| HS Code | 760464 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190c 2 16kg | 0.35 g/10 min |
| Tensile Yield Strength | 24 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 1000 MPa |
| Vicat Softening Point | 125 °C |
| Brittleness Temperature | -70 °C |
| Environmental Stress Crack Resistance | >1000 h |
| Hardness Shore D | 65 |
| Melting Point | 130 °C |
| Water Absorption | <0.01% |
| Volume Resistivity | >10^16 Ω·cm |
As an accredited Sinochem Quanzhou HDPE 5502 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinochem Quanzhou HDPE 5502 packed in 25 kg PP woven bags or 1,000 kg jumbo bags, palletized for bulk handling. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Sinochem Quanzhou HDPE 5502 high-density polyethylene resin, 25 kg bags, floor-loaded and secured for export. |
| Shipping | Sinochem Quanzhou HDPE 5502 is shipped as non-hazardous high-density polyethylene pellets, HS code 3901.20, in 25 kg PP bags or 1,000 kg jumbo bags, palletized, stretch-wrapped, and loaded into 20-foot FCL containers. Store cool, dry, ventilated; no dangerous goods documentation required under IMDG/IATA/ADR. |
| Storage | Store Sinochem Quanzhou HDPE 5502 in a clean, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags sealed and palletized off the floor. Avoid moisture, contamination, and physical damage. Maintain ambient temperature, stack securely, and follow local regulations and supplier recommendations. Do not expose to ignition sources or incompatible materials. Ensure good ventilation and first-in-first-out stock rotation. |
| Shelf Life | Sinochem Quanzhou HDPE 5502 typically has a 12-month shelf life under cool, dry, ventilated storage, protected from sunlight and moisture. |
Sinochem Quanzhou HDPE 5502 is specified as a high-molecular-weight, high-density polyethylene for continuous extrusion blow moulding, with a typical density of 0.955 g/cm³ when tested to ISO 1183-1:2019 and a melt mass-flow rate of 0.35 g/10 min at 190 °C/2.16 kg when determined by ISO 1133-1:2022. The material’s processing envelope is centred on accumulator-head and reciprocating-screw blow moulding machines with screw L/D between 24:1 and 30:1, melt temperatures from 180 °C to 220 °C, and blow-up ratios from 2:1 to 3.5:1. The application routes below are restricted to industrial segments where these rheological and mechanical properties are matched to specific container performance requirements; no claim is extended to rotational moulding, film, cast sheet, or injection moulding.
Industrial jerrycans and open-head drum liners intended for UN-certified dangerous goods are produced from 100 wt% virgin Sinochem Quanzhou HDPE 5502, with no post-consumer recyclate added unless the design type is re-qualified under Chapter 6.1 of the UN Recommendations on the Transport of Dangerous Goods, Model Regulations. The addition ratio for a PE-carrier dark blue or carbon black masterbatch is held to 1–2 wt%, and external lubricants or processing aids are excluded to preserve the low melt flow rate and high parison hang strength required for tall containers. Modal compliance is documented under ADR/RID/IMDG Code packing instruction P001 for liquid dangerous goods, and the finished container must carry the UN packaging code, material symbol, design-type approval reference, and hydrostatic test pressure marking. On the production line, accumulator-head extrusion blow moulding machines with a screw L/D of 25:1 to 30:1 are operated at a melt temperature of 190–210 °C and a die gap of 2–4 mm, with continuous parison programming to increase wall thickness at the top and bottom pinch-off zones.
The critical failure modes observed at production scale are parison sag above 220 °C, fold-over at the flash pocket when pre-blow delay is too short, and brittle cracking at the pinch-off weld after contact with aggressive surfactant or hypochlorite solutions. Wall-thickness distribution is measured at the container shoulder, sidewall, and chime; typical minimum values are 0.8–1.2 mm for 5–10 L jerrycans and 1.2–2.0 mm for 20–30 L containers. Environmental stress crack resistance is evaluated under ASTM D1693-15b, Condition B, 100% Igepal CO-630, with F50 values specified by the design type; stacking performance is verified against ISO 12048, and leak testing is conducted at 0.03 MPa internal pressure for packaging group II and 0.02 MPa for packaging group III. Terminal products include 5 L, 10 L, 20 L, 25 L, and 30 L jerrycans, in addition to open-head drum liners with a wall thickness between 1.0 mm and 2.5 mm.
In automotive underhood fluid systems, windshield washer fluid and coolant overflow reservoirs are blow-moulded from HDPE 5502 at 100 wt% with 2–3 wt% high-load carbon black masterbatch for UV and heat resistance; clean internal regrind from the same reservoir production line is restricted to 10 wt% maximum to stabilise impact behaviour at −30 °C. The governing test framework includes ISO 6603-1 for multi-axial impact and ISO 527-1:2019 for tensile properties, while coolant compatibility is assessed by immersion in 50/50 ethylene glycol/water at 90 °C for 1,000 h. Processors should note that at regrind fractions above 10 wt%, the melt flow rate shifts upward and the parison becomes measurably more prone to sag, requiring a 5–10 °C reduction in melt temperature to restore the specified hang strength.
Production is carried out on reciprocating-screw extrusion blow moulding machines with a fitted accumulator head and a converged die geometry; the melt temperature is maintained at 195–215 °C, while the mould is cooled at 10–20 °C. A blow-up ratio of 2.0–2.6:1 and programmed parison thickness generate local wall sections of 2.0–3.5 mm, because the reservoir must withstand pressure pulses generated by windshield washer pumps and under-bonnet temperatures up to 105 °C. Terminal products include 2–5 L washer reservoirs and 1–3 L coolant overflow bottles, with leak testing at 0.05 MPa and drop impact at −20 °C defined by the vehicle platform specification.
For hypochlorite-containing household and institutional formulations, HDPE 5502 is used as the sole polymer component at 100 wt% because high environmental stress crack resistance is required for contact with linear alkylbenzene sulphonate, alcohol ethoxylate, and sodium hypochlorite solutions at pH values between 10 and 13. The addition ratio for a PE-based colour masterbatch is limited to 0.5–2.0 wt%; polypropylene-based colour concentrates are excluded because they reduce weld-line elongation and increase drop-impact variability. Compliance for bleach-containing consumer containers is evaluated under ASTM D2463-15 for drop impact and the surface-active agent stability requirements of 21 CFR 178.1010 where sanitising formulations are involved.
Extrusion blow moulding is performed on long-bed extruders with a grooved feed section and screw L/D of 25:1 to 30:1, at melt temperatures between 185 °C and 205 °C. Parison programming is configured to create a minimum sidewall thickness of 0.5 mm for 500 mL trigger-bottle formats and 1.0–1.5 mm for 4 L floor-cleaning bottles, with the blow-up ratio held below 3.0:1. Terminal products include 500 mL and 1 L trigger spray bottles, 750 mL viscous-product bottles, and 4 L janitorial bleach containers with standard neck finishes.
When non-sterile pharmaceutical and personal care packaging requires ambient filling, containers blow-moulded from HDPE 5502 are limited to solid-dose tablets, capsules, effervescent tubes, topical creams, and oral care preparations. The formulation is normally 100 wt% HDPE 5502 with no intentional addition of processing aids other than a 0.5–1.5 wt% white titanium dioxide masterbatch used to achieve opacity and light protection. Compliance is evaluated under USP <661.1> for plastic packaging systems, Ph. Eur. 3.1.3 for polyolefins, and 21 CFR 177.1520(c) 3.1a/3.2a for olefin polymers intended for food and drug contact; because the additive package may vary by production campaign, the converter must request the relevant regulatory status from the resin manufacturer.
The processing route is continuous extrusion blow moulding on high-output wheel machines with multiple moulds, where melt temperature is held at 180–200 °C and mould cooling temperature is set between 6 °C and 12 °C to meet tight body diameter tolerances. Wall thickness for 30–250 mL tablet bottles is controlled at 0.6–1.0 mm, while 500 mL topical containers require 1.2–1.8 mm sidewalls to pass closure integrity testing under ASTM D4991-07(2015) for vacuum leak detection. Terminal products include cylindrical and square tablet bottles, ophthalmic and nasal wash bottles without preservative release concerns, and tube-shaped personal care containers with tamper-evident neck finishes.
| Application route | HDPE 5502 addition ratio | Key standard or test method | Critical control parameter |
|---|---|---|---|
| UN-certified jerrycans and drum liners | 100 wt% virgin, 1–2 wt% masterbatch | UN Model Regulations Chapter 6.1, ISO 12048, ASTM D1693-15b | Melt temperature 190–210 °C, die gap 2–4 mm |
| Automotive washer and coolant reservoirs | 100 wt%, 2–3 wt% carbon black masterbatch, ≤10 wt% regrind | ISO 6603-1, ISO 527-1:2019 | Blow-up ratio 2.0–2.6:1, melt temperature 195–215 °C |
| Detergent and hypochlorite bottles | 100 wt%, 0.5–2.0 wt% PE masterbatch | ASTM D2463-15, 21 CFR 178.1010 | Melt temperature 185–205 °C, blow-up ratio <3.0:1 |
| Pharmaceutical and personal care containers | 100 wt%, 0.5–1.5 wt% TiO₂ masterbatch | USP <661.1>, Ph. Eur. 3.1.3, 21 CFR 177.1520 | Melt temperature 180–200 °C, mould cooling 6–12 °C |
| Lubricant and metalworking fluid containers | 85–100 wt% virgin, 0–15 wt% regrind | ASTM D543-14 | Melt temperature 190–210 °C; reduce 5–10 °C with regrind |
| Agrochemical containers | 98–100 wt%, 0–2 wt% UV masterbatch | UN Model Regulations, FAO/WHO Guidelines on Packaging for Pesticides | Blow-up ratio 2.0–2.8:1, leak test 0.02–0.03 MPa |
In the production of lubricant and metalworking fluid containers, HDPE 5502 is processed at 85–100 wt% virgin resin with 0–15 wt% clean internal regrind generated from the same bottle line, provided the regrind is dried and screened through a 2 mm mesh to remove gels and char particles. External post-consumer recyclate is excluded because peroxides and polar contaminants from prior packaging can reduce environmental stress crack resistance in contact with ester-based synthetic lubricants and chlorinated metalworking fluids. The governing methodology is ASTM D543-14 for chemical resistance of plastics, with tensile strength retention measured after 500 h immersion in a representative 10W-40 engine oil at 70 °C.
These bottles are blow-moulded on continuous rotary or shuttle machines with a melt temperature of 190–210 °C; when 10–15 wt% regrind is present, the melt viscosity shifts lower and the head temperature is reduced by 5–10 °C to maintain parison hang strength. The die gap is adjusted to 2.5–4.5 mm for 1 L and 4 L finished containers, and the mould is cooled at 12–18 °C; container wall thickness is programmed to 0.8–1.5 mm to resist panel deformation under top load. Terminal products include 1 L, 4 L, and 5 L motor oil bottles, gear oil and automatic transmission fluid containers, and 20 L metalworking fluid pails with UN packaging markings where required.
For crop protection product formulations classified as flammable or toxic, agrochemical containers are moulded from HDPE 5502 at 98–100 wt% with 0–2 wt% UV-stabilised colourant masterbatch. The core regulatory references are the FAO/WHO Guidelines on Packaging for Pesticides and the UN Model Regulations for dangerous goods when formulated products carry a transport classification. Barrier performance for cyclohexanone, xylene, and ester-based formulation systems is addressed not by increasing the resin addition level but by post-mould fluorination to a surface fluorine-to-carbon ratio typically between 0.5:1 and 1:1 on the inner wall, as measured by X-ray photoelectron spectroscopy.
Extrusion blow moulding is run on accumulator-head machines at melt temperatures from 190 °C to 210 °C, with a blow-up ratio of 2.0–2.8:1 and programmed parison to prevent thin spots at the handle bridge and base chime. The mould cooling medium is maintained at 8–14 °C, and containers are leak-tested under 0.02–0.03 MPa internal pressure after 24 h conditioning at 23 °C. Terminal products include 0.5 L, 1 L, 5 L, and 10 L high-density polyethylene bottles with UN markings, child-resistant closures, and induction-sealed neck finishes.
Competitive Sinochem Quanzhou HDPE 5502 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinochem Quanzhou HDPE 5502 is a high-density polyethylene extrusion blow molding resin supplied in pellet form. The model designation 5502 identifies a controlled melt-flow grade intended for hollow container manufacture. The material is characterized by a melt mass-flow rate in the low end of the HDPE range. Under ISO 1133-1:2022 at 190 °C and 2.16 kg load, typical values fall between 0.25 g/10 min and 0.35 g/10 min. Density under ISO 1183-1:2019 is between 0.954 g/cm³ and 0.958 g/cm³. These specifications place HDPE 5502 in the high-density polyethylene class for extrusion blow molding rather than injection molding or film extrusion. The product is typically used for non-food and industrial hollow containers such as household chemical bottles, detergent containers, lubricant packs, and agricultural chemical containers up to 25 L. In blow molding, the low melt flow rate preserves parison melt strength during intermittent accumulator discharge, while the density is kept below 0.960 g/cm³ to retain impact toughness and environmental stress crack resistance. The material is not a universal HDPE; its processing window is narrower than that of higher-melt-flow grades and its properties depend on the additive package and regrind handling.
The molecular weight and comonomer content of HDPE 5502 act together to produce a balance of stiffness, melt strength, and stress crack resistance. The melt mass-flow rate determined under ISO 1133-1:2022 is used as a reverse indicator of average molar mass; a value of 0.25–0.35 g/10 min corresponds to a melt that is significantly more viscous than an injection molding grade. This high viscosity creates greater extruder torque but provides the extensional viscosity needed to support a falling parison. Density by ISO 1183-1:2019 is 0.954–0.958 g/cm³; at this density the crystallinity is lower than that of a 0.965 g/cm³ HDPE injection or pipe grade. Lower crystallinity reduces modulus but improves impact and environmental stress crack resistance. Typical tensile yield stress by ISO 527-2 is 26–28 MPa; flexural modulus by ISO 178:2019 is 1050–1250 MPa. Notched Izod impact strength by ISO 180:2023 at 23 °C is 8–12 kJ/m², which is acceptable for containers that must survive room-temperature drop testing but should not be treated as a low-temperature impact guarantee. Environmental stress crack resistance determined by ASTM D1693 condition B in 10% Igepal CO-630 solution shows F50 times above 100 h for this molecular weight class. Published data for this specific Sinochem Quanzhou grade at every lot is limited; the certificate of analysis and material safety data sheet should be consulted before qualification.
| Property | Test method | Typical value or range | Unit |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.954–0.958 | g/cm³ |
| Melt mass-flow rate | ISO 1133-1:2022 at 190 °C, 2.16 kg | 0.25–0.35 | g/10 min |
| Tensile yield stress | ISO 527-2 | 26–28 | MPa |
| Tensile elongation at break | ISO 527-2 | >600 | % |
| Flexural modulus | ISO 178:2019 | 1050–1250 | MPa |
| Notched Izod impact strength, 23 °C | ISO 180:2023 | 8–12 | kJ/m² |
| Environmental stress crack resistance, F50 | ASTM D1693 condition B, 10% Igepal CO-630 | >100 | h |
Lot-to-lot variation in melt flow rate is typically controlled within ±0.05 g/10 min at the petrochemical producer level, based on standard statistical process control procedures for HDPE blow molding grades. Die swell and spiral flow are not always published but are relevant for tooling design; typical die swell for low-melt-flow HDPE in this density range is 25–35% at moderate shear rates. The values in the table are class-representative ranges, not certified lot values. The manufacturer’s certificate of analysis should govern release testing.
Processing on intermittent extrusion blow molders begins with pellet handling. HDPE 5502 is not hygroscopic in the manner of polyamide or PET, but surface moisture from storage in high-humidity environments can produce pinholing and surface defects. Pre-drying at 80 °C for 2 h in a desiccant or hot-air dryer is recommended whenever storage relative humidity has exceeded 60%. The extruder barrel should be profiled from 170 °C in the feed zone to 200 °C at the die head. Melt temperatures between 185 °C and 205 °C produce stable parison formation in this MFR class. Temperatures above 220 °C accelerate oxidative chain scission, resulting in reduced parison melt strength, higher gel content, and possible odor. Screw designs with L/D ratios from 24:1 to 30:1 and shear mixing sections are used; grooved-barrel extruders are preferred when high output and stable pressure are required under low melt flow conditions. Accumulator head machines are recommended for containers above 5 L because the rapid accumulator discharge limits parison sag. Continuous extrusion heads are suitable for smaller bottles but require careful die gap and temperature control. Blow air pressure of 0.6–0.8 MPa and mold temperatures of 10–30 °C are typical for this class. The die gap is set between 1.5 mm and 2.5 mm to achieve final wall thicknesses from 0.6 mm to 2.0 mm, although specific tooling may require wider ranges. Clamp force requirements scale with container size; a 20 L container tool may require at least 250 kN clamping force to resist blowing pressure and flash formation. These parameters are representative of industrial practice for low-melt-flow HDPE blow molding and must be confirmed on the specific machine because screw geometry and head design can shift the window by 10–20 °C.
Regrind from trimmed flash and reject containers can be incorporated at levels up to 30% by weight if it is dry and free from contamination. Higher regrind levels reduce environmental stress crack resistance and drop impact and increase the risk of black specks. Contamination with polypropylene or PVC must be avoided. Polypropylene contamination above 5% can cause delamination and reduced stress crack resistance, while PVC degrades and releases hydrogen chloride, which corrodes tooling and causes surface defects. Common processing defects include parison sag, uneven wall thickness, weld line weakness, and pinholes. Parison sag is controlled by lowering melt temperature or increasing accumulator discharge speed; uneven wall thickness is corrected by adjusting die eccentricity and head tooling. Pinholes are often caused by moisture or contamination, while weak weld lines in handle crossing areas are affected by melt temperature and mold venting.
The useful container life of blow molded HDPE 5502 is often limited by environmental stress cracking rather than yield strength. ESCR depends on molecular weight, comonomer type, density, thermal history, and the chemical environment. Containers for surfactant-based household chemicals, lubricant additives, or agricultural formulations are subjected to low-magnitude stress from internal pressure or top load while being exposed to stress-cracking agents. The low density of 0.954–0.958 g/cm³ and the relatively low melt flow rate of 0.25–0.35 g/10 min provide a baseline ESCR that is better than a high-density injection grade at 0.965 g/cm³ but lower than a bimodal film or pipe grade designed for maximum slow crack growth resistance. Drop impact at low temperature follows the same trade-off; the grade is typically evaluated at -20 °C under ASTM D2463-15 for blow-molded containers, but published data for this specific Sinochem Quanzhou grade is limited. Top-load strength of empty containers is measured under ISO 12048 or comparable compression test methods. A typical 20 L general-purpose container may show top-load values in the range of 400–800 N depending on wall thickness and geometry, but this is a container design property, not an intrinsic resin property. UN dangerous goods packaging is not certified by resin choice alone; it requires container-specific testing under ADR/RID or IMDG Code for drop height, leakproofness, hydraulic pressure, and stacking. The resin can be used in packaging that is subsequently tested to those standards, but the grade data sheet alone does not grant UN approval.
Differences from other polyethylene grades are best assessed by melt flow rate, density, and molecular architecture. An HDPE injection molding grade with a melt flow rate of 20–30 g/10 min and density of 0.952–0.965 g/cm³ cannot be used in an intermittent blow molder because its low melt viscosity allows the parison to sag and collapse before mold closure. Conversely, HDPE 5502 cannot fill thin-wall closure molds due to its low flow. Compared with a bimodal HDPE film grade with a melt flow rate of 0.05–0.15 g/10 min and density 0.949–0.952 g/cm³, HDPE 5502 has a moderately higher melt flow and lower melt viscosity, which reduces extruder torque and allows higher output on a given screw. However, the bimodal film grade has a higher molecular weight tail and higher ESCR; it also has higher shear sensitivity and can be more difficult to process on simple smooth-bore extruders. Compared with an HDPE pipe grade such as PE 100 with density in the 0.958–0.963 g/cm³ range, HDPE 5502 has slightly lower density and lower hydrostatic strength because it is not designed for piping pressure ratings under ISO 9080. The differences within the 5502 class from different producers are less visible in melt flow and density but may appear in comonomer type, catalyst residuals, stabilizer package, and the resulting color, odor, ESCR, and die swell characteristics. Direct substitution of a 5502 from another supplier should be qualified by comparing the certificate of analysis, notched Izod impact at 23 °C and -20 °C, ESCR F50, and a spiral flow test at a fixed melt temperature.
| Material class | Melt mass-flow rate | Density | Processing method | Comparative limitation |
|---|---|---|---|---|
| HDPE blow molding 5502 class | 0.25–0.35 g/10 min | 0.954–0.958 g/cm³ | Intermittent extrusion blow molding | Low MFR restricts injection molding |
| HDPE injection molding high-flow | 20–30 g/10 min | 0.952–0.965 g/cm³ | High-speed injection molding | Excessive parison sag in blow molding |
| HDPE bimodal film grade | 0.05–0.15 g/10 min | 0.949–0.952 g/cm³ | Blown and cast film extrusion | Higher screw torque; narrower die swell control |
| HDPE pipe PE 100 | 0.20–0.45 g/10 min | 0.958–0.963 g/cm³ | Pipe and profile extrusion | Higher density and hydrostatic strength requirement |
The table summarizes comparative distinctions across material classes; however, values are representative of material classes and not equivalent to the actual certificate of analysis of any specific commercial grade. Published comparative data for HDPE 5502 from Sinochem Quanzhou against each listed class is limited, and end-use qualification should include container-specific testing rather than reliance on class-level property comparisons.
Regulatory status should be verified from the supplier’s Safety Data Sheet and product stewardship declaration. High-density polyethylene polymers of this density class may satisfy FDA 21 CFR 177.1520 for olefin polymers used in contact with food, but no food-contact claim should be inferred without written confirmation. REACH and RoHS compliance should be checked against the European Chemicals Agency candidate list and lot-specific documentation. The resin is not intended for medical implant use or for applications requiring sustained pressure piping. The presence of processing aids and stabilizers may affect extraction and odor profiles in sensitive applications. Containers intended for aggressive solvents, strong acids, or high-temperature hot fill above 60 °C require end-use testing because ESCR and creep performance are strongly dependent on chemical environment and stress level. Published data for this specific product in aggressive solvent environments is limited; container-specific chemical compatibility tests are recommended before commercial use.