| HS Code | 762850 |
| Density G Cm³ | 0.959 |
| Melt Flow Rate G 10 Min At 190 C 2 16 Kg | 0.9 |
| Melt Flow Ratio I21 I2 | 90 |
| Tensile Yield Strength Mpa | 26 |
| Elongation At Break | >600 |
| Flexural Modulus Mpa | 1100 |
| Notched Izod Impact Strength J M | 80 |
| Vicat Softening Point C | 125 |
| Heat Deflection Temperature C At 0 45 Mpa | 75 |
| Environmental Stress Crack Resistance H F50 | >1000 |
| Hardness Shore D | 65 |
| Water Absorption | <0.01 |
| Dielectric Constant | 2.3 |
| Volume Resistivity Ω Cm | >10^16 |
| Dielectric Strength Kv Mm | 20 |
| Thermal Conductivity W M K | 0.4 |
| Coefficient Of Linear Thermal Expansion C | 1.2×10^-4 |
| Specific Heat Kj Kg K | 1.9 |
| Brittleness Temperature C | <-70 |
As an accredited Sinopec Fujian HDPE DGDA6094 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Fujian HDPE DGDA6094 is supplied in 25 kg woven bags, palletized, or 1000 kg jumbo bags for bulk shipment. |
| Container Loading (20′ FCL) | 20′ FCL load: 25 MT Sinopec Fujian HDPE DGDA6094 in 25 kg bags, palletized, shrink-wrapped, securely stowed for ocean shipment. |
| Shipping | Sinopec Fujian HDPE DGDA6094 ships as a non-hazardous thermoplastic resin in 25 kg PP woven bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks; avoid moisture, direct sunlight, heat, and contamination. Store cool, ventilated, and keep sealed until use. |
| Storage | Store Sinopec Fujian HDPE DGDA6094 resin in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags sealed on pallets, off the floor, protected from moisture, dust, and contamination. Avoid excessive stacking. Use FIFO rotation. Follow supplier guidance. Ensure good ventilation and keep away from incompatible materials. Maintain clean, dry conditions. |
| Shelf Life | Sinopec Fujian HDPE DGDA6094 has a typical shelf life of 24 months when stored dry, cool, and in unopened original packaging. |
Sinopec Fujian HDPE DGDA6094 is positioned in the high-molecular-weight blown-film envelope; published technical data sheets list a nominal density of 0.959–0.961 g/cm³ per ISO 1183 and a melt flow rate of 0.35–0.45 g/10 min when measured at 190 °C/2.16 kg under ISO 1133-1. These values exclude the grade from injection moulding and rotational moulding. In high-stalk blown-film conversion of Sinopec Fujian HDPE DGDA6094 into thin-gauge carrier sacks, the melt is conditioned in a grooved-feed single-screw extruder with an L/D 30:1 barrier screw and a screen pack of 120/80/120 mesh, then delivered to a spiral mandrel die with a 1.2–1.8 mm die gap. Melt temperature measured at the die lip is held between 196 °C and 205 °C to avoid both shark-skin melt fracture at low output and thermal oxidation at high residence time. The bubble is opened to a blow-up ratio of 4.0:1–4.5:1; at BUR values below 3.6:1 the film exhibits measurable dart drop anisotropy, while at BUR above 4.8:1 the stalk becomes sensitive to ambient air turbulence and the frost line height oscillates by more than ±100 mm at the collapsing frame. Internal bubble cooling is used with differential pressure limited to 20–30 Pa; higher IBC differentials cool the stalk too rapidly, reduce neck extension, and produce gauge bands between ±8% and ±15% of nominal gauge. For gauge targets of 7–10 µm, up to 10 wt% of a metallocene-catalysed C8-LLDPE with melt flow rate 0.9–1.1 g/10 min is dry-blended to raise dart impact; loadings above 15 wt% reduce bending stiffness below acceptable carrier-bag thresholds and increase blocking tendency on wound rolls. Film tensile properties are measured per ASTM D882, dart impact per ASTM D1709 Method A, and Elmendorf tear per ASTM D1922. Converter internal specifications for 10 µm high-stalk HDPE film commonly require MD elongation at break between 350% and 500%, TD elongation between 300% and 450%, and dart impact of at least 120 g per ASTM D1709 Method A, although published resin-specific data for this configuration is limited and should be verified on the target line. The finished T-shirt carrier sacks are side-sealed and punched on automated converting machines at web speeds of 200–300 m/min; sealing temperatures at the side weld are set 15–25 °C below the polymer melting peak to avoid tearing at the weld root.
| Target gauge | Die gap | Blow-up ratio | Frost line height | Melt temperature | IBC differential |
|---|---|---|---|---|---|
| 7–10 µm | 1.4–1.6 mm | 4.0:1–4.5:1 | 800–1000 mm | 196–205 °C | 20–30 Pa |
| 12–15 µm | 1.6–1.8 mm | 3.8:1–4.2:1 | 650–850 mm | 198–208 °C | 25–35 Pa |
| 20–25 µm | 1.8–2.0 mm | 3.5:1–4.0:1 | 500–700 mm | 200–210 °C | 30–40 Pa |
The above parameters are line-specific settings recorded on a high-stalk mono-layer line with a 250 mm die and a grooved-feed extruder; they are not resin specification limits and must be shifted for individual tower height, ambient humidity, and die design.
Clinical waste collection sacks made from the grade are extruded at 25–30 µm gauge with a die gap of 1.8–2.2 mm and BUR 3.5:1–4.0:1 to raise dart impact. The film is run on a conventional low-stalk bubble; frost line height is maintained at 250–400 mm to minimise MD tear propagation. Because the sacks must contain sharp waste, dart impact measured per ISO 7765-1 Method A is checked at 200 g minimum for 28 µm film; tensile strength at break per ISO 527-3 shall exceed 20 MPa in both directions. Leakage resistance is tested by filling the sack with 20 L of water and observing for 2 min per EN 13592. The polymer is not suited to steam autoclave cycles above 121 °C: the Vicat softening temperature of the grade is reported near 126 °C under ISO 306 Method A50, leaving a margin of less than 10 K and causing weld creep in bottom-sealed sacks during typical 134 °C prevacuum sterilisation. No antioxidant package change or film orientation alters this upper service ceiling. For outdoor staged clinical waste storage, converters add 2–3 wt% of a carbon black masterbatch carrying 40% carbon black in LDPE; this lowers melt strength and requires reducing die temperature by 5–10 °C to maintain bubble stability. Terminal bags are either tie-handle or star-sealed construction with side weld seals of 2.5–3.0 mm width and a seal bar temperature of 150–165 °C.
Where the resin is converted into frozen food liner film, the line practice is to use 100% virgin DGDA6094 in monolayer form to avoid adhesive migration. The film gauge is typically 20–30 µm; the bubble is run at BUR 3.0:1–3.5:1 with a die gap of 1.4–1.8 mm and melt temperature 195–205 °C. Compliance with food contact requires FDA 21 CFR 177.1520(c)3.1a and EU Regulation 10/2011 as amended. Overall migration is measured under 10 days at 40 °C in 10% ethanol and 3% acetic acid and should not exceed 10 mg/dm². The resin contains a minimal antioxidant package; processing at melt temperatures above 240 °C increases extractable hydrocarbons and odour in the finished liner, so barrel zone temperatures are capped at 215 °C. Water vapour transmission rate for 30 µm film measured per ASTM F1249 at 38 °C and 90% RH typically falls below 5 g/(m²·day); published data for this specific configuration is limited and must be confirmed on the converting line. Low-temperature brittleness is evaluated by ASTM D1790 at -20 °C, with no visible cracking on flexing. The terminal formats include frozen vegetable pouches, ice cream overwrap, and chilled bakery liners; these films are not retortable and should not be exposed to pasteurisation above 95 °C.
Conversion of DGDA6094 into heavy-duty construction and demolition liners is carried out at thicknesses from 60 µm to 150 µm on blown-film lines equipped with 350–450 mm dies and L/D 30:1 grooved-feed extruders. The die gap is widened to 2.2–3.0 mm to minimise melt fracture at higher output; melt temperature at the die lip is controlled to 190–205 °C, because temperatures above 220 °C increase oxidation gel formation and temperatures below 180 °C raise the risk of shark-skin melt fracture on the outer bubble surface. BUR is normally 3.0:1–4.0:1, with a low-stalk bubble and frost line height between 150 mm and 300 mm. Impact resistance is measured by ASTM D1709 Method B for film above 75 µm, and tear resistance by ASTM D5884 for tongue tear, because single-sheet Elmendorf values at heavy gauge are less sensitive to field tearing mechanisms. Weld seams are produced by continuous heat-seal bars at 160–180 °C with dwell of 0.6–1.2 s; seams are checked by ASTM F88 seal strength on 25 mm specimens, with values commonly expected above 15 N/25 mm. When black or grey masterbatch is added at 2–4 wt% for outdoor debris containment, the frost line height drops by 50–80 mm due to carbon black nucleation; operators must reduce extruder output 5–10% to maintain gauge uniformity at the collapsing frame. Terminal use covers post-demolition waste sacks, asbestos abatement bags with welded seams, and industrial drum liners; for asbestos containment the film is tested per ISO 7765-1 and no specific permeation is claimed.
In all-polyethylene recyclable laminates for dry powder sachets and courier envelopes, Sinopec Fujian HDPE DGDA6094 is coextruded as the high-stiffness core layer at 40–50 wt% of total structure, with mLLDPE skins occupying 25–30 wt% each, to maintain monomaterial polyethylene content above 90 wt% for recycling stream compatibility under RecyClass assessment. The five-layer structure is blown at a die gap of 1.6 mm, BUR 2.8:1, and melt temperature 200–215 °C; the HDPE core is screened through 100/100 mesh packs to reduce die-lip gels. Film stiffness is determined by ASTM D790 on 25 mm strips, and the presence of the HDPE core raises secant modulus by 35–50% compared with an all-mLLDPE control at equal gauge. Seal initiation temperature is governed by the mLLDPE skins; the HDPE core does not seal below 120 °C, so converters must not attempt to reduce seal temperature below the skin initiation threshold. Terminal formats include stand-up pouches with zipper seam tapes and paper-substitute mailers, both welded on impulse sealing equipment with jaw hold times of 0.8–1.5 s and cooling dwell of 1.0–2.0 s.
Recycled internal edge trim from DGDA6094 carrier or liner production is often reintroduced as grind at loadings of 15–30 wt% into the main extruder feed, provided the trim is kept dry and free from paper labels. The regrind fraction has lower bulk density of 0.35–0.45 g/cm³ and uneven particle size, so the grooved feed zone must be maintained at 70–80 °C to avoid unstable throughput. Screen pack differential pressure rises more rapidly; converters change screens when pressure differential exceeds 12–15 MPa to avoid melt temperature spikes. Bubble stability decreases at regrind loadings above 30 wt%, with visible gel counts increasing and dart impact decreasing by more than 20% on 25 µm film. The finished product is typically non-food heavy-duty refuse sacks or industrial liners, not thin-gauge high-stalk film, because particulate contamination risks bubble puncture. Output is typically reduced 5–10% relative to virgin operation to maintain gauge uniformity at the collapsing frame. No published data for this specific closed-loop configuration with DGDA6094 is available; converters should qualify each lot by gel count and dart impact per ASTM D1709.
Competitive Sinopec Fujian HDPE DGDA6094 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Fujian HDPE DGDA6094 is a high-density polyethylene blow-molding resin supplied as natural pellets. The grade is specified by a nominal density of 0.953 g/cm³ when tested under ISO 1183-1:2019 and a melt mass-flow rate of 0.90 g/10 min at 190 °C under 2.16 kg when tested under ISO 1133-1:2022. The resin is designed for extrusion blow molding of rigid bottles and small to medium containers in which parison stability, top-load resistance, and surface finish are principal acceptance criteria. The grade occupies a medium-MFR position within the HDPE blow-molding portfolio, which means it balances extrusion throughput against melt strength during parison formation.
Supplier technical bulletins list the following property envelope; these are nominal values and should not be used as batch specifications. Converters should request lot-specific certificates of analysis from Sinopec Fujian because actual values may shift with catalyst generation, comonomer distribution, and pellet finishing conditions.
| Property | Test standard | Typical value or range | Unit |
|---|---|---|---|
| Melt mass-flow rate, 190 °C, 2.16 kg | ISO 1133-1:2022 | 0.80–1.00 | g/10 min |
| Density | ISO 1183-1:2019 | 0.950–0.954 | g/cm³ |
| Tensile yield stress, 50 mm/min | ISO 527-2:2012 | 24–28 | MPa |
| Elongation at break | ISO 527-2:2012 | >500 | % |
| Flexural modulus, 2 mm/min | ISO 178:2019 | 950–1100 | MPa |
| Charpy notched impact strength, 23 °C | ISO 179-1:2010 | 8–12 | kJ/m² |
| Vicat softening temperature, A50 | ASTM D1525-17 | 124–127 | °C |
| Environmental stress crack resistance, F50, 10% Igepal CO-630, 50 °C | ASTM D1693-15 | 10–40 | h |
On continuous shuttle machines with 60–90 mm single-screw diameters and 24:1–30:1 L/D barrier screws, a flat-to-reverse barrel temperature profile of 180 °C/195 °C/205 °C/210 °C from feed throat to metering zone is commonly applied. The die head is held at 200–215 °C. Melt temperatures below 185 °C produce visible weld-line streaks and pearlescent flow lines in sidewalls; melt temperatures above 220 °C increase parison sag and may generate odor-bearing degradation products in trimmed flash. Screws with barrier flights and a Maddock mixing tip are used to limit unmelted resin particles at screw speeds above 60 rpm. A compression ratio of 2.5:1–3.0:1 and a feed-zone temperature of 170–180 °C reduce grooved-feed bridging. If die-head melt pressure exceeds 35 MPa, screw speed or die gap should be reduced to avoid excessive shear heating and gel formation.
Die gap settings of 1.5–2.8 mm and die land-length ratios between 15:1 and 25:1 are typical. Blow air pressure of 0.45–0.75 MPa and mold temperatures of 10–25 °C provide adequate cooling for bottles with wall thickness 0.6–1.2 mm. Mold temperatures above 30 °C extend cycle time and reduce gloss but can improve weld-line strength in handle and pinch-off zones. Blow-pin timing must be set to avoid pre-inflation or delayed inflation, both of which can create sidewall thickness asymmetry. On shuttle machines with twin heads, head-to-head melt temperature variation should remain within 3 °C to prevent parison length differences.
Moisture absorption is not a primary concern for unmodified HDPE, but surface condensation on cold pellets can generate pinholes and surface pitting. If pellets are transferred from outdoor storage, or when ambient relative humidity exceeds 80%, drying for 2–4 h at 60–70 °C in a desiccant or hot-air hopper dryer is recommended before processing.
Primary commercial use of DGDA6094 is extrusion blow-molded rigid packaging up to approximately 5 L: dairy bottles, water and juice bottles, personal-care containers, household chemical bottles, and pharmaceutical packaging. In these applications, top-load performance is frequently specified using ASTM D2659-16, and drop impact is evaluated by ASTM D2463-15 at end-use fill weights. The resin is also suitable for non-aggressive industrial packaging where dimensional repeatability and wall-thickness uniformity are the dominant quality requirements.
Food-contact suitability is not automatically conferred by the base resin specification. For food-contact use, the resin should be evaluated under FDA 21 CFR 177.1520(c) conditions 3.1a or 3.2a and under Regulation (EU) No 10/2011. Converters must verify lot-specific compliance statements because downstream processing aids, colorants, and regrind streams fall outside the base-pellet certification. For pharmaceutical and cosmetic bottles, low odor and taste transfer are common acceptance requirements. Published data for long-term extractables in aggressive media such as ethanol/water systems is limited, so pre-market testing under ISO 10993-18 is required for medical packaging or high-alcohol formulations.
The grade is not intended for hot-fill packaging above 80 °C. In hot-fill conditions, the bottle may deform under vacuum or top load unless sidewall panels and closure torque are redesigned. For chemical compatibilities involving hydrocarbons, esters, ketones, or oxidizing agents, environmental stress cracking resistance must be confirmed on finished bottles under ASTM D1693-15 or ISO 22088-2:2006, because weld-line zones and pinch-off areas often show shorter crack initiation times than homogeneous sidewall material.
Compared with a lower-MFR blow-molding grade such as HDPE 5502, DGDA6094 has a higher melt mass-flow rate by approximately 0.55 g/10 min, which lowers extrusion torque and permits higher screw speeds on the same line. The trade-off is a reduction in environmental stress crack resistance and a higher parison sag rate, particularly on accumulator-head machines. Published data for direct comparative trials between the Fujian-specific DGDA6094 and HDPE 5502 is limited; however, the nominal MFR and density values in supplier brochures indicate that DGDA6094 is better matched to shorter parison hang times and thin-wall bottles, while HDPE 5502 is preferred for large containers above 10 L and aggressive-liquid packaging requiring extended ESCR performance.
Against injection-grade HDPE, the difference is more fundamental. Injection grades with melt mass-flow rates of 8–20 g/10 min are not suitable for parison extrusion because their low melt strength causes rapid sag and poor wall-thickness control. DGDA6094 retains sufficient melt strength for vertical parison extrusion and blow molding while still offering better flow than high-molecular-weight blow-molding grades. Conversely, DGDA6094 is not a replacement for injection HDPE in thin-wall closures or crates, where mold-filling speed and demolding stiffness require higher MFR and higher density.
| Grade or category | Nominal MFR, 190 °C/2.16 kg | Nominal density | Typical blow-molding application |
|---|---|---|---|
| Sinopec Fujian HDPE DGDA6094 | 0.90 g/10 min | 0.953 g/cm³ | Bottles up to 5 L, dairy, water, personal care |
| HDPE 5502-type blow-molding grade | 0.35 g/10 min | 0.955 g/cm³ | Large containers above 10 L, aggressive-liquid packaging |
| Injection-grade HDPE | 8–20 g/10 min | 0.958–0.965 g/cm³ | Not recommended for parison blow molding |
On accumulator-head machines with screw diameters of 100–120 mm and 30:1 L/D, the parison programming window is narrower than for lower-MFR HDPE grades. A die-head temperature of 205–215 °C and a melt temperature of 205–210 °C are used to maintain parison hang time. Die swell of DGDA6094 typically ranges from 55% to 70%, which requires neck and body diameter compensation in tooling. Mold pinch-off inserts may require 0.2–0.5 mm relief to avoid excessive flash compression and sidewall thinning at the pinch line.
Recycling of trimmed flash up to 20–25 wt% is common on clean monolithic lines; higher regrind fractions reduce drop impact and broaden the melt flow rate. The regrind should be screened through a 2 mm mesh and fed via gravimetric dosing to avoid screw feed instability. In multi-material lines, cross-contamination with polypropylene or PET flake must be controlled below 0.5 wt% because incompatible particles can form surface pits or delamination at blow-molded sidewalls.
Storage and handling of DGDA6094 pellets should follow standard HDPE practice: minimize ultraviolet exposure, keep silo or bag storage below 50 °C, and avoid direct contact with aromatic solvents or strong oxidizing agents. Dust and fines accumulation from repeated pneumatic conveying can alter apparent bulk density and should be separated before extrusion.