| HS Code | 165177 |
| Product Name | Shanxi PCEC HDPE DMDA8007 |
| Manufacturer | Shanxi PCEC |
| Grade | DMDA8007 |
| Polymer Type | High-density polyethylene |
| Density | 0.956 g/cm³ |
| Melt Flow Rate | 7.0 g/10 min |
| Tensile Strength At Yield | ≥25 MPa |
| Elongation At Break | ≥500% |
| Flexural Modulus | ≥1000 MPa |
| Vicat Softening Temperature | ≥120 °C |
| Brittleness Temperature | ≤-70 °C |
| Hardness Shore D | ≥60 |
| Environmental Stress Cracking Resistance | ≥1000 h |
| Melt Temperature | 180-230 °C |
| Mold Temperature | 30-70 °C |
| Molding Shrinkage | 1.5-3.0% |
As an accredited Shanxi PCEC HDPE DMDA8007 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Shanxi PCEC HDPE DMDA8007 is packed in 25 kg PP woven bags, 40 bags per pallet, totaling 1,000 kg. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Shanxi PCEC HDPE DMDA8007 in 25kg bags, palletized, shrink-wrapped, and secured for export ocean freight. |
| Shipping | Shanxi PCEC HDPE DMDA8007 is shipped as a non-hazardous thermoplastic resin, normally in 25 kg PP woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Use clean, dry containers or trucks; protect from moisture, heat, and direct sunlight. Standard sea and land freight documentation applies. |
| Storage | Store Shanxi PCEC HDPE DMDA8007 in a cool, dry, well-ventilated warehouse. Keep original bags sealed on pallets, away from direct sunlight, heat, moisture, oxidizers, and open flames. Maintain ambient temperature, avoid static and physical damage, do not stack excessively, and follow first-in, first-out inventory. Protect from dust, contamination, and bag tearing. |
| Shelf Life | Shelf life: 24 months from production when stored in cool, dry, ventilated conditions, away from direct sunlight. |
Thin-wall dairy spread and deli tub production is one downstream track for DMDA8007. Melt flow index measured under ISO 1133-1:2022 at 190°C with a 2.16 kg piston load falls within the 7.2–8.8 g/10 min band on production certificates from Shanxi PCEC, while density determined by ASTM D1505-18 is approximately 0.956 g/cm³. This combination allows filling of 0.8–1.1 mm nominal sidewalls in multi-cavity cold-runner tools on 250–400-tonne hydraulic injection molding machines without exceeding clamp force margins above 85% of machine rating. Barrel temperature profiles are typically set at 180°C at the feed throat, 190°C in zone 2, 205°C in zone 3, 215°C in zone 4, and 220°C at the nozzle. Mold temperature is held at 12–18°C by chilled water with a pressure of 3.0–4.0 bar and a Reynolds number above 10,000 in the cooling channels. Injection speed is limited to 60–120 mm/s to avoid jetting in thin rectangular cavities; holding pressure is maintained at 45–60 MPa for 1.5–2.5 s and back pressure at 8–12 bar. Cooling time for 250 mL tubs weighing 9–12 g is 6–10 s across 16-cavity tools when wall sections are below 1.0 mm. The finished articles are used for margarine, cottage cheese, deli salads, and dairy spreads.
Food-contact compliance is documented under FDA 21 CFR 177.1520 for olefin polymers, EU Regulation 10/2011 with Annex I overall migration below 10 mg/dm² in 3% acetic acid and 10% ethanol simulants, and GB 4806.7-2016 where Chinese import inspection requires total migration and potassium permanganate consumption limits. White opacity in 1.0 mm sidewalls is obtained with 2.0–3.5 wt% of a 60% TiO₂ masterbatch in a PE carrier; erucamide slip agent at 0.05–0.15 wt% is used only where lid removal torque below 1.2 N·m is specified. Dimensional stability issues in rectangular tubs are dominated by post-mold shrinkage. Mold shrinkage measured at 48 h after molding is 1.5–2.0% parallel to flow and 1.8–2.2% perpendicular to flow under ASTM D955-21; gate position must keep flow length-to-wall thickness ratio under 150:1 to prevent core shift and sidewall thickness variation greater than 0.1 mm. Gate blush is controlled by placing submarine gates with vestige thickness below 0.1 mm at the tub base, away from stack lugs and rim seals.
| Application track | Melt temperature (°C) | Mold temperature (°C) | Injection speed (mm/s) | Pack pressure (MPa) | Nominal wall (mm) | Cycle time (s) |
|---|---|---|---|---|---|---|
| Thin-wall food tubs | 200–220 | 12–18 | 60–120 | 45–60 | 0.8–1.1 | 8–14 |
| Caps and closures | 195–215 | 8–15 | 60–100 | 50–70 | 0.7–1.2 | 5.0–8.5 |
| Industrial crates | 200–240 | 15–25 | 80–150 | 55–75 | 2.0–4.0 | 30–55 |
| Open-head pails | 195–225 | 12–20 | 70–110 | 50–75 | 1.3–2.0 | 18–35 |
| Household storage articles | 190–220 | 15–25 | 80–140 | 35–55 | 0.9–1.5 | 15–30 |
In closure manufacture, dimensional requirements are more severe than in open-packaging applications. The grade is processed in 24- and 48-cavity valve-gated hot runner molds with cycle times of 5.0–8.5 s for closure weights of 2.5–4.0 g. Injection molding machines of 120–250 tonnes clamp force are sufficient; melt temperature is maintained at 195–215°C and mold coolant is held at 8–15°C using turbulent flow at 3.5–4.0 bar pressure across individual cavity circuits. Injection velocity is set between 60 and 100 mm/s; hold pressure is 50–70 MPa for 1.0–2.0 s. Continuous thread profiles must hold dimensional tolerances of ±0.10 mm on thread crest diameter and ±0.08 mm on bore diameter. With DMDA8007, ejection is commonly accomplished with ejector sleeves and air assist to prevent distortion of the tamper-evident band. Removal torque is tested under ASTM D2063-22; typical unaged removal torques for 28 mm PE screw caps range from 0.9 to 1.5 N·m depending on thread engagement and erucamide level.
Formulation commonly uses 1.0–2.0 wt% of a 60% TiO₂ white masterbatch and 0.05–0.10 wt% erucamide for slip; no other fillers are added because the increased melt viscosity would raise fill pressure. Food-contact compliance for closures follows FDA 21 CFR 177.1520, EU Regulation 10/2011, and GB 4806.7-2016; Chinese product standards for plastic tamper-evident closures include GB/T 17876-2010 for dimensions and physical performance. The high melt flow index of DMDA8007 imposes a boundary in carbonated beverage closures. Because higher MFI resins generally show lower environmental stress cracking resistance under ASTM D1693-15 Condition B in 100% Igepal CO-630 at 50°C, the grade is not suited to pressurized CO₂ contents above 2.0 bar when the closure experiences hoop stress and repeated temperature excursions above 40°C. Published comparative ESCR data for this specific configuration is limited; closure validation therefore requires trial molding and torque retention after 24 h at 40°C and 85% relative humidity. For still water and dairy closures, mold cooling consistency is the dominant production risk; cavity-to-cavity temperature variation above 5°C produces measurable thread diameter drift and changes stripping torque outside the control limit.
For industrial crates and logistics totes, the medium-wall-thickness band of 2.0–4.0 mm places rib-bearing capacity ahead of thin-wall filling. Production tools run on 400–800-tonne injection molding machines with accumulator-assisted injection to maintain shot weights of 1.5–4.0 kg. Barrel temperatures from feed to nozzle are 200°C, 210°C, 225°C, 235°C, and 240°C. Mold temperatures of 15–25°C are maintained with water circuits; cycle time ranges from 30 to 55 s depending on wall thickness, rib density, and cooling channel layout. The resin is frequently used as 100% virgin polymer or with up to 20 wt% post-industrial regrind generated from the same production line; regrind fractions above 20 wt% can shift multi-axial impact under ASTM D3763-18 by more than 10% when granulate particle size distribution exceeds 5–10 mm. UV stabilization for outdoor beverage crates and agricultural trays uses 0.3–0.5 wt% of a hindered amine light stabilizer masterbatch plus 0.1–0.2 wt% phenolic antioxidant, with 2.0–3.0 wt% carbon black masterbatch where extended ultraviolet exposure is specified.
Compression resistance is measured under ASTM D642-20 at 23°C and 40°C; stack performance of filled crates is assessed under ISO 12048. Rib design is the controlling mechanical variable. Primary ribs are gated at 2.5–3.5 mm base width with 0.4–0.6° draft angle and root radius not less than 0.8 mm to avoid notch-sensitive failure at the rib-to-wall junction. Rib intersections above three ribs in one node create sink marks deeper than 0.05 mm, which reduce top-load distribution and are rejected under visual inspection. DMDA8007 high fluidity can produce jetting at injection speeds above 150 mm/s; fan gates or flash gates with land length 0.5–0.8 mm are used to reduce flow streaking in large crates. Weld lines at handle openings are oriented away from top-load corners and must retain at least 80% of un-welded tensile strength when tested under ISO 527-2. REACH 1907/2006 SVHC screening and RoHS Directive 2011/65/EU Annex II limits apply to crates entering EU supply chains. The finished products include stack-and-nest beverage crates, agricultural harvesting trays, fish crates, and general logistics boxes used in closed-loop distribution systems.
When open-head pail molders reduce wall thickness below 1.6 mm, the controlling variables shift from fill pressure to environmental stress cracking resistance. Open-head pail molding from DMDA8007 targets 5–20 L containers with nominal wall thickness of 1.3–2.0 mm and thickened rim sections of 3.0–4.0 mm for handle boss retention. Injection molding machines of 600–1,200 tonnes clamp force are specified; the barrel profile runs 195°C at the feed zone, 205°C, 215°C, and 225°C at the nozzle, with mold temperature 12–20°C and cycle times 18–35 s. Shot volume is filled at 70–110 mm/s screw advance, and hold pressure is set to 50–75 MPa for 2.0–4.0 s to pack rim and boss regions. Formulation generally uses 2.0–3.0 wt% color masterbatch; for industrial pails, up to 30 wt% in-house post-industrial regrind from the same grade is allowed when final melt flow index remains within 6.5–9.5 g/10 min under ISO 1133-1:2022. Food-contact pails use only virgin resin and masterbatch components listed under FDA 21 CFR 177.1520 and EU Regulation 10/2011.
Where the container is certified as UN 1H2 for open-head plastics packaging, production formulations must not deviate from the type-tested formulation without requalification; replacing more than 10 wt% virgin resin with regrind generally triggers a new certification test under the applicable UN testing protocol. Drop impact at -18°C is assessed under ASTM D5276-19 after conditioning; the test height is determined by packaging group and filled density, not by wall thickness alone. Stacking behavior is verified under ISO 2234:2015 with a static load corresponding to 1.5 to 1.8 times the rated gross mass. The key weakness of high-MFR HDPE in this application is environmental stress cracking when filled products contain wetting agents. DMDA8007 should not be used for open-head pails holding undiluted alkylbenzene sulfonates, bleach solutions above 5% active chlorine, or ketonic solvents without liner testing; published ESCR data for the grade under ASTM D1693-15 Condition B is limited, so candidate products must be screened against the actual chemical formulation at 40°C for 30 days. Handle boss dimensions must maintain a minimum boss wall-to-adjacent-wall ratio of 0.55–0.65 to avoid sink marks that compromise lid seal integrity under hydrostatic load.
Rectangular bins with snap-fit lids, storage baskets, hangers, and toy components are the main household articles molded from DMDA8007. The processing window falls between 190°C and 220°C melt temperature and 15–25°C mold temperature; injection molding machines of 120–350 tonnes clamp force are adequate for shot sizes of 0.3–1.5 kg. Thin-wall housewares at 0.9–1.5 mm nominal wall thickness are filled at injection speeds of 80–140 mm/s; pack pressure is maintained at 35–55 MPa for 1.5–3.0 s. Snap-fit undercuts of 0.6–1.2 mm are released by ejector plates because HDPE flexural modulus near 900 MPa under ASTM D790-17 does not permit deep undercuts with standard ejector pins. Mold shrinkage measured under ASTM D955-21 is 1.6–2.2% after 48 h; box lids require balanced gating at the hinge area or center to avoid warp above 1.0 mm over a 400 mm length.
Formulation for indoor articles uses 1.0–3.0 wt% masterbatch; outdoor storage bins are stabilized with 0.25–0.50 wt% hindered amine light stabilizer and 0.1–0.2 wt% antioxidant. Toy component compliance is tested under EN 71-3:2019+A1:2021 for migration of 19 elements and under ASTM F963-23 where the U.S. retail channel is specified. REACH SVHC screening and RoHS Directive 2011/65/EU Annex II limits apply to electrical or electronic storage accessories. Low-temperature toughness is verified by ISO 180/A notched Izod impact; production trials show acceptable snap-fit assembly down to -20°C, but assembly below -30°C is outside the documented operating range. The primary processing defect in these articles is gate blush and sink over thick bosses; boss thickness should not exceed 60% of adjacent wall thickness, and a delay in pack pressure of 0.5–1.0 s reduces sink depth to less than 0.03 mm. Finished applications include stackable storage crates for home organization, garment hangers with molded hook sections, and toy building components that require repeated snap-fit engagement without fracture.
Competitive Shanxi PCEC HDPE DMDA8007 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Shanxi PCEC HDPE DMDA8007 is a high-density polyethylene blow-moulding resin produced with an alpha-olefin comonomer to increase slow crack growth resistance relative to homopolymer HDPE. The grade is used in extrusion blow-moulded containers for detergent, surfactant, and industrial-chemical packaging, where stress-cracking resistance and melt strength are critical. Published technical data for the DMDA8007 designation list a melt mass-flow rate of 0.70–0.85 g/10 min at 190 °C under 2.16 kg load when determined in accordance with ISO 1133-1:2022 or ASTM D1238. Annealed density is reported as 0.956–0.959 g/cm³ under ISO 1183-1:2019 / ASTM D1505. Tensile yield stress under ASTM D638-14 is typically 24–27 MPa, with elongation at break exceeding 600%. Flexural modulus under ASTM D790-17 or ISO 178:2019 falls between 950 MPa and 1,100 MPa. Environmental stress-cracking resistance measured as F50 under ASTM D1693-15 condition B in 100% Igepal CO-630 at 50 °C generally exceeds 100 h for virgin pellets. The Vicat softening temperature under ASTM D1525 is commonly reported at 123–127 °C. Actual shipment values vary by lot; the supplier certificate of analysis remains the controlling specification.
Shanxi PCEC HDPE DMDA8007 occupies the low-melt-index segment of the high-density polyethylene product family. Injection-moulding HDPE grades are typically specified at 8–20 g/10 min melt mass-flow rate under 190 °C/2.16 kg to fill spiral-flow lengths above 300 mm at 2 mm wall thickness. The 0.70–0.85 g/10 min range of DMDA8007 reflects a higher average molecular weight and produces the melt elasticity needed for parison extrusion, whereas injection grades are optimised for shear-thinning and rapid solidification. Yield stress may be similar between the two families, but ESCR F50 under ASTM D1693-15 condition B is frequently an order of magnitude lower for homopolymer-rich injection grades. DMDA8007 is comonomer-modified to improve slow crack growth resistance; the higher melt strength reduces parison drawdown on accumulator-head blow-moulding lines but also reduces spiral flow and increases injection-pressure requirements if misapplied.
In continuous shuttle blow-moulding equipment with single-screw extruders of 24:1 to 30:1 L/D ratio and compression ratios between 2.8:1 and 3.5:1, Shanxi PCEC HDPE DMDA8007 is processed with rear barrel zones from 180 °C to 190 °C and front zones from 190 °C to 200 °C. The accumulator die head is commonly maintained at 190–200 °C, and the measured melt temperature at the die exit is controlled to 190–205 °C. Blow air pressure of 0.6–0.9 MPa and mould cooling water at 8–15 °C are typical for wall-thickness control and cycle-time reduction. Regrind fractions up to 25 wt% are used in monolayer industrial container production, provided the recycled stream is free of polypropylene contamination and the blend is re-certified for ESCR under ASTM D1693-15 condition B. Dry pellets stored below 60% relative humidity require no forced predrying; if surface condensation occurs, a 2 h hopper dryer cycle at 80 °C restores feed consistency.
Accumulator-head production of 25 L to 200 L containers with Shanxi PCEC HDPE DMDA8007 requires active parison programming because the low melt index does not eliminate sag at long hang times. If wall-thickness variation exceeds ±0.3 mm in the pinch-off zone, the first corrective action is a 2 °C reduction in die-head temperature, which raises elongational viscosity and reduces parison drawdown. Die-head temperature below 185 °C may induce sharkskin surface defects on the parison and should be avoided. For a 25 L cylindrical mould with a blow-up ratio of 2.5:1 and target wall thickness of 1.5 mm, the parison preblow pressure is typically set to 0.3–0.5 MPa and the final blow pressure to 0.6–0.8 MPa. Tooling with a die gap of 1.4–1.8 mm and a mandrel land length of 20–25 mm is used to stabilise the parison surface. The same die-head temperature reduction may not apply to coextruded structures where the HDPE layers are less than 30% of total wall thickness.
The primary service requirement for Shanxi PCEC HDPE DMDA8007 is resistance to slow crack growth in the presence of surface-active packaging contents. Under ASTM D1693-15 condition B, F50 failure time in 100% Igepal CO-630 at 50 °C exceeds 100 h for virgin pellets and forms the basis for selecting the grade in detergent, surfactant, and agricultural-chemical containers. Chemical compatibility is not universal: strong oxidising acids, aromatic hydrocarbons, and halogenated solvents can plasticise the amorphous tie-chain regions or accelerate cracking and must be evaluated by immersion tests according to ASTM D543 or ISO 175. At service temperatures above 60 °C, the ESCR lifetime of any HDPE can be shorter than the room-temperature value, and long-term pack testing is required before commercial filling. Free-radical-generating additives or oxidising process aids should be avoided because they reduce melt stability and slow crack growth resistance.
For six-layer extrusion blow-moulded articles with ethylene-vinyl alcohol copolymer barrier layers, Shanxi PCEC HDPE DMDA8007 is used as the polyolefin skin and inner heat-seal layer. The HDPE skin layers are processed at 190–205 °C, while the EVOH layer is normally melt-processed at 190–220 °C depending on ethylene content. Maleic anhydride-grafted polyethylene tie layers between the HDPE and EVOH are processed at 190–210 °C. The moisture-barrier contribution of the HDPE layers is critical because EVOH oxygen permeability increases by more than an order of magnitude above 85% relative humidity; the thickness of the HDPE skin layer is therefore adjusted to maintain the EVOH layer below this humidity threshold under real filling and storage conditions. Adhesion between HDPE and tie-layer is tested by peel or delamination resistance according to the converter’s internal method aligned with ASTM D1876 for flexible laminates; published data for this exact coextruded configuration is limited, so line trials with the selected tie-layer grade are required.
Finished containers moulded from Shanxi PCEC HDPE DMDA8007 are qualified by closure torque retention, weld-line burst strength, and drop impact resistance. Top-load strength of 1 L bottles is measured under ASTM D2659 or ISO 12048; typical HDPE blow-moulded packaging values are 200–600 N depending on geometry. Drop impact resistance of filled containers is evaluated according to ASTM D2463 at -18 °C and 23 °C. Weld-line burst pressure is measured hydraulically at 0.2–0.5 MPa for small containers; published data for this exact grade in specific container geometries is limited, so converter-specific capability studies are required.
When compared with high-molecular-weight HDPE drum grades specified at melt mass-flow rates below 0.5 g/10 min, DMDA8007 provides a shorter parison hang time for bottles and containers up to approximately 25 L, but the long hang times involved in 200 L drum production generally require a higher-molecular-weight grade to prevent excessive drawdown. The following representative property table separates the processing families; the DMDA8007 supplier certificate of analysis should be used for lot-specific acceptance.
| Property | Test method | Shanxi PCEC HDPE DMDA8007 | HDPE injection grade | HMW-HDPE drum grade |
|---|---|---|---|---|
| Melt mass-flow rate, 190 °C/2.16 kg | ISO 1133-1:2022 / ASTM D1238 | 0.70–0.85 g/10 min | 8–20 g/10 min | 0.25–0.45 g/10 min |
| Density | ASTM D1505 | 0.956–0.959 g/cm³ | 0.960–0.965 g/cm³ | 0.954–0.958 g/cm³ |
| Tensile yield stress | ASTM D638-14 | 24–27 MPa | 28–31 MPa | 23–26 MPa |
| ESCR F50, condition B | ASTM D1693-15 | >100 h | 5–20 h | >300 h |
| Vicat softening temperature | ASTM D1525 | 123–127 °C | 124–128 °C | 122–126 °C |
The grade is hydrophobic and does not require pre-drying when pellets are stored in closed silos at ambient relative humidity below 60%. If silo breathing or bag storage allows moisture uptake, a hopper dryer at 80 °C for 2 h is sufficient; longer drying at temperatures above 100 °C may cause pellet agglomeration and should be avoided. In twin-screw reprocessing of regrind, co-rotating screws with 32:1 L/D ratio, moderate shear screw configuration, and zone temperatures of 180–200 °C maintain molecular weight retention. Excessively aggressive kneading blocks should be avoided because shear-induced chain scission reduces the high-molecular-weight tail responsible for melt strength and ESCR. The melt pressure before the screen changer should be kept below 25 MPa to avoid excessive shear heating. The regrind fraction should be limited to 20–25 wt% for monolayer containers when the acceptance criterion is retention of at least 80% of virgin ESCR under ASTM D1693-15 condition B.
For food-contact and industrial packaging qualification, the following matrix is used. Compliance must be verified on the finished article because additives, regrind, and conversion history can affect the final status.
| Regulation / standard | Scope | Test method / clause | Relevant limit or condition |
|---|---|---|---|
| US FDA 21 CFR 177.1520 | Olefin polymers for food contact | Specific paragraph selected by density and extractables | Finished article extraction testing under FDA conditions of use |
| EU 10/2011 | Plastics intended for food contact | Specific migration tests; overall migration | Overall migration ≤ 10 mg/dm² |
| REACH | Registration and SVHC screening | EC No. 1907/2006 Annex XVII | No listed substance above threshold |
| RoHS | Electrical/electronic packaging not usually in scope | Directive 2011/65/EU Annex II | Pb, Cd, Hg, Cr VI ≤ 0.1 wt%; Cd ≤ 0.01 wt% |
| ASTM D1693 | Environmental stress-cracking resistance | Condition B, 100% Igepal | F50 >100 h virgin |