| HS Code | 328111 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Tensile Strength At Yield | 24 MPa |
| Tensile Elongation At Break | >600% |
| Flexural Modulus | 1000 MPa |
| Notched Izod Impact Strength 23 C | 50 kJ/m² |
| Notched Izod Impact Strength 30 C | 10 kJ/m² |
| Vicat Softening Temperature | 127 °C |
| Environmental Stress Cracking Resistance 10 Igepal | >1000 h |
| Shore D Hardness | 65 |
| Melting Point | 132 °C |
| Thermal Expansion Coefficient | 1.2E-4 /°C |
As an accredited Sinochem Quanzhou HDPE HHM5502BN factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinochem Quanzhou HDPE HHM5502BN is packed in 25 kg woven bags, palletized and stretch-wrapped for safe industrial transport. |
| Container Loading (20′ FCL) | Typically loaded in 25 kg bags, palletized; a 20′ FCL holds about 18–20 MT of Sinochem Quanzhou HDPE HHM5502BN. |
| Shipping | Sinochem Quanzhou HDPE HHM5502BN is shipped as a non-hazardous polymer resin in 25 kg PP woven bags or jumbo bags, palletized and stretch-wrapped. It is transported by sea/land in clean, dry containers. Keep away from moisture, heat, and direct sunlight. No special hazardous shipping requirements apply. |
| Storage | Store Sinochem Quanzhou HDPE HHM5502BN in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original bags or octabins sealed, palletized, and off the floor. Prevent moisture, dust, oil, and chemical contamination. Avoid prolonged UV exposure and excessive stacking. Do not store outdoors. Use clean handling equipment; rotate stock and follow local regulations. |
| Shelf Life | Typically, Sinochem Quanzhou HDPE HHM5502BN shelf life is 24 months when stored unopened in cool, dry conditions away from sunlight. |
Sinochem Quanzhou HDPE HHM5502BN is a hexene-copolymer blow-molding high-density polyethylene with a nominal melt flow rate of 0.35 g/10 min at 190 °C/2.16 kg under ASTM D1238 and a density of 0.955 g/cm³ under ISO 1183-1. United Nations certified monolayer jerrycans and tight-head drums produced from this grade are specified for aggressive liquid chemicals, aqueous agrochemical intermediates, cleaning agents, and oil additives. Packaging intended for dangerous goods transport is qualified under ADR/RID, IMDG Code, and DOT 49 CFR Part 178, with compatibility guidance under ISO 16101; hydrocarbon-based substances require evidence of environmental stress crack resistance under ASTM D1693 Condition B before the packaged goods are approved. In 5 L–30 L 3H1/Y jerrycan production, the charge typically runs 100 wt% virgin HHM5502BN or 85 wt% virgin with 15 wt% in-house regrind recovered from flash and rejected preforms; carbon black masterbatch is metered at 1.0–2.0 wt%, processing aid at 0.2–0.5 wt%, and the regrind fraction is kept below 20 wt% to limit lot-to-lot ESCR variation. The extrusion blow molding line uses a grooved-barrel extruder with 55–75 mm screw diameter and L/D 24:1–30:1, an accumulator head with servo-operated parison programming, melt temperature 180–210 °C, mold circuit temperature 12–18 °C, and blow pressure 0.6–0.8 MPa; wall profiling is biased toward the lift-handle bridge and bottom pinch-off to pass UN stacking and drop tests. Terminal products include 5 L, 10 L, 20 L, 25 L, and 30 L jerrycans, 60 L tight-head drums, and twin-neck liquid fertilizer containers.
For agricultural chemical packaging, the capacity to process uncontaminated plant scrap at up to 20 wt% without destroying notched-tensile environmental stress crack resistance is the main qualification criterion. Agrochemical bottles and jerrycans are qualified as UN 3H1/Y packages and are placed on the EU market under Regulation (EC) No 1272/2008 classification and labelling obligations; the decisive polymer test methods are ASTM D1693 for ESCR and ISO 16770 for full-notch creep. In a monolayer 1 L–20 L bottle formulation, HHM5502BN represents 75–90 wt%, in-house regrind 10–20 wt%, carbon black/UV masterbatch 1.5–2.5 wt%, and antistatic masterbatch 0.1–0.3 wt% where filling lines require surface resistivity control. The blow molding process runs on single-station shuttle machines with 40–60 mm grooved-barrel extruders, L/D 24:1–28:1, melt temperature 190–210 °C, mold temperature 10–15 °C, and parison profiling that increases the pinch-off region wall thickness to 3.0–4.5 mm to resist cracking along the parting line. Terminal products include 1 L, 5 L, 10 L, and 20 L bottles for emulsifiable concentrates, suspension concentrates, and soluble powders. Regrind levels above 20 wt% are not recommended because ESCR retention may become batch-dependent, and lot-specific testing under ISO 16770 is then required.
| Application | Compliance reference | Test method reference |
|---|---|---|
| UN-certified jerrycans and drums | ADR/RID, IMDG Code, DOT 49 CFR Part 178, ISO 16101 | UN drop test, stacking test, hydraulic pressure test, ASTM D1693 |
| Agrochemical bottles and jerrycans | UN 3H1/Y, Regulation (EC) No 1272/2008 | ASTM D1693, ISO 16770 |
| Automotive fuel tanks and fluid reservoirs | ECE R34, FMVSS 301, SAE J2665 | Hydrocarbon permeation, fuel soak ESCR, SAE J2665 |
| IBC inner bottles | UN 31HA1/Y, ISO 16106, REACH | UN hydrostatic pressure test, UN vibration test |
| Barrier food bottles | EU 10/2011, FDA 21 CFR 177.1520, GB 9685-2016 | Overall migration, specific migration limit |
| Industrial water storage tanks | NSF/ANSI/CAN 61, DVS 2205 | Design verification under DVS 2205 |
Fuel tanks, diesel exhaust fluid reservoirs, and hydraulic oil tanks blow-molded from HHM5502BN exploit the resin’s high melt strength to minimize parison sag and the high molecular weight to resist stress cracking from fuel constituents. Regulatory compliance for automotive fuel tanks is governed by ECE R34 for approval of fuel tanks in vehicles, FMVSS 301 for fuel system integrity in the United States, and SAE J2665 for permeation measurement; emission limits are aligned with EPA and Euro evaporative requirements. In monolayer fluorinated tank production, HHM5502BN is used at 100 wt% by mass, carbon black concentrate at 1.5–2.5 wt%, antioxidant masterbatch at 0.2–0.5 wt%, and the interior surface is post-fluorinated with a fluorine-nitrogen mixture containing 0.5–2.0 vol% fluorine at 25–60 °C to reduce hydrocarbon permeation; for coextruded six-layer tanks, HHM5502BN forms the outer and inner structural layers at 70–85 wt% of the total wall, EVOH barrier at 1.5–2.5 wt%, and maleic anhydride-grafted polyethylene tie resin at 3–7 wt%. Production requires a 3D blow molding machine with servo-controlled die gap, mold temperature 40–70 °C, post-molding cooling fixtures, and fuel sender boss dimensional verification; extrusion melt temperature is kept at 190–215 °C to avoid thermal degradation of barrier layers. Terminal products include 40–90 L passenger car fuel tanks, 10–30 L construction machinery auxiliary tanks, and 10–50 L diesel exhaust fluid containers. Monolayer fluorinated tanks are limited to fuels with low aromatic content unless barrier performance is validated by the fuel supplier; EVOH coextruded structures are required for aggressive oxygenated fuel blends.
When molding intermediate bulk container inner bottles, the converter uses HHM5502BN as the monolayer liner resin because the grade provides the required side-wall stiffness, stress-crack resistance, and weld-line integrity under hydrostatic pressure. The IBC inner bottle is qualified under UN 31HA1/Y for liquid dangerous goods and, where the liner is used for non-hazardous foodstuffs, EU 10/2011 and FDA 21 CFR 177.1520 must be verified for the specific grade and conversion plant. Formulation for a 1,000 L or 1,250 L liner typically consists of 80–100 wt% virgin HHM5502BN, 0–20 wt% uncontaminated regrind, UV masterbatch at 0.5–1.5 wt% for outdoor storage, and antistatic masterbatch at 0.1–0.5 wt% when solvent-based products are filled. Production uses a large accumulator-extrusion blow molding machine with die diameter 200–350 mm, shot weight capacity 15–25 kg, platen width above 2,000 mm, mold cooling water inlet 8–12 °C, and parison profiling that compensates for measured die swell and parison sag over the 2–4 m drop length; wall thickness is mapped to maintain 2.0–3.5 mm in the lower sidewall and 4.0–6.0 mm around the top fill neck and discharge valve boss. Terminal products include 1,000 L and 1,250 L IBC inner bottles with top fill neck diameters of 150–225 mm, integrated discharge valve sockets, and calibrated sight lines for fill level control.
For barrier bottle structures intended for edible oil, soy sauce, vinegar, mayonnaise, and shelf-stable concentrates, HHM5502BN functions as the load-bearing polyolefin layer. The compliance framework includes EU 10/2011 with Annex II specific migration limits for plastic food-contact materials, FDA 21 CFR 177.1520 for olefin polymers, and GB 9685-2016 for food-contact additives used in the Chinese market; converters must validate organoleptic neutrality and overall migration on the finished bottle, because additive masterbatch composition and regrind quality can shift migration resistance. In a four-layer coextrusion blow molding formulation, HHM5502BN structural layers account for 60–85 wt% of the wall, regrind layer 10–25 wt%, EVOH or PA barrier 1–3 wt%, and tie resin 1–3 wt%; the barrier layer is kept separate from the regrind layer to prevent interfacial contamination. Extrusion blow molding is run with a multilayer die head at 190–210 °C for the HDPE streams, 200–220 °C for the EVOH stream, and 10–15 °C for the mold circuit; the parison program is adjusted to maintain barrier layer continuity in the pinch-off zone and around the neck finish. Terminal products include 0.5 L–5 L bottles for edible oil, soy sauce, vinegar, and shelf-stable sauces, as well as 3 L–10 L barrier bottles for liquid food concentrates. Regrind levels above 25 wt% or non-food-contact scrap are not admissible in the outer food-contact layers unless migration testing demonstrates compliance.
Large-volume industrial water storage tanks, dosing vessels for water treatment chemicals, and chemical neutralization sumps are blow-molded from HHM5502BN when stiff side walls and corrosion resistance are required without the weight of steel. For potable-water contact applications, certification under NSF/ANSI/CAN 61 and relevant EU 10/2011 or national approvals is required; for industrial service, mechanical design is verified under DVS 2205 for thermoplastic tanks or the purchaser’s pressure and thermal load specification. Formulation ratios for outdoor UV-stable service are HHM5502BN 100 wt% virgin, carbon black masterbatch 2.0–3.0 wt%, regrind up to 15 wt%, and antioxidant masterbatch 0.2–0.4 wt%; calcium carbonate filler is kept below 5 wt% to limit low-temperature impact loss. Production is carried out on single-station or rotary blow molding equipment with melt temperature 180–205 °C, mold temperature 8–15 °C, and blow pressure 0.8–1.0 MPa; for tanks above 500 L, cooling time is the main cycle driver and is set to maintain 3–8 °C mold exit surface temperature before demolding. Terminal products include 200 L, 500 L, and 1,000 L closed-top storage tanks, 300 L conical dosing tanks, chemical filter housings, and float balls for level control in water and wastewater systems. For potable-water service, the converter must confirm that the specific HHM5502BN lot, pigment package, and processing conditions do not introduce substances exceeding the applicable migration limits.
Competitive Sinochem Quanzhou HDPE HHM5502BN prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinochem Quanzhou HDPE HHM5502BN is a high-density polyethylene blow moulding grade produced at the Sinochem Quanzhou petrochemical site. The resin is supplied as pellets and is controlled for melt rheology, density, and environmental stress crack resistance. Typical release characterisation includes a nominal density of 0.955 g/cm³ when measured in accordance with ISO 1183-1:2019 and a melt mass-flow rate of 0.30 g/10 min at 190 °C under a 2.16 kg load using ISO 1133-1:2022. These values place HHM5502BN in the medium-molecular-weight high-density polyethylene class used for extruded blow moulding of rigid containers, industrial packaging, and technical parts. The grade is formulated to maintain melt strength during parison hang time while providing sufficient flow for die swell control. Because polymerisation control includes comonomer addition and molecular weight regulation, converters can expect reduced lot-to-lot variation in container top-load performance, measured in accordance with ISO 12048:1994, and drop-impact behaviour. Bulk density of packaged material is typically 550–600 kg/m³, but exact silo and bag values should be confirmed from the lot certificate rather than generic literature.
On shuttle blow moulding machines with screw diameters of 45 mm to 90 mm and barrel L/D ratios from 24:1 to 30:1, HHM5502BN is processed with barrel set temperatures in the range of 180 °C to 220 °C. The recommended melt temperature measured at the die head is 190–210 °C. Operation below 190 °C increases head pressure and can produce melt fracture on the parison surface; operation above 210 °C lowers parison hang strength and increases drawdown in containers with shot weights greater than 1.5 kg. Under die shear rates of 100–1000 s⁻¹, the melt displays pseudoplastic behaviour typical for medium-molecular-weight HDPE. Die swell is controlled through die gap, land length, and melt temperature. A starting die gap of 1.5–2.5 mm and a blow-up ratio of 2:1 to 3:1 are used for cylindrical and rectangular containers. On accumulator-head and reciprocating-screw machines, first-in, first-out melt delivery avoids melt stagnation. Screw cooling is required on continuous extrusion rotary wheel machines to prevent barrel overheating and parison surging. Parison programming is recommended for containers above 10 L to redistribute wall thickness at handle pinch-off and bottom corners.
| Parameter | Typical range | Unit |
|---|---|---|
| Melt temperature at die head | 190–210 | °C |
| Barrel set temperature | 180–220 | °C |
| Die gap | 1.5–2.5 | mm |
| Blow-up ratio | 2:1–3:1 | — |
| Blow air pressure | 0.6–1.0 | MPa |
| Mould cooling water inlet | 8–15 | °C |
| Pellet drying at RH > 60% | 80 for 2–4 | °C, h |
On commercial blow moulding lines, cooling and exhaust air removal dominate cycle time for containers with wall thickness above 2 mm. Mould cooling-water temperatures below 8 °C can cause condensation and internal stress, while temperatures above 15 °C extend cycle time and increase warpage. Blow air pressure above 0.6 MPa improves mould detail and pinch-off definition. At relative humidity below 60%, pre-drying is not required. When stored or conveyed at relative humidity above 60%, pellets are hopper-dried at 80 °C for 2–4 h to prevent splay in the parison. The resin is compatible with standard nitrided steel screws and does not require corrosion-resistance upgrades. If the machine is idled at melt temperature for more than 15 min, the barrel should be purged with a lower-density polyethylene to remove stagnant melt before production resumes. Fluoropolymer purge compounds are not required unless die-lip build-up interferes with parison release.
The short-chain branch comonomer selection in HHM5502BN influences solid-state morphology. In the density region near 0.955 g/cm³, butene-modified HDPE typically develops a crystalline fraction between 60% and 70% as characterised by differential scanning calorimetry at a heating rate of 10 K/min in accordance with ISO 11357-3:2018. The melting peak is normally located near 131–135 °C. These thermal data are not release specifications but are included in product stewardship information for processors setting heating and cooling rates. Higher comonomer content reduces lamellar thickness and improves toughness but lowers upper-use temperature; the density of HHM5502BN therefore represents a compromise between stiffness, top-load resistance, and stress crack resistance.
Differences between HHM5502BN and generic unimodal HDPE grades of similar density appear primarily in molecular weight distribution, die swell, and environmental stress crack resistance. A unimodal grade with a melt mass-flow rate near 0.30 g/10 min often shows a narrow parison temperature window and lower stress crack resistance; HHM5502BN is formulated to maintain a wider processing window on shuttle machines. Film-grade HDPE with melt mass-flow rates of 0.7–1.2 g/10 min is unsuitable for thick-walled containers because its lower melt strength produces excessive drawdown and off-centre parison distribution. Injection-moulding HDPE grades with melt mass-flow rates above 15 g/10 min cannot maintain a stable parison. High-molecular-weight blow moulding grades with MFR₂.₁₆ values below 0.10 g/10 min provide higher ultimate ESCR but require more torque and longer cycle times; HHM5502BN offers a middle point for containers up to 60 L where stress crack resistance, processability, and cooling time are balanced. When service conditions involve aggressive surfactants or solvents, a high-molecular-weight grade with ESCR F₅₀ above 100 h may be required. Published data for direct comparison of HHM5502BN with every commercial alternative is limited, so end-use testing under the intended filling and storage conditions is necessary.
Although HHM5502BN is normally converted as a neat blow moulding resin, it can be dry-blended with polyethylene-based colour masterbatch or UV stabiliser masterbatch at addition rates of 1–3 wt%. High-shear compounding in a corotating twin-screw extruder with L/D ratio 40:1 and specific energy input above 0.20 kWh/kg is not required for simple colour addition and may unnecessarily reduce molecular weight. If compounding is performed, barrel temperatures should not exceed 220 °C, and melt temperature should remain below 230 °C. The resultant compound must be re-characterised for MFR and density because additive carriers can shift rheology and affect parison sag.
The following table lists typical property values from manufacturer-published data. Release values may differ according to production lot and should always be verified against the certificate of analysis.
| Property | Test method | Typical value | Unit |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.955 | g/cm³ |
| Melt mass-flow rate at 190 °C/2.16 kg | ISO 1133-1:2022 | 0.30 | g/10 min |
| Tensile yield stress | ISO 527-2:2012 | 28 | MPa |
| Elongation at break | ISO 527-2:2012 | >600 | % |
| Flexural modulus | ISO 178:2019 | 1200 | MPa |
| ESCR F₅₀, 100% Igepal CO-630, Condition B | ASTM D1693-15 | 30–50 | h |
These values are not design limits. Structural container calculations require stress crack resistance and creep data generated at the specific service temperature and chemical environment. Long-term hydrostatic strength is not specified for HHM5502BN as a pressure pipe grade because the product is not intended for pressurised pipe systems designed to ISO 9080:2012 or ASTM D2837-21. The resin should not be exposed to oxidising acids above the concentration limits established by the chemical compatibility review for the final container. Pellets are insoluble in water and can be stored for up to 6 months from production when kept below 40 °C and away from direct ultraviolet exposure. Processing above 240 °C should be limited in residence time because oxidative degradation increases gel particle formation and reduces ESCR.
Processors requiring food-contact or potable-water compliance must obtain the manufacturer’s regulatory statement for the specific lot because additive packages and colorants can alter compliance status. The base high-density polyethylene may fall within the scope of FDA 21 CFR 177.1520 for olefin polymers and the positive list in Commission Regulation (EU) No 10/2011, but use conditions including temperature, food type, and contact time must be assessed by the packaging manufacturer. REACH SVHC content must be confirmed through the supplier safety data sheet. If the container is intended for hazardous liquids, packaging must be tested in accordance with ADR 6.1 or relevant UN packing group requirements; HDPE chemical resistance alone does not establish regulatory transport compliance.
Reprocessing trials with HHM5502BN show that addition of clean post-industrial regrind up to 10 wt% does not significantly alter tensile yield stress or ESCR when the regrind is dried to the same moisture limit as virgin pellets. Above 10 wt%, reductions in parison surface quality and weld-line integrity have been observed because of cumulative molecular weight loss. In high-gloss containers, regrind addition should remain below 5 wt% unless gloss is measured in accordance with DIN 67530 and found acceptable. Recycled feedstock containing more than 2 wt% polypropylene caps, labels, or silicone-based lubricants should be cleaned by density separation because these contaminants reduce top-load performance and produce localised delamination.
If HHM5502BN serves as the structural layer in multi-layer coextruded containers, the melt streams must be matched in viscosity to avoid flow instability. The layer-to-layer viscosity ratio at the die should remain near 1:1 to 1.5:1 within the die shear-rate range of 100–1000 s⁻¹. A mismatch above this range can produce layer non-uniformity, parison curling, and reduced interlayer adhesion. Published data for coextrusion of this specific grade is limited; converter trials are required to define the optimal layer ratio and die temperature profile for each container geometry. Drying of EVOH or polyamide barrier layers is conducted separately from the HHM5502BN layer. HHM5502BN pellets stored or conveyed at relative humidity above 60% are hopper-dried at 80 °C for 2–4 h. Amine-based flame retardant masterbatches should be avoided unless the masterbatch supplier validates compatibility, because amine additives can cause discolouration and surface deposition at sustained melt temperatures above 200 °C. Any addition of colorants, fillers, or processing aids must be followed by re-testing of ESCR and drop-impact performance because dispersed particulates can nucleate stress concentrations in the container wall.
On accumulator-head machines with shot weights near 2.5 kg and clamp forces below 300 kN, the processing window narrows when wall thickness exceeds 3 mm. An accumulator pressure of 8–12 MPa is typical, and the parison controller should use at least 20 programming points to prevent corner thinning. Flow marks at the pinch-off are often eliminated by increasing die zone temperature by 5 °C and drying pellets at 80 °C for 3 h. The grade’s melt strength permits production of containers up to 60 L, but for capacities above 100 L, a higher-molecular-weight HDPE with MFR₂.₁₆ below 0.10 g/10 min should be evaluated. At the end of a production campaign, the accumulator head should be purged with a medium-density polyethylene to reduce residue build-up in the die land.