Sibur Hdpe Hd12500 Lh

SIBUR HDPE HD12500 LH

    • Product Name: SIBUR HDPE HD12500 LH
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 410929
    Material Type High Density Polyethylene (HDPE)
    Density 0.950 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 12.5 g/10 min
    Tensile Strength At Yield 27 MPa
    Tensile Strength At Break 20 MPa
    Elongation At Break 500%
    Flexural Modulus 1200 MPa
    Notched Izod Impact Strength At 23 C 6 kJ/m²
    Notched Izod Impact Strength At 20 C 3 kJ/m²
    Vicat Softening Temperature 125°C
    Heat Deflection Temperature At 0 45 Mpa 70°C
    Shore D Hardness 65
    Melting Point 130°C
    Water Absorption <0.01%
    Volume Resistivity >10^16 ohm·cm
    Dielectric Constant 2.3
    Thermal Conductivity 0.4 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C

    As an accredited SIBUR HDPE HD12500 LH factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SIBUR HDPE HD12500 LH is packaged in 25 kg polyethylene bags, palletized for transport, or 1,000 kg bulk bags.
    Container Loading (20′ FCL) SIBUR HDPE HD12500 LH loaded in 20′ FCL: 25 kg bags, 880 bags, 22,000 kg net, floor-loaded and securely stowed.
    Shipping SIBUR HDPE HD12500 LH is a non-hazardous high-density polyethylene resin. It is shipped in 25 kg polyethylene bags, stacked on pallets, stretch-wrapped, and transported in clean, dry trucks or containers. Store in a cool, dry area away from direct sunlight, heat, and moisture. No special dangerous goods requirements apply.
    Storage Store SIBUR HDPE HD12500 LH in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original bags or octabins closed to prevent moisture, dust, and contamination. Use stable pallet stacking, avoid excessive pressure and UV exposure. Store separately from incompatible substances. Follow supplier SDS and local fire codes.
    Shelf Life Typically 24 months from production date when stored sealed in original packaging, dry, away from direct sunlight, at ambient temperature.
    Application of SIBUR HDPE HD12500 LH

    Dairy and Still Beverage Closure Systems on High-Cavitation Hot-Runner Tools

    In the injection moulding of single-piece closures for still water, pasteurised milk, UHT dairy drinks, and ambient juice, the melt flow rate of 12.5 g/10 min at 190 °C/2.16 kg measured per ISO 1133-1:2022 and density in the 0.950–0.955 g/cm³ range measured per ISO 1183-1:2019 set the flow-length and cycle-time boundary for multi-cavity tools. For natural closures the neat resin fraction is 100.0 wt%; for coloured closures the neat resin fraction is reduced to 97.0–98.0 wt%, a colour masterbatch is introduced at 2.0–3.0 wt%, and an erucamide slip concentrate is added at 0.05–0.10 wt%. Post-industrial regrind from the same food-contact production cell is incorporated up to 30 wt% only when the feedstock is generated and reused within the same closed-loop system and migration testing under EU 10/2011 and 21 CFR 177.1520(c) remains valid for the closure. Production is typically run on an accumulator-assisted injection machine with clamp force between 250 and 500 t, a 48- to 96-cavity valve-gated hot runner, screw length-to-diameter ratio of 22:1–25:1, and injection speed of 80–150 mm/s. Melt temperature is held at 200–230 °C, mould cooling water at 8–15 °C, holding pressure at 40–60 MPa, and back pressure at 5–10 MPa; cycle times of 6–12 s are attainable. Batch-to-batch variation in melt flow rate of ±0.8 g/10 min is normally corrected by adjusting melt temperature by ±5 °C rather than by increasing holding pressure. End products include tamper-evident screw caps, push-pull sports caps, and snap-on closures for dairy and still beverage containers with neck finishes from 28 mm to 38 mm. The grade is not recommended for carbonated soft drink closures unless carbon dioxide retention is validated on the finished cap at the target torquing condition.

    What Limits Cycle Time When Wall Sections Drop Below 0.9 mm?

    Thin-wall injection moulding of dairy cups, fruit portion packs, deli rounds, and spread containers from SIBUR HDPE HD12500 LH is constrained primarily by the solidification window created by the grade’s thermal diffusivity and by the uniformity of the tool cooling circuit. The melt temperature window narrows to approximately ±5 °C around 230–250 °C in wall sections between 0.6 and 0.9 mm: below 225 °C short shots appear at the rim, while above 255 °C flash occurs in stack moulds with clamp force below 800 t. Accumulator injection speeds of 350–600 mm/s are required to achieve flow-length-to-wall-thickness ratios up to 150:1 in 4+4 or 8+8 stack tools, and screw decompression is set at 3–5 mm to prevent gate drool. Mould cooling water is run at 5–10 °C, holding pressure is applied at 60–90 MPa for 0.3–0.8 s, and total cycle time is held within 3.5–7.0 s. The combined masterbatch addition is 2.5–4.5 wt%, consisting of a nucleating masterbatch at 0.5–1.5 wt% and a colour masterbatch at 2.0–3.0 wt%; the neat resin fraction makes up the balance to 100.0 wt%. Differential scanning calorimetry per ISO 11357-3:2018 is used to verify the active nucleating package and the resulting crystallisation peak shift. Slip agent is kept below 0.15 wt% of the total compound because higher levels create interlaminar delamination at high shear rates. Post-industrial regrind is limited to 30 wt% only when generated from clean start-up and rejected containers on the same line. Compliance is maintained under EU 10/2011, FDA 21 CFR 177.1520, and EN 13428. End products include round deli containers, rectangular snack packs, and shallow dairy dessert cups with wall thickness from 0.6 to 1.2 mm. The main control variable for warpage is the core/cavity mould temperature difference, which is kept below 5 °C, while hot-runner pressure drop is balanced within ±2 MPa across all gates.

    When Post-Consumer Recyclate Replaces Virgin HDPE in Heavy-Duty Crate Moulds

    Production of returnable distribution crates, logistics trays, and pallet sleeves from SIBUR HDPE HD12500 LH is run on single-face injection machines with clamp force between 800 and 1600 t because wall thickness from 3.0 to 6.0 mm and multi-ribbed bases require controlled hold-pressure decay rather than very high injection speed. Tooling uses a cold sprue bush or a valve-gated hot runner at 1–4 cavities; melt temperature is set at 220–260 °C, mould temperature at 15–30 °C, holding pressure at 50–80 MPa, and cooling time at 20–40 s. Post-industrial regrind is incorporated at 20–50 wt%, while post-consumer recyclate is limited to 20–35 wt% because incoming melt viscosity variability of ±15% shifts shot weight by ±0.5% on four-cavity tools unless adaptive shot-size correction is active. Carbon black masterbatch is dosed at 2.0–3.0 wt%, and a hindered amine light stabilizer masterbatch at 2.0–4.0 wt% is added when crates are stored outdoors beyond 12 months. Compliance is anchored to REACH Annex XVII and EU Directive 94/62/EC, with recycled-content claims verified under ISO 14021:2016; direct food-contact crates are outside scope unless a separate migration assessment under EU 10/2011 is completed. Charpy impact is measured at 23 °C by ISO 179-1/1eA and should remain above 4.0 kJ/m²; above 35 wt% post-consumer recyclate, impact strength becomes the limiting property. End products include stack-nest bottle crates, bakery trays, fish boxes, pallet side walls, and agricultural harvest crates. The primary field failure is incomplete fill at corner bosses when recyclate lot melt flow rate deviates from the 12.5 g/10 min reference; each recyclate lot is pre-tested at 190 °C/2.16 kg and the virgin/recyclate ratio corrected by ±5 wt% before tool start-up.

    Packing Pressure, Not Melt Temperature, Determines Detergent Cap Dimensional Stability

    Injection-moulded measuring cups, laundry detergent caps, trigger spray collars, and spouted closures for non-food chemical formulations use SIBUR HDPE HD12500 LH because the 12.5 g/10 min melt flow rate allows narrow thread features to fill at moderate melt temperature. The decisive processing parameter is the packing-pressure curve: cavity pressure sensors are placed behind the thread ring 0.5 mm from the gate, and the packing setpoint is held at 45–70 MPa for 2–5 s, followed by a pressure decay of 10–15 MPa/s to prevent overpacking of the cap skirt. Melt temperature is maintained at 200–230 °C with a clamp force of 120–350 t and 16- to 64-cavity cold-runner or hot-runner tooling, mould cooling at 10–15 °C, and total cycle time from 8 to 15 s. Colour masterbatch is dosed at 2.0–4.0 wt%, slip agent at 0.05–0.15 wt%, and the neat resin fraction is the balance to 100.0 wt%; regrind is held at or below 30 wt% because higher fractions reduce environmental stress crack resistance in aggressive surfactant solutions. Chemical packaging under EU CLP Regulation (EC) No 1272/2008 and REACH requires compatibility testing of the finished cap with the filled formulation; child-resistant closures, where specified, are validated under ISO 8317:2015. The grade is suitable for mild to moderate alkalinity and non-oxidising surfactant systems, but if the formulation contains strong oxidisers, high aromatic solvent loadings, or hypochlorite bleach above 2.0 wt%, environmental stress crack testing under ASTM D1693 condition B is required before commercialisation. End products include measuring cup caps, two-piece flip-top caps, trigger sprayer shrouds, and dose chamber closures for liquid detergent, fabric softener, and non-food cleaner packaging. The primary field failure is cap skirt deformation from unbalanced clamping; the acceptance limit is maximum out-of-roundness of 0.25 mm at the open end within 24 h after ejection.

    Application zoneCore compliance anchorProcess acceptance test method
    Dairy and still beverage closuresEU 10/2011; FDA 21 CFR 177.1520(c)ISO 1133-1:2022; ISO 527-2:2012; ISO 178:2019
    Thin-wall dairy cups and deli packagingEU 10/2011; FDA 21 CFR 177.1520; EN 13428ISO 1133-1:2022; ISO 11357-3:2018; ISO 527-2:2012
    Returnable crates and pallet sleevesREACH Annex XVII; EU Directive 94/62/EC; ISO 14021:2016ISO 1133-1:2022; ISO 179-1/1eA
    Household chemical closuresREACH; EU CLP (EC) No 1272/2008; ISO 8317:2015ISO 1133-1:2022; ASTM D1693 condition B
    Personal care rigid packagingREACH; EU Regulation (EC) No 1223/2009; EU Directive 94/62/ECISO 1133-1:2022; ISO 178:2019
    Industrial open-top pailsUN 1H2; EU 10/2011; FDA 21 CFR 177.1520; EU Directive 94/62/ECISO 2248:1985; ISO 2234:2000; ISO 1133-1:2022

    For personal care and cosmetic rigid packaging, including jars, overcap shells, deodorant stick housings, and lotion spouts, the neat resin fraction of SIBUR HDPE HD12500 LH is set at the balance to 100.0 wt% after colour masterbatch at 2.0–3.0 wt% and in-house regrind from the same tool that is limited to 20 wt% to maintain gloss uniformity and sink-free sidewalls. Compliance is set by REACH and by packaging compatibility testing under EU Regulation (EC) No 1223/2009 when the pack contacts the cosmetic formulation; heavy-metal restrictions follow EU Directive 94/62/EC. Moulding is performed on all-electric injection machines with clamp force of 100–300 t and 24- to 64-cavity valve-gated hot runners, using melt temperature 200–225 °C, mould temperature 10–15 °C, injection speed 60–120 mm/s, holding pressure 35–55 MPa, and total cycle times of 7–12 s. High-gloss sidewall quality requires gas-venting groove depths no larger than 0.02 mm, because deeper vents create visible witness lines at the melt flow front. End products include thick-wall jars with wall thickness from 1.5 to 3.0 mm, thin-wall overwrap caps, and snap-fit spouted closures for shampoos and skin cleansers. Published data for the interaction between mould release residues and labelling adhesion on high-gloss HDPE jars is limited; adhesion validation should be performed on every new tool surface treatment.

    Open-top pail production from SIBUR HDPE HD12500 LH on 1- to 4-cavity injection machines with clamp force between 500 and 1200 t uses a neat resin fraction that makes up the balance to 100.0 wt% after post-industrial regrind up to 30 wt%, colour masterbatch at 2.0–4.0 wt%, and UV stabilizer masterbatch at 2.0–3.0 wt% when outdoor storage is specified. Melt temperature is held at 200–240 °C, mould temperature at 15–25 °C, holding pressure at 45–70 MPa, and cooling time at 15–25 s for pail wall thickness between 2.0 and 3.5 mm. Dangerous goods packaging is tested and certified under the UN 1H2 designation, with drop testing in accordance with ISO 2248:1985 and stacking resistance verified under ISO 2234:2000; food-contact pails additionally comply with EU 10/2011 and FDA 21 CFR 177.1520, while all packaging is subject to EU Directive 94/62/EC and REACH. The critical processing boundary is top-load strength: increasing regrind fraction above 30 wt% reduces top-load capacity by approximately 10–15%, measured after conditioning at 40 °C for 48 h on filled and closed pails. End products include open-top pails from 5 to 25 L, tamper-evident lids with tear bands, food-ingredient containers, and water-based emulsion pails for paints and coatings. The primary field failure is base cracking at the ejector pin location, which is controlled by maintaining ejector speed below 100 mm/s and using air-assisted ejection on pails with base diameters above 300 mm.

    Free Quote

    Competitive SIBUR HDPE HD12500 LH prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SIBUR HDPE HD12500 LH

    SIBUR HDPE HD12500 LH is a high-density polyethylene grade supplied in pellet form and positioned for injection moulding of thin-walled packaging, closures, caps, housewares, toys and small technical parts. The manufacturer’s published nominal values include a melt mass-flow rate of 12.5 g/10 min under ISO 1133-1:2022 at 190°C with a 2.16 kg load and a density of 950 kg/m³ under ISO 1183-1:2019 at 23°C. The high-flow character reduces injection pressure requirements and assists cavity filling in multi-cavity tools, but it also restricts the grade to injection moulding and excludes it from extrusion blow moulding or pressure-pipe service where high melt strength is required.

    What separates HD12500 LH from extrusion blow-moulding HDPE of the same density class?

    The principal distinction is melt strength and molecular weight. Extrusion blow-moulding HDPE grades in the 950 kg/m³ density range typically show melt mass-flow rates from 0.25 g/10 min to 0.45 g/10 min under ISO 1133-1, giving the high viscosity needed to maintain a stable parison. HD12500 LH flows at 12.5 g/10 min, which is too fluid for continuous parison formation and causes excessive sag on industrial blow-moulding lines. Conversely, low-flow blow-moulding grades generate high pressure drop in thin-wall injection tools and often produce short shots in sections below 1.0 mm. The molecular-weight difference also affects environmental stress crack resistance: HD12500 LH has lower ESCR than high-molecular-weight blow-moulding grades, especially in contact with polar solvent mixtures, surface-active cleaning fluids and hydrocarbon-based oils. Critical packaging applications should be validated according to ASTM D1693-15 or ISO 22088-1:2006 because published data for this specific case is limited.

    The nominal property profile for material selection is shown below. The values are single-point data from the grade technical documentation and are not specification limits.

    Nominal properties reported for SIBUR HDPE HD12500 LH
    PropertyTest standardNominal value
    Melt mass-flow rateISO 1133-1:202212.5 g/10 min at 190°C/2.16 kg
    DensityISO 1183-1:2019950 kg/m³ at 23°C
    Tensile stress at yieldISO 527-2:201225.0 MPa
    Nominal tensile strain at breakISO 527-2:2012200%
    Flexural modulusISO 178:20191,050 MPa
    Charpy notched impact strength at 23°CISO 179-1/1eA:20235.0 kJ/m²
    Vicat softening temperature VST/A50ISO 306:2022124°C
    Heat deflection temperature at 0.45 MPaISO 75-2:201373°C

    Processing window and cavity-fill rheology on standard injection presses

    The recommended melt temperature range for HD12500 LH is 180°C to 240°C, with mould surface temperature controlled from 10°C to 40°C. On a 120-tonne hydraulic injection moulding machine running an 8-cavity hot-runner closure tool, stable filling has been observed at a melt temperature near 220°C and mould surface temperature of 20°C to 25°C, although independent published data for this exact tool configuration is limited. Holding pressure is normally set between 40 MPa and 70 MPa, while back pressure at 0.5 MPa to 1.5 MPa is sufficient to avoid screw slip and to maintain a consistent shot mass. Screw speed should be limited to 50 rpm to 100 rpm depending on screw diameter and plastication capacity.

    Pellets are normally processed without predrying when stored in sealed packaging below 50% relative humidity. If the resin has been exposed to ambient air at relative humidity above 60%, surface moisture should be removed using a desiccant dryer at 60°C to 70°C for 2 h to 3 h, with a supply-air dew point no higher than -20°C. Regrind of sprues and runners may be added up to 20 wt% without materially altering the nominal melt mass-flow rate, provided the regrind is free of dust, oil and incompatible pigments. Higher regrind fractions narrow the processing window and tend to reduce notched impact strength, particularly in hinge or snap-fit design elements.

    When mould temperature falls below 10°C, surface gloss and weld-line strength degrade

    Mould surface temperatures below 10°C accelerate the formation of a thick semicrystalline skin layer before cavity packing is complete. Weld lines in closure hinge zones and at narrow gate vestiges become brittle, and surface gloss decreases because the quenched melt freezes before it replicates the polished tool surface. Mould temperatures from 15°C to 35°C generally provide a stable balance between cycle time and part quality. In hot-runner tools, gate freeze time must be verified against gate diameter: vestige gates below 0.8 mm may freeze prematurely and increase residual stress and warpage. When post-mould shrinkage is critical, parts should be conditioned at 23°C and 50% relative humidity for 24 h according to ISO 291:2008 before dimensional inspection.

    Regulatory compliance, food contact and handling restrictions

    Food-contact references for this olefin polymer include EU Regulation 10/2011 and U.S. FDA 21 CFR 177.1520. The final article must be tested for overall migration against the appropriate food simulant; the general EU overall migration limit is 10 mg/dm² of food-contact surface area unless a specific surface-to-volume ratio applies. Compliance is not automatic and depends on processing conditions, masterbatch composition, regrind content and the intended food type. Under REACH Regulation (EC) No 1907/2006, the monomer and intentional additives require registration, and no intentionally added Substances of Very High Concern are declared for the grade. For electrical and electronic articles, the material is assessed against restricted substances listed in Directive 2011/65/EU and Commission Delegated Directive (EU) 2015/863. For the Customs Union market, the finished article must satisfy TR CU 005/2011 on packaging safety and, where applicable, TR CU 007/2011 on children’s products.

    For material substitution studies, the following matrix compares HD12500 LH with other HDPE processing classes. The matrix uses class-level behaviour rather than individual grade specifications.

    Comparative placement of SIBUR HDPE HD12500 LH against other HDPE classes
    ParameterHD12500 LH injection mouldingExtrusion blow-moulding HDPEPE100 pipe-grade HDPE
    Melt mass-flow rate12.5 g/10 min at 190°C/2.16 kg under ISO 1133-10.25 g/10 min to 0.45 g/10 min at 190°C/2.16 kg0.20 g/10 min to 0.35 g/10 min at 190°C/5 kg depending on grade
    Primary conversion processInjection mouldingExtrusion blow mouldingPipe extrusion
    Melt strengthLow; unsuitable for open parisonHigh; parison stabilityHigh; pipe sag resistance
    Environmental stress crack resistanceLower; require validation with aggressive mediaHigher; suitable for bottles and containersHigh; required for long-term hydrostatic service
    Density class950 kg/m³950 kg/m³ to 958 kg/m³958 kg/m³ to 959 kg/m³
    ClassificationNot a pipe resinNot a pipe resinPE100 under ISO 12162/ISO 9080
    LimitationsDo not extrude or blow mould; not for continuous pressure pipeUnsuitable for thin-wall injection moulding below 1.0 mmUnsuitable for injection moulding and blow moulding

    Storage should be maintained below 40°C and away from direct ultraviolet exposure. Opened bags should be re-sealed to prevent moisture adsorption and surface contamination. During silo transfer, dust generation should be controlled to avoid segregation of pellet fines, and metal separation is recommended before processing to protect valve gates and hot-runner tips.

    Top