Sinochem Quanzhou Hdpe Qzf144

Sinochem Quanzhou HDPE QZF144

    • Product Name: Sinochem Quanzhou HDPE QZF144
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 508127
    Product Name Sinochem Quanzhou HDPE QZF144
    Manufacturer Sinochem Quanzhou Petrochemical Co., Ltd.
    Grade QZF144
    Material High Density Polyethylene (HDPE)
    Appearance White pellets
    Form Pellets
    Density 0.945 g/cm³
    Melt Flow Rate 0.18 g/10 min (190°C, 2.16 kg)
    Tensile Strength At Yield ≥23 MPa
    Elongation At Break ≥500%
    Flexural Modulus ≥900 MPa
    Vicat Softening Temperature ≥120°C
    Melting Point 130°C
    Hardness 60 Shore D
    Brittleness Temperature ≤-70°C
    Environmental Stress Cracking Resistance ≥1000 h
    Water Absorption <0.01%
    Ash Content <0.03%
    Volatile Content <0.1%
    Bulk Density 0.55 g/cm³

    As an accredited Sinochem Quanzhou HDPE QZF144 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinochem Quanzhou HDPE QZF144 is supplied in 25 kg woven bags, with 40 bags per pallet (1,000 kg total).
    Container Loading (20′ FCL) Sinochem Quanzhou HDPE QZF144 loaded in 20′ FCL containers, typically 25 kg bags, palletized or floor-stacked, sealed for export.
    Shipping Sinochem Quanzhou HDPE QZF144 ships as non-hazardous polyethylene resin pellets, typically in 25 kg PP woven bags or 1,000 kg jumbo bags, palletized and shrink-wrapped. Transport by sea, rail, or truck in clean, dry containers. Store sealed in a dry, ventilated warehouse, avoiding moisture, heat, sunlight, and contamination.
    Storage Store Sinochem Quanzhou HDPE QZF144 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and oxidizing agents. Keep original bags or containers sealed, palletized, and off the floor. Avoid moisture, dust, and contamination. Maintain good housekeeping, follow the manufacturer’s SDS and local regulations, and prevent static charge buildup during handling.
    Shelf Life Shelf life is 24 months when stored unopened in original packaging, in a cool, dry, ventilated area, away from sunlight.
    Application of Sinochem Quanzhou HDPE QZF144

    On extrusion blow moulding lines configured with a reciprocating screw and a 45 mm to 75 mm barrier screw, Sinochem Quanzhou HDPE QZF144 is charged as the monolayer wall resin for narrow-neck detergent, household-cleaner, and water-based agrochemical bottles. A starting production formulation for a 1 L pour bottle comprises 96.4 wt% QZF144, 2.8 wt% white titanium dioxide masterbatch with 60 wt% pigment loading, 0.5 wt% silicone-based slip additive, and 0.3 wt% antioxidant masterbatch. The dry blend is gravimetrically dosed at the feed throat; feed-zone temperature is 35–45 °C, compression-zone temperature 180–195 °C, metering-zone temperature 195–205 °C, and die head temperature 180–200 °C. Melt temperature at the die exit is kept between 190 °C and 208 °C and measured with an immersion thermocouple; this window controls parison elongation consistency. Blow-up ratio is set at 2.2:1 to 3.0:1 for cylindrical bottles, and mould temperature is maintained at 8–18 °C in bottle-contact zones to suppress surface haze. Cycle time on a two-cavity shuttle blow moulder ranges from 12 s to 18 s for a 1 L bottle. Axial parison programming with a 10-point wall-thickness profile is required; label-panel minimum wall thickness is 0.45 mm, while pinch-off zones are validated by a 1.2 m drop test per GB/T 4857.17 or ASTM D2463-15 Procedure B. Food-contact compliance for this segment is limited to grades specifically declared under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011; for non-food household chemicals, REACH Annex XVII restrictions on phthalates and heavy metals apply. Terminal parts include 250 mL to 5 L bottles for liquid detergent, laundry softener, surface cleaner, wet-wiper solution, and water-based agrochemical formulations.

    How Does QZF144 Behave as the Structural Layer in Six-Layer EVOH Barrier Containers?

    In six-layer coextrusion blow moulding of solvent-based industrial chemicals, QZF144 is specified as the outer virgin skin and inner virgin skin, while central regrind, tie, and barrier resins complete the structure. The layer configuration is HDPE skin/regrind/tie/EVOH/tie/HDPE skin with a thickness distribution of 15/25/2/4/2/52 % of total wall. EVOH with 32 mol% ethylene content is selected for aromatic solvent barrier, and the tie layer is a maleic anhydride-grafted HDPE with a graft level of 0.8–1.2 wt%. Melt temperatures are 200–215 °C for the QZF144 skins, 203–213 °C for EVOH, and 198–210 °C for the tie layer; die temperature is held at 205–210 °C. The die gap is set between 2.0 mm and 3.5 mm for a 10 L jerrycan, and the blow-up ratio is 2.5:1. Mould clamping force per cavity is 180–220 kN. Adhesion of the coextruded structure is tested by peel according to ASTM D1876; a peel value below 2 N/15 mm at the tie/EVOH interface triggers line-stop and die-gap correction. Resultant 5 L to 20 L containers are type-approved under UN 3H1 for liquid dangerous goods packaging when wall thickness, leak-tightness, and drop tests meet ADR 6.1.5.2.4. For food contact, EU Regulation (EU) No 10/2011 requires an overall migration limit of 10 mg/dm² using 10% ethanol, 3% acetic acid, and 20% ethanol simulants; the use of QZF144 is permissible only when the producer’s batch declaration covers food-contact grade. Terminal products include barrier jerrycans for aromatic hydrocarbon solvents, methyl ester-based products, and liquid fertilizers.

    Compounding plants that process post-industrial HDPE regrind in excess of 60 wt% introduce QZF144 as a virgin let-down resin to restore melt strength and drop-impact toughness in non-food injection-moulded articles. A trials formulation for structural storage crates uses 70 wt% washed post-industrial HDPE flake with a melt flow rate of 0.6 g/10 min at 190 °C/2.16 kg, 21 wt% QZF144, 5 wt% calcium carbonate masterbatch with 80 wt% filler loading, 3 wt% carbon black masterbatch, and 1 wt% processing lubricant. The mixture is fed to a Coperion ZSK 58 MC18 twin-screw extruder with a 52:1 L/D ratio, run at 300–450 min⁻¹ screw speed and barrel profile 160/180/190/195/195/190/180 °C. The melt temperature is maintained below 210 °C by adding filler through a side feeder at barrel 7 to reduce viscous heating. Vacuum degassing at -0.08 MPa is applied at barrel 9. Pellets are formed on an underwater pelletizer with die-face cutter speed 1900–2500 min⁻¹. Resulting pellets are tested for tensile yield stress per ISO 527-2/1A at 4 mm thickness; values below 21 MPa trigger reformulation or a reduction in regenerated flake. Formulators should not blend QZF144 with propylene-dominant regrind above 5 wt% because separate-phase polypropylene domains reduce environmental stress crack resistance and produce delamination at gate regions. Compliance for non-food compound under REACH Article 33 and EU Directive 2011/65/EU Annex II restricts cadmium, lead, mercury, and hexavalent chromium to no more than 100 mg/kg per homogeneous material. Terminal products include structural crates, industrial pallets, outdoor furniture slats, and underground cable covers.

    Application-to-compliance and processing-anchor matrix
    Downstream sectorFormulation anchorCritical processing boundaryPrimary standard
    Monolayer narrow-neck bottle blow moulding96.4 wt% QZF144 / 2.8 wt% TiO₂ masterbatch / 0.5 wt% slip / 0.3 wt% antioxidantMelt 190–208 °C; blow ratio 2.2–3.0:1FDA 21 CFR 177.1520; EU 10/2011; GB 4806.7
    Six-layer EVOH barrier jerrycan blow mouldingSkin/regrind/tie/EVOH layer ratio 15/25/2/4/2/52 %Melt 200–215 °C; die gap 2.0–3.5 mmUN 3H1; ADR 6.1.5.2.4; EU 10/2011
    High-regrind non-food compounding70 wt% post-industrial HDPE flake / 21 wt% QZF144 / 5 wt% CaCO₃ masterbatch / 3 wt% carbon black / 1 wt% lubricantTwin-screw 52:1 L/D; melt below 210 °CREACH Article 33; EU 2011/65/EU Annex II
    Closure modification by injection moulding15–25 wt% QZF144 in 8–15 g/10 min MFR HDPE base96-cavity hot runner; clamp 4000–6000 kNEU 1935/2004; EU 10/2011; EN 1186-1
    Sheet extrusion and thermoforming94 wt% QZF144 / 4 wt% UV masterbatch / 1 wt% antistatic / 1 wt% slip-antiblockSheet surface 160–175 °C; roll stack 70–85 °CGB/T 4857.5; ISO 12048
    Open-head pail accumulator blow moulding5–10 wt% white masterbatch / 0.5 wt% processing aid in QZF144Melt 185–200 °C; cycle 75–110 sUN 1H2; ADR 6.1.5; ISO 12048

    When Closure Manufacturers Blend QZF144 into High-MFI HDPE to Lift Environmental Stress Crack Resistance

    Multi-cavity injection moulding of tamper-evident closures uses a high-flow HDPE base resin with an MFR of 8–15 g/10 min at 190 °C/2.16 kg; QZF144 is dry-blended at 15–25 wt% to raise environmental stress crack resistance without reducing screw recovery excessively. The blend is mixed in a high-intensity paddle mixer at 200 min⁻¹ for 90 s; batch-to-batch variation is controlled by melt flow rate checks per ISO 1133-1:2022 Procedure A. Moulding is performed on a 96-cavity hot-runner mould with valve-gate sequencing and a clamping force of 4000–6000 kN. Barrel temperatures are 200–240 °C, hot runner manifold 215–225 °C, nozzle tip 225–235 °C, and mould temperature 8–15 °C. Hold pressure is 40–60% of injection peak pressure, with hold time 1.5–3.0 s. Deflection temperature is measured per ISO 75-2 Method B at 0.45 MPa. The closures are tested for removal torque at 1.5–2.5 N·m and for stress cracking in 20% sodium hydroxide at 50 °C for 24 h according to an internal method derived from ASTM D1693-15. Published data for QZF144 in this specific closure-modifier application is limited; each blend ratio must be validated on the target mould because gate freeze-off and weld-line strength vary with hot-runner design. Compliance includes EU Regulation (EC) No 1935/2004 Articles 3, 11, and 12, and EU Regulation (EU) No 10/2011; migration testing uses EN 1186-1 total-immersion methods. The end closures include 28 mm and 38 mm water bottle caps, 1881-style carbonated soft-drink closures, and pharmaceutical vial caps.

    Sheet Extrusion and Plug-Assist Thermoforming Window for Returnable Transit Packaging

    QZF144 is converted into monolayer sheet for heavy-gauge thermoformed transit trays and dunnage. A monolayer flat-die sheet line with a 120 mm vented extruder, 32:1 L/D, and a 1200 mm coat-hanger die supplies 3–6 mm sheet. The formulation is 94 wt% QZF144, 4 wt% UV-stabilized HDPE carrier masterbatch, 1 wt% antistatic masterbatch, and 1 wt% slip/antiblock masterbatch. Barrel zones 1–5 are set at 175/185/190/195/200 °C; gear pump inlet pressure is 12–18 MPa; melt temperature after the screen changer is 195–205 °C. Die-lip opening is set at 3.5 mm for 4 mm finished sheet, and roll-stack temperature is 70–85 °C on polished chrome rolls. The sheet is thermoformed on a plug-assisted machine with a ceramic composite plug, sheet surface temperature 160–175 °C, forming pressure 0.6–1.0 MPa, and cycle time 20–30 s. Critical acceptance is bottom-corner thinning below 15% of nominal when measured by ultrasonic thickness mapping; gel counts above 50 particles/kg captured by a 50 µm screen pack are treated as lot failure. Pre-drying at 80 °C for 2 h is required when ambient relative humidity exceeds 60% and regrind content exceeds 20 wt%. Compliance for industrial returnable transit packaging references GB/T 4857.5 drop testing and ISO 12048 stacking-compression testing. Terminal products include reusable thermoformed trays, rack dunnage, and protective corner boards.

    Accumulator-Head Blow Moulding of 20 L Open-Head Shipping Pails Demands a Lower Melt-Temperature Ceiling

    On accumulator-head blow moulders producing 20 L open-head shipping pails, QZF144 is run at a melt temperature of 185–200 °C; operation above 210 °C in the accumulator increases the probability of black speck formation because of extended melt residence time. A single-station machine with a 3.5–4.0 kg shot accumulator, 80 mm plasticating screw, and 2.5:1 blow-up ratio is used. The formulation is 5–10 wt% white masterbatch and 0.5 wt% processing aid in QZF144; the white masterbatch is increased to 10 wt% only for high-opacity outdoor containers. The parison die gap is programmed from 3.0 mm at the base to 2.0 mm at the top to compensate for parison sag over a 600 mm shot length. Mould cooling water is 8–15 °C in turbulent-flow service. Cycle time is 75–110 s, with blow-air pressure at 0.8 MPa for 40–50 s. Stacking strength is tested at 40 °C for 24 h per ISO 12048; top-rim warpage below 2 mm measured on a granite surface plate is the release criterion. Pails are type-approved as UN 1H2 solid dangerous goods packaging under ADR 6.1.5. Terminal products include open-head shipping pails for grease, ink, water-based adhesive, and non-corrosive granular chemicals.

    Free Quote

    Competitive Sinochem Quanzhou HDPE QZF144 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinochem Quanzhou HDPE QZF144 is a pelletized high-density polyethylene resin intended for blown film and thin-gauge packaging structures in which stiffness, tear resistance, and convertibility must be controlled without the high melt strength required by thick-gauge film. The grade carries a nominal density of 0.944 g/cm³ when tested in accordance with ISO 1183-1:2019 and a melt flow rate of 0.40 g/10 min at 190 °C/2.16 kg when tested in accordance with ISO 1133-1:2022. These two values define the product as a medium-molecular-weight HDPE film resin: the density is slightly below the 0.949 g/cm³ to 0.952 g/cm³ range common for high-stiffness HDPE film, while the melt flow rate is substantially higher than the 0.04 g/10 min to 0.10 g/10 min range used for high-melt-strength blown film. The practical consequence is that QZF144 processes with lower extruder head pressure and improved draw-down but requires tighter control of bubble stability and die lip condition than conventional high-molecular-weight HDPE film grades.

    The resin is supplied as uniform pellets with a typical lot-to-lot density variation of ±0.002 g/cm³ and a melt flow rate tolerance of ±10% of the nominal value. These tolerances are consistent with gas-phase HDPE production and are significant for converters running closed-loop gauge control because density shifts alter film yield and melt flow rate shifts alter screw feed stability. On a production-scale blown film line with a 65 mm single-screw extruder and 30 L/D barrier screw, batch-to-batch MFR variation of ±10% may require a barrel temperature offset of 5 °C to 7 °C to maintain constant die pressure and gauge profile.

    What Differentiates QZF144 from Conventional HDPE Blown Film Resins?

    The principal differences are melt flow rate, density, and their combined effect on orientation. Conventional HDPE blown film grades with melt flow rates of 0.04 g/10 min to 0.10 g/10 min retain high molecular weight and high melt strength, allowing stable bubble formation at blow-up ratios of 4.0:1 or higher on air-cooled lines. QZF144 has a melt flow rate of 0.40 g/10 min, which lowers viscosity at equivalent processing temperature and reduces bubble stability on unmodified air rings. The advantage is lower head pressure and higher output on torque-limited extruders. The disadvantage is that the bubble is less tolerant of abrupt air ring velocity changes, die-lip contamination, or winder tension variation. Field observations on a 65 mm extruder with a 300 mm die indicate that the bubble responds more quickly to blower voltage changes than a 0.04 g/10 min resin, so air ring control loops with proportional-integral tuning should be set with shorter integral times and lower gain to avoid oscillation.

    The density of 0.944 g/cm³ is also different. Film grades at 0.949 g/cm³ to 0.952 g/cm³ have higher crystallinity, higher tensile yield strength, and lower water vapour transmission. The 0.944 g/cm³ level shifts failure behaviour away from brittle puncture and toward ductile yielding, but it lowers film modulus. Specifiers selecting QZF144 instead of a 0.952 g/cm³ grade typically accept a modulus reduction in exchange for improved dart impact and reduced film splitting. Under ASTM D1709-16a Method A, HDPE film in this density range generally shows higher gram-per-micrometre dart drop than higher-density HDPE of the same gauge, although exact values depend on die gap, frost line height, and cooling rate. Comparative tear strength measured to ASTM D1922-15 is also influenced by orientation: transverse direction tear is usually higher than machine direction tear, and the imbalance becomes more pronounced at higher blow-up ratios.

    Die Gap and Blow-Up Ratio Sensitivity in Medium-Melt-Strength Film

    Because the melt flow rate of 0.40 g/10 min provides less melt strength than high-molecular-weight HDPE, the die gap must be kept narrow to maintain adequate shear and melt integrity. On a 50 mm single-screw extruder with a 30 L/D barrier screw, a die gap of 1.0 mm to 1.4 mm is typically suitable for QZF144. Wider gaps above 1.6 mm increase heavy-edge formation and make frost line control more difficult because the thicker melt web retains heat longer. A blow-up ratio of 3.0:1 to 3.5:1 is generally more stable for this melt flow rate than the 4.0:1 to 5.0:1 ratios used for high-molecular-weight HDPE film. Frost line height should be set between 8 and 12 die diameters on a conventional single-lip air ring; lower frost lines increase quench rate and improve film clarity but reduce transverse direction tear strength.

    Output can be improved by using internal bubble cooling or a dual-lip air ring, but the melt strength of QZF144 is not sufficient to tolerate rapid bubble diameter changes during start-up. On lines fitted with a capacitance gauge and closed-loop air ring control, bubble diameter variation should be held below ±2% of the lay-flat width to prevent gauge-band formation. Winder tension should be maintained below 15 N/100 mm of film width; higher tension tends to neck the film and produce permanent crease memory in laminated structures. Die lip cleaning must be performed at intervals short enough to prevent localised die-lip buildup, because the lower melt strength makes the bubble more sensitive to local draw acceleration from contamination points.

    Typical barrel temperature settings for a 65 mm extruder with a 30 L/D barrier screw are 180 °C in zone 1, 190 °C in zone 2, 200 °C in zone 3, and 205 °C in zone 4, with the adapter and die held at 210 °C. The target melt temperature is 204 °C to 215 °C at the die lip. Screw speed should be limited to the range where melt pressure remains below 350 bar; higher pressure indicates excessive shear heating or improper die gap. A barrier screw with a Maddock mixing section provides better melt homogeneity for this grade than a conventional three-zone screw, particularly when the resin is run with high levels of masterbatch.

    If Moisture Pickup Exceeds 200 ppm, Drying Becomes Mandatory

    HDPE is generally considered non-hygroscopic, but pellet surface moisture can accumulate during high-humidity storage or after railcar unloading in warm, humid environments. For QZF144, moisture levels above 200 ppm can produce surface streaking, micro-bubbles, and poor melt pressure stability. A desiccant-hot-air dryer set at 80 °C to 90 °C with residence time of 2 to 4 hours is recommended when the resin has been exposed to relative humidity above 60% for more than 24 hours. The drying air dew point should be -20 °C or lower. Pellets stored in outdoor silos in south-coastal climates should be transferred to indoor hoppers at least 12 hours before extrusion to reduce surface condensation risk.

    Oxidative degradation during processing is controlled by the stabilizer package, but melt temperatures above 220 °C sustained for more than 15 min can generate gel defects and yellowing. Extruder start-up after shutdown should avoid long hold times at full barrel temperature; the screw should be turned at low speed within 10 min or the rear zones should be cooled to 150 °C during idle. The grade should not be blended with polypropylene reclaim at levels above 3 wt% unless a compatibilizer and additional stabilizer are added, because incompatible PP domains create haze and reduce dart impact under ASTM D1709-16a testing.

    Mechanical Property Development Depends on Orientation Balance

    Film property development for QZF144 is controlled primarily by the balance between machine direction orientation and transverse direction relaxation. In a film of 25 µm nominal thickness produced at a blow-up ratio of 3.0:1 and a freeze line of 250 mm, tensile properties measured to ASTM D882-18 normally show machine direction yield strength in the range of 20 MPa to 24 MPa and elongation at break above 500%. These ranges are not product-specific certificates; they are typical for HDPE film with a density of 0.944 g/cm³ and should be confirmed by laboratory testing. Elmendorf tear strength measured to ASTM D1922-15 is expected to be higher in the transverse direction than in the machine direction, but the magnitude depends on molecular orientation. Dart drop measured to ASTM D1709-16a Method A is sensitive to gauge uniformity; a 2% gauge band can lower dart drop by 10–15% relative to uniform film.

    Water vapour transmission rate should be measured to ASTM E96/E96M-22a at 38 °C/90% RH; lower density HDPE films generally transmit more moisture than 0.952 g/cm³ film, but the difference is small at thicknesses below 30 µm. Oxygen permeability measured to ASTM D3985-17 is higher than high-density HDPE film grades but lower than LDPE film. These barrier differences matter in dry food packaging and industrial interleaving film where moisture uptake or odour retention must be controlled.

    PropertyQZF144Conventional HDPE film grade (0.950/0.04)LLDPE film grade (0.918/1.0)
    Density (g/cm³)0.9440.949–0.9520.918–0.920
    Melt flow rate at 190 °C/2.16 kg (g/10 min)0.400.04–0.100.90–1.10
    Film stiffnessintermediatehighlow
    Dart impactintermediate to highmoderatehigh
    Bubble stabilitymoderatehighmoderate to low
    Moisture barriermoderatehighlow to moderate

    Applications for QZF144 include carrier bags, flat bags, interleaving film, and light-gauge overwrap where a balance of stiffness and tear resistance is required. The lower density compared with higher-density HDPE grades makes the film more tolerant of creasing and less prone to split propagation along machine-direction scoring. In coextrusion or lamination, QZF144 can be used as a high-modulus core layer between sealant skins, but the high melt flow rate requires stable extruder output and fast die temperature control to prevent viscosity mismatch at the interface. The grade is not recommended for high-pressure pipe or sheet where a bimodal molecular weight distribution and density of 0.948 g/cm³ or higher are required. It is also not suitable for thick-walled blow-moulded containers exposed to high environmental stress cracking; a dedicated blow-moulding grade with a density of 0.950 g/cm³ or higher and an ESCR rating tested to ASTM D1693-21 should be specified.

    Food-contact compliance must be verified for the specific conversion process under FDA 21 CFR 177.1520 or EU Regulation No 10/2011. The resin is not universally approved for all food types, and migration testing should be performed on the finished film because processing aids, print inks, and coating layers affect the final compliance status. Converters should also verify the lot-level certificate of analysis for density, melt flow rate, and ash content before releasing film for use in sensitive packaging.

    Top