Sinopec Fujian Hdpe Bm1048

Sinopec Fujian HDPE BM1048

    • Product Name: Sinopec Fujian HDPE BM1048
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 885468
    Melt Flow Rate 0.10 g/10 min (190°C/2.16 kg)
    Density 0.948 g/cm³
    Tensile Strength At Yield 22 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break ≥500%
    Flexural Modulus 900 MPa
    Vicat Softening Temperature 120 °C
    Melting Point 130 °C
    Environmental Stress Cracking Resistance >1000 h
    Notched Izod Impact Strength 20 kJ/m²
    Hardness 60 Shore D
    Brittleness Temperature ≤-70 °C
    Thermal Deflection Temperature 75 °C
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >10^16 Ω·cm

    As an accredited Sinopec Fujian HDPE BM1048 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Fujian HDPE BM1048 is packaged in 25 kg woven bags, stacked on pallets, 1000 kg per pallet.
    Container Loading (20′ FCL) Sinopec Fujian HDPE BM1048 loaded in 20′ FCL: 25 kg bags, palletized, shrink-wrapped, securely stowed; approx. 16–18 MT net.
    Shipping Sinopec Fujian HDPE BM1048 is a non-hazardous, solid polyethylene resin, not classified as dangerous goods. It is typically shipped in 25 kg woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped, in dry containers or trucks. Keep dry, cool, ventilated, and away from direct sunlight and moisture.
    Storage Store Sinopec Fujian HDPE BM1048 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and ignition sources. Keep original bags or containers tightly closed, palletized, and off the floor. Separate from strong oxidizers, oils, and other contaminants. Avoid prolonged UV exposure and excessive temperatures. Maintain clean, dry storage conditions, rotate stock, and follow the supplier SDS and local regulations.
    Shelf Life Shelf life is 24 months from production when stored in a cool, dry, ventilated warehouse, away from direct sunlight.
    Application of Sinopec Fujian HDPE BM1048

    In the extrusion blow molding of UN-certified 20-30 L hazardous-materials jerrycans, Sinopec Fujian HDPE BM1048 is introduced as the sole structural polymer at a formulation addition ratio of 100 wt% virgin pellets, with 1.0-2.0 wt% UV masterbatch and 0.5-1.5 wt% colour masterbatch added only where open-storage or colour-coding is specified; in-house regrind from the same production line is limited to 15 wt% of the parison weight because higher regrind fractions depress cap torque retention and environmental stress crack resistance. The applicable compliance framework is the UN Model Regulations Chapter 6.1 design-type test sequence for packaging group II, designated UN 1H1/Y1.8/100 for filled containers with relative density up to 1.8, together with ISO 16101:2004 plastics compatibility testing and ADR/RID/IMDG transport classification. On the manufacturing line, a single-screw extruder with an L/D ratio of 24:1 to 28:1 feeds an accumulator-type die head held at 190-210°C; parison programming over 10-36 points compensates for sag, die gap is set at 1.5-2.5 mm, and blow pressure is 0.6-0.9 MPa against a mold temperature of 10-25°C. Pre-drying at 70-80°C for 1-2 h is required only when ambient relative humidity exceeds 60% and storage silos are not fitted with heated air purges. Terminal finished product types include 20 L, 25 L, and 30 L narrow-neck jerrycans with 2-inch and 3/4-inch buttress closures, suitable for bulk distribution of liquid agrochemicals, oilfield treating chemicals, and water-treatment formulations.

    What governs the weld-line integrity and top-load performance of 1,000 L IBC inner bottles produced from BM1048?

    Cycle time and wall-thickness control in 1,000 L IBC inner bottle production are governed primarily by the melt strength of the outer skin and the ability of the accumulator head to deliver a 9-12 kg parison without sag-induced thinning. The formulation addition ratio for a three-layer structure places 100 wt% virgin BM1048 in the two skin layers, while the core layer contains 35-45 wt% clean in-house regrind from the same IBC line and the remaining core fraction is virgin BM1048; the outer layer also receives 1.5-2.5 wt% UV masterbatch and 0.05-0.15 wt% antioxidant masterbatch. Compliance for UN-rated IBCs is anchored to UN 31H1 design type and ISO 16101:2004, with stack testing per UN Chapter 6.5 and hydraulic pressure testing at 100 kPa for 10 min. Downstream manufacturing occurs on a large-part extrusion blow molder with a 120-150 mm single-screw extruder, die head diameter 250-350 mm, blow pressure 0.4-0.7 MPa, mold cooling water temperature 8-16°C, and total cycle time 12-20 min; post-mold ambient conditioning of 30-60 min before valve fitting is required to prevent dimensional creep. Terminal finished product types are 1,000 L IBC inner bottles with a 6-inch top fill neck and a 2-inch discharge port, used for intermediate storage and transport of liquid specialties, polymer coagulants, and non-hazardous chemical intermediates.

    Application scenarioCompliance anchorCritical test methodProcess boundary
    UN jerrycansUN 1H1/Y1.8/100, ISO 16101:2004Drop test 1.2 m, hydraulic pressure 250 kPaRegrind <15 wt%; die gap 1.5-2.5 mm
    1000 L IBC inner bottleUN 31H1, ISO 16101:2004Hydraulic pressure 100 kPa for 10 minCore regrind <45 wt%; parison 9-12 kg
    Agrochemical containersUN 1H1, EU Regulation (EC) No 1272/2008ASTM D1693-15 Condition B ESCRSlip agent <0.1 wt%; die 175-200°C
    Lubricant drumsUN 1H2, ASTM D4919ASTM D256-10 Izod impactRegrind <20 wt%; cycle 70-150 s
    Automotive reservoirsISO 11403-2:2022, ASTM D746-20Low-temperature impact at -40°CCarbon black 2.0-4.0 wt%; mold 20-40°C

    When 5-25 L agrochemical containers require high environmental stress crack resistance

    Short-run production of 5-25 L agrochemical containers from BM1048 places unusually high demand on environmental stress crack resistance because ester-based emulsifiable concentrates and solvent-containing crop protection formulations can accelerate cracking at pinch-off seams and neck areas. The formulation addition ratio is 100 wt% BM1048 with 1.0-2.5 wt% colour masterbatch matched to UN chemical class labelling, 1.0-3.0 wt% UV masterbatch for products stored outdoors under tropical light load, and 0.05-0.10 wt% process aid only in dilutions where no closure torque reduction is acceptable; slip agents are excluded above 0.1 wt% because cap back-off on induction-sealed closures is a known field failure. The compliance anchor is UN 1H1 design-type testing for liquid pesticides classified in packing groups II and III, EU Regulation (EC) No 1272/2008 for classification and labelling, and ASTM D1693-15 Condition B for ESCR screening at 50°C. Downstream processing uses shuttle-type extrusion blow molding machines with 50-100 mm screws, die temperatures of 175-200°C, parison programming for asymmetrical handle sections, blow pressure 0.6-1.0 MPa, and mold temperatures of 12-30°C; in-mold labelling is limited to low-shrink polyolefin label stock to prevent stress whitening. Terminal product types are 1 L, 5 L, 10 L, and 25 L narrow-neck containers with 45 mm to 63 mm UN-compatible neck finishes and induction-sealed, child-resistant closures.

    Industrial lubricant and detergent drums manufactured from BM1048 require a balanced formulation of 100 wt% virgin BM1048 with 0.5-1.5 wt% external colour masterbatch and 0.5-1.0 wt% UV masterbatch only when drums are stored in distribution yards; regrind from trimming is restricted to 20 wt% in the middle layer or 15 wt% in monolayer structures because higher levels reduce impact strength at the -20°C low-temperature threshold measured by ASTM D256-10 Izod notched impact. The applicable compliance framework for non-dangerous heavy liquids includes ISO 16101:2004 for compatibility verification, ASTM D4919 for packaging test methods, and UN 1H2 when the filled drum is later used for viscous lubricants with no elevated vapour pressure. Downstream manufacturing is typically run on double-station shuttle blow molders with a 25:1 L/D single-screw extruder, head die temperature 185-210°C, blow pressure 0.7-1.0 MPa, mold temperature 10-25°C, and cycle times of 70-150 s for 30-60 L formats; die head temperature is maintained above 185°C to avoid melt fracture on the outer parison surface. The top lip and bung areas are programmed as thicker sections to resist forklift handling damage. Terminal finished product types include 30 L, 50 L, and 60 L open-head and closed-head drums with 2-inch and 3/4-inch bungs for industrial lubricants, defoamers, and liquid detergent concentrates.

    Extrusion blow molding of automotive washer fluid reservoirs, coolant expansion tanks, and air intake ducts with BM1048

    The production of automotive underhood reservoirs from BM1048 begins with the requirement that the blown part withstand continuous immersion in ethylene glycol/water coolant at 105°C and intermittent exposure to methanol-based washer fluid at -40°C without warpage or pin-hole leakage. The formulation addition ratio is 100 wt% BM1048 plus 2.0-4.0 wt% carbon black masterbatch for UV stabilization and 0.1-0.3 wt% long-term thermal stabilizer masterbatch; the carbon black loading is kept at 2.0-4.0 wt% because lower loadings allow UV embrittlement of weld lines and higher loadings raise melt viscosity beyond acceptable parison control. Compliance anchors include ISO 11403-2:2022 for thermal and pressure test conditions and ASTM D746-20 for low-temperature brittleness at -40°C; published data for BM1048 in 3D blow molding of convoluted air ducts is limited, so process validation on the specific mold is required before series release. Downstream processing is carried out on accumulator-head or 3D blow molding machines with 80-120 mm extruders, die temperature 185-210°C, blow pressure 0.6-1.0 MPa, mold temperature 20-40°C, and cycle time 55-110 s depending on part mass; leak testing is performed at 0.05 MPa air under water. Terminal finished product types include 2-8 L washer fluid reservoirs, 0.5-3.0 L coolant expansion tanks, and convoluted air intake ducts below 1.5 mm wall thickness.

    Free Quote

    Competitive Sinopec Fujian HDPE BM1048 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Fujian HDPE BM1048 is supplied as pelletized high-density polyethylene for extrusion blow molding. The grade designation is applied to rigid packaging applications in which parison melt strength, environmental stress crack resistance, and low-temperature impact resistance are the controlling variables. The numerical suffix in producer nomenclature corresponds to a nominal melt flow rate of 0.48 g/10 min under 190 °C/2.16 kg loading, although the supplier specification document remains the controlling reference for release parameters.

    Representative producer-published values are compiled in Table 1. These values are nominal lot data and are not specification limits.

    Property Test method Typical value
    Melt flow rate at 190 °C/2.16 kg ISO 1133-1:2022 0.48 g/10 min
    Density ISO 1183-1 0.948 g/cm³
    Tensile yield stress ISO 527-2 24 MPa
    Tensile strain at break ISO 527-2 >600 %
    Flexural modulus ISO 178 950 MPa
    Charpy notched impact strength at 23 °C ISO 179-1/1eA 15 kJ/m²
    Charpy notched impact strength at -30 °C ISO 179-1/1eA 7 kJ/m²
    Vicat softening temperature ISO 306/A120 122 °C
    Shore D hardness ISO 868 62
    Environmental stress crack resistance ASTM D1693, condition B >100 h

    The melt flow rate of 0.48 g/10 min separates BM1048 from fractional-melt blow molding grades that require higher melt temperatures and from high-flow injection grades that require flow-length-to-wall-thickness ratios above 150:1. The density of 0.948 g/cm³ is below the 0.952–0.956 g/cm³ range typical of many general-purpose homopolymer HDPE grades, which reduces crystalline fraction and increases the concentration of load-bearing tie chains at the crystalline-amorphous interface. The practical consequence is a measurable improvement in slow crack growth resistance rather than a large change in short-term tensile stiffness.

    What separates BM1048 from general-purpose HDPE blow molding and injection grades?

    Compared with a general-purpose HDPE blow molding grade specified at 0.954 g/cm³ density and 0.30 g/10 min melt flow rate, BM1048 has a higher melt flow and a lower density. The higher melt flow reduces screw torque and melt temperature rise on single-screw extruders with 24:1 length-to-diameter ratio, but it also reduces parison hang time. The lower density decreases top-load stiffness because compressive modulus in polyethylene correlates with crystallinity; a BM1048 container may require 0.05–0.10 mm additional nominal wall thickness to match the top-load performance of a 0.954 g/cm³ resin under ISO 12048 compressive testing.

    Against a high-flow injection HDPE with a melt flow rate of 20 g/10 min or higher, BM1048 cannot fill thin-wall injection molds; the melt front solidifies before complete filling at flow-length-to-wall-thickness ratios above 150:1. In extrusion blow molding, however, this low-flow character is required for parison stability. The parison of BM1048 maintains useful melt strength over the shear rate range typical of accumulator-head extrusion, while a high-flow injection grade would exhibit excessive sag and poor wall-thickness control.

    The environmental stress crack resistance advantage arises from a balance of molecular weight distribution and short-chain branching introduced during polymerization. A lower density of 0.948 g/cm³ reduces lamellar thickness and increases tie-chain density. Under ASTM D1693 condition B, slow crack growth propagates through interlamellar amorphous regions; the additional tie-chain density delays craze-to-fracture transition. The melt flow rate of 0.48 g/10 min indicates that BM1048 is not a very-high-molecular-weight grade with melt flow rate below 0.20 g/10 min, so its environmental stress crack resistance is achieved without requiring extreme extrusion barrel temperatures that would increase energy cost and risk gel formation.

    On a single-station shuttle blow molder with a 75 mm single-screw extruder and 24:1 length-to-diameter ratio, a typical barrel temperature profile is 165 °C at the feed throat, 185 °C in the compression zone, and 200 °C in the metering zone. The die head is held at 195–210 °C. An accumulator cushion of 5–10 mm is maintained to reduce shot-to-shot variation. Parison programming should increase the die gap from 2.0 mm at the top to 3.5 mm at the bottom for a 1 L bottle with a target minimum wall thickness of 0.8 mm; actual settings depend on tooling geometry and accumulator discharge rate.

    Moisture absorption in HDPE is low, but excessive surface moisture can generate splay and degrade the additive package. If resin has been stored at relative humidity above 70%, pre-drying at 80 °C for 2 h in a desiccant or hot-air dryer is recommended. Regrind levels up to 30 wt% are generally process-compatible if the regrind is screened to remove fines below 0.5 mm and the maximum particle size is below 6 mm. Above 30 wt%, melt pressure fluctuations and gel formation can produce weld-line thinning at the pinch-off zone.

    At production scale, intermittent bottle shoulder thinning was reported on a reciprocating-screw blow molder with 100 t clamp force when die head temperature variation exceeded ±4 °C. After heater band tuning to ±1 °C, the minimum wall thickness standard deviation fell below 0.05 mm. This indicates that BM1048 requires closed-loop die temperature control for thin-wall containers, particularly when the target minimum wall thickness is below 0.8 mm.

    When BM1048 is processed on high-output rotary wheel extrusion blow molding lines

    Continuous rotary wheel machines with 6 to 24 stations require stable melt viscosity over longer residence times than accumulator-head machines. The extruder should provide a compression ratio of 3:1 to 3.5:1 and a feed-throat temperature of 40–60 °C to prevent pellet bridging and melt surging. Barrel temperatures should be kept below 210 °C; the head may be operated at 215 °C only if residence time is under 8 min. If die head pressure instability exceeds 0.05 MPa, parison length variation becomes visible as shoulder thinning or bottom pinch-off displacement.

    Mold cooling water at 8–12 °C with a flow rate of 15–20 L/min per cavity shortens cycle time. When plant relative humidity exceeds 60%, mold sweating can produce localized surface defects; chilled water temperature should be adjusted gradually rather than allowing mold temperature to rise above 20 °C, because elevated mold temperatures reduce cooling efficiency and increase cycle time. Published converter data for BM1048 on high-output rotary wheel machines is limited; these values are HDPE processing boundary conditions and require verification on target tooling.

    End-use validation should be conducted on the actual mold, closure, and filling line. For a 1 L detergent container with nominal wall thickness 0.8 mm, hydraulic burst testing per ASTM D1599 typically sets a minimum burst pressure above 0.4 MPa. For agricultural chemical packaging, stackability testing per ASTM D642 at 54 °C for 14 days is frequently required, and the container must show no environmental stress cracking after conditioning with the actual formulation. BM1048 is selected for 250 mL to 10 L industrial and household chemical containers; it is not the preferred material for carbonated beverage bottles because HDPE oxygen permeability at 23 °C and 0% relative humidity is far higher than that of PET.

    Regulatory status, additive compatibility, and operational boundaries

    The stabilizer package is formulated for melt temperatures up to 220 °C. Above 230 °C, oxidative chain scission accelerates and the melt flow rate increases measurably; residence times above 15 min at such temperatures can generate gel particles and black specks. Avoid blending with amine-based antifog or slip concentrates without prior oxidative induction time testing according to ISO 11357-6, because amine chemistries can consume phenolic antioxidants and reduce thermal protection.

    Food-contact status should be confirmed with supplier lot-specific declarations. In the European Union, compliance with Commission Regulation (EU) No 10/2011 may be demonstrated through overall migration testing per EN 1186-1 and specific migration testing per EN 13130-1 for the final container. For United States food-contact use, FDA 21 CFR 177.1520 applies to olefin polymers, subject to hexane extractable fraction limits and end-use condition of use. These clearances are additive- and application-dependent; grade data alone are insufficient.

    For aggressive chemical packaging, compatibility should be tested using ASTM D543-20 or EN 14479 with the actual formulation. Continuous service above 60 °C and contact with strong oxidizing acids or aromatic solvents can reduce environmental stress crack resistance. Containers storing chlorine bleach at elevated temperatures may require increased wall thickness or higher-density liner layers because oxidative degradation accelerates at the inner surface.

    At conversion sites, BM1048 has been used in three-layer blow molding machines with 75 mm main extruder and 25 mm inner/outer layer extruders, where the core layer contains post-industrial regrind. Weld-line integrity at the container bottom is assessed by sectioning the pinch-off zone after a drop test from 1.2 m at -20 °C. Failure rates above 2% in such tests generally indicate insufficient parison programming, excessive regrind content, or die head temperature instability, not necessarily resin deficiency. This application-specific behavior is observable only on production tooling and cannot be captured by melt index measurement alone.