| HS Code | 643649 |
| Polymer Type | High-density polyethylene (HDPE) |
| Density | 0.958 g/cm³ |
| Melt Flow Rate 190 C 5 Kg | 0.25 g/10 min |
| Mrs Classification | 10.0 MPa |
| Tensile Yield Strength | 23 MPa |
| Tensile Strength At Break | 34 MPa |
| Elongation At Break | >600% |
| Flexural Modulus | 1100 MPa |
| Charpy Notched Impact Strength 23 C | 20 kJ/m² |
| Charpy Notched Impact Strength 20 C | 8 kJ/m² |
| Vicat Softening Temperature | 125°C |
| Brittleness Temperature | -70°C |
| Hardness Shore D | 60 |
| Thermal Conductivity | 0.38 W/(m·K) |
| Coefficient Of Linear Thermal Expansion | 1.2e-4 1/°C |
| Water Absorption | <0.01% |
| Oxidative Induction Time 200 C | >20 min |
| Melting Point | 130°C |
| Color | Natural |
| Form | Pellets |
As an accredited SIBUR HDPE HD10500 NP factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SIBUR HDPE HD10500 NP is typically supplied in 25 kg polyethylene bags, 55 bags per pallet (1,375 kg), shrink-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with SIBUR HDPE HD10500 NP, 25 kg polyethylene bags, palletized and securely stowed for shipment. |
| Shipping | SIBUR HDPE HD10500 NP is a non-hazardous polyethylene resin shipped as pellets. Typical packaging includes 25 kg bags, jumbo bags, or bulk containers. Transport in clean, dry trucks, railcars, or shipping containers. Store away from moisture, heat, and direct sunlight; no special dangerous goods handling required. |
| Storage | Store SIBUR HDPE HD10500 NP in a cool, dry, well-ventilated warehouse, preferably below 40°C. Keep original bags sealed on pallets, off the floor, away from direct sunlight, UV, heat, ignition sources, moisture, and incompatible chemicals. Avoid contamination, excessive stacking, and dust generation. Ensure adequate ventilation, prevent static accumulation, and follow local regulations and the manufacturer’s SDS. |
| Shelf Life | SIBUR HDPE HD10500 NP typically has a 12-month shelf life when stored dry, sealed, away from sunlight, heat, and moisture. |
In high-speed beverage closure moulding, SIBUR HDPE HD10500 NP enters the melt stream as a natural pellet with a nominal melt flow rate of 10.5 g/10 min at 190°C/2.16 kg measured to ISO 1133-1:2022 and a nominal density of 0.950 g/cm³ measured to ISO 1183-1:2019. The formulation step on the conversion floor is limited to dosing of a polyolefin-based colour concentrate at 2.0–3.0 wt% and a slip/antistat masterbatch at 1.5–2.5 wt%, introduced through a gravimetric side feeder or throat feeder calibrated to ±0.1 wt%; because HD10500 NP is supplied unpigmented, the masterbatch carrier melt index must overlap the base resin melt-flow window to avoid localised viscosity striation in the hot-runner manifold. Moulders run high-cavitation closure tools with 48 to 96 cavities, valve-gated hot runners, screw L/D ratios of 20:1 to 24:1, front-zone melt temperatures of 210–240°C, and mould temperatures held at 10–20°C; injection speed is set to fill the annular tamper-evident band before skin freeze-off, with hold pressures of 35–50 MPa, back pressure of 5–15 bar, and total cycle times of 5.5–7.5 s. The resulting article types include tamper-evident beverage caps, tethered closures produced under EU Single-Use Plastics Directive design requirements, sports caps, and push-pull closures. Food-contact compliance is evaluated under FDA 21 CFR 177.1520(c) for olefin polymers, EU 10/2011 with overall migration limit 10 mg/dm², and EC 1935/2004; closure torque retention and strip torque are tested according to ASTM D3474 or equivalent internal specifications. Surface moisture above 0.05 wt% from condensation after outdoor silo storage is removed by drying at 80°C for 2 h; processing above 250°C is not required and can shift colour masterbatch carrier rheology.
Warpage in thin-walled dairy spread containers is controlled less by melt temperature alone than by the interaction between cavity filling pressure, anisotropic shrinkage after ejection, and the crystallisation rate of the HDPE skin layer. SIBUR HDPE HD10500 NP with MFR 10.5 g/10 min at 190°C/2.16 kg is processed in stack moulds with 0.35–0.65 mm nominal wall thickness at melt temperatures of 220–245°C, mould temperatures of 15–25°C, and injection speeds of 200–350 mm/s, using accumulator-assisted injection units on machines with 2500–6000 kN clamping force. The hold-pressure phase is switched by screw position at 8–12 mm before transfer, with hold pressures of 40–60 MPa and cooling times of 2.5–4.0 s; total cycle time is 4.0–7.0 s. The pigmentation package for dairy packaging consists of a titanium dioxide white masterbatch at 2.0–4.0 wt% and a fluoropolymer-free processing aid at 0.5–1.0 wt%; TiO₂ loadings above 4.0 wt% are avoided because the abrasive effect on valve-gate pins and the increase in melt viscosity can increase gate blush and reduce notched impact measured to ISO 179-1:2010. Differential shrinkage between flow direction and transverse direction is reduced when mould cooling variation across the cavity is held within ±2°C; wider deviations produce visible sidewall warpage after 48 h post-moulding conditioning. Terminal products are yoghurt cups, dairy spread tubs, and frozen dessert containers. Compliance for these articles is established under FDA 21 CFR 177.1520(c), EU 10/2011, and migration testing according to EN 1186-1:2002, with overall migration not exceeding 10 mg/dm² and specific migration of the masterbatch additives within their authorised limits.
For non-food household articles with nominal wall thickness between 1.2 mm and 2.5 mm, SIBUR HDPE HD10500 NP is processed on conventional three-zone screw injection units without hot-runner complexity, at melt temperatures of 200–230°C and mould temperatures of 15–30°C. The formulation ratio is 3.0–5.0 wt% colour masterbatch and 0.5–1.0 wt% antistatic masterbatch; regrind from sprues and rejected parts is tolerated up to 20 wt% only when impact strength after recycling is verified to ISO 179-1:2010. Hold pressure is set at 30–45 MPa with clamp force between 800 kN and 2500 kN depending on projected area. Terminal article types are storage boxes, clothes hangers, buckets, and baskets. Chemical compliance is driven by REACH Annex XVII entry restrictions, and if the article may be placed on the market as a children's item, the accessible heavy-metal migration limits in EN 71-3:2019+A1:2021 apply. No food-contact declaration is required in this segment.
UN-certified pail moulding from SIBUR HDPE HD10500 NP requires qualification of the finished pail geometry, not the raw material alone, under the UN 1H2 open-head plastics packaging specification for packing groups I, II, or III. The moulding process uses melt temperatures of 210–235°C, mould temperatures of 10–20°C, wall thicknesses of 2.0–3.5 mm, and hold pressures of 35–50 MPa; clamp force requirements for a 10 L to 20 L pail body and lid normally fall between 4000 kN and 8000 kN. The screw should have an L/D of 20:1 to 24:1 and a compression ratio of 2.5:1 to 3.0:1, with cycle time of 25–45 s for solid-wall injection pails. Formulation addition is 2.5–4.0 wt% colour masterbatch and 0.3–0.5 wt% UV stabiliser masterbatch if the pail is specified for exterior storage; clean in-house regrind is used at up to 20–30 wt%, but each regrind-containing lot must pass the same UN performance tests. Products include 5 L, 10 L, and 20 L injection-moulded industrial pails, lids, bails, and tamper-evident ring components. Published drop-test data for this specific SIBUR grade and pail geometry is limited, so converter qualification is conducted on the finished article rather than inferred from resin datasheet values.
| UN test | Reference condition | Pass criterion |
|---|---|---|
| Drop test, PG I | Height 1.8 m, filled and conditioned | No leakage after impact |
| Drop test, PG II | Height 1.2 m | No leakage after impact |
| Drop test, PG III | Height 0.8 m | No leakage after impact |
| Stacking load | 40°C for 28 days | No deformation affecting closure integrity |
Injection moulding of cosmetic jar bases and compact housings from SIBUR HDPE HD10500 NP is governed by packaging compatibility requirements rather than food-contact migration limits, with article testing aligned to ISO 22715:2006 and EC 1223/2009 for cosmetic packaging safety. The chosen formulation includes a polyolefin-based colour masterbatch at 2.0–3.0 wt% and a slip/antistat masterbatch at 0.5–1.0 wt%; thick-section jar bases above 3.0 mm may require an additional antioxidant masterbatch at 0.2–0.5 wt% to prevent yellowing after extended residence time. Processing on a standard screw machine is set to melt temperatures of 210–235°C, mould temperatures of 15–25°C, and cycle times of 25–50 s. Mould surfaces require SPI A-2 or A-3 polish because surface defects are replicated directly onto the visible jar base; ejection uses stripper plates or air-assisted ejection to avoid pin marks. Terminal article types are cream jars, compact housings, and oversized closure bases for cosmetic tubes. Scrap rate is highest at colour-change sequences, so the natural HD10500 NP base permits purge-to-colour transitions that are shorter than pigmented grades.
Substitution of polypropylene by SIBUR HDPE HD10500 NP in crates, logistics totes, and pallet boxes is evaluated through flexural modulus, impact, and environmental stress crack resistance rather than melt flow alone. The grade is processed at melt temperatures of 210–240°C, mould temperatures of 15–35°C, and wall thicknesses of 2.5–4.0 mm; injection speeds of 30–80 mm/s reduce jetting in large flat panels, and hold pressures of 30–50 MPa with clamp forces of 5000–10000 kN are typical. Formulation addition consists of 3.0–5.0 wt% colour masterbatch and 1.0–2.0 wt% UV stabiliser masterbatch when the crate is specified for outdoor exposure; antistatic masterbatch at 0.5–1.0 wt% is used where dust attraction interferes with automated sorting. The lower flexural modulus of HDPE compared with PP, measured to ISO 178:2019, must be offset by rib depth or wall thickness increases; Charpy impact at 23°C and -20°C is measured to ISO 179-1:2010, and stress-crack resistance in detergent environments is screened by ASTM D1693-15. Terminal article types include fruit and vegetable crates, reusable logistics totes, and pallet boxes. Compliance for non-food industrial articles falls under REACH Annex XVII, with packaging environmental evaluation guided by ISO 18601:2013. Processors should verify low-temperature impact before replacing PP in cold-chain distribution, because HDPE grades can show a sharper ductile-to-brittle transition near 0°C compared with PP.
Competitive SIBUR HDPE HD10500 NP prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SIBUR HDPE HD10500 NP is a high-density polyethylene grade supplied as natural pellet stock for extrusion blow moulding and related hollow-body processing. The grade identifier carries two controlling values under SIBUR coding convention: a nominal density of 0.950 g/cm³ and a high-load melt flow rate of 10 g/10 min at 190 °C with 21.6 kg load. The NP suffix is not a chemical modification of the ethylene homopolymer backbone; it is associated with natural-pellet packaging and should be confirmed against the lot-specific certificate of analysis. Because the material is an ethylene homopolymer with a predominantly linear structure, the melt is classified as a high-molecular-weight blow moulding resin rather than a low-flow injection-moulding grade.
Processors requiring exact batch acceptance limits should obtain the current SIBUR technical passport. The values reproduced in industrial sources are typically control bands rather than universal material constants. Polyethylene oxidation behaviour, melt rheology, and part performance depend on catalyst residues, additive package, storage history, and processing conditions. A single numeric property without the associated test method designation therefore has limited control utility for release testing.
The high-load melt flow rate is determined under ISO 1133-1:2022 at 190 °C and 21.6 kg piston load. This condition is used for blow moulding grades because a standard 2.16 kg loading would produce values too low for practical differentiation among high-molecular-weight resins. The nominal high-load melt flow rate of 10 g/10 min positions HD10500 NP in the medium-high molecular weight region of HDPE blow moulding materials. The density of 0.950 g/cm³, measured under ISO 1183-1, reflects the crystalline fraction established by thermal history and the absence of significant comonomer content. Increasing density within the HDPE family generally raises modulus and water-vapour barrier, but may reduce environmental stress crack resistance and low-temperature impact. HD10500 NP is therefore selected where processability, container integrity, and surface finish require a controlled balance rather than maximal crystallinity.
The following release indicators are commonly referenced for this grade. The ranges in the table should be treated as process-control values, not as a substitute for the SIBUR certificate of analysis.
| Property | Test method | Typical release or control range | Notes |
|---|---|---|---|
| Density | ISO 1183-1 method A | 0.948–0.952 g/cm³ | Nominal code value 0.950 g/cm³ |
| High-load melt flow rate | ISO 1133-1:2022, 190 °C, 21.6 kg | 8.0–12.0 g/10 min | Nominal code value 10 g/10 min |
| Ash content | ISO 3451-1 | ≤0.10 wt% | Residue after calcination |
| Moisture content | In-house Karl Fischer or ASTM D6868 | ≤0.02 wt% after drying | Pre-drying threshold for humid storage |
Typical mechanical values for high-density polyethylene of this density and high-load melt flow class are reported under ISO 527-2 tensile testing and ISO 178 flexural testing. Published control data for HD10500 NP generally place tensile yield stress above 20 MPa and flexural modulus in the 800–1100 MPa band. These values are not acceptance limits unless stated on the certificate of analysis; they shift with cooling rate, wall-thickness-induced shrinkage, and test specimen conditioning.
Environmental stress crack resistance of HDPE class materials is evaluated under ASTM D1693 or ISO 22088. For grades with density near 0.950 g/cm³, slow crack growth behaviour is generally better than for 0.953 g/cm³ or 0.955 g/cm³ copolymers. However, published data for HD10500 NP under all stress-cracking conditions is limited. Substitution in aggressive surfactant-containing packaged liquids should be validated by testing the actual bottle or container geometry.
On single-station and double-station shuttle blow moulding machines with extruder L/D ratios of 24:1 to 30:1, HD10500 NP is processed at die melt temperatures in the 180–220 °C range. Head zone settings are typically maintained at 190–210 °C to control parison swell and avoid surface melt fracture. A die gap of 1.5–2.5 mm is common for articles with wall thicknesses from 0.8 mm to 3.5 mm. Blow ratio is usually set between 2.0:1 and 3.0:1. Mould temperatures of 10–30 °C are used to remove heat rapidly from the crystallizing HDPE matrix.
Screw speed for a 60 mm general-purpose melt extruder is normally 20–60 rpm, with barrel profile from 170 °C at feed to 200 °C at metering. Excessive shear at high screw speeds may raise melt temperature above 220 °C and reduce melt strength. The parison then becomes non-uniform, often producing clamp-side webbing and handle-region thinning. Operators on continuous wheel machines have observed that melt-temperature overshoot above 230 °C increases die swell variability and degrades pinch-off weld thickness. The addition of 10–20 wt% clean in-house regrind is standard for non-food-contact moulding; for food-contact applications, regrind usage is constrained by food-contact regulatory conditions and requires validation under (EU) No 10/2011 and FDA 21 CFR 177.1520.
Difference in parison behavior with die gap is a critical processing variable for this grade. Narrowing the die gap below 1.5 mm increases shear stress at the die lip and can raise extruder backpressure to 45 MPa or more, leading to melt-temperature overshoot and parison curl. Widening the gap to 2.5 mm reduces shear stress but increases the draw-down ratio required to reach the target wall. The optimum gap for an article with an average wall of 0.8 mm is commonly 1.6–2.0 mm, but grade-specific validation on the actual tool is required.
Quality control on finished bottles and containers includes top-load testing per ASTM D2659, drop impact per ASTM D2463, and environmental stress crack resistance per ASTM D1693. These outcomes are influenced by processing history. A direct material-only conclusion from a burst or drop result is not technically valid unless parison uniformity, pinch-off geometry, and cooling rate are held constant.
Storage and drying constraints for HD10500 NP follow the general behaviour of HDPE homopolymer pellets. Moisture content above 0.02 wt% can create surface defects in extrusion blow moulding because water vapour expands at the die exit and produces pinholes or streak lines. Pre-drying at 80 °C for 2–4 h in a desiccant dryer is recommended when sacks are stored in ambient relative humidity above 60%. Regrind from edge trim should be sized below 10 mm to prevent feed bridging and maintain consistent melt pumping. Avoid blending with polypropylene or high-melt-flow LDPE streams because phase separation may reduce weld-line strength in pinch-off zones.
Within the SIBUR HDPE grade family, the numeric density code is a primary differentiator. HD10500 NP carries a nominal density of 0.950 g/cm³; grades with a 530 density code are closer to 0.953 g/cm³. That increase raises modulus and top-load strength but may reduce environmental stress crack resistance and low-temperature impact. HD10530 LB is therefore used in rigid packaging where higher top-load and dimensional stability dominate, while HD10500 NP is selected when better stress crack resistance or lower shrinkage is required. The high-load melt flow rate code also differentiates processing: HD20500 PE, with a nominal high-load melt flow rate near 20 g/10 min, flows more readily and is suited to thinner walls or shorter cycle times, but it provides lower sag resistance for large parisons.
The following code-derived comparison is a starting point for grade selection, not a replacement for current technical passports.
| Grade code | Code-derived nominal density | Code-derived nominal HLMI | Downstream implication |
|---|---|---|---|
| HD10500 NP | 0.950 g/cm³ | 10 g/10 min | Balanced stress crack resistance and melt strength for extrusion blow moulding |
| HD10530 LB | 0.953 g/cm³ | 10 g/10 min | Higher top-load; reduced ESCR margin |
| HD20500 PE | 0.950 g/cm³ | 20 g/10 min | Higher flow; lower melt strength |
The relationship between density and slow crack growth in high-density polyethylene is well established. An increase from 0.950 g/cm³ to 0.953 g/cm³ raises crystallinity by approximately 1.5–2.0%, which can reduce the number of tie molecules between crystalline lamellae. Under constant stress at 50 °C, this may lead to earlier crack initiation in aggressive wetting agents such as 10% Igepal CO-630 solution under ASTM D1693 conditions. Because HD10500 NP has a lower nominal density than HD10530 LB, it retains a larger ESCR margin but also exhibits lower top-load stiffness for the same bottle geometry.
Compared with linear low-density polyethylene of equivalent melt flow, HD10500 NP has higher crystallinity and therefore greater modulus, lower elongation, and lower resistance to puncture under multiaxial strain. It should not be used where high dart impact or low-temperature toughness is required; LLDPE or metallocene-catalysed LLDPE film grades are preferred for those conditions. For injection-blow moulding preforms, the high molecular weight of HD10500 NP may raise injection pressure and produce short shots in thin preforms. Batch-to-batch variance in high-load melt flow rate within the 8.0–12.0 g/10 min band can shift injection pressure by 5–10% on a reciprocating screw machine with a 25 mm diameter injection unit. Processors should apply a hold-pressure buffer rather than adjusting cycle time alone.
Compliance with food-contact legislation for HD10500 NP should be verified against the supplier’s declaration for the specific production campaign. Under FDA 21 CFR 177.1520, polyethylene homopolymers may be used for food contact, subject to extractives limitations and end-use conditions. In the European Union, compliance with Regulation (EU) No 10/2011 requires migration testing under worst-case time and temperature conditions; an overall migration limit of 10 mg/dm² applies for plastic food-contact materials. The grade is also subject to REACH information obligations depending on import conditions. These statements are regulatory status descriptors, not performance claims, and must be confirmed on the batch-specific compliance certificate.
The main operational boundary for HD10500 NP is the processing temperature ceiling near 220 °C. Above this limit, oxidative degradation can reduce molecular weight and lower melt strength, producing parison fold defects and reduced pinch-off weld integrity. The grade is not optimized for injection moulding with narrow gates below 0.8 mm or for stretched blow moulding of high-clarity containers, because the natural-pellet high-density structure yields opacity and higher crystallinity than clarified polypropylene or PET alternatives.