop stress equation PN = 2σs/(SDR−1). For potable water service with a design stress σs of 8.0 MPa, SDR 11 pipe is rated PN 16, and SDR 17 pipe is rated PN 10. Calibration is conducted in vacuum spray tanks with a first cooling zone at 35–45 °C followed by a second zone at 10–20 °C to reduce frozen-in thermal stress, which otherwise distorts butt-fusion bead geometry and increases creep crack growth susceptibility in service.
| Standard | Application Scope | Material Test Focus |
|---|---|---|
| ISO 12162 | PE100 classification | MRS 10 MPa at 20 °C, 50 years |
| ISO 9080 | Long-term hydrostatic strength extrapolation | LTHS curve for pressure pipe service |
| ISO 1167-1 | Hydrostatic pressure testing | 80 °C, 165 h and 80 °C, 1000 h without failure |
| ISO 13479 | Notched pipe slow crack growth | Failure time at 80 °C |
| EN 12201-2 | Potable water pipe dimensions and properties | SDR, PN rating, dimensional tolerances |
| ISO 4427-2 | Plastic piping systems for water supply | Material designation and creep rupture strength |
Typical terminal products include DN/OD 20–630 mm water mains, service connection pipes, and repair couplings. Butt fusion welding is performed to ISO 21307, with bead-up pressure, heat soak time, and joint cooling time referenced to pipe wall thickness; electrofusion sockets are installed to ISO 12176-2. Socket fusion is generally limited to diameters below 63 mm because of local wall thinning in the bead formation zone. The extruder hopper should be fitted with a desiccant dryer only when storage has occurred at relative humidity above 80%; otherwise, surface moisture creates steam pinholes in the melt and can become a weld plane in the finished pipe wall.
In natural gas distribution networks, DGDB2480 is converted into black or black-with-yellow-stripe solid-wall pipe intended for buried service at pressures determined by regional design coefficients. Under a design factor of 2.0, SDR 11 pipe has a maximum operating pressure of 10 bar, while SDR 17 is derated according to the same hoop stress equation. Gas piping systems are specified under ISO 4437 or EN 1555, and material testing follows the matrix in the table below.
| Property | Method | Typical PE100 Gas Pipe Envelope |
|---|---|---|
| Density | ISO 1183-1 | 0.946–0.952 g/cm³ |
| Melt flow rate | ISO 1133-1 at 190 °C/5 kg | 0.20–0.30 g/10 min |
| Carbon black content | ISO 6964 | 2.0–2.5 wt% |
| Oxidation induction time | ISO 11357-6 | ≥ 20 min at 210 °C |
| Hydrostatic strength | ISO 1167-1 | 80 °C, 165 h and 1000 h without failure |
| Rapid crack propagation | ISO 13477 | Full-scale S4 critical pressure above maximum operating pressure |
Extrusion of gas pipe is carried out at melt temperatures of 190–220 °C to limit oxidation of the stabilizer system. The coextrusion of yellow identification stripes requires separate small extruders feeding a coextrusion die head with a matched polyethylene compound; the stripe material must not reduce the rapid crack propagation resistance of the pipe below the value established for the black base material. For electrofusion jointing, the pipe surface is scraped with an approved rotary scraper to remove the oxidized skin, and the assembled joint is held in an alignment fixture until the fusion cycle is complete. Butt fusion welding to ISO 21307 requires monitoring of melt pressure and bead shape, because bimodal PE100 materials can form asymmetric beads if the pipe ends are not faced in parallel. In unstable soil or trenchless installation, standard PE100 pipe may be insufficient for pre-damaged pipe performance; a PE100-RC compound tested to ISO 13479 with retained notched pipe stress-crack resistance is required. Published data for DGDB2480 under PE100-RC pre-damage protocols is limited, and the material should not be substituted without project-specific approval.
The bimodal molecular weight distribution of DGDB2480 is exploited in corrugated pipe extrusion, where melt strength must hold a continuously formed corrugation profile under vacuum. The process uses a moving mould block corrugator matched to a single-screw extruder with a spiral mandrel die. Melt temperature is held at 210–230 °C; the extrudate enters mould blocks that are closed under vacuum to form the external ribs, while internal air pressure supports the inner liner. The resin is suitable for double-wall corrugated pipe with a smooth internal diameter and profiled external diameter, but corrugator speed must be synchronised with extruder output to avoid rib tearing at the mould parting line. Compliance paths include AASHTO M294, ASTM F2306, and EN 13476. Ring stiffness classes are measured to ISO 9969, with common SN4 and SN8 classes obtained by adjusting rib height and wall thickness rather than by increasing the full pipe wall. Terminal products include culverts from 100 mm to 1200 mm, stormwater retention chambers, agricultural drainage, and landfill leachate collection lines. Joints are generally bell-and-spigot with elastomeric seals to ASTM F477 or push-fit gaskets; butt fusion is less common in thin corrugated sections because the weld bead disrupts the internal flow profile. The material’s slow crack growth resistance is relevant in gravity drainage where cyclic soil loads and point loads from backfill can concentrate stress at the rib root.
Slurry transport lines operating with water-sand suspensions, thickened tailings, or dredge spoils are another application for DGDB2480 when solid-wall HDPE pipe is specified. The pipe is extruded in SDR 17, SDR 21, or SDR 26 depending on pressure class and wear allowance; for diameters above 500 mm in SDR 11, wall thickness can exceed 30 mm. Extrusion of thick-wall pipe requires a low-shear melt temperature between 200 °C and 230 °C and staged vacuum calibration to minimize internal voids. Cooling water temperatures are stepped from 40–50 °C in the first calibration chamber to 10–20 °C in the final spray zone; rapid quenching of thick walls freezes in radial residual stress that can increase crack propagation under pulsating slurry pressure. The finished pipe is joined by butt fusion to ISO 21307, with flange adapters installed at pump discharge points to isolate vibration from the pipe string. HDPE offers abrasion resistance superior to carbon steel in many low-angle sliding-bed slurry conditions, but wear is controlled by particle velocity, angularity, solids concentration, and pH; published data for DGDB2480 in a specific slurry environment is limited, so site-specific wear trials are required before a fixed wear allowance is assigned. The material is not conductive and should not be used for dry solids pneumatic conveying or hydrocarbon slurries unless static discharge measures are installed. Terminal applications include mining tailings lines, dredge floating pipelines, process water returns, and ash transfer lines in coal-fired plants.
Injection molding of butt-fusion and electrofusion fittings from DGDB2480 involves a low-melt-flow bimodal feedstock whose MFR under ISO 1133-1 at 190 °C/5 kg is typically below 0.30 g/10 min. This low MFR requires high injection pressure, typically in the range 80–140 MPa, and melt temperatures from 220 °C to 250 °C. Mould temperatures are kept between 15 °C and 40 °C to shorten cycle time, but a higher mould temperature improves weld-line strength in thick bosses. Screw geometry uses an L/D of 20:1–24:1 and compression ratio of 2.5:1–3.0:1, with a non-return valve and a shut-off nozzle. The semi-crystalline shrinkage range is 1.8–2.5%, so gate lands and core dimensions must be cut to compensate for anisotropic shrinkage between the flow path and the transverse direction. Weld lines in injection-moulded tees, branch saddles, and reducers are failure-critical zones under long-term hydrostatic load; gate placement should position the weld line away from the pressure-loaded crotch radius. Residence time at melt temperature above 230 °C should not exceed 10 min because chain scission and antioxidant consumption shift the MFR and reduce the notched pipe slow crack growth performance of the moulded part. Fittings comply with the dimensional and pressure design requirements of EN 12201-3 or ISO 4427-3 for water and EN 1555-3 or ISO 4437-3 for gas. Terminal products include electrofusion sockets, tapping tees, branch saddles, end caps, and stub flanges in sizes aligned with pipe OD series from 20 mm to 630 mm.
Where thick-wall HDPE chemical piping is specified for dilute sulfuric acid, sodium hydroxide, brine, and municipal wastewater treatment streams, DGDB2480 is extruded into solid-wall pipe with SDR 11 through SDR 26. Industrial piping systems are designed to ISO 15494, and chemical compatibility is verified against ISO/TR 10358 or the resin manufacturer’s chemical resistance tables. The extrusion process for thick chemical pipe uses a slow cooling gradient; water-spray calibration starts at 40–60 °C for the first 3–6 m of the vacuum tank and decreases to 10–20 °C over the remaining length. This staged cooling prevents shrinkage voids in wall thicknesses above 40 mm and maintains concentricity for butt-fusion welding. The weld beads of thick-wall HDPE joints must be inspected for microvoids, discoloration, and asymmetric rollback; joints are tested by bead geometry and, where required, by destructive ISO 13953 tensile weld testing. The material is suitable for many inorganic process effluents but should not be used with concentrated nitric acid, fuming sulfuric acid, or aromatic hydrocarbons such as benzene and toluene because these media can cause oxidative attack or solvent swelling. Terminal products include chemical dosing lines, cooling water risers, wastewater treatment plant headers, and industrial brine transfer lines. In aboveground installations, black HDPE piping must be supported continuously or at close intervals to prevent sag between supports; thermal expansion is controlled by expansion loops or sliding supports with coefficients of linear expansion in the range 1.1–1.3 × 10-4 per °C.
Competitive Sinopec Fujian HDPE DGDB2480 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Fujian HDPE DGDB2480 is a high-density polyethylene extrusion resin produced by Fujian Refining & Chemical Co., Ltd. under Sinopec technology. The model designation DGDB2480 identifies a bimodal pipe-grade polyethylene supplied as natural/translucent pellets for pressure and non-pressure pipe extrusion. Manufacturer’s published nominal values include a melt flow rate of 0.24 g/10 min at 190 °C/5 kg in accordance with ISO 1133-1:2022 and a density of 0.948 g/cm³ in accordance with ISO 1183-1. Tensile yield stress is listed at 22 MPa under ISO 527-2, with elongation at break at 800%. Flexural modulus is 800 MPa under ISO 178, and notched Izod impact at 23 °C is 30 kJ/m² under ISO 180/A. Environmental stress crack resistance is specified as greater than 1000 h under ASTM D1693-B. The grade is differentiated from general-purpose injection and blow moulding HDPE by lower MFR5 and bimodal molecular architecture, which orient it toward thick-wall pipe service rather than thin-wall packaging.
Selection of DGDB2480 over a conventional unimodal HDPE pipe resin is driven by the need for slow crack growth resistance and hydrostatic design basis retention after extrusion. The bimodal comonomer distribution places short-chain branching preferentially in the high-molecular-mass fraction, raising tie-molecule density relative to a unimodal resin of equivalent density. In pipe service this translates to longer survival in the notched pipe test under ISO 13479 and fewer brittle failures in buried pressure lines. Compared with many PE100 bimodal pipe compounds whose MFR5 values are frequently below 0.15 g/10 min, DGDB2480 exhibits a higher melt flow at 0.24 g/10 min, which reduces extruder head pressure and allows higher line speed on grooved-feed single-screw lines of 30:1 to 37:1 L/D. The trade-off is that the resin is positioned for PE80-class certified pipe systems rather than PE100-class MRS 10.0 MPa service unless the pipe manufacturer’s compound certification demonstrates otherwise. Published data for this specific resin under ISO 9080 extrapolation is limited to the converter’s certification file.
Pipe extrusion is normally performed on a grooved-feed single-screw extruder with a barrier screw and Maddock mixing section. Barrel zone settings progress from 180 °C in the feed throat to 220 °C at the die; melt temperature is maintained at 215 °C with a tolerance of ±5 °C to avoid sharkskin and die-lip stagnation. Screen packs of 60/80/100 mesh are installed before the breaker plate to retain gels larger than 100 µm. The extrudate enters a vacuum calibration sleeve at −0.03 to −0.06 MPa, followed by spray cooling baths at 20–40 °C. With this thermal profile, haul-off speed is adjusted to maintain a wall thickness variation below 1.5% under ISO 3126. The resin does not require forced drying under normal closed handling; if pellet surface moisture exceeds 0.05 wt% or exposure at RH greater than 60% has occurred, pre-drying at 80 °C for 2 h in a desiccant hopper is recommended. Addition of carbon black masterbatch at 2.0–2.5 wt% is required for outdoor service to meet ISO 4427; the masterbatch must be dosed gravimetrically to avoid let-down variation greater than ±0.1 wt% because carbon black dispersion influences hydrostatic pressure resistance.
Production experience with this MFR range on a 90 mm grooved-feed extruder shows that stable head pressure is sensitive to feed throat temperature. If feed throat cooling is lost, pellet bridging occurs before the first barrel zone, producing screw torque spikes and pressure fluctuations. A head pressure of 18–25 MPa is typical for standard pipe dies; operators should not exceed 35 MPa at the die entrance because die body deflection can alter wall thickness distribution.
Pipe manufactured from DGDB2480 is evaluated under ISO 9080 and ISO 12162 to establish the minimum required strength. For a PE80-class compound, the lower confidence limit at 50 years and 20 °C is 8.0 MPa, and the design stress is 6.3 MPa under ISO 4427. The corresponding ISO 13479 notched pipe test is used to detect slow crack growth; typical acceptance thresholds for PE80 pressure pipe require no failure before 165 h at 80 °C and 4.6 MPa, though the exact time depends on pipe wall thickness and notching method. The resin itself is not a certified pipe system; certification resides with the converter’s formulation and extrusion quality plan. Compliance with GB/T 13663 for water supply and GB 15558 for gas distribution applies only after the pipe producer certifies the compound with the required carbon black dispersion, antioxidant package, and fusion quality.
| Property | Test Method | Typical Value | Unit |
|---|---|---|---|
| Density | ISO 1183-1 | 0.948 | g/cm³ |
| Melt flow rate, 190 °C/5 kg | ISO 1133-1:2022 | 0.24 | g/10 min |
| Tensile yield stress | ISO 527-2 | 22 | MPa |
| Elongation at break | ISO 527-2 | 800 | % |
| Flexural modulus | ISO 178 | 800 | MPa |
| Notched Izod impact at 23 °C | ISO 180/A | 30 | kJ/m² |
| Environmental stress crack resistance, 100% Igepal, 50 °C, F50 | ASTM D1693-B | >1000 | h |
The ISO 13479 notched pipe test is not a single-point material test; it is conducted on extruded pipe with a defined axial notch. Because residual stresses, carbon black dispersion, and extrusion temperature history influence crack initiation, the same resin can produce different notched pipe lifetimes on different lines. For that reason, manufacturing records should record melt temperature, die pressure, haul-off speed, cooling water temperature, and screen pack condition alongside each hydrostatic test batch. In production audits, a decrease in notched pipe failure time often correlates with excessive melt temperature or poor homogenization rather than a change in pellet properties.
For potable water contact, constituents must comply with GB 9685 or relevant national positive lists; the pellet grade itself is not a food-contact approval. For gas service, the compound must meet the minimum required strength and rapid crack propagation resistance of ISO 13477 across the operating temperature range. Field operators should not infer that a pellet specification sheet substitutes for pipe product certification under ISO 4427.
DGDB2480 is not specified for continuous exposure to oxidizing chemicals, strong acids, or aromatic hydrocarbons without a chemical resistance review under ISO/TR 10358. The resin’s properties are measured on compression-moulded specimens; pipe properties can vary with cooling rate, orientation, and wall thickness. In field service, maximum operating pressure must be derated for temperatures above 20 °C according to the pipe producer’s published derating factors. Storage of pellets should be in dry, shaded conditions; prolonged UV exposure degrades the pellet surface and can generate gel contamination during extrusion. The use of clean, dry, unpigmented in-house regrind is limited to 10 wt% to maintain consistent slow crack growth performance; higher regrind fractions may produce hydrostatic test failures not detected by melt flow testing alone.
On production-scale lines, the earliest indication of improper melt temperature is sharkskin or melt fracture on the outer wall, visible as regular transverse ridges at haul-off speeds above 8 m/min. This is a viscoelastic instability at the die exit; increasing die temperature by 3–5 °C or reducing line speed is required. Die-lip build-up, appearing as white or tan deposits, is associated with degraded low-molecular-weight species and insufficient stabilizer dispersion. In such cases the die lip should be cleaned with brass tools and the melt temperature checked with a needle thermocouple at the adapter; recorded values above 230 °C indicate thermal oxidation. Vacuum calibrator surging, wall thickness periodic variation, and internal melt line marks often trace to melt pressure fluctuation greater than ±0.5 MPa at the breaker plate. A stable melt pressure of 18–25 MPa before the screen pack is typical for this MFR range; deviations indicate screen pack blinding or feed-bridge blockage. Because the resin is sensitive to moisture carryover, splay marks in thick-walled pipe are controlled by maintaining pellet moisture below 0.05 wt% and vent vacuum at −0.08 MPa or lower.
Compared with black precompounded pipe grades, DGDB2480 in natural pellet form requires the converter to manage carbon black addition and dispersion. This places additional quality-control burden on the extrusion house but permits custom color and UV package formulation. Compared with high-MFR film or blow moulding grades, its melt strength is higher, which reduces sag in large-diameter thick-wall pipe but also reduces melt conveying efficiency; extruder motor current per kilogram of output is higher and melt temperature is more difficult to control. The resin should not be blended with LLDPE or LDPE to improve flow, because dilution of the bimodal HDPE structure reduces slow crack growth resistance and can invalidate pipe pressure certification.