| HS Code | 362583 |
| Polymertype | High Density Polyethylene (HDPE) |
| Form | Pellets |
| Color | Natural |
| Processingmethod | Injection Molding |
| Meltflowrate | 8.0 g/10 min (190°C/2.16 kg) |
| Density | 0.960 g/cm³ |
| Tensilestrengthatyield | 30 MPa |
| Elongationatbreak | 600% |
| Flexuralmodulus | 1200 MPa |
| Izodnotchedimpactstrength | 40 kJ/m² |
| Vicatsofteningtemperature | 125°C |
| Heatdeflectiontemperature | 70°C |
| Meltingpoint | 130-137°C |
| Hardnessshored | 65 |
| Moldshrinkage | 1.5-3.0% |
| Waterabsorption | <0.01% |
| Dielectricconstant | 2.3 |
| Volumeresistivity | >10^16 Ω·cm |
| Dielectricstrength | >20 kV/mm |
As an accredited Shanxi PCEC HDPE HDMD-8007 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaging: Shanxi PCEC HDPE HDMD-8007 comes in 25 kg polyethylene-lined woven bags, stacked and palletized for industrial delivery. |
| Container Loading (20′ FCL) | 20′ FCL loading: Shanxi PCEC HDPE HDMD-8007 in 25 kg bags, palletized or loose, about 20–25 MT per container. |
| Shipping | Shanxi PCEC HDPE HDMD-8007 is shipped as non-hazardous high-density polyethylene pellets in 25 kg woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers/trucks; keep away from moisture, direct sunlight, heat, and contamination. Store in a ventilated, dry area. Not classified as dangerous goods for transport. |
| Storage | Store Shanxi PCEC HDPE HDMD-8007 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags sealed, palletized, off the floor, and protected from moisture, dust, and contamination. Maintain ambient temperature, avoid excessive stacking, use FIFO stock rotation, and prevent prolonged UV exposure. Store separately from incompatible materials. |
| Shelf Life | Shanxi PCEC HDPE HDMD-8007 has a 12-month shelf life when stored in original packaging, cool, dry, and away from direct sunlight. |
In monolayer extrusion blow moulding of high-density polyethylene milk and edible oil containers, Shanxi PCEC HDPE HDMD-8007 is processed at melt temperatures of 180 °C to 220 °C. Food-contact suitability is confirmed by supplier certification against FDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011 Annex I Table 1, and GB 4806.6-2016. A production formulation contains 98.0–99.5 wt% HDMD-8007, 0.5–2.0 wt% titanium dioxide masterbatch, and 0.05–0.15 wt% processing antioxidant. The TiO₂ loading is set by light transmission requirements for UHT milk. Loading above 2.5 wt% can lower parison melt strength and increase die lip build-up on shuttle machines. Die gap is held between 1.5 mm and 2.5 mm. Blow air pressure is held between 0.6 MPa and 0.9 MPa. Mould cooling water is held at 8–15 °C. On a single-station shuttle blow moulder with a 24:1 to 30:1 L/D barrier screw, 1 L bottle cycle times of 12–18 s are typical. The resulting containers include 500 mL to 5 L pasteurized milk, UHT milk, and edible oil bottles. Drop impact resistance after filling is evaluated using ASTM D2463-23. Environmental stress crack resistance of the finished container is evaluated by ASTM D1693-15 Condition B. Off-taste risk is controlled by limiting melt residence time below 5 min and by purging with a purging compound after every 72 h of continuous extrusion. Published data for this specific grade under high-speed rotary wheel dairy lines is limited.
For 10–30 L jerry cans used in dangerous goods transport, HDMD-8007 is processed on accumulator-head extrusion blow moulding machines with shot capacities of 1–3 kg. The moulding formula normally contains 70–80 wt% virgin HDMD-8007, 20–30 wt% dry, dust-free in-house regrind from pinch-off waste, and 1.0–2.0 wt% carbon black masterbatch where UV stabilization is required. Regrind above 30 wt% is not recommended because repeated shear reduces the high-molecular-weight fraction. This reduction lowers parison hang strength and can create micro-voids at pinch-off weld lines. The parison is programmed across 10–30 angular positions to achieve wall thickness distribution of 1.8–2.8 mm in chime and sidewall regions. Melt temperatures are set at 170–210 °C from feed throat to die head. Blow air pressure is 0.7–1.0 MPa. Mould clamps are set at 80–150 t for 25 L closed-head drums. Compliance requires performance testing under UN Model Regulations Chapter 6.1.5.3 drop test, 6.1.5.4 leakproofness, and 6.1.5.5 hydraulic internal pressure. Finished containers are classified as UN 1H2/Y with design type approval. End products include jerricans for lubricants, pesticides, surfactants, and industrial solvents. Published data for this specific configuration is limited for stacking performance beyond 6 high at 40 °C.
| Segment | Standard | Test method | Critical control |
|---|---|---|---|
| Dairy and edible oil bottles | FDA 21 CFR 177.1520(c); EU 10/2011; GB 4806.6-2016 | ASTM D2463-23; ASTM D1693-15 B | Melt residence time below 5 min |
| UN jerricans | UN Model Regulations 6.1.5.3/6.1.5.4/6.1.5.5 | Drop, leakproofness, hydraulic pressure | Regrind ≤30 wt% |
| Detergent and bleach bottles | EU 94/62/EC Annex II; REACH Article 33 | ASTM D256-23; ISO 16770:2004 | Active chlorine above 10% at 40 °C requires fluorination |
| Automotive reservoirs | ISO 527-2:2012; ISO 179-1:2010; ISO 16770:2004 | Charpy impact at -30 °C; burst cycling | Continuous service temperature ≤80 °C |
| Pharmaceutical containers | Ph. Eur. 3.1.3; USP 661.1; FDA 21 CFR 177.1520(c) | Extractables; biological reactivity | No regrind permitted |
Monolayer extrusion blow moulding of 500 mL to 5 L detergent and disinfectant containers places sustained environmental stress crack resistance on HDMD-8007. Package compatibility is verified by storage contact tests at 40 °C for 7 days. Regulatory compliance for the package is assessed under EU Packaging and Packaging Waste Directive 94/62/EC Annex II and REACH Regulation (EC) No 1907/2006 Article 33 communication obligations. Mechanical acceptance includes ASTM D256-23 Izod notched impact and ISO 16770:2004 slow crack growth. A production formula contains 97.0–99.0 wt% HDMD-8007, 0.1–0.3 wt% hindered phenolic antioxidant, 0.05–0.15 wt% phosphite stabilizer, and 1.0–2.5 wt% color masterbatch. Processing is performed on continuous shuttle or rotary wheel blow moulders with 24:1 to 30:1 L/D screws. Melt temperature is set at 180–215 °C. Mould cooling water is held at 8–15 °C. Blow pressure is held at 0.6–0.9 MPa. For sodium hypochlorite bleach above 10% active chlorine stored above 40 °C, stress crack failure can occur. If such service is intended, fluorination of the inner surface is required. Terminal articles include laundry detergent bottles, bleach bottles, and hard-surface cleaner bottles. Published data for this specific grade with fluorinated barrier is limited.
For automotive windshield washer reservoirs and air ducts, HDMD-8007 is formed by 3D suction blow moulding because fixed parison tooling cannot place a closed-loop parison around multiple axes without excessive pinch-off seams. The resin is processed at 190–230 °C melt temperature. A typical formula is 97.5–99.0 wt% HDMD-8007, 1.0–2.0 wt% carbon black masterbatch, and 0.1–0.3 wt% heat stabilizer masterbatch. Mechanical acceptance is judged by ISO 527-2:2012 tensile yield and elongation, ISO 179-1:2010 Charpy notched impact at -30 °C, and ISO 16770:2004 slow crack growth. Vibration and burst tests are performed on finished reservoirs with internal pressure cycling of 0.05–0.15 MPa. The process uses a suction blow moulding machine with parison wall thickness programmed across 20–40 points. Mould cooling water is held at 10–25 °C. Terminal components include 3–8 L washer reservoirs and HVAC ducts. The resin should not be specified for continuous under-hood service above 80 °C or direct contact with brake fluid, which can cause environmental stress cracking. Published data for this specific grade under long-term coolant exposure is limited.
In primary pharmaceutical packaging, HDMD-8007 is processed by extrusion blow moulding into 50–500 mL tablet bottles and cosmetic jars. Compliance with Ph. Eur. 3.1.3 requires extractable tests for heavy metals, sulfated ash, and reducing substances. USP 661.1 plastic materials of construction and FDA 21 CFR 177.1520(c) are applied for oral solid dose containers. The manufacturing formula is 98.5–99.5 wt% HDMD-8007 and 0.5–1.5 wt% pharma-grade titanium dioxide or white masterbatch. No recycled material is permitted. Process conditions include melt temperature 175–205 °C, validated autoclave or ethylene oxide sterilization compatibility, and continuous ionized air cleaning to keep particulate counts below ISO 14644-1 Class 8 in the blow moulding enclosure. Die lip purge intervals are shortened to 24 h to prevent degraded gel formation. Cooling water is held at 8–12 °C. Terminal articles include desiccant-capped tablet bottles, ophthalmic ointment jars, and cosmetic cream pots. Extractable testing follows Ph. Eur. 3.1.3 and USP 661.1 biological reactivity procedures. Published data for this specific grade under terminal gamma sterilization is limited.
Competitive Shanxi PCEC HDPE HDMD-8007 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Shanxi PCEC HDPE HDMD-8007 is a high-density polyethylene blow-moulding resin supplied as a pelletized copolymer for rigid containers, large-volume industrial packaging, and multilayer barrier structures. The material occupies the low-melt-flow-rate segment of high-density polyethylene, with nominal density controlled between 0.955 g/cm³ and 0.959 g/cm³ and melt flow rate controlled between 0.7 g/10 min and 0.9 g/10 min under ASTM D1238-20 at 190 °C and 2.16 kg. Because published data for this specific configuration is limited, the property envelope in this document is representative of the product class and must be confirmed against the supplier certificate of analysis. These coordinates distinguish the grade from high-flow injection-moulding HDPE, which commonly operates above 20 g/10 min, and from high-molecular-weight film resins with melt flow rates below 0.2 g/10 min. The primary conversion route is extrusion blow moulding, in which parison melt strength, die-swell consistency, environmental stress-crack resistance, and sub-ambient impact toughness determine process capability.
| Property | Method | Typical control range |
|---|---|---|
| Melt flow rate | ASTM D1238-20, ISO 1133-1:2022 | 0.7 g/10 min–0.9 g/10 min |
| Density | ASTM D792-20, ISO 1183-1:2019 | 0.955 g/cm³–0.959 g/cm³ |
| Tensile stress at yield | ASTM D638-22, ISO 527-2:2012 | 25 MPa–29 MPa |
| Elongation at break | ASTM D638-22 | > 600 % |
| Flexural modulus | ASTM D790-17, ISO 178:2019 | 1,000 MPa–1,200 MPa |
| Environmental stress-crack resistance | ASTM D1693-15, Condition B, 100 % Igepal | F50 > 600 h |
| Notched Izod impact, 23 °C | ASTM D256-10e1 | 8 kJ/m²–12 kJ/m² |
| Vicat softening temperature, A50 | ASTM D1525-17e1 | 125 °C–129 °C |
| Water content | ISO 15512:2019 | < 0.05 % |
The melt flow rate is measured by extrusion plastometer under ASTM D1238-20 or ISO 1133-1:2022. The value is a single-point shear-viscosity indicator: the resin is extruded through a standardized die with diameter 2.095 mm and length 8.000 mm under a piston load of 2.16 kg at 190 °C. A low value in this class is a direct marker of high melt strength and low gravity-driven drawdown. Lot-to-lot variation in melt flow rate is more sensitive to changes in the high-molecular-weight tail than to average molecular weight alone; a shift from 0.70 g/10 min to 0.85 g/10 min can require adjustment of die gap or parison programming, even though both values remain within specification. Capillary viscosity at 190 °C and an apparent shear rate of 100 s⁻¹ is typically in the range 4,000 Pa·s to 6,000 Pa·s for HDPE grades in this melt-flow band. Oscillatory shear rheology under ISO 6721-10:2021 at 190 °C and 1 rad/s can be used to assess melt elasticity; a batch with a higher high-molecular-weight tail shows lower loss tangent and improved parison hang time.
Accumulator-head extrusion blow moulding is the standard conversion route for HDMD-8007. Production-scale equipment for 200 L drums typically comprises a grooved-feed single-screw extruder with 25:1 to 30:1 length-to-diameter ratio, a barrier screw with a compression ratio of 2.8:1, a screen pack of 40/60/80 mesh, and an accumulator head with a shot capacity between 10 kg and 30 kg. Clamp force for single-cavity drum tools is typically 400 t to 600 t; smaller 20 L containers are produced on shuttle presses of 60 t to 120 t clamp force. Blow pressure is maintained at 0.6 MPa to 1.0 MPa, and mould cooling water is held at 10 °C to 20 °C to reduce warpage at the pinch-off weld line.
Barrel temperature profile from hopper to adapter is commonly set at 180 °C, 190 °C, 200 °C, 205 °C, and 210 °C; melt temperature measured at the die entrance should not exceed 220 °C during continuous operation. If the melt temperature remains above 230 °C for more than 15 min, thermal-oxidative degradation reduces the high-molecular-weight tail and increases melt index drift, which manifests as parison sag and loss of top-load performance. The die gap is set between 1.5 mm and 4.0 mm depending on container mass, with die swell in the range 25 % to 50 %. Accumulator-head machines require parison programming with 20 to 100 points to compensate for wall-thickness variation in the chime and handle regions of tight-head drums.
On a 90 mm extruder, screw speeds of 40 rpm to 60 rpm typically yield outputs of 180 kg/h to 250 kg/h. Higher speeds above 70 rpm may generate melt-pressure spikes above 320 bar and shear heating beyond the thermal window. At 200 L scale, cooling time of 120 s to 180 s per cycle is typical; shorter cooling times produce post-mould shrinkage and dimensional instability in the closure neck. Pre-drying at 80 °C for 2 h is generally unnecessary unless surface moisture exceeds 0.08 % by weight after storage at relative humidity above 60 %. Wet pellets generate splay on the parison surface and increase blow-hole reject rates. The resin should not be blended with amine-based antistatic additives because amine migration can reduce environmental stress-crack resistance and alter food-contact surface properties. For antistatic performance, a non-amine migratory antistat must be selected and validated by surface resistivity measurement under IEC 61340-2-3:2016.
Tooling design must consider the grade's low flowability and high die swell. The parison drop time for a 200 L drum can exceed 10 s; therefore the accumulator head must maintain uniform melt temperature across the annular die, and the die bushing and mandrel must be concentric within 0.02 mm total indicated runout. Any eccentricity greater than this value produces uneven wall thickness that cannot be corrected by parison programming alone. The blow pin for bung openings is mechanically guided; misalignment above 0.1 mm creates weld-line defects that fail drop tests in the chime area. Blow mould tooling uses pinch-off lands with flash clearance of 0.1 mm to 0.3 mm; improper pinch-off geometry creates notch geometry that concentrates stress and lowers environmental stress-crack resistance. Cavity venting is controlled to less than 0.03 mm depth to prevent air entrapment.
Regrind use levels up to 20 % are common for non-food containers, provided the regrind is clean and processed at similar melt temperature. Higher levels increase gel specks and reduce environmental stress-crack resistance; levels above 30 % are generally rejected for UN-certified packagings unless verified by batch drop testing under the applicable design-type test. Gel count measured on 25 cm² of 0.2 mm sheet is typically controlled below 20 gels larger than 0.5 mm for high-integrity surfaces. The molecular architecture in this density band is typically bimodal, with a low-molecular-weight fraction that reduces melt viscosity and a high-molecular-weight fraction that increases chain entanglement and parison melt strength. A measurable reduction in melt flow rate ratio indicates loss of the high-molecular-weight component from shear degradation or contaminated regrind and requires immediate verification of the lot before use in large packagings.
Environmental stress-crack resistance is the controlling long-term property for rigid packaging that contains surfactants, agricultural adjuvants, oxidizer solutions, or hydrocarbon-modified liquids. The test uses a bent strip specimen with a controlled notch, immersed in 100 % Igepal CO-630 at 50 °C under ASTM D1693-15, Condition B. The failure time at which 50 % of specimens crack is specified above 600 h for this product class; some certificates of analysis report F50 values above 1,000 h when comonomer distribution and cooling rate are optimized. This performance level is required for United Nations certified intermediate bulk containers and large packagings subjected to stack loading and drop impact sequences.
The combination of high molecular weight and moderate density near 0.957 g/cm³ balances environmental stress-crack resistance against stiffness. Lowering density further would improve crack resistance but reduce container top-load strength; increasing density above 0.960 g/cm³ would stiffen the wall but sharply reduce crack resistance. Notched Izod impact at 23 °C for the density band is typically 8 kJ/m² to 12 kJ/m²; at -40 °C the value declines, and blow-moulded parts must be drop-tested according to ASTM D2463-15 or the relevant UN drop test rather than relying solely on notched specimen data. Chemical compatibility boundaries include continuous contact with strong oxidizing acids above 10 % concentration at temperatures above 40 °C, aromatic hydrocarbons, and chlorinated solvents, which can cause swelling, environmental stress cracking, or oxidative chain scission.
The material is not recommended for pressure-rated pipe classified under ISO 9080-1:2022, because no minimum required strength value is declared for this grade. For fuel tank structures, direct coextrusion with EVOH requires a tie resin; without a maleic anhydride grafted polyethylene adhesive layer, interlayer peeling occurs in adhesion tests such as ASTM D1876. Acceptance testing of incoming lots should include melt flow rate, density, environmental stress-crack resistance, and gel count; a lot with ESCR below 600 h or water content above 0.05 % is not suitable for UN-certified packagings without further treatment. The resin should be stored in unopened, sealed packaging at temperatures below 40 °C and protected from ultraviolet exposure; outdoor storage should be limited because progressive photo-oxidation reduces molecular weight and crack resistance, a defect that is not reversed by drying or remelting.
Regulatory status for rigid packaging is distinct from resin certification. The following reference framework applies to HDPE blow-moulded containers; supplier declarations and end-use testing are required for food-contact and dangerous-goods applications.
| Regulatory area | Reference document | Key test or limit |
|---|---|---|
| Food-contact resin in the United States | 21 CFR 177.1520 | Olefin polymer extraction and end-use migration testing |
| Food-contact plastics in the European Union | Regulation (EU) No 10/2011 | Overall migration ≤ 10 mg/dm²; specific migration limits for authorized additives |
| European chemical registration | REACH (EC) No 1907/2006 | SVHC declaration at 0.1 % weight by weight per article |
| Restriction of hazardous substances | RoHS Directive 2011/65/EU, Annex II | Pb ≤ 0.1 %; Hg ≤ 0.1 %; Cd ≤ 0.01 %; Cr(VI) ≤ 0.1 % in homogeneous material |
| Dangerous goods packaging | UN Model Regulations, Chapter 6.1 | Hydraulic pressure, drop, and stack tests on design type |
Food-contact status is not automatic from the resin specification alone; a supplier compliance statement under 21 CFR 177.1520 and Regulation (EU) No 10/2011 must cover the specific lot, additive package, and processing temperature. Extractables testing of the blow-moulded article, rather than the pellet, is required because degradation products generated during extrusion and trimming can migrate into the packaged medium. For pharmaceutical containers, compendial testing under USP <661.1> is applied to the formed article; the use of recycled or reprocessed material is controlled under the applicable pharmacopoeia and regional packaging regulations.
Differences from adjacent polyethylene grades are defined by melt-flow rate, density, molecular-weight distribution, and long-term mechanical classification. Injection-moulding HDPE with melt flow rates above 20 g/10 min has lower viscosity but also lower environmental stress-crack resistance and melt strength; it is unsuitable for large parison blow moulding but can fill thin-wall closures and crates. Unimodal blow-moulding HDPE of similar density often has a narrower molecular-weight distribution, which reduces die swell and parison melt strength; it is more suitable for small bottles but not for long parisons on large accumulator machines. Narrow-MWD resins can run at lower melt temperature and higher screw speed without excessive pressure, but their processing window narrows when parison length exceeds 1.5 m. Film-grade HDPE with melt flow rates below 0.2 g/10 min and density near 0.950 g/cm³ is designed for downgauged film tear and dart-drop performance; its melt strength is too high for conventional blow-moulding throughput and can overload the extruder drive. Pipe-grade HDPE classified as PE100 under ISO 9080-1:2022 has long-term hydrostatic strength and resistance to slow crack growth that are validated for pressure piping; HDMD-8007 is not assigned an MRS classification and should not be substituted in pressure-rated pipe, fittings, or gas distribution. The practical boundary for HDMD-8007 is therefore the extrusion-blow-moulded rigid container in the 5 L to 200 L range, where the combination of low melt flow rate, moderate density, and high environmental stress-crack resistance provides an operations-compatible balance among parison stability, wall stiffness, and crack resistance.