Shanxi Pcec Hdpe Dmda8907

Shanxi PCEC HDPE DMDA8907

    • Product Name: Shanxi PCEC HDPE DMDA8907
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 340880
    Product Name Shanxi PCEC HDPE DMDA8907
    Manufacturer Shanxi PCEC
    Grade DMDA8907
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.954 g/cm³
    Melt Flow Rate 7.0 g/10 min (190°C/2.16 kg)
    Melting Point 130-135 °C
    Tensile Yield Strength 25 MPa
    Elongation At Break >500%
    Flexural Modulus 1100 MPa
    Vicat Softening Temperature 125 °C
    Hardness 65 Shore D
    Notched Izod Impact Strength 50 J/m
    Water Absorption <0.01%
    Volume Resistivity >10^16 Ω·cm
    Dielectric Constant 2.3
    Processing Method Injection Molding
    Form Pellet
    Color Natural
    Applications Crates, containers, housewares, toys, industrial parts

    As an accredited Shanxi PCEC HDPE DMDA8907 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Shanxi PCEC HDPE DMDA8907 is packaged in 25 kg woven bags with PE liners, stacked on pallets for transport.
    Container Loading (20′ FCL) 1x20′ FCL container loaded with Shanxi PCEC HDPE DMDA8907 in 25 kg bags, palletized and securely stowed for ocean shipment.
    Shipping Shanxi PCEC HDPE DMDA8907 is shipped as a non-hazardous solid resin, typically in 25 kg woven bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks, avoiding moisture, heat, and direct sunlight; standard freight documentation and labeling apply.
    Storage Store Shanxi PCEC HDPE DMDA8907 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags sealed and palletized to prevent moisture, dust, and contamination. Avoid excessive stacking and prolonged UV exposure. Follow first-in, first-out stock rotation. Handle gently to prevent bag damage. Do not store near food, feed, or incompatible materials.
    Shelf Life Shanxi PCEC HDPE DMDA8907 typically has a two-year shelf life when stored sealed, cool, dry, and out of direct sunlight.
    Application of Shanxi PCEC HDPE DMDA8907

    In high-output thin-wall food packaging lines running 2×64 cavity stack molds with valve-gated hot runners and in-mold labelling cells, the base polymer is charged at 100 parts per hundred resin (phr). Titanium dioxide white masterbatch is dry-blended at 2–4 wt%, slip/antiblock concentrates are held between 0.5 wt% and 1.5 wt%, and internally generated regrind is restricted to ≤15 wt% by shot mass. Regrind use above 20 wt% in 0.6–0.8 mm sidewalls is specified against because shot-to-shot viscosity drift increases gate blush and sidewall sink-mark rejects in multicavity production audits. Compliance for U.S.-bound food contact is FDA 21 CFR 177.1520(c) 3.1a, with EU shipments assessed under Regulation (EU) No 10/2011 at overall migration ≤10 mg/dm²; China GB 4806.7-2016 governs domestic distribution. Processing uses melt temperatures of 200–220 °C, mold temperatures of 10–30 °C, injection pressure 80–120 MPa, and cooling times of 6–12 s. The melt flow rate measured at 7 g/10 min under ISO 1133-1:2022 permits long flow-length-to-wall-thickness ratios in high-cavitation layouts. Barrel residence time above 10 min at 240 °C increases gel specks in thin-wall parts. Terminal products include dairy tubs, delicatessen containers, cut-fruit trays, microwaveable trays, and freezer soup containers.

    How Does DMDA8907 Behave in High-Cavitation Closure Molding with Hot-Runner Needle Gates?

    Closure manufacturing with this grade is centred on high-cavitation molds using hot-runner needle gates and unscrewing or collapsible-core tooling on 1,800–2,800 kN toggle presses. The starting formulation is 100 phr DMDA8907, with 1–2 wt% color masterbatch and 0.5–1.5 wt% lubricant/mold-release masterbatch; post-industrial regrind is limited to 10 wt% for press-on and tamper-evident skirts because higher levels are correlated with inconsistent annular seating and torque loss after 48 h of aging. For applications requiring -20 °C drop impact, an EVA-based impact modifier at 2–4 wt% is introduced and notched Izod impact is verified under ISO 180/A. Compliance includes FDA 21 CFR 177.1520(c) 3.1a, EU 10/2011 for food-contact closures, and torque release/opening force characterization under ISO 10143:2019; pharmaceutical closure lots additionally reference USP 661.1 plastic packaging system conditions. Injection processing requires melt temperatures of 210–230 °C, chilled mold temperatures of 10–20 °C, injection pressures of 100–140 MPa, and total cycle times of 8–14 s. Hold pressure must be adjusted to prevent sink opposite the bridge; gate stringing is controlled by individual hot-runner tip profiling rather than blanket temperature reduction. Terminal outputs include 28 mm and 38 mm beverage caps, 24 mm pharmaceutical vial closures, flip-top dispensers, and tamper-evident closures.

    Logistics Crate Molding: Gate Freeze, Regrind Limits, and Stack-Load Performance

    When logistics containers are molded with a target service temperature between -10 °C and 40 °C, the injection process prioritizes gate freeze, tie-bar balancing, and stack-load deformation resistance. The formulation uses 100 phr DMDA8907, 5–15 wt% post-industrial regrind from same-grade rejected crates, 2–3 wt% carbon black masterbatch for UV screening, and 0.3–0.6 wt% HALS stabilizer masterbatch for outdoor storage. Post-consumer recyclate above 20 wt% is not recommended because the low-temperature notched Izod impact under ISO 180/A and the stacking strength under ISO 2234:2012 show measurable deterioration. Molding is performed on 2,000–4,000 kN hydraulic or servo-driven toggle presses with sequential valve-gate control to shift weld lines away from corner radii; melt temperature is held at 220–240 °C, mold temperature 15–25 °C, injection/filling pressure 80–110 MPa, packing pressure 60–80 MPa, and cooling time 20–35 s. Compliance for repeated-use transport packaging includes REACH Annex XVII and producer food-contact declarations when crates are used in direct food transport; mechanical acceptance uses ASTM D638-22 and ISO 178:2019. Terminal product types are nestable logistics crates, bottle crates, fruit and vegetable crates, automotive parts bins, and stackable warehouse totes.

    Processing envelope and primary compliance anchors for DMDA8907 injection segments
    Downstream segmentMelt temperatureMold temperatureInjection/filling pressurePrimary compliance anchor
    Thin-wall food packaging200–220 °C10–30 °C80–120 MPaFDA 21 CFR 177.1520(c) 3.1a
    Caps and closures210–230 °C10–20 °C100–140 MPaISO 10143:2019
    Logistics crates220–240 °C15–25 °C80–110 MPaISO 2234:2012
    Housewares and storage200–230 °C20–40 °C70–100 MPaEU (EU) No 10/2011
    Pails and open-head containers215–235 °C8–15 °C90–130 MPaUN Model Regulations, chapter 6.1
    Thin-wall reels and freezer containers200–230 °C10–20 °C120–150 MPaRoHS Directive 2011/65/EU

    For houseware sidewalls with polished SPI A-1 cavity surfaces and texture depths of 3–8 µm, conventional cold-runner or hot-runner injection cells are used to mask flow lines while maintaining demolding consistency. The recommended dry-blend is 100 phr DMDA8907, 2–6 wt% color masterbatch, 0.2–0.5 wt% antistatic masterbatch where dust pickup is a rejection criterion, and up to 25 wt% in-house regrind. Regrind above 25 wt% reduces high-gloss sidewall consistency and increases splay when surface moisture is above 0.05 wt%. Although HDPE does not require drying, silo transfer in relative humidity above 80% may warrant hopper drying at 70–80 °C for 1–2 h. Melt temperature is set at 200–230 °C, mold temperature 20–40 °C, injection pressure 70–100 MPa, and total cycle time 15–30 s depending on wall sections from 1.2 mm to 3.0 mm. Compliance for food-contact housewares follows FDA 21 CFR 177.1520(c) 3.1a and EU 10/2011; child-use storage articles may additionally require EN 71-3 migration testing and REACH Annex XVII screening. Finished categories include storage bins, drawer organizers, household pails, hangers, waste baskets, and laundry baskets.

    Open-Head Pail and Tamper-Evident Container Molding: Fill Pressure, Drop-Weight, and Stacking Test Limits

    Open-head pails between 1.5 mm and 3.0 mm wall stock place the highest demand on gate-seal pressure and cooling uniformity. The formulation starts at 100 phr DMDA8907, plus 2–4 wt% UV-stabilized color masterbatch and 5–12 wt% same-grade regrind. Where UN certification is required for the carriage of dangerous goods, regrind is capped at 10 wt% and limited to unpigmented or same-batch feedstock to preserve lot-to-lot impact consistency. The injection sequence uses melt temperature 215–235 °C, mold temperature 8–15 °C, injection pressure 90–130 MPa, holding pressure staged from 60 MPa to 40 MPa, and cooling time 10–20 s; total cycle times fall between 20 s and 35 s. Compliance for food-contact pails is evaluated against FDA 21 CFR 177.1520(c) 3.1a and EU 10/2011; UN-certified pails are tested under the applicable provisions of the UN Model Regulations, chapter 6.1, for drop, leakproofness, and stack loading. Terminal products include 1–25 L paint pails, adhesive and coating pails, food-ingredient buckets, and tamper-evident open-head containers.

    When Part Weight Drops Below 4 g and Cycle Time Below 9 Seconds in Freezer-Duty Thin-Wall Reels

    In fast-cycle stack molds running below 9 s, thin-wall reels, spools, and freezer-duty food storage containers push the lower wall thickness boundary to 0.5 mm at part weights under 4 g, requiring melt temperatures of 200–230 °C and accelerated injection speeds on accumulator-equipped machines. The formulation is 100 phr DMDA8907, with 2–4 wt% masterbatch and 0.1–0.3 wt% synthetic silica antiblock to stabilize stacking and denesting; regrind is held at or below 10 wt% because shot-to-shot viscosity rise in fast-cycle stack molds increases short shots and core shift. Compliance for food-contact freezer containers is FDA 21 CFR 177.1520(c) 3.1a, EU 10/2011, and GB 4806.7-2016; technical reels for electrical or electronic service are screened against EU RoHS Directive 2011/65/EU and REACH candidate list obligations. The process envelope includes mold temperature 10–20 °C, injection pressure 120–150 MPa, pack pressure 80–100 MPa, and total cycle time below 9 s, with hot-runner tip temperatures individually profiled to prevent stringing at gate diameters below 0.6 mm. Terminal products include tape hubs, wire spools, textile bobbins, dental floss reels, and freezer storage containers.

    Free Quote

    Competitive Shanxi PCEC HDPE DMDA8907 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Shanxi PCEC HDPE DMDA8907 is a virgin high-density polyethylene resin supplied in pellet form for extrusion blow moulding of industrial hollow articles and thick-wall profiles. The grade is characterized by a nominal solid-state density of 0.957 g/cm³ determined according to ISO 1183-1:2019 and a melt mass-flow rate of 0.7 g/10 min at 190°C under a 5 kg load determined according to ISO 1133-1:2022. The melt index places the material below general-purpose injection moulding HDPE and above high-molecular-weight blow moulding grades, a position that produces a measurable parison hang strength suitable for containers up to approximately 200 L on accumulator-head machines. The resin is not a bimodal pipe-grade polyethylene; its property set is tuned for rigid packaging, industrial tanks, and extruded panels requiring resistance to slow crack growth rather than long-term hydrostatic pressure classification.

    Does DMDA8907 occupy an intermediate rheological position between injection HDPE and high-molecular-weight blow moulding grades?

    The differentiation is visible in the shear-viscosity response. Under ISO 1133-1:2022, injection HDPE grades routinely fall between 8 g/10 min and 20 g/10 min at 190°C/2.16 kg, whereas DMDA8907 is tested at 5 kg to obtain a measurable 0.7 g/10 min value. High-molecular-weight blow moulding grades intended for 1000 L IBCs typically show 5 kg values near 0.25–0.35 g/10 min. This places DMDA8907 in a flow range that allows shorter cycles on shuttle-type blow moulders but reduces maximum parison length before sag failure. Compared with injection grades, DMDA8907 has lower cold-flow and greater environmental stress crack resistance; compared with high-molecular-weight grades, it offers higher output per screw revolution on continuous shuttle lines but requires tighter parison programming for asymmetrical parts.

    The following typical property values are compiled from producer product data and should be confirmed against the batch certificate of analysis. Ranges reflect lot-to-lot variation rather than absolute release limits.

    PropertyTypical valueTest methodCondition
    Melt mass-flow rate0.7 g/10 minISO 1133-1:2022190°C, 5 kg
    Density0.957 g/cm³ISO 1183-1:201923°C as received
    Tensile yield stress25 MPaISO 527-2:2012 Type 1A50 mm/min
    Tensile elongation at break>600%ISO 527-2:2012 Type 1A50 mm/min
    Flexural modulus1000 MPaISO 178:20192 mm/min
    Notched Izod impact>25 kJ/m²ISO 180:2019/A23°C
    Environmental stress crack resistance>200 hASTM D1693-15 Condition B10% Igepal, 50°C
    Vicat softening point124°CISO 306:2013 A5010 N, 50°C/h
    Brittleness temperature<-70°CASTM D746-20impact failure

    Extrusion Blow Moulding Window and Accumulator-Head Parameter Limits

    On a production accumulator-head blow moulding line using a 90 mm extruder with L/D 30:1 and a grooved feed section, the recommended barrel profile is reverse from 185°C at the feed zone to 205°C at the metering zone and 210°C at the head. The critical threshold is die-head melt temperature: sustained operation above 225°C for more than 20 min of residence time initiates localized gel formation and shifts the apparent parison sag rate. If the die gap is narrowed below 0.8 mm on a 120 mm head, shear heating raises melt temperature beyond the set point by 4–8°C, producing visible melt fracture at the parison surface. Blow-pin pressure is typically set between 0.6 MPa and 0.8 MPa, with pre-blow delay adjusted from 0.3 s to 0.8 s based on parison closure. Mould temperature should remain between 15°C and 25°C; higher mould temperatures increase surface gloss but extend cooling time non-linearly.

    Because HDPE is hydrophobic, drying is not required in ambient plant conditions below 70% RH. Condensation on cold pellets can occur when silo storage is below 10°C and plant air is above 80% RH; in that case, surface moisture produces splay and weld-line porosity. Batch drying should be limited to 70°C for 1–2 h in a desiccant hopper dryer with a dew point below -20°C. Overtemperature drying above 90°C causes pellet surface softening and feed-throat clumping.

    Batch-to-batch variation of melt mass-flow rate for this HDPE grade is typically held within ±0.05 g/10 min around the nominal 0.7 g/10 min value. This variation corresponds to detectable changes in parison weight of approximately 0.8–1.2% on a fixed die gap and timer. Accumulator-head machines with axial parison control compensate by adjusting die-gap opening through a 100-point wall-thickness program; without such control, wall thickness at the sidewall of a 200 L drum may vary by ±0.3 mm when regrind ratio changes from 5 wt% to 15 wt%.

    On twin-screw compounding lines used for cleanup or masterbatch let-down, the screw speed is limited to 250 rpm with a side-stuffer feed of 5–10 wt% color masterbatch. Above 300 rpm, viscous heating at the kneading blocks raises melt temperature to 235°C even when barrel set points are 200°C, producing oxidative degradation detectable as a decrease in melt flow stability and brown specks in film inserts. If color change is required, purging with a high-melt-index HDPE or acrylic-based purging compound at 220°C should precede DMDA8907 re-introduction; direct transition from nylon or transparent polycarbonate can cause cross-contamination and delamination in blow-moulded walls.

    For industrial containers in the 30 L to 60 L range, DMDA8907 is run on single-station shuttle machines with clamp force from 150 kN to 350 kN and parison length control based on wall-thickness programming. The typical drop time for a 2.5 kg shot is 2.5–4.0 s at a die temperature of 205°C. Parts moulded under these conditions exhibit minimum wall thickness at the pinch-off of 1.2 mm without cracking when flash removal is performed above 10°C. For tight-head drums of 200 L, the grade is processed on a 120 mm accumulator-head machine with a 6 kg shot, drop time 6–10 s, and blow time 120–180 s. Published data for this specific configuration is limited; the operation must be validated on the target machine because accumulator design and parison die geometry alter drop time by as much as 30%.

    Top-load performance of 60 L open-top containers is tested under ISO 12048:1994 using a compression testing machine with platen speed of 10 mm/min. Acceptance values are set by container design and wall-thickness profile rather than resin alone; however, failures at loads below the design target often trace to insufficient parison programming at the handle pinch-off. Stacking life at 40°C is evaluated by compressive creep testing under ISO 9969:2016 with static load corresponding to a 3 m column of filled containers. Creep rupture below 200 h indicates underblowing, excessive flash thinning, or regrind content above the validated limit.

    The principal differentiation from other HDPE grades is not melt index alone. High-load melt index of 0.7 g/10 min at 5 kg is higher than HMW blow moulding grades such as DMDA-8920-type products, which operate near 0.3 g/10 min, causing DMDA8907 to exhibit shorter parison hang time but lower specific energy input. Conversely, the product is less suitable for injection moulding at high shear rates because its cold flow is slower than injection HDPE grades with MI 6–20 g/10 min. In extruded sheet and profile, DMDA8907 does not carry the PE100 classification of pipe-grade bimodal HDPE; therefore, it is not selected for pressure piping under ISO 9080:2012 hydrostatic strength regression. It fits instead the low-pressure structural container segment where ASTM D1693-15 ESCR and ISO 180:2019 impact toughness are dominant design inputs.

    When the part is intended for food contact, confirmation is required under FDA 21 CFR 177.1520(c) for the specific conditions of use. For European Union applications, overall migration testing under Regulation (EU) No 10/2011 with food simulants 10% ethanol, 3% acetic acid, and vegetable oil is applicable depending on food type. The following matrix summarizes the normative status of the base resin, not processor-specific additives or colourants.

    RequirementStatusStandard or regulationCritical parameter
    Food contactConforms as olefin polymerFDA 21 CFR 177.1520(c)Density of 0.957 g/cm³ meets HDPE identification; extractives limited by end-use condition
    EU food contactBase resin may be usedRegulation (EU) No 10/2011Overall migration <10 mg/dm²
    Heavy metalsConforms to generic plastic limitsDirective 2011/65/EU Annex IIPb <1000 mg/kg, Cd <100 mg/kg, Hg <1000 mg/kg, Cr(VI) <1000 mg/kg
    SVHCNo SVHC intentionally addedREACH Regulation (EC) No 1907/2006Candidate list declaration per batch
    China food contactTest before useGB 4806.7-2023Overall migration and consumption limits per simulant

    When Ultraviolet Exposure and Chemical Contact Govern Additive Selection

    When outdoor service is required, DMDA8907 should be specified with a UV-stabilized masterbatch containing carbon black at 2.0–2.5 wt% and a particle size below 30 nm; otherwise, unmodified HDPE embrittles after approximately 12–18 months of continuous UV exposure in temperate climates. The test method for UV aging is ISO 4892-2:2013 UVA-340, with chalking and tensile elongation retention measured by ISO 527-2:2012. In chemical containment, the resin exhibits acceptable ESCR in 10% Igepal under ASTM D1693-15, but the grade is not suitable for contact with strong oxidizing acids or aromatic solvents at temperatures above 40°C; such service can reduce ESCR F50 by an order of magnitude. No post-consumer regrind should exceed 15 wt% of the extrusion charge unless the blend is requalified under ISO 180:2019 at -20°C; higher addition levels of uncontrolled regrind can create gels and lower pinch-off impact strength. For batch-specific compliance, the producer’s certificate of analysis and migration test report remain the controlling documents.

    Top