| HS Code | 946133 |
| Materialtype | Polybutylene terephthalate (PBT), 30% glass fiber reinforced, electronic grade |
| Fillercontent | 30% glass fiber |
| Density | 1.50–1.56 g/cm³ |
| Tensilestrength | 100–130 MPa |
| Elongationatbreak | 2–4% |
| Flexuralstrength | 160–200 MPa |
| Flexuralmodulus | 7500–9000 MPa |
| Notchedimpactstrength | 7–12 kJ/m² |
| Heatdeflectiontemperature | 200–210 °C at 1.82 MPa |
| Meltingpoint | 220–225 °C |
| Volumeresistivity | ≥1×10^15 Ω·cm |
| Dielectricconstant | 3.2–3.8 at 1 MHz |
| Dielectriclosstangent | 0.01–0.02 at 1 MHz |
| Moldingshrinkage | 0.2–0.5% |
| Waterabsorption | ≤0.1% |
As an accredited Shengquan Group PBT Electronic Grade SQ-PBT-G30 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Shengquan Group PBT Electronic Grade SQ-PBT-G30 is packed in 25 kg net moisture-barrier bags, palletized for bulk shipment. |
| Container Loading (20′ FCL) | 20′ FCL dry container loaded with palletized 25 kg bags, stretch-wrapped, labeled, and secured for export transport. |
| Shipping | Shengquan Group PBT Electronic Grade SQ-PBT-G30 is shipped as non-hazardous polymer pellets in sealed moisture-barrier bags or containers. Keep dry, cool, ventilated, and away from sunlight, heat, and contamination. Use clean, dry transport equipment; protect from moisture, humidity, and physical damage during loading, transit, and unloading. |
| Storage | Store Shengquan Group PBT Electronic Grade SQ-PBT-G30 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and ignition sources. Keep original packaging tightly sealed and palletized; avoid dust generation and static buildup. Maintain dry conditions to prevent moisture absorption. Follow local regulations and the manufacturer’s safety data sheet for handling and shelf life. |
| Shelf Life | Shengquan Group PBT Electronic Grade SQ-PBT-G30 has a shelf life of 12 months when stored dry, cool, and sealed. |
Competitive Shengquan Group PBT Electronic Grade SQ-PBT-G30 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Shengquan Group SQ-PBT-G30 is an electronic-grade polybutylene terephthalate compound reinforced with a nominal 30 wt% chopped glass fiber. The G30 designation refers to the glass fiber mass fraction, not the total inorganic content after addition of flame-retardant synergists, nucleants, or mineral fillers. Electronic-grade qualification for PBT is defined by low aqueous extract conductivity, controlled halide release, low outgassing during short-term solder exposure, and stable surface insulation resistance after damp-heat aging. Compared with general-purpose PBT-GF30, the electronic-grade variant is released with narrower lot-to-lot limits on melt volume-flow rate, residual moisture, and pin-to-pin dielectric performance. The material is intended for injection-molded electrical connectors, relay bases, coil bobbins, switch housings, and sensor enclosures that require dimensional stability after soldering and low surface leakage current. Melt volume-flow rate measured under ISO 1133-1:2022 at 250 °C and 2.16 kg typically falls between 10 cm³/10 min and 25 cm³/10 min; the exact value is fixed on the batch certificate. Because publicly available data for this specific grade is limited, the following values represent the typical envelope for 30% glass-reinforced electronic-grade PBT and should be confirmed against the supplier’s technical datasheet.
The suppression of oxidative degradation in PBT relies on hindered phenol and phosphite stabilizer combinations; in electronic grades, stabilizer degradation products must not migrate to the surface because surface migration raises contact resistance and increases dielectric loss in humid service. Ionic contamination is evaluated by aqueous extraction conductivity using a supplier-defined ultrapure-water extraction protocol. Electronic-grade PBT for relay bases and connector insulators commonly limits extract conductivity to below 20 µS/cm after 24 h immersion in deionized water at 80 °C, although the mandatory acceptance value for SQ-PBT-G30 must be obtained from the material specification. Volume resistivity measured under IEC 62631-3-1 after conditioning at 23 °C and 50 % RH is not less than 1 × 1015 Ω·cm for this glass-reinforced polyester class. Surface resistivity under IEC 62631-3-2 remains above 1 × 1014 Ω on molded surfaces free of external mold-release agents. Glass fiber interfaces can create microvoids that adsorb moisture; electronic-grade compounding therefore uses silane coupling chemistry to reduce the dielectric loss tangent at 85 °C and 85 % RH. Water absorption after 24 h under ISO 62 is generally 0.04–0.06 %, roughly an order of magnitude lower than glass-reinforced polyamide 66.
Under tensile loading per ISO 527-2/1A, 30% glass-reinforced PBT in the electronic-grade class typically exhibits tensile strength of 120–135 MPa at 23 °C, compared with 55–65 MPa for unfilled PBT. Tensile modulus is generally 9000–10000 MPa, up from 2500–2800 MPa. Flexural strength and flexural modulus determined by ISO 178 are approximately 190–210 MPa and 8500–9500 MPa, respectively. Notched Izod impact resistance under ISO 180/A is commonly 8–10 kJ/m², lower than unfilled PBT but sufficient for rigid insulator housings. The mechanical response is anisotropic because short glass fibers orient in the shear field during mold filling. Tensile values measured on specimens cut perpendicular to flow can be 20–35 % lower than flow-direction values. On production-scale injection tools with 1200–1600 kN clamping force, weld lines become the primary mechanical failure mode because fiber orientation discontinuity at the melt front reduces local tensile strength to 50–70 % of the nominal value. Sequential valve gating or overflow wells are specified for bosses and snap features to displace weld lines away from load-bearing sections. The difference from standard PBT-GF30 is not primarily tensile strength but the electronic-grade requirement for tighter control of ionic extractables, outgassing, and post-mold warpage.
| Property | Test method | Typical range for electronic-grade PBT-GF30 |
|---|---|---|
| Density | ISO 1183-1 | 1.55–1.60 g/cm³ |
| Tensile strength at break | ISO 527-2/1A | 120–135 MPa |
| Tensile modulus | ISO 527-2/1A | 9000–10000 MPa |
| Flexural strength | ISO 178 | 190–210 MPa |
| Flexural modulus | ISO 178 | 8500–9500 MPa |
| Notched Izod impact at 23 °C | ISO 180/A | 8–10 kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-2/A | 200–210 °C |
| CLTE, flow / transverse, 23–80 °C | ISO 11359-2 | 2.5 × 10-5 1/K / 7.0 × 10-5 1/K |
| Volume resistivity | IEC 62631-3-1 | 1 × 1015 Ω·cm |
| Surface resistivity | IEC 62631-3-2 | 1 × 1014 Ω |
| Dielectric strength, 2 mm | IEC 60243-1 | 20–24 kV/mm |
| Comparative tracking index | IEC 60112 | 250–300 V |
| Water absorption, 24 h | ISO 62 | 0.04–0.06 % |
| Mold shrinkage, flow / transverse | ISO 294-4 | 0.2–0.5 % / 0.7–1.0 % |
Values are representative of 30% glass-reinforced electronic-grade PBT compounds. Exact SQ-PBT-G30 values must be verified against the supplier’s technical datasheet.
Relative to lower glass loadings, the 30% grade shifts the stiffness-to-elongation balance toward rigidity. PBT-GF10 typically shows tensile modulus near 4500–5500 MPa, PBT-GF20 near 6500–7500 MPa, and the G30 variant reaches 9000–10000 MPa; however, the G30 variant exhibits lower elongation at break and more anisotropic shrinkage. Compared with PBT/PC blends, SQ-PBT-G30 has higher flexural modulus but lower notched impact, especially below -20 °C. Compared with PA66-GF30, SQ-PBT-G30 provides lower water uptake and better dimensional stability in humid service, but PA66-GF30 retains higher heat deflection temperature near 250 °C under the same 1.8 MPa load. Compared with PPS-GF40, the PBT electronic grade processes at lower melt temperatures but does not match the continuous-use temperature or chemical resistance of polyphenylene sulfide. These differences guide substitution decisions in connector platforms where soldering thermal load, chemical cleaning, and dimensional stability are simultaneous constraints.
Under cyclic thermal loading typical of infrared and convection soldering, dimensional stability is governed by the heat deflection temperature and the coefficient of linear thermal expansion. For SQ-PBT-G30, deflection temperature under ISO 75-2/A at 1.8 MPa is expected in the range of 200–210 °C. Flow-direction CLTE determined by ISO 11359-2 from 23 °C to 80 °C is approximately 2.5 × 10-5 1/K; transverse CLTE is typically 7.0 × 10-5 1/K and is the main driver of warpage in thin-wall parts. Peak soldering temperatures above 260 °C exceed the continuous-use window of standard PBT; short-term reflow performance depends on part mass, wall thickness, and peak duration, and published data for this specific SQ-PBT-G30 configuration is limited. In wave soldering, preheat at 100–120 °C for 60–90 s reduces thermal shock and prevents surface blistering. Connector bodies with wall thickness below 0.8 mm should be validated for flatness after a full thermal profile because differential CLTE can produce bowing beyond the typical coplanarity limit of 0.1 mm across a 50 mm span.
Electrical connectors and relay bases require defined dielectric strength across narrow contact barriers. Dielectric strength measured under IEC 60243-1 on 2 mm specimens is commonly 20–24 kV/mm after conditioning at 23 °C and 50 % RH. The comparative tracking index under IEC 60112 is typically 250–300 V for glass-filled non-flame-retardant PBT, placing the material in PLC 1 to PLC 2; the actual value for SQ-PBT-G30 must be confirmed from the UL Yellow Card or equivalent test report. The electronic-grade difference appears most clearly in damp-heat aging at 85 °C and 85 % RH for 1000 h, after which surface insulation resistance is specified to remain above 1 × 1012 Ω. Glass fibers near the part surface increase roughness and can adsorb a conductive moisture film; a resin-rich skin of 10–20 µm is generally required. This skin is produced by mold temperatures near 100 °C and by avoiding excessive melt shear that transports glass to the cavity surface. In multi-pin connectors, flash and exposed glass at the parting line must be controlled because they reduce creepage distance and compromise pin-to-pin dielectric performance.
Electronic-grade PBT compounds are sometimes offered in flame-retardant configurations. If SQ-PBT-G30 is supplied with a flame-retardant system, classification is typically verified to UL 94 V-0 at the declared minimum thickness and halide limits are checked against IEC 61249-2-21; the flame-retardant chemistry influences comparative tracking index, water uptake, and hot-runner residence stability. The exact SQ-PBT-G30 classification must be taken from the UL Yellow Card or technical datasheet.
Before compounding or molding, residual moisture must be reduced below 0.02 wt% by Karl Fischer titration to ISO 15512:2019 in order to limit hydrolytic chain scission of the ester backbone. Desiccant drying at 120 °C for 4–6 h with a dew point of -40 °C or lower is standard for virgin material; reground open material may require 6–8 h. Barrel set points from rear to nozzle are ordinarily 235–250 °C, 245–260 °C, 250–265 °C, and 255–270 °C, with measured melt temperature held between 245 °C and 265 °C. Sustained melt temperature above 270 °C accelerates thermal degradation, releasing tetrahydrofuran and reducing molecular weight; residence time above 5 min at 270 °C is not recommended. Screw geometry should use a low-compression thermoplastic screw with a length-to-diameter ratio of 20:1 to 24:1 and a wear-resistant check ring designed for glass-filled materials. Barrel and screw surfaces should be bimetallic or otherwise hardened because 30 wt% glass fiber is abrasive. Mold temperature must be controlled between 80 °C and 100 °C; below 80 °C the surface may form with exposed glass and the part can exhibit higher warpage, while above 100 °C cycle time and mold maintenance cost increase without proportional property gain. Clamp force for thin-wall connectors should be estimated at 4–7 kN/cm² of projected cavity area. Typical injection pressure is 90–130 MPa with hold pressure of 60–100 MPa; hold time should follow gate freeze and is commonly 3–5 s for a gate diameter of 1.0–1.5 mm. Hot-runner valve gates reduce fiber-orientation anisotropy but require insert materials and shut-off surfaces rated for continuous glass-fiber abrasion.
Polyamides absorb 1.5–2.5 % moisture at equilibrium at 23 °C and 50 % RH, whereas 30% glass-reinforced electronic-grade PBT absorbs less than 0.1 % under the same condition. This difference is relevant for humid electrical housings where dimensional movement must remain below 0.1 %. Water absorption after 24 h immersion per ISO 62 is typically 0.04–0.06 % for SQ-PBT-G30. Saturated linear dimensional change is usually below 0.2 %, compared with 0.5–1.0 % for glass-filled PA66 in the same environment. Mold shrinkage under ISO 294-4 is 0.2–0.5 % in the flow direction and 0.7–1.0 % in the transverse direction. The differential shrinkage is lower than unfilled PBT and is closer to that of a filled thermoset; the trade-off is part anisotropy. If wall thickness variations exceed 2:1, the shrinkage differential can produce bowing. Tool designs should therefore maintain uniform wall sections and gate placement that minimizes transverse-to-flow differential. Relative to PBT/PC blends, SQ-PBT-G30 has higher stiffness and better chemical resistance to aromatic hydrocarbons used in connector cleaning, but lower notched impact at low temperature.
Prolonged contact with hot water above 80 °C or aqueous alkaline media with pH above 9 hydrolyzes the ester groups in polybutylene terephthalate and should be avoided. Concentrated sulfuric acid and hydrochloric acid attack the polymer at elevated temperature. The material is resistant to aliphatic hydrocarbons, room-temperature alcohols, and mineral oils used in electrical assembly. Amine-based processing aids and certain flame-retardant masterbatches can accelerate hydrolytic chain scission or produce surface splay in glass-filled PBT; compatibility must be verified by plate-out trials on a production-scale twin-screw extruder before introduction. For ultrasonic welding, unprotected thin sections may be damaged by glass-fiber disruption at the weld interface; low-amplitude and reduced trigger force settings are advised. Chemical exposure tests on molded parts under ASTM D543-21 are recommended before deployment in aggressive wash processes.