| HS Code | 876470 |
| Product Name | Sinochem Quanzhou HDPE HHM5502LN |
| Manufacturer | Sinochem Quanzhou Petrochemical Co., Ltd. |
| Polymer Type | High Density Polyethylene (HDPE) |
| Grade | HHM5502LN |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Density | 0.955 g/cm³ |
| Tensile Yield Strength | ≥26 MPa |
| Tensile Strength At Break | ≥30 MPa |
| Elongation At Break | ≥600% |
| Flexural Modulus | ≥1100 MPa |
| Vicat Softening Temperature | ≥125 °C |
| Environmental Stress Cracking Resistance | ≥1000 h |
| Hardness Shore D | ≥65 |
| Brittleness Temperature | ≤-70 °C |
| Bulk Density | 0.55-0.60 g/cm³ |
| Ash Content | ≤0.03% |
| Moisture Content | ≤0.05% |
As an accredited Sinochem Quanzhou HDPE HHM5502LN factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinochem Quanzhou HDPE HHM5502LN is packed in 25 kg woven bags, with 40 bags per pallet (1,000 kg). |
| Container Loading (20′ FCL) | Container Loading (20′ FCL) for Sinochem Quanzhou HDPE HHM5502LN: 25 kg bags, around 17–18 MT per container, palletized or loose. |
| Shipping | Sinochem Quanzhou HDPE HHM5502LN is a non-hazardous polyethylene resin, not regulated for transport. It is shipped in 25 kg bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped, in 20'/40' sea containers from Quanzhou, China. Keep dry, away from heat and direct sunlight. |
| Storage | Store Sinochem Quanzhou HDPE HHM5502LN in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, UV radiation, and strong oxidizing agents. Keep original bags or containers tightly closed. Use pallets, avoid floor contact, and prevent moisture, dust, or contamination. Maintain moderate stacking to avoid deformation. Follow first-in, first-out stock rotation under normal ambient conditions. |
| Shelf Life | Sinochem Quanzhou HDPE HHM5502LN has a shelf life of approximately 24 months when stored dry, cool, ventilated, and away from sunlight. |
Shuttle blow molding machines equipped with accumulator heads and 70–90 mm diameter, 24:1–30:1 L/D screws convert HHM5502LN into industrial liquid chemical packaging. The resin is processed at a melt temperature of 185–205 °C, with die gap settings held between 1.8 mm and 2.4 mm to control parison wall thickness. A 10–30 point parison programmer is required because the bottom pinch-off zone of a 60 L jerrican demands thicker wall sections than the sidewall body; without programmed parison distribution, the weld line exhibits batch-to-batch thickness variability. Blow air pressure is set between 0.6 MPa and 0.8 MPa, and mold circulation water is maintained at 15–25 °C to prevent sink marks near the handle bridge and closure area. The compliance framework rests on UN 3H1 performance certification under the UN Model Regulations for the transport of dangerous goods, combined with ADR/RID 6.1 and IMDG Code requirements for Class 3, 6.1, 8, and 9 liquids. Where food contact service is declared, the base resin is assessed under FDA 21 CFR 177.1520(c); EU 10/2011 overall migration testing at 40 °C for 10 days applies. The formulation addition ratio comprises 97.0–98.5 wt% HHM5502LN plus 1.5–3.0 wt% pigment and processing masterbatch. Closed-loop regrind from flash and trim is added at 20–25 wt% of total shot weight; this is the practical upper limit because UN retest performance becomes lot variable above 25 wt%. Terminal finished product types include 20 L, 25 L, 30 L, and 60 L narrow-neck jerricans for petroleum additives, surfactants, crop protection adjuvants, liquid dyestuffs, and water treatment chemicals. External post-consumer recyclate above 15 wt% is not recommended in this configuration without requalification due to ESCR reduction and variable melt strength.
In coextrusion of 1000 L intermediate bulk container inner bottles, HHM5502LN is assigned to the outer structural layers where drop-test robustness and top-load stability are required from the blow molded inner bottle. The downstream production process uses a six-layer coextrusion blow molding line with three extruders—typically 75 mm, 60 mm, and 35 mm screw diameters, each with L/D ratios of 24:1–30:1—feeding a spiral mandrel die and accumulator head. The melt temperature window is constrained by the thermal degradation of the PA or EVOH barrier; the HHM5502LN outer layers are processed at 190–210 °C, while the barrier layer is maintained below 220 °C, creating a narrow process window of approximately ±5 °C at the die. The layer mass balance in this construction is 50–60 wt% HHM5502LN across the outer and inner skins, 3–5 wt% PA or EVOH barrier, 2–4 wt% maleic anhydride grafted tie-layer, and 2.5–3.5 wt% carbon black/UV masterbatch in the outer skin. Reintroduced regrind is limited to 25–35 wt% and is directed only to the middle layers to avoid direct food-contact migration risk. The compliance framework includes UN 31H1 certification for rigid plastics IBCs under ADR 6.5.2, ISO 16106:2006 for design and testing of packaging for dangerous goods, and EU 10/2011 with FDA 21 CFR 177.1520(c) where the inner bottle is used for liquid food ingredients. Terminal finished product types are 1000 L IBC inner bottles for agrochemical formulations, solvent-based cleaning concentrates, liquid fertilizers, and oxidation-sensitive products where the barrier layer reduces oxygen permeation below the level achievable with monolayer HHM5502LN. Published data for this exact six-layer HHM5502LN structure are limited; permit-by-qualification tests based on drop impact at -18 °C and stack load at 40 °C are therefore specified before service.
Pharmaceutical container shells are blown on single-station shuttle or long-stroke reciprocating machines with polished stainless steel contact surfaces and 0.2 µm filtered cooling air. HHM5502LN is processed at 180–200 °C melt temperature; mold surfaces are held at 10–18 °C to minimize shrinkage variation and dimensional drift in the thread finish. The compliance framework includes USP 661.1 plastic materials of construction, Ph. Eur. 3.1.3 polyethylene for containers for oral solid dosage forms, FDA 21 CFR 177.1520(c), and EU 10/2011. Organoleptic and total organic carbon limits are part of the release panel; low-odor behavior is evaluated by sensory threshold methods referenced in USP 661.1 rather than by a single chemical assay. The formulation addition ratio is 100 wt% virgin HHM5502LN for the product-contact layer; if an external antistatic masterbatch is needed, it is kept at 1.5–2.5 wt% and is not introduced into the contact layer without migration testing. Regrind from the same plant may be used in the outer shell up to 20 wt% only when the container is not intended for sterile or parenteral service. The downstream production process is extrusion blow molding, not injection blow molding; the 0.35 g/10 min MFR of HHM5502LN measured under ISO 1133-1:2022 at 190 °C/2.16 kg is too low for injection blow molding cores. Terminal finished product types include 100 mL–1000 mL tablet and desiccant bottles, oral liquid dosage containers with induction-sealed liners, and veterinary product bottles. Amine-based slip additives must not be added to HHM5502LN in this application because they alter the sensory threshold results; silicone-free external lubricants are used on the extrusion screw only.
Automotive washer fluid reservoirs and coolant expansion tanks impose among the most severe pinch-off weld requirements on blow molded HDPE. The downstream production process is continuous extrusion blow molding on machines with 45–65 mm screws and 20:1–24:1 L/D ratios; the parison is dropped between moving mold halves, and the bottom pinch-off is subjected to 0.30–0.50 MPa leak testing after deflashing. The compliance framework references ISO 4892-2 for xenon-arc weathering, ISO 527-2 for tensile yield stress, and ISO 179-1/1eA for Charpy notched impact at -30 °C. Published data for this exact grade in washer reservoir configurations are limited; OEM qualifications therefore use the above standards with lot-specific HHM5502LN data rather than a single generic datasheet value. The formulation addition ratio is 96.0–98.0 wt% HHM5502LN with 2.0–4.0 wt% carbon black masterbatch; for color-matched white or grey tanks, the masterbatch loading is reduced to 1.5–2.5 wt% and a separate UV stabilizer masterbatch at 0.5–1.0 wt% is added. Regrind is limited to 10–15 wt% because higher regrind fractions shift the failure mode from ductile to brittle at the pinch-off under sub-zero impact. Terminal finished product types include 2.5 L–5.0 L windshield washer fluid reservoirs, 1.5 L–3.0 L coolant expansion tanks, and auxiliary reservoir bottles for off-highway equipment. Carbon black masterbatch loadings above 4 wt% require additional ISO 179-1/1eA lot testing because carbon black dispersion quality, not only loading, influences sub-zero impact behavior.
Thick-walled agricultural sprayer tanks are blown on stationary blow molding machines with clamp forces above 600 kN, screw diameters of 80–120 mm, and L/D ratios of 25:1–30:1. The downstream production process uses a diverging die gap of 2.0–3.0 mm and parison programming with 50–100 points to maintain wall thickness above 3 mm at the lower pinch-off and 1.8–2.2 mm in the sidewall. Internal parison cooling at 0.10–0.20 MPa compressed air is cycled for 20–40 s to reduce cycle time in sections thicker than 4 mm. The compliance framework for the terminal products references ASTM D1998-21 for polyethylene upright storage tanks, ISO 527-2 for tensile yield stress, and ISO 179-1/1eA for impact strength. Where the tanks contact agricultural chemical solutions, chemical compatibility is assessed by immersion at 23 °C for 30 days under ASTM D543-21; published data for this specific grade are limited for high-concentration solvent-based crop protection mixtures, so compatibility testing on the final tank geometry is required. The formulation addition ratio is 96–98 wt% HHM5502LN, 2.0–4.0 wt% UV stabilizer masterbatch, and 0.5–1.0 wt% color masterbatch; regrind is added at 15–20 wt% from the same production line. Terminal finished product types include 30 L–100 L tractor-mounted sprayer tanks, water softener brine tanks, hydroponic nutrient reservoirs, and portable foam marker tanks. UV masterbatch loadings above 4 wt% reduce weld-line ductility and are not used because the bottom pinch-off is already the lowest elongation region.
Competitive Sinochem Quanzhou HDPE HHM5502LN prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinochem Quanzhou HDPE HHM5502LN is a high-molecular-weight high-density polyethylene grade formulated for extrusion blow moulding of rigid containers and industrial packaging. The resin is produced on a slurry-loop polymerisation line with a chromium-based catalyst system; the LN suffix identifies a low-odour post-finishing sequence that reduces residual volatile compounds after pelletization. At 23 °C, the nominal density is 0.953–0.958 g/cm³ when measured according to ISO 1183-1:2019. Melt flow rate under a 21.6 kg load at 190 °C is 0.30–0.40 g/10 min using ISO 1133-1:2022. This rheological position places HHM5502LN in the high-melt-strength blow moulding segment: the low melt index supports parison hang strength for large bottles and drums, but the resin is not intended for thin-wall injection moulding, blown film, or high-speed small-bottle applications. Pellets are cylindrical, supplied in 25 kg multi-wall bags or octabins, and the bulk density is typically 0.55–0.60 g/cm³. Storage below 50 °C and protection from condensation are required to prevent surface moisture defects during subsequent processing.
The grade is positioned for applications in which the mechanical property envelope of an HHM5502-class high-density polyethylene is required, but volatile-related odour or taste rejection thresholds are tighter than those for standard blow moulding grades. Finished containers should be qualified in filled-container stack tests, drop tests at -20 °C, and permeation trials before commercial adoption. The values contained in this document are nominal and do not replace a lot-specific certificate of analysis.
Lot release data are reported against a defined property schedule. The table below assembles the manufacturer’s nominal property envelope and the corresponding test designations. Certificates of analysis for individual batches supersede the values listed here, particularly where a converter is qualifying a new lot for dangerous goods packaging or food-contact service.
| Property | Nominal value | Test method | Specimen or condition |
|---|---|---|---|
| Density | 0.953–0.958 g/cm³ | ISO 1183-1:2019 | 23 °C, immersion method |
| Melt flow rate | 0.30–0.40 g/10 min | ISO 1133-1:2022 | 190 °C, 21.6 kg, Method A |
| Tensile stress at yield | 24–28 MPa | ISO 527-2:2012 | Type 1B, 50 mm/min |
| Tensile elongation at break | >600% | ISO 527-2:2012 | Type 1B, 50 mm/min |
| Flexural modulus | 1050–1250 MPa | ISO 178:2019 | 2 mm/min |
| Charpy notched impact strength | 18–24 kJ/m² | ISO 179-1/1eA:2010 | 23 °C, edgewise |
| Environmental stress crack resistance | >600 h | ASTM D1693-15 | Condition B, 100% Igepal CO-630 |
| Heat deflection temperature | 72–80 °C | ISO 75-2:2013 | 0.45 MPa, Method B |
| Vicat softening temperature | 125–129 °C | ISO 306:2022 | A50, 10 N |
Environmental stress crack resistance is the principal long-term failure boundary for rigid high-density polyethylene packaging containing surfactants, esters, or aggressive hydrocarbon mixtures. The ASTM D1693-15 F50 result exceeding 600 h is measured on a compression-moulded specimen; blow-moulded parts with high frozen-in stress, sharp bending radii, or poorly formed weld lines can fail earlier. The laboratory value is therefore a ranking tool rather than a direct service-life prediction. If finite-element simulation of parison sag is required, zero-shear viscosity should be measured by parallel-plate rheometry because it is not stated in typical lot-release certificates. Published data for this specific configuration is limited.
On shuttle blow moulding lines with gravimetric dosing and grooved-barrel extruders of 60–90 mm screw diameter and L/D ratios between 24:1 and 30:1, HHM5502LN can be plastified at melt-temperature set points of 200–230 °C. The die-head temperature should be maintained in the 205–225 °C band to limit melt fracture; heater zones below 180 °C can generate gels and surface roughness. Accumulator-head machines for 20–200 L containers require parison programming with a radial die-gap reduction of 15–30% at the pinch zone to compensate for parison sag. Blow air pressure of 0.6–1.0 MPa and mould coolant temperatures of 10–30 °C are standard boundary conditions for medium-wall containers from 1.5 mm to 3.0 mm wall thickness. For 200 L drum production on accumulator machines, clamp force is typically 400–800 tonnes; the parison programmer should avoid axial wall-thickness gradients steeper than 1:0.55 to maintain pinch-off weld integrity. Pellet surface moisture from storage at relative humidity above 60% should be removed by drying at 80 °C for 2 hours; the resin does not require desiccant drying, but cold pellets can carry condensation into the feed throat and produce splay. Regrind addition up to 20 wt% is tolerated when the regrind is dry, dust-free, and of identical grade. Higher regrind fractions reduce parison hang strength and may lower environmental stress crack resistance. Contamination with polypropylene, polyvinyl chloride, polyethylene terephthalate, or metal fines must be prevented through magnetic separation and sieve screens in the material-handling system.
Compliance of the finished article is jurisdiction-specific. For food-contact packaging, the converter must validate the complete container against FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 overall migration limits. The base resin’s low-odour post-treatment reduces residual extractables, but processing aids, regrind, colour concentrates, and barrier layers can alter the extractive profile of the moulded part. For automotive fuel tanks, finished-part permeation testing under ECE R34 or oxygen permeation testing per ASTM D3985-17 is required; the property table does not provide hydrocarbon permeation coefficients. The product is not intended for continuous service above 80 °C, steam sterilisation, or repeated autoclave cycles, because warpage and accelerated stress cracking occur beyond the heat deflection boundary. Do not combine the grade with amine-based antistatic additives or certain hindered-amine light stabilizers at high melt temperatures unless neutralization is verified; acid-base interaction with chromium-catalyst residues can produce yellowing, surface deposits, and organoleptic defects. If amine-containing masterbatches are unavoidable, pre-production trials must include odour, extractables, and surface-defect inspection.
Differentiation from the standard HHM5502 grade is primarily a reduction in volatile organic residue rather than a shift in molecular weight distribution. The LN variant is intended for applications where paint-shop, food-package, or closed-vehicle interior odour rejection thresholds impose a tighter ceiling on residual oligomers. Both grades share a similar density and melt flow envelope, and both can be processed on the same blow moulding equipment without barrel, screw, or die changes. HHM5502LN should not be considered a drop-in for HXM50100-type film grades; blown film requires lower melt viscosity and a different bubble-stability rheology. Compared with butene-comonomer blow moulding high-density polyethylene of similar density, HHM5502LN typically exhibits higher die swell and greater parison hang strength, but lower melt extensibility at deep draw ratios. Against metallocene-catalysed high-density polyethylene, HHM5502LN provides a wider processing window for wall-thickness consistency in non-round bottles, but lower clarity and a higher seal-initiation temperature. Against bimodal PE100 pipe compounds, HHM5502LN carries no long-term hydrostatic strength classification under ISO 9080:2022 and must not be used for pressure pipe. The product is also poorly matched to small blow moulded containers below 10 L capacity, where its high die swell can generate excessive flash and require die-lip modification.
The most common failure signature at the lower processing-temperature boundary is shark-skin surface roughness on the parison outer skin. The correction is to raise the die-head zone to at least 205 °C or reduce line speed. At the upper temperature boundary, parison sag becomes measurable as non-uniform wall thickness in the top and bottom pinch-off zones. Weld-line cracking in drop tests at -20 °C is typically associated with insufficient clamp pressure, contaminated pinch-off edges, or excessively steep parison programming rather than with base-resin lot variation. Batch-to-batch variation of melt flow rate within the specification band is normally less than ±0.03 g/10 min under plant statistical process control; nevertheless, converters should verify certificates of analysis for lots near the specification boundaries. For 20 L diesel exhaust fluid containers coextruded with an ethylene-vinyl alcohol barrier layer, the high-molecular-weight polyethylene layer supports the parison during accumulator transfer; pre-blow delay of 0.3–0.8 s and pre-blow pressure of 0.15–0.30 MPa are typical starting conditions. Published data for this specific configuration is limited, and machine-specific trials are required to establish the acceptable operating window.
Before converting an existing mould or downstream automation cell, the converter should verify die swell, parison length, and pinch-off geometry using a short-run trial. The molecular weight distribution supports high die swell, which can require die-lip widening or reducer rings in some tooling. Wall-thickness distribution should be mapped by segmenting moulded parts at 12 radial positions, and top-load performance should be measured according to ISO 12048:1994 or the applicable packaging-group test. For UN-certified dangerous goods packaging, drop, stack, and leakproofness tests under the applicable UN Model Regulations are mandatory. The resin lot data alone are not sufficient for certification of the finished container.