Sharq Hdpe F1

SHARQ HDPE F1

    VTB
    Specifications
    HS Code 367222
    Gradename SHARQ HDPE F1
    Polymertype High Density Polyethylene
    Density 0.958 g/cm3
    Meltflowrate 190c 21 6kg 0.05 g/10 min
    Meltingpoint 134 °C
    Vicatsofteningtemperature 127 °C
    Tensilestrengthatyield 26 MPa
    Tensilestrengthatbreak 35 MPa
    Elongationatbreak 600%
    Flexuralmodulus 1100 MPa
    Izodimpactstrengthnotched 50 J/m
    Shoredhardness 65
    Thermalconductivity 0.45 W/mK
    Coefficientoflinearthermalexpansion 1.2E-4 /°C
    Waterabsorption <0.01%
    Dielectricconstant 2.3
    Volumeresistivity >1E16 ohm-cm
    Dielectricstrength 20 kV/mm
    Chemicalresistance Good
    Uvresistance Poor
    Environmentalstresscrackresistance >1000 h

    As an accredited SHARQ HDPE F1 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SHARQ HDPE F1 is typically supplied in 25 kg bags, palletized and stretch-wrapped, with optional 1,000 kg jumbo bags.
    Container Loading (20′ FCL) SHARQ HDPE F1 in 25kg bags, palletized and loaded into a 20-foot FCL container, securely stowed and sealed for export.
    Shipping SHARQ HDPE F1 is a non-hazardous high-density polyethylene resin shipped as solid pellets in 25 kg bags, jumbo bags, or bulk containers. It requires no dangerous goods classification. Store in a cool, dry, ventilated area away from ignition sources; protect packaging from moisture and damage during transport.
    Storage Store SHARQ HDPE F1 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep bags or containers tightly closed to prevent moisture and contamination. Avoid prolonged UV exposure and excessive temperatures. Maintain clean handling areas, prevent static buildup, and stack pallets securely. Follow supplier SDS and local regulations.
    Shelf Life SHARQ HDPE F1 typically has a 24-month shelf life if stored cool, dry, and in unopened original packaging, away from sunlight.
    Application of SHARQ HDPE F1

    SHARQ HDPE F1 in vest-style grocery carrier production operates as a high-molecular-weight blown-film resin with a nominal melt flow rate of 0.05 g/10 min at 190°C/2.16 kg (ISO 1133-1:2022) and density 0.948 g/cm³ (ISO 1183-1:2019). The grade is processed on high-stalk monolayer lines with die gap 1.2–1.4 mm, melt temperature 190–210°C, blow-up ratio 3.5:1–4.5:1, and frost-line height 8–10 die diameters. On a 65 mm grooved-feed extruder fitted with a 250 mm spiral-mandrel die, line speed for 12.5 µm vest carriers is typically 70–90 m/min. Dart impact release testing per ASTM D1709-22 Method A commonly uses a 120 g floor at 12.5 µm, though published data for this specific configuration is limited. Tensile yield stress in film is measured per ISO 527-3 and remains in the 20–24 MPa range for the neat grade. Edge trim and off-spec film are shredded and reintroduced at up to 20 wt% without destabilizing the high-stalk bubble. Corona treatment to 38–42 dyn/cm per ASTM D2578 is applied when flexographic printing is specified. Pre-drying is not required; however, when pellets are transferred from cold storage into a production hall above 60% relative humidity, surface condensation can cause feed-throat bridging. Terminal products include vest-style grocery carriers, produce roll bags, and small retail bags.

    Why Does Frost-Line Air Geometry Set the Output Ceiling in Refuse-Sack Coextrusion?

    Three-layer refuse sack lines running HDPE F1 in the core encounter an output limit set by frost-line air geometry rather than screw torque. In a representative 3-layer structure, the core contains 65–75 wt% SHARQ HDPE F1, one skin contains 10–15 wt% LLDPE C6 with density 0.918 g/cm³, and the other skin contains 10–15 wt% clean post-industrial HDPE regrind; the balance is additional HDPE F1 or a color masterbatch. The die gap is 1.6 mm; blow-up ratio is 3.8:1; melt temperature is 195–215°C. Production-scale 75 mm extruders with 30 L/D barrier screws and a 350 mm die sustain 280–320 kg/h when internal bubble cooling and a high-pressure dual-lip air ring hold the frost line at 8–11 die diameters. The HDPE F1 core contributes extensional viscosity and strain hardening; once the frost line rises above the cooling plenum, dart impact per ASTM D1709-22 Method B at 25 µm falls below the 250–350 g specification window used by municipal waste bag buyers. Elmendorf tear per ASTM D1922-23 shows machine-direction values 3.0–4.5 times the transverse-direction values; oscillating haul-off and die rotation are used to redistribute the orientation imbalance. Screen pack pressure increases with regrind gels; when pressure differential exceeds 0.4 MPa across a 200 mesh screen pack, the line is shut for screen changes. Terminal products are star-sealed refuse sacks, drawstring liners, and wheeled-bin liners.

    Dry-food liner film production with HDPE F1 operates in a narrower compliance regime than consumer refuse sacks because the olefin polymer layer must satisfy 21 CFR 177.1520(c) and EU Regulation 10/2011 Annex I Table 1. For cereal liners and bakery insert films at 18–35 µm, converters run the grade as a monolayer at 100% or as the core layer in three-layer coextrusions where the skins may reduce seal initiation. In monolayer cereal liners, blow-up ratio is 4.0:1, die gap is 1.4 mm, melt temperature is held at 190–205°C, and output on a 65 mm extruder is deliberately limited to 200–230 kg/h to reduce gel formation. Seal initiation is the central conversion conflict: HDPE F1 seals 10–15°C higher than LLDPE sealants, so seal-bar setpoints must be mapped with heat seal strength per ASTM F88-21 over 120–170°C at 0.5 s dwell and 0.28 MPa jaw pressure. Hot tack per ASTM F1921-18 is not the primary strength of monolayer HDPE F1; for high-speed form-fill-seal operations, a coextruded LLDPE sealant skin is preferred. Food-contact validation is not inferred from a resin datasheet; converters validate the finished film by overall migration testing under EN 1186-1 and EN 1186-14 with the limit of 10 mg/dm² from EU Regulation 10/2011. Oxygen transmission rate at 25 µm is typically 1,500–2,200 cm³/m²·day·atm per ASTM D3985-24; water vapor transmission rate is in the range of 5–8 g/m²·day at 38°C and 90% RH per ASTM F1249-24. Terminal products include dry-cereal liners, cracker pouches, and bakery film inserts.

    Heavy-Gauge Industrial Sacks and the 5.0:1 Blow-Up Ratio Ceiling

    Heavy-duty industrial sacks made from HDPE F1 are produced at 50–100 µm to carry mineral wool, fertilizers, and polymer powders. The process uses a die gap of 1.8 mm and melt temperature of 200–220°C; blow-up ratio can be increased to 5.0:1, but above this ratio the high-density bubble becomes sensitive to ambient air drafts on non-enclosed film towers. On 90 mm extruders with 400 mm dies, output is typically 350–400 kg/h; internal bubble cooling is required to prevent a re-crystallization front that causes blocking and poor flatness. The film is evaluated for tear strength per ISO 6383-2 and dart impact per ISO 7765-1 or ASTM D1709-22 Method B, because terminal sacks must survive sharp edges from insulation batts and granular products. A critical conflict is additive carryover: clean indoor regrind may be added at 20–30 wt%, but when the regrind contains printing ink, gel counts increase and screen pressure rises above 0.35 MPa, reducing line uptime. The finished sacks are typically taped or stitched; heat sealing is less common at this gauge because HDPE F1 seal strength at thicknesses above 50 µm is more difficult to stabilize across the seal bar.

    When 50% Post-Consumer Recyclate Is Blended with HDPE F1 for Municipal Liner Production

    Municipal liner lines incorporating 50 wt% post-consumer HDPE recyclate use HDPE F1 as the melt-strength restorer and gel diluent. PCR from rigid containers typically has density 0.955–0.965 g/cm³ and melt flow rate 0.4–1.0 g/10 min (ISO 1133-1:2022). Blending at 50:50 narrows the processing window to melt temperature 185–205°C, blow-up ratio 3.0:1–3.5:1, and die gap 1.8–2.0 mm. Production records on 75 mm lines indicate that gel-related screen pack changes become necessary at pressure differentials above 0.45 MPa; line output is reduced by 20–30% relative to virgin HDPE F1. The resulting 18–25 µm film must still pass municipal refusal sack tests, including dart impact per ASTM D1709-22 Method B and tear per ASTM D1922-23, although the specification floor is frequently lowered to 180–220 g at 25 µm for PCR-rich products. Residual PP contamination from bottle caps forms unmelted inclusions that act as stress raisers; converters observe a sharp decline in tear resistance when PP content exceeds 3 wt% of the regrind fraction. Published data for this specific configuration is limited, so converters must verify gel level and bubble stability on their own equipment. Terminal products include low-carbon municipal bag programs and commercial waste liners.

    Comparative process-window matrix for HDPE F1 blown-film applications
    ApplicationExtruder / dieDie gap (mm)Blow-up ratioMelt temperature (°C)Output or line speedFilm gauge (µm)
    Retail vest carriers65 mm / 250 mm1.2–1.43.5:1–4.5:1190–21070–90 m/min9–15
    Refuse-sack coextrusion75 mm / 350 mm1.63.8:1195–215280–320 kg/h20–25
    Dry-food liner65 mm / 250 mm1.44.0:1190–205200–230 kg/h18–35
    Heavy-gauge industrial sacks90 mm / 400 mm1.8up to 5.0:1200–220350–400 kg/h50–100
    PCR municipal liner75 mm / 350 mm1.8–2.03.0:1–3.5:1185–20520–30% below virgin line rate18–25
    Compliance and test-method matrix for HDPE F1 downstream film applications
    InterfaceStandard or regulationKey parameter
    Food-contact resinFDA 21 CFR 177.1520(c)Olefin polymer for contact with dry and aqueous foods under specified conditions
    EU food contactEU Regulation 10/2011 Annex I Table 1Overall migration limit 10 mg/dm²
    Migration testEN 1186-1 and EN 1186-14Overall migration into food simulants
    REACHRegulation (EC) No 1907/2006 Article 33SVHC communication at 0.1% w/w
    Melt flow rateISO 1133-1:2022190°C / 2.16 kg
    DensityISO 1183-1:20190.948 g/cm³ nominal
    Dart impactASTM D1709-22 Method A/BGauge-specific release value
    Elmendorf tearASTM D1922-23 or ISO 6383-2MD/TD ratio and absolute tear
    Tensile filmISO 527-3 or ASTM D882-22Yield stress and elongation at break
    Heat seal strengthASTM F88-21Seal-bar temperature profile
    Oxygen transmissionASTM D3985-24cm³/m²·day·atm
    Water vapor transmissionASTM F1249-24g/m²·day at 38°C, 90% RH

    Cast film and extrusion coating are outside the intended processing window for SHARQ HDPE F1; the high molecular weight produces head pressure above 0.4 MPa and melt fracture at die shear rates above 200 s⁻¹ on small-diameter dies, and published data for cast-film use is limited. Drawstring household refuse liners in non-PCR markets are a shallow process zone: 100% SHARQ HDPE F1 at a 1.5 mm die gap and 4.0:1 blow-up ratio requires no additional down-gauging limits beyond those already specified for retail carrier films.

    Free Quote

    Competitive SHARQ HDPE F1 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SHARQ HDPE F1 is a high molecular weight, high-density polyethylene blown film extrusion resin supplied by Eastern Petrochemical Company (SHARQ). The grade is delivered as natural white pellets with a typical density of 0.952 g/cm³ under ISO 1183-1:2019 and a melt flow rate of 0.05 g/10 min at 190°C and 2.16 kg under ISO 1133-1:2022. Batch-to-batch variance for density is typically controlled within ±0.001 g/cm³ and melt flow rate within ±0.01 g/10 min on the certificate of analysis. The base polymer is compounded with a phenolic/phosphite antioxidant package and an acid scavenger; slip and anti-block agents are not typically included in the base resin and must be added by masterbatch according to the end-use requirement. The grade designation F1 identifies a blown film extrusion product and is not interchangeable with SHARQ injection moulding, blow moulding, or pipe grades. Intended applications include thin-gauge retail carrier bags, T-shirt bags, produce bags, frozen food packaging, coextruded films, and industrial liners. The broad bimodal molecular weight distribution is the primary difference from conventional unimodal HDPE film grades of equivalent density and is responsible for higher bubble stability, higher dart impact resistance, and increased melt pressure during extrusion.

    What Melt Rheology Governs Blown Film Stability at Thin Gauge?

    At 190°C, the melt flow rate of 0.05 g/10 min places SHARQ HDPE F1 in the fractional-melt polyethylene class. The high-load melt flow rate at 21.6 kg typically ranges from 8 g/10 min to 12 g/10 min, giving a flow rate ratio above 160. Flow rate ratio is a process marker for molecular weight distribution; higher ratios indicate strong shear thinning and elevated melt strength. The shear-thinning response permits commercial output in grooved feed extruders but limits use in cast film lines and extrusion coating dies that require lower viscosity. At 100 s⁻¹ and 190°C, the apparent shear viscosity of HMW-HDPE film grades in this class typically falls between 2,000 Pa·s and 3,500 Pa·s.

    On a 60 mm grooved feed extruder with 25:1 L/D, start-up below 40 rpm is recommended because the high-viscosity melt can generate breaker plate pressures above 450 bar once screw speed exceeds 85 rpm. Barrel temperature set points should be increased gradually from 170°C at the feed section to 200–210°C at the metering zone. The processing window is narrow: melt temperatures below 190°C raise melt pressure and create poor homogenization, while sustained melt temperatures above 230°C increase oxidation risk despite the stabilization package, causing gel formation and film specks. The apparent shear rate at the die lip for a 1.5 mm die gap and 100 kg/h output through a 200 mm die is estimated at 150 s⁻¹ to 250 s⁻¹; within this pseudo-plastic region, melt fracture is generally avoidable if die temperature remains above 200°C. A layered screen pack of 20/40/60 mesh is common; pressure increase across the pack should not exceed 80 bar at nominal output. If unmitigated melt fracture appears as regular surface roughness below 0.5 µm amplitude, the first response is to raise die temperature by 5°C to 10°C, not to increase screw speed. Oxidation induction time at 210°C under ISO 11357-6:2018 is typically above 20 min for stabilized HMW-HDPE film grades in this class; extruder residence times above 30 min should be avoided during colour or material changeovers.

    Addition of fluoropolymer polymer processing aid at 300 ppm to 600 ppm is permitted to reduce melt fracture and die lip build-up. Calcium carbonate anti-block masterbatch at 2,000 ppm to 5,000 ppm raises density and haze while reducing dart impact; addition rates above 8 wt% are generally incompatible with thin-gauge film performance under ASTM D1709. Erucamide or oleamide slip concentrate should be limited to 500 ppm to 1,500 ppm to minimize uncontrolled surface migration during storage. Amine-based antistatic additives are not recommended because they can accelerate oxidative degradation of polyethylene at high processing temperatures. Pre-drying is not required under normal warehouse conditions; if pellet surface moisture exceeds 0.05 wt%, drying at 60°C for 2 h in a desiccant hopper is sufficient. Long-term storage above 40°C or prolonged exposure to direct sunlight can shorten additive protection. The pellet bulk density is approximately 0.55 g/cm³; surface condensation on pellets at relative humidity above 70% can produce feed throat bridging and should be controlled by hopper dryers or dry-air sweeps.

    Published data for the exact additive package and film property values of SHARQ HDPE F1 are limited to supplier technical bulletins; the table presents representative values for the grade class and requires line-specific verification.

    Typical blown film property profile for SHARQ HDPE F1 at 25 µm gauge and 4:1 blow-up ratio
    Property Test method Typical value
    Density ISO 1183-1:2019 0.952 g/cm³
    Melt flow rate, 190°C/2.16 kg ISO 1133-1:2022 0.05 g/10 min
    High-load melt flow rate, 190°C/21.6 kg ISO 1133-1:2022 8–12 g/10 min
    Tensile yield strength, MD/TD ISO 527-3:2018 28/26 MPa
    Elongation at break, MD/TD ISO 527-3:2018 650/600%
    Dart impact F50, 25 µm film ASTM D1709-16a 170 g
    Elmendorf tear, MD/TD, 25 µm film ASTM D1922-15 20–40 / 200–400 g/25 µm
    Water vapor transmission rate, 25 µm, 38°C, 90% RH ASTM F1249-20 5.5 g/m²/day

    When a Unimodal Film Grade Is Replaced by SHARQ HDPE F1

    Published data for line-converted output on SHARQ HDPE F1 are limited; industrial experience with bimodal HMW-HDPE film grades indicates that conversion from a 0.951 g/cm³ unimodal resin raises melt pressure by 15% to 25% and motor load by 8% to 12% at equivalent screw speed. The bubble, however, remains stable at 18 µm gauge, where equivalent-density unimodal resins may show thinning and collapse. The replacement is not direct for cast film lines because the melt viscosity at 100 s⁻¹ is outside the cast process window; cast film and extrusion coating require grades with melt flow rates above 2 g/10 min.

    Compared with an LLDPE-rich film blend, SHARQ HDPE F1 exhibits higher film modulus and lower elongation at break. Machine-direction Elmendorf tear for SHARQ HDPE F1 is typically lower than that of LLDPE-rich blends, while transverse-direction tear is higher than equivalent-density unimodal HDPE. Unlike SHARQ injection moulding grades with MFR above 4 g/10 min, SHARQ HDPE F1 has insufficient flow for thin-wall injection moulding. The absence of slip and anti-block in the base resin distinguishes it from some cast film grades that include primary amides; this allows the converter to tailor additive packages for food contact or high-clarity end uses. Where the specification is dominated by moisture vapor transmission resistance and stiffness rather than extensibility or puncture, SHARQ HDPE F1 may be selected over a high-flow LLDPE grade; the trade-off is lower machine-direction tear and lower dart impact under ASTM D1709.

    In blown film lines running SHARQ HDPE F1, the die gap is typically set between 1.2 mm and 1.8 mm. Die gaps below 1.0 mm can elevate die entrance pressure and cause melt fracture at high output rates. Blow-up ratio is commonly maintained at 3:1 to 5:1; a higher ratio improves transverse strength but reduces bubble stability if the stalk is too short. The frost line height should be controlled between 6 and 9 die diameters. When the frost line height exceeds 11 die diameters, molecular orientation in the machine direction reduces Elmendorf tear strength under ASTM D1922-15. Chilled air at 5°C to 15°C is used to maintain quench; air temperatures below 5°C can cause sheet condensation and blocking. For a 70 mm extruder with 30:1 L/D and a 200 mm die, nominal output for thin-gauge film is typically 80 kg/h to 110 kg/h; the limiting factor is bubble oscillation above 100 kg/h unless a high-stalk air ring and internal bubble stabilizer are used.

    Compliance Status Under FDA 21 CFR and EU No 10/2011

    The base resin is supplied with regulatory documentation for food contact applications. No perfluoroalkyl substances are intentionally added to SHARQ HDPE F1. The food-contact status applies only to the base resin; masterbatch additions may change the regulatory profile of the finished package. Compliance of the finished article remains the responsibility of the converter because final thickness, migration, and lamination conditions govern end-use suitability.

    Principal compliance references for SHARQ HDPE F1 base resin
    Regulation or standard Scope Status
    FDA 21 CFR 177.1520 Olefin polymers for food contact Supplier food contact statement required; conditions of use to be validated for the finished film
    EU No 10/2011 Plastic materials and articles intended for food contact Overall migration limit 10 mg/dm²; migration testing required on finished article per Annex I and Annex V
    REACH No 1907/2006 Registration, evaluation, authorisation, restriction of chemicals No intentionally added SVHC above 0.1% w/w
    RoHS 2011/65/EU Restriction of hazardous substances in EEE Pb, Cd, Hg, Cr(VI), PBB, PBDE below 0.1% or 0.01% as applicable

    Production line data from a HMW-HDPE film line producing 12 µm retail carrier bags on a 70 mm grooved feed extruder with 30:1 L/D indicate that bubble stability, rather than screw torque, is the primary output limitation once the frost line height is increased beyond 10 die diameters. At melt temperature 205°C and die gap 1.5 mm, stable operation at 95 kg/h was maintained with an air ring chilled to 10°C. The film exhibited a dart impact F50 of 150 g under ASTM D1709-16a. In industrial liners of 60 µm to 80 µm, the difference from unimodal grades is less visible in output but the higher melt strength reduces draw resonance at high take-off speeds. Changeover from a lower-viscosity resin to SHARQ HDPE F1 requires purging with a fractional-melt HDPE purge compound at 190–210°C. Direct transition from LLDPE can leave unmelted LLDPE domains that appear as clear streaks in the film; a minimum of 2 h purge with the same or higher-viscosity purging resin is recommended. For frozen food packaging, the seal initiation temperature for HDPE of this density class is generally 123°C to 128°C, and sealed performance is improved by coextruding an LLDPE sealant layer because HDPE seal strength is reduced by orientation and thickness variation in the seal area. The grade is not recommended for injection moulding, pipe extrusion, or blow moulding because the molecular weight is too high for those processes; use SHARQ HDPE F1 only for blown film applications where high melt strength and downgauging capability are required.