Shinkong Shinite Pbt Fr E202g30

Shinkong SHINITE® PBT-FR E202G30

    • Product Name: Shinkong SHINITE® PBT-FR E202G30
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 660751
    Grade Shinkong SHINITE PBT-FR E202G30
    Polymer Type Polybutylene terephthalate (PBT)
    Flame Retardant Yes
    Reinforcement Glass fiber
    Glass Fiber Content 30%
    Density 1.55 g/cm³
    Melt Flow Rate 15 g/10 min (250°C/2.16 kg)
    Tensile Strength 105 MPa
    Elongation At Break 2.0%
    Flexural Modulus 9000 MPa
    Notched Izod Impact Strength 8 kJ/m²
    Heat Deflection Temperature 200°C (1.82 MPa)
    Flammability Rating UL94 V-0
    Water Absorption 0.06% (24 h)
    Molding Shrinkage 0.3-0.6%
    Processing Method Injection molding

    As an accredited Shinkong SHINITE® PBT-FR E202G30 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-resistant bags, palletized and sealed, protecting Shinkong SHINITE PBT-FR E202G30 compound during transport and storage.
    Container Loading (20′ FCL) Shinkong SHINITE® PBT-FR E202G30 is packed and loaded into a 20′ FCL container, palletized, moisture-protected, and securely sealed for shipment.
    Shipping Shinkong SHINITE® PBT-FR E202G30 is a flame-retardant, 30% glass-fiber-reinforced PBT resin supplied as pellets. It is generally non-hazardous and not classified for transport. Ship in sealed moisture-barrier bags or containers, kept dry, cool, ventilated, and away from direct sunlight and ignition sources.
    Storage Store Shinkong SHINITE® PBT-FR E202G30 in a cool, dry, well-ventilated area out of direct sunlight. Keep containers sealed to prevent moisture pickup and contamination, away from heat, flames, sparks, and strong oxidizers. Maintain good housekeeping and grounding to control dust/static. Follow the manufacturer’s SDS and local regulations for safe handling and shelf life.
    Shelf Life Shinkong SHINITE® PBT-FR E202G30 has a shelf life of about 24 months when stored dry, cool, and in unopened original packaging.
    Free Quote

    Competitive Shinkong SHINITE® PBT-FR E202G30 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Shinkong SHINITE® PBT-FR E202G30 is a 30 wt% glass-fiber-reinforced, flame-retardant polybutylene terephthalate injection-molding grade supplied by Shinkong Synthetic Fiber Corporation. The E202 series places the product within the producer’s flame-retardant PBT portfolio; the G30 suffix denotes a nominal glass loading of 30 wt%. The compound is formulated for thin-wall electrical components that must meet UL 94 V-0 at 0.8 mm and 1.6 mm nominal thickness while maintaining higher stiffness and lower mold shrinkage than unreinforced flame-retardant PBT. Typical producer data report tensile stress at break of approximately 120 MPa under ISO 527-2/1A, flexural modulus of approximately 9,000 MPa under ISO 178, and density near 1.69 g/cm³ under ISO 1183-1. Notched Izod impact strength at 23°C is commonly reported near 8 kJ/m² under ISO 180/1A, and heat deflection temperature at 1.82 MPa is in the region of 200–210°C under ISO 75-2/A. These values are representative for natural-color lots; pigmented and regrind-containing feedstock can shift the property envelope.

    The primary usage area is electrical and electronic structural components: connector housings, relay bobbins, circuit-breaker internal carriers, terminal blocks, fuse holders, motor brush holders, coil forms, and sensor enclosures. In each case the material is selected where a combination of flame resistance, dielectric strength, and elevated-temperature rigidity is required, and where metal inserts or snap-fit features demand high tensile stress and resistance to creep. The glass reinforcement increases the material’s stiffness and lowers mold shrinkage to approximately 0.2–0.5% in the flow direction, but the same reinforcement introduces anisotropic mechanical properties and flow-front weld lines that must be addressed in tool design. The compound’s flame-retardant classification is thickness-dependent and color-sensitive. Unpigmented and black lots are usually covered by the producer’s UL 94 file; custom colors may require separate evaluation because pigments can reduce the effective flame-retardant concentration at the surface. Components with weld lines, knit lines, or exposed glass fibers at the surface should be subjected to lot-level flammability testing at the minimum wall thickness.

    When Thin-Wall Connector Housings Need Both Flame Resistance and Low Anisotropic Mold Shrinkage

    In a thin-wall connector housing with nominal wall thickness 0.5–1.0 mm, the grade is processed at melt temperatures closer to the upper limit of the recommended range to avoid short shots. The practical minimum wall thickness for 30% glass-filled PBT is generally 0.5 mm; below this value, the glass fiber length distribution and gate freeze-off can prevent complete mold filling. The flame-retardant package increases melt viscosity relative to non-FR PBT of the same glass loading, so filling analysis using Moldflow fiber-orientation models is used to locate the gate and to predict warp. Shrinkage is anisotropic: flow-direction mold shrinkage is typically 0.2–0.5%, while transverse shrinkage is often 0.5–0.9%. Unbalanced packing across the cavity can produce warpage exceeding 0.1 mm over a 100 mm span, which is often outside the flatness tolerance for multi-pin connectors.

    For a connector with a pitch below 2.54 mm, the tool should use pinpoint gates or submarine gates with a land length below 1.0 mm and gate diameter of 0.8–1.2 mm to allow rapid gate freeze-off without excessive shear heating. The grade’s 30% glass content creates visible fiber orientation at the weld line; this is acceptable for internal structural parts but may be unacceptable for cosmetic surfaces without painting or texturing. Melt temperature at the flow front should remain above 250°C to prevent cold-slug formation at weld lines. If fill time exceeds 2 s in wall sections below 0.8 mm, the material may freeze prematurely at the gate, producing short shots or high residual stress. Process engineers therefore set injection velocity profiles to fill the cavity quickly and transfer to hold pressure before cavity pressure rises into the flash zone near the parting line.

    What Separates E202G30 from Lower Glass-Content Flame-Retarded PBT Grades?

    Within the flame-retardant PBT family, the 30 wt% glass loading moves the property profile away from the more flowable E202G15 and the unreinforced FR PBT base resin. The most direct consequence is an increase in flexural modulus and heat deflection temperature, accompanied by a reduction in melt flow length. In thin-wall tools designed for unreinforced FR PBT, E202G30 will typically require higher injection pressure and may exhibit shorter spiral-flow length by about 30–50%. The change is not linear with glass content because fiber orientation, fiber aspect ratio, and wall thickness interact with the flame-retardant carrier.

    Representative property classes reported for natural-color lots; not lot-specific specification limits.
    PropertyTest methodE202G30E202G15Unfilled FR PBT
    Glass fiber contentISO 3451-130 wt%15 wt%0 wt%
    DensityISO 1183-11.68–1.72 g/cm³1.55–1.60 g/cm³1.45–1.50 g/cm³
    Tensile stress at breakISO 527-2/1A115–130 MPa90–110 MPa55–70 MPa
    Flexural modulusISO 1788,500–9,500 MPa5,000–6,500 MPa2,400–2,800 MPa
    Notched Izod impact at 23°CISO 180/1A7.0–9.0 kJ/m²5.0–7.0 kJ/m²3.0–5.0 kJ/m²
    HDT at 1.82 MPaISO 75-2/A200–210°C190–200°C90–100°C
    Mold shrinkage, flow directionISO 294-40.20–0.50%0.25–0.60%0.80–1.60%

    The practical consequence is that E202G30 is selected when rigidity, creep resistance, or dimensional stability is the limiting requirement. If flow length or weld-line strength is the limiting requirement, E202G15 or an unreinforced flame-retardant PBT may be considered, though at the cost of lower modulus and higher mold shrinkage.

    A desiccant dryer with a dew point no higher than -35°C is used to reduce pellet moisture to 0.02 wt% or lower before molding. Drying at 110–120°C for 4 h is typical for sealed-foil or freshly opened containers; material exposed to ambient air at relative humidity above 60% may require 6 h or longer. Melt processing is performed with barrel set temperatures from 250°C to 270°C, with the nozzle at approximately 260°C. The practical melt-temperature window is narrower than for non-FR PBT. At 245°C the melt viscosity can be too high for thin-wall filling; at 275°C the flame-retardant package can begin to produce discoloration and acidic decomposition products. The processing window is therefore approximately 250–270°C, and barrel settings are monitored with melt pyrometry rather than relying solely on barrel thermocouples.

    Mold surface temperature is controlled between 60°C and 90°C; the upper half of that range improves weld-line strength and dimensional stability but extends cycle time. Injection speed is set from medium to high; thin-wall sections may require fill times of 0.5–1.5 s and injection pressure up to 150 MPa, depending on flow length and gate size. Hold pressure is set to pack the part after gate freeze-off; typical hold pressures are 60–100 MPa for hot-runner systems with restricted gates. A screw cushion of 3–5 mm is maintained to reduce fiber breakage and to ensure consistent packing. Lot-to-lot variation in glass fiber length distribution and flame-retardant additive concentration can change melt viscosity by ±5–10%; injection process limits are set with this variation in mind. Production-scale machines with clamp force below 800 kN may be unable to hold the parting line closed at high packing pressure, especially for multi-cavity tools with projected area above 200 cm².

    The injection unit should use a screw with length-to-diameter ratio of 20:1 to 24:1 and compression ratio of 2.5:1 to 3:1. A low-compression, low-shear screw is preferred to minimize glass fiber attrition. Total residence time at melt temperature should not exceed 5 min; longer residence times can reduce flame retardancy and produce black specks or silver streaks. Regrind use is limited to 20 wt% with properly dried, uncontaminated feed; higher levels or mixed-color regrind can compromise UL 94 classification and mechanical impact strength.

    Weld-Line Strength and Fiber Orientation in Hot-Runner Tooling

    Hot-runner tooling with multiple valve gates produces weld lines at the meeting of melt fronts. In a 30% glass-filled PBT, weld-line tensile strength can be 40–60% lower than the unwelded flow-region tensile value because glass fibers orient parallel to the weld interface rather than bridging across it. The location of the weld line is managed by sequential valve-gate timing, but the strength reduction cannot be eliminated by melt temperature alone. Raising mold temperature to 80–90°C and increasing wall thickness locally can improve weld-line strength by allowing fibers to reorient across the interface.

    Venting is critical at weld areas. Vent depth for glass-filled PBT is typically 0.01–0.02 mm; deeper vents allow flash. The clamp force required for E202G30 is generally 6–8 kN/cm² of projected area, based on melt pressure at the gate. For multi-cavity tools with unbalanced runner layouts, cavity-to-cavity fill variation can be several percent, which is enough to shift fiber orientation and create inconsistent flame ratings across cavities. Runner systems should be geometrically balanced, and any hot-runner manifold must maintain melt temperature within the recommended range at every nozzle. When metal inserts are overmolded, the insert temperature should be maintained at 100–130°C to prevent the resin from freezing before the insert surface is fully wetted. A cold insert creates a weak boundary layer and can lower weld-line strength, particularly in flame-retardant PBT where the crystallizing front is fast.

    The grade is supplied to meet the substance restrictions of Directive 2011/65/EU Annex II, as amended by (EU) 2015/863, and the SVHC communication obligations under Regulation (EC) No 1907/2006. Electrical and electronic component producers should verify the latest supplier declaration for the specific color and production lot. Because the product is a flame-retardant PBT and the producer does not classify it as halogen-free, applications calling for halogen-free designations under IEC 61249-2-21 or proprietary limits of 900 ppm chlorine and 900 ppm bromine may require a different resin. E202G30 is intended for applications in which UL 94 V-0 thin-wall performance is the primary flammability requirement and the flame-retardant chemistry is accepted by the end-use specification.

    In hot-humid electrical contact environments, designers should evaluate contact resistance stability after 85°C/85% RH aging under IEC 60068-2-78, because halogenated flame-retardant packages can release trace acidic species that accelerate metal contact corrosion. The grade should not be exposed to high-pH aqueous solutions for prolonged periods; PBT is subject to hydrolytic chain scission above 80°C in water or steam, and the glass reinforcement does not prevent this degradation. Compounding with amine-based additives or excessive alkaline metal stearates is avoided because these can act as halogen acid scavengers or transesterification agents and destabilize the flame-retardant system.

    For arcing and surface-tracking exposure, comparative tracking index is commonly reported under IEC 60112 at 250 V for glass-filled flame-retardant PBT formulations; exact CTI values are color- and formulation-dependent. The glass fiber reinforcement creates a slightly more conductive surface at high humidity than unfilled PBT because fiber-rich surface layers can adsorb moisture. Dielectric strength under IEC 60243-1 is specified on the same thickness and conditioning state as the part drawing. For applications requiring repeated soldering or high IR reflow temperatures, the short-term heat resistance of the grade is defined by HDT at 1.82 MPa and not by continuous-use temperature. Published data for specific thermal-oxidative aging kinetics of this exact configuration is limited; long-term thermal indexing should be determined by end-use testing or by request from the producer.

    Top