    Specifications
    HS Code 503303
    Density G Cm3 0.954
    Melt Index 190c 2 16kg G 10min 0.70
    Tensile Yield Strength Mpa ≥26
    Elongation At Break Percent ≥600
    Flexural Modulus Mpa ≥1100
    Vicat Softening Temperature C ≥120
    Brittle Temperature C ≤-70
    Environmental Stress Cracking Resistance H ≥1000
    Shore D Hardness ≥60
    Melting Point C 130
    Water Absorption Percent <0.01
    Volume Resistivity Ohm Cm >1×10^16
    Dielectric Constant 2.3
    Bulk Density G Cm3 ≥0.55

    As an accredited Sinopec Fujian HDPE DGDA6097 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Fujian HDPE DGDA6097 is packaged in 25 kg polyethylene-lined woven bags, typically palletized for industrial shipment.
    Container Loading (20′ FCL) Sinopec Fujian HDPE DGDA6097 in 25kg bags, 20′ FCL container loading, approx. 17–18MT, non-hazardous, suitable for export.
    Shipping Sinopec Fujian HDPE DGDA6097 is shipped as a non-hazardous thermoplastic, typically in 25 kg PP woven bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry vehicles. Keep away from moisture, heat, sunlight, and ignition sources. Store in a cool, ventilated warehouse. Protect from contamination.
    Storage Store Sinopec Fujian HDPE DGDA6097 in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, heat, and ignition sources. Keep original bags sealed, palletized, and off the floor to prevent moisture pickup. Avoid contact with oils, chemicals, and prolonged UV exposure. Use first-in-first-out rotation, observe safe stacking limits, and maintain good housekeeping. Protect from physical damage and contamination.
    Shelf Life Sinopec Fujian HDPE DGDA6097 typically has a 24-month shelf life when stored dry, cool, ventilated, and away from direct sunlight.
    Application of Sinopec Fujian HDPE DGDA6097

    Why High-Stalk Bubble Geometry Is Preferred for Thin-Gauge Retail Bags

    At gauge targets between 8 µm and 18 µm, high-density polyethylene blown film stability is controlled primarily by the distance from the die lip to the frost line. The high-stalk configuration, with a neck height of 6 to 9 die diameters, is selected for Sinopec Fujian HDPE DGDA6097 because it permits the melt to strain-harden before expansion and reduces the likelihood of draw resonance at blow-up ratios of 3.5:1 to 4.5:1. On monolayer lines constructed with 45 mm to 65 mm grooved-feed extruders and L/D ratios from 24:1 to 30:1, the melt temperature at the die adapter is normally held between 210 °C and 230 °C. The die gap is set at 0.8 mm to 1.2 mm because a wider gap at this gauge encourages excessive transverse direction orientation and produces film with lower handle tear resistance. Dual-lip air ring cooling is preferred over single-lip cooling at outputs above 0.8 kg/h per millimetre of die circumference, and internal bubble cooling is added when die diameters exceed 200 mm. The principal failure mode in this process is not bubble burst but cyclic gauge-band formation: local die lip temperature differences greater than 5 °C generate alternate thick and thin bands that become visible after gusseting and block separation on high-speed bag machines. Finished retail carrier film is tested under ASTM D1709-16a, Method A, for dart impact, and under ISO 527-3:2018 for tensile properties. Elongation at break below 350 % in the transverse direction is usually rejected because it produces handle splitting when the vest-style bag is loaded.

    Formulation for this segment is kept intentionally simple. Typical mixtures contain 100 wt% DGDA6097, plus 0.5 wt% to 1.5 wt% silica-based antiblock masterbatch and 0.2 wt% to 0.5 wt% erucamide slip concentrate. Adding more than 2 wt% low-density polyethylene to soften the film lowers melt tension enough to force lower blow-up ratios and changes the high-stalk bubble from a tall neck to a less stable low-stalk geometry. The end product is a die-cut or heat-sealed vest carrier bag in the 10 µm to 15 µm range after conversion. Storage before dart impact testing must be performed at 23 °C ± 2 °C for at least 24 h because polyethylene impact strength is sensitive to conditioning temperature and strain rate.

    Dry food liner extrusion with DGDA6097 is governed by organoleptic neutrality rather than film toughness. Cereal, cracker, and powdered beverage liners are typically converted at melt temperatures no higher than 220 °C because oxidised low-molecular-weight fractions generated in the barrel can transfer taste and odour to packaged food even when the base resin meets compositional requirements. The olefin polymer is covered under FDA 21 CFR 177.1520(c) as an olefin homopolymer, and the finished food-contact film must also satisfy the overall migration limit of 10 mg/dm² in Commission Regulation (EU) No 10/2011 when tested with food simulants assigned to the intended food type. For dry cereal liners, the common converter specification is a film gauge of 25 µm to 50 µm, haze below 15 % under ASTM D1003-21, and gloss above 60 GU at a 60° measurement angle. Because DGDA6097 is a high-molecular-weight film grade, gel formation is aggravated by dead spots in screen changers and by residence times above 230 °C. The recommended conversion practice is to use a continuous screen changer rather than a manual breaker plate, and to purge for 15 min to 30 min after any shutdown that exceeds 3 h. The primary end products are heat-sealed inner liners for bag-in-box dry food packaging and block-bottom liners for dry pet food. On horizontal form-fill-seal machines, jaw temperatures between 140 °C and 160 °C are generally required to achieve hermetic seals at production speed without burn-through at seal corners.

    Heavy-Duty Industrial Liners and the Dart Impact Trade-Off

    Construction debris sacks and chemical drum liners in the 50 µm to 80 µm range expose a direct trade-off between dart impact and secant modulus. Blending 10 wt% to 25 wt% of an octene-based mLLDPE with a melt index near 1.0 g/10 min before the feed throat raises dart impact measured under ASTM D1709-16a, Method B, but reduces stiffness measured under ISO 527-3:2018. On a blown film line using a 75 mm grooved-feed extruder with 28:1 L/D and a 250 mm die, the die gap is increased to 1.5 mm to 2.0 mm to reduce orientation of the high-molecular-weight fraction and preserve machine-direction Elmendorf tear strength under ASTM D1922-15. A blow-up ratio below 3.0:1 is selected to shift orientation toward the machine direction; this improves bottom-seal bag making but lowers transverse direction dart impact. Frost line height is maintained between 7 and 9 die diameters because a lower frost line raises bubble instability when the blend contains a low-viscosity mLLDPE fraction. The processing window is narrower than in single-component HDPE film: a melt temperature above 225 °C reduces bubble stability, while a melt temperature below 200 °C raises extruder backpressure and increases the chance of melt fracture at the die lip.

    Conversion variableThin-gauge retail bagDry food linerHeavy-duty industrial liner
    Melt temperature210 °C to 230 °C190 °C to 220 °C200 °C to 225 °C
    Die gap0.8 mm to 1.2 mm1.0 mm to 1.4 mm1.5 mm to 2.0 mm
    Blow-up ratio3.5:1 to 4.5:12.5:1 to 3.5:12.5:1 to 3.2:1
    Film gauge8 µm to 18 µm25 µm to 50 µm50 µm to 80 µm
    Key testASTM D1709-16aASTM D1003-21ASTM D1693-15

    Environmental stress cracking resistance is tested under ASTM D1693-15, Condition B, in 10 % Igepal CO-630 at 50 °C. Liners intended for agricultural chemical intermediates often require failure time above 500 h. Published data for the exact DGDA6097/mLLDPE blend at these thicknesses is limited, so converter trials must verify the drop in dart impact at low storage temperatures. In cold-climate service, the minimum handling temperature is typically set at 0 °C unless the film is qualified by ISO 8570:1998 puncture resistance at the intended service temperature. The end products are self-standing construction waste sacks, drum liners, and heavy-gauge shipbuilding lay-up films; each requires a different antiblock package because the coefficient of friction under ISO 8295:2004 must be adjusted for either manual opening or automated bag insertion.

    Bulk rice, salt, and mineral fertilizer sacks assembled from woven polypropylene use a blown HDPE inner ply of 30 µm to 50 µm to provide moisture resistance and clean discharge. The film is produced from DGDA6097 at a blow-up ratio of 3.0:1 to 3.5:1, with a die gap of 1.0 mm to 1.4 mm, to keep the coefficient of friction low enough for automated bag filling. Where the liner is pre-sealed into a tube, seal strength is measured under ASTM F88/F88M-21. The critical processing constraint is thickness uniformity: gauge variation greater than ±8 % across the web causes the inner ply to bridge or fold during lamination, and pinholes appear after the filled sack is dropped. Drop testing follows ISO 7965-1:2022 at a mass selected by the converter, while tear resistance is assessed by ASTM D1922-15. Because the woven outer fabric carries most of the tensile load, the HDPE film does not need to retain high machine-direction stiffness, but it must resist flex cracking during repeated handling. The Gelbo flex test under ASTM F392/F392M-21 is frequently specified for 1000 cycles, with a post-flex pinhole count below 5 holes per 300 cm².

    Compliance for this segment is determined by the filled product rather than the film alone. Packaging for food-grade rice and salt must use film that meets FDA 21 CFR 177.1520(c) or China GB 4806.7-2016, while packaging for chemical fertilizers falls under national transport and safety regulations. Heavy metals in the packaging material are limited to 100 mg/kg total for lead, cadmium, mercury and hexavalent chromium under EU 94/62/EC. The laminate structure also requires an adhesive or extrusion coating layer between the woven fabric and the HDPE film; without adequate adhesion the inner ply can delaminate during moisture expansion of the fill.

    Regulation/standardApplication contextCritical requirementTest method reference
    FDA 21 CFR 177.1520(c)Dry food linersOlefin homopolymer; migration covered by end-use testingFood simulant exposure
    Commission Regulation (EU) No 10/2011Plastic food contact materialsOverall migration ≤ 10 mg/dm²EN 1186-1:2002
    EU 94/62/ECPackaging and packaging wasteSum of lead, cadmium, mercury and hexavalent chromium ≤ 100 mg/kgAcid digestion and ICP-OES
    ASTM F88/F88M-21Sealed inner plies and pouchesSeal strength at specified jaw temperatureASTM F88/F88M-21

    When Three-Layer Coextrusion Positions DGDA6097 as the Stiff Core

    Multi-layer film for dry pet food pouches and bag-in-box beverage liners uses DGDA6097 as a 10 µm to 25 µm core layer between LLDPE or LDPE skin layers. The objective is to increase the secant modulus of the total film without moving the sealing layer to a higher initiation temperature. The core layer is extruded at a melt temperature of 210 °C to 230 °C, while the skin layers are usually run 10 °C to 15 °C lower to limit surface oxidation. A three-layer die with adjustable layer distribution is required; the core proportion is kept between 30 wt% and 50 wt% of total film mass. If the core layer exceeds 50 wt%, the film loses puncture resistance and the heat-seal strength under ASTM F88/F88M-21 declines because the high-modulus layer reduces deformation at the sealing interface. Film blocking between layers is controlled by adding 0.3 wt% to 0.8 wt% of silica or talc antiblock to the skin layers only; adding antiblock to the core increases haze without improving blocking. The end structure is often printed and laminated to PET or BOPP, so film surface tension must be maintained above 38 mN/m before corona treatment, with treated retention above 38 mN/m for at least 30 days under controlled storage.

    The main process risk in this structure is interfacial instability between the core and skin layers when the viscosity ratio is too high. If the skin resin has a melt index more than 1.5 g/10 min above the core resin, flow disturbance inside the feedblock can produce wavy interlayers and visible optical defects. Layer thickness measurement after the die is performed on pressed cross-sections under optical microscopy, and the total film gauge is monitored with a scanning capacitance gauge to maintain a variance below ±5 %. Puncture resistance of the final structure is measured under ISO 7765-1:1988, and tear resistance under ASTM D1922-15.

    Deadfold Retention Drops at Blow-Up Ratios Above 3.0:1

    Courier envelopes, document sleeves, and map sleeves require film that retains crease memory after folding. The high modulus of DGDA6097 contributes deadfold, but the blown film process must avoid excessive transverse orientation. A blow-up ratio of 2.5:1 to 3.2:1 is selected, combined with a die gap of 1.2 mm to 1.6 mm and a gauge of 25 µm to 60 µm. In this configuration, the machine-direction secant modulus is higher than in general-purpose packaging film, but tear initiation resistance measured by ASTM D1004-21 may be lower in the crease area because localized yielding occurs after repeated folding. The film is corona treated in line to a wetting tension of 40 mN/m to 44 mN/m. Ink adhesion for flexographic printing is evaluated by a tape test after 24 h aging. Because the material is paper-like only when pigmented, converters add 4 wt% to 8 wt% titanium dioxide white masterbatch; this reduces tensile strength and requires verification of the coefficient of friction under ISO 8295:2004 before envelope inserting machines can run at rated speed. The end products include self-adhesive mailers, document pouches, and map sleeves, each of which must be folded manually or by a plough folder without spring-back.

    The process conflict is that increasing the blow-up ratio above 3.0:1 may improve film gauge uniformity but reduces deadfold by orienting more polymer chains in the transverse direction. Converters that require both deadfold and high gauge uniformity often use a rotating die or counter-rotating die centre rather than increasing blow-up ratio. This preserves the orientation balance and avoids the haze increase associated with higher TiO₂ loading. Published data for the specific deadfold retention of DGDA6097 after flexo printing is limited, so trial measurements are necessary before commercial mailer conversion.

    Free Quote

    Competitive Sinopec Fujian HDPE DGDA6097 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Fujian HDPE DGDA6097 is a high-density polyethylene blown film extrusion resin produced at Sinopec Fujian Refining & Chemical Co., Ltd. The grade code DGDA6097 is positioned within the producer's high molecular weight film portfolio for thin-gauge, high-strength applications, including T-shirt sacks, grocery sacks, bin liners, and overwrap. Commercial technical documentation for this grade class indicates a nominal melt index of 0.85 g/10 min when determined under ASTM D1238 at 190 °C with 2.16 kg load, and a nominal density of 0.953 g/cm³ under ASTM D1505. The resin is normally supplied as natural pellets without slip or antiblock. Downstream addition of masterbatch is required to control coefficient of friction and blocking in finished film. Because the Sinopec Fujian grade is less widely covered in open technical literature than equivalent HDPE film grades from other producers, the following process and property discussion draws on published data for HDPE blown film resins of the same melt index and density class, and on production-scale blown film line observations.

    Resin Specification and Typical Mechanical Properties

    The following table consolidates typical property values reported for HDPE blown film resins with a nominal melt index of 0.85 g/10 min and density of 0.953 g/cm³. These values should not be read as guaranteed lot-release specifications for the Fujian DGDA6097 production campaign; certificate-of-analysis data from Sinopec should govern acceptance testing. Film property values are sensitive to die gap, blow-up ratio, frost line height, and gauge.

    PropertyTest methodTypical valueUnit
    Melt indexASTM D1238, 190 °C/2.16 kg0.85g/10 min
    DensityASTM D15050.953g/cm³
    Tensile yield strength, MDASTM D88225–30MPa
    Tensile yield strength, TDASTM D88224–29MPa
    Elongation at break, MDASTM D882500–800%
    Elongation at break, TDASTM D882600–900%
    Elmendorf tear strength, MDASTM D192215–25g
    Elmendorf tear strength, TDASTM D192212–20g
    Dart drop impact, F50, 25 µm filmASTM D1709 Method A200–300g

    Processing trials on high-stalk blown film lines have shown that the most sensitive control variable is the relationship between die gap and neck height. The grade class is commonly run through grooved-feed extruders with L/D ratios of 24:1 to 30:1 and compression ratios of 3.0:1 to 3.5:1. Rear barrel temperatures are typically set between 180 °C and 210 °C, while adapter and die zones are held between 200 °C and 220 °C. On a 90 mm extruder with a 200 mm die, die pressure commonly falls between 25 MPa and 35 MPa at output rates of 100–160 kg/h. Split runs at these conditions indicate that bubble diameter variation increases sharply when the melt temperature at the die is allowed to exceed 240 °C, and surface melt fracture appears when the die temperature falls below 180 °C. A die gap of 1.0–1.4 mm is standard for film gauges between 20 µm and 40 µm; narrower gaps raise die-lip shear rate and can produce sharkskin on the bubble surface. The high-stalk configuration is operated with neck height of 5–8 die diameters and blow-up ratio of 4:1 to 5:1. Frost line height is usually maintained above 800 mm to stabilize gauge uniformity, though the exact setpoint is line-specific.

    The grade's processing behavior can be differentiated from conventional unimodal HDPE by dynamic oscillatory shear measurements. A broader molecular weight distribution appears as a shallower terminal slope in the storage modulus curve and a higher value of the crossover frequency. For the resin class represented by DGDA6097, the crossover modulus at 190 °C is generally lower than that of a narrow-distribution film grade of the same melt index, indicating longer relaxation times. This longer relaxation time is the rheological basis for the high-stalk bubble stability noted at die gaps below 1.2 mm. However, the same characteristic increases extruder pressure and requires the adapter and die zones to be held in the upper end of the specified range. A screw with a low-shear, high-mixing barrier section is preferred to avoid localized temperature spikes. The use of screen packs below 60 mesh is not recommended for high-viscosity HDPE because it increases melt temperature without a proportional improvement in gel elimination.

    What distinguishes DGDA6097 from conventional unimodal HDPE film grades in thin-gauge extrusion?

    The main difference is molecular weight distribution and melt extensional strain-hardening. A conventional unimodal HDPE film resin of the same density shows a less stable bubble neck when the frost line height is raised, limiting the minimum gauge that can be run on air-cooled high-stalk lines. DGDA6097-type HDPE film resins are designed with a broader molecular weight distribution that increases extensional viscosity during melt stretching. Under typical high-stalk conditions, this behavior supports a stable neck at die gaps below 1.2 mm and permits downgauging to 12–15 µm on lines that would otherwise require a heavier film from lower molecular weight HDPE. The molecular architecture also shifts the property balance: tensile yield strength and secant modulus are higher than in LLDPE-rich blends, while dart drop impact is retained more effectively than in lower molecular weight HDPE grades under ASTM D1709 Method A. The trade-off is transverse tear strength, which is lower than that of LLDPE-based film of equal gauge. The property difference is process-dependent; high-stalk orientation raises machine-direction tensile properties but also increases machine-direction tear propagation.

    When Fujian DGDA6097 is processed on high-stalk blown film lines

    The downstream processor confronts two competing constraints. A high blow-up ratio improves transverse orientation and dart drop impact but reduces line speed stability if the bubble is quenched too early. A low frost line height increases impact resistance but can increase haze and gauge variation. For film between 20 µm and 30 µm, typical machine settings cluster around a BUR of 4:1, frost line height of 800–900 mm, and die gap of 1.2 mm. Under these conditions, film converted from this grade class has been observed to exhibit dart drop impact values of 200–300 g by ASTM D1709 Method A and Elmendorf tear values of 15–25 g MD by ASTM D1922. Raising the BUR to 5:1 raises transverse tensile yield strength by roughly 5–10% in production trials, but it also requires a more uniform air ring and may extend the bubble beyond the available calibration cage on small lines. Reducing the die gap to 0.8 mm improves gauge control but increases die-lip shear rate; this can initiate sharkskin unless melt temperature is raised 5–10 °C, which in turn narrows the oxidative stability margin.

    Gauge reduction below 15 µm changes the failure mode from dart impact to tear propagation. At 12 µm, the film's dart drop impact under ASTM D1709 Method A can fall below 150 g even when the resin is processed within the optimum window. This is not a resin defect but a consequence of the relationship between film thickness and impact energy absorption. In high-speed bag conversion, the low gauge also raises the sensitivity to film blocking; therefore, the masterbatch addition level for slip and antiblock must be adjusted after measuring the coefficient of friction according to ASTM D1894. High-stalk films made without antiblock can block in the roll under storage temperatures above 35 °C. The processor should avoid winding rolls at tensions above 0.1 N/mm of film width for gauges below 15 µm, because residual stress accelerates core blocking and telescoping.

    For lot acceptance, the certificate of analysis from Sinopec Fujian should be checked against the incoming resin melt index and density by ASTM D1238 and ASTM D1505. Direct food-contact use should not be assumed without written confirmation that the grade meets U.S. FDA 21 CFR 177.1520 and applicable food-contact requirements in the destination market. REACH and RoHS obligations are generally managed at the finished-article level. The grade is not intended for injection molding or blow molding; its high melt viscosity at low shear rates makes it unsuitable for molding machines with short flow paths and limited clamp force. In comparison with a high-melt-index HDPE film grade of 1.5–3.0 g/10 min, DGDA6097 requires higher motor torque and higher die pressure but delivers better high-stalk bubble stability and greater downgauging capacity. In comparison with an LLDPE film resin of 0.9 g/10 min, DGDA6097 yields higher tensile yield strength and modulus but lower Elmendorf tear and lower dart drop impact at the same gauge. The most common production failure mode observed with this grade class is bubble instability during high-stalk operation caused by inadequate frost line control or by cross-contamination with polypropylene pellets in the conveying system; die-lip build-up and variable gauge are typical symptoms. Published data for the specific Fujian DGDA6097 formulation is limited in peer-reviewed literature, so process parameters should be verified by trial on the actual line rather than transferred directly from an equivalent grade.