Shanghai Jinfei Hdpe Hxm50100ca

Shanghai Jinfei HDPE HXM50100CA

    • Product Name: Shanghai Jinfei HDPE HXM50100CA
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 366797
    Manufacturer Shanghai Jinfei Petrochemical Co., Ltd.
    Product Grade HDPE HXM50100CA
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.959 g/cm³
    Melt Flow Rate 190 C 5 Kg 0.25 g/10 min
    Tensile Yield Strength ≥23 MPa
    Elongation At Break ≥600%
    Flexural Modulus 1100 MPa
    Vicat Softening Temperature 125 °C
    Melting Point 130-135 °C
    Hardness Shore D 62
    Environmental Stress Cracking Resistance >5000 h
    Carbon Black Content 2.0-2.5%
    Oxidation Induction Time >20 min

    As an accredited Shanghai Jinfei HDPE HXM50100CA factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Shanghai Jinfei HDPE HXM50100CA comes in 25 kg woven bags or 1,000 kg jumbo bags for industrial supply.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Shanghai Jinfei HDPE HXM50100CA, 25 kg bags, palletized, stretch-wrapped, securely stowed, suitable for ocean freight.
    Shipping Shanghai Jinfei HDPE HXM50100CA is shipped as a non-hazardous polymer in 25 kg woven bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers/trucks, avoiding moisture, direct sunlight, heat, and sharp objects. No special IMDG/ADR classification; standard sea/land freight applies. Export packaging is suitable for ocean freight.
    Storage Store indoors in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, sparks, and open flames. Keep original packaging sealed to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers. Stack bags, boxes, or octabins securely, not exceeding safe heights. Maintain clean handling areas and use first-in, first-out stock rotation.
    Shelf Life Shelf life is typically 24 months when stored unopened in a dry, cool, ventilated place, protected from sunlight and moisture.
    Application of Shanghai Jinfei HDPE HXM50100CA

    In thin-wall logistics packaging and rigid crates, HXM50100CA is processed on reciprocating-screw injection molding machines with clamp force selection commonly between 150 t and 600 t depending on projected area. The melt temperature at the nozzle is held between 210 °C and 250 °C, with mold surface temperature controlled at 20 °C–60 °C. HDPE crystallizes rapidly, and skin-solidification time on the cavity wall governs gate freeze and sink mark depth. Injection velocity is profiled: a fast initial stage of 80–150 mm/s screw displacement is used to fill the flow front before the wall freezes, followed by a shorter holding-pressure stage at 40–80 MPa hydraulic pressure for gate seal. Gate size for thin-wall pails with 1.2–2.5 mm nominal wall should be at least 0.7–1.0 mm diameter for pin-type gates to avoid premature gate solidification before packing. Shrinkage after cooling is measured following ASTM D955-21; HDPE of this class typically exhibits linear mold shrinkage between 1.5% and 3.0%, with anisotropic differential between flow and transverse directions of 0.2–0.7 percentage points. Warpage is minimized by balancing cavity wall thickness and by using cooling time of 15–35 s for 3–5 mm wall sections. Residual stress is evaluated by annealing coupons at 80 °C for 2 h and measuring dimensional change. Weld-line strength in lattice crates is evaluated by ISO 527-2:2012 tensile tests on molded plaques cut across the weld line. A reduction greater than 25% compared with un-welded material indicates insufficient melt temperature or excessive use of regrind. Environmental stress crack resistance is tested under ASTM D1693-15, condition B, at 50 °C in 10% Igepal CO-630. Injection molded parts that require detergent contact should exceed 24 h without failure. Because HXM50100CA is a high-density polyethylene, drying is generally not required before injection molding when internal moisture is below 0.05%, but hopper magnets and screen packs at the nozzle are recommended to protect hot-runner valve gates from carbonized contamination.

    What Governs Slow Crack Growth in Pressurized Pipe Compounds?

    For pressure pipe compounds based on high-density polyethylene of the HXM50100CA class, the limiting long-term failure mechanism is not short-term yield but slow crack growth through the tie-molecule network between lamellae. A pipe resin qualified under ISO 12162:2009 must demonstrate a minimum required strength of 10.0 MPa for PE100 classification, derived from hydrostatic strength data generated per ISO 9080:2012. Extrusion of HXM50100CA into solid-wall pipe is performed on single-screw extruders with 30:1–37:1 L/D and barrier screws. Temperature profile from feed to die is typically 180 °C, 200 °C, 210 °C, 215 °C, and 215 °C. Melt pressure at the screen pack must remain below 35 MPa to limit shear heating, which would reduce molecular weight at the pipe inner wall. During calibration, the vacuum in the spray tank is held at -0.02 MPa to -0.04 MPa gauge to control collapse and inner diameter. The critical processing conflict is between surface melt fracture and output. Die land length is selected at 20–30 times the annulus gap, and melt temperature is kept above 190 °C to avoid sharkskin at line speeds above 1.2 m/min. Slow crack growth resistance is evaluated by notched pipe test ISO 13479:2022 at 80 °C under 4.6 MPa hoop stress. Failure before 500 h indicates insufficient comonomer incorporation or inadequate gel control. Batch-to-batch variance in extrusion torque is monitored; a torque drift greater than 5% at constant screw speed signals gel content changes from reactor grade transitions. Pipe surface oxidation induction time is measured by ISO 11357-6:2018 differential scanning calorimetry. HDPE pipe compounds should exceed 20 min at 200 °C to ensure residual antioxidant stabilization. For non-pressure corrugated drainage pipe, the same extrusion principle applies, but the hydrostatic design basis is not required. Short-term ring stiffness is assessed per ISO 9969:2016 and creep ratio per ISO 9967:2016. Published data for HXM50100CA specifically listed under pressure pipe standards may be limited; converter qualification must include full hydrostatic testing under the applicable national standard.

    Conversion routeTest methodMeasured propertyCondition
    Injection molded cratesASTM D955-21Linear mold shrinkage23 °C ± 2 °C after 48 h
    Pressure pipe compoundISO 13479:2022Notched pipe slow crack growth80 °C, 4.6 MPa hoop stress
    Blow molded containerASTM D1693-15ESCR50 °C, 10% Igepal CO-630
    Thermoformed sheetISO 11357-3:2018CrystallinitySecond heating 10 K/min
    Closure skirtASTM D638-14Tensile yield strength50 mm/min test speed

    Accumulator extrusion blow molding of HXM50100CA into 20–200 L industrial containers places parison sag control at the centre of the process window. The extruder is operated at 180 °C–220 °C with a diverging die gap of 2.0–4.0 mm and a parison programming curve that opens the die during the last 20–30% of drop to thicken the bottom pinch-off. Die swell for HDPE of this density class is commonly 35–60%, measured as the ratio of parison diameter to die diameter under low-shear conditions. A parison length exceeding 1.8 m must be supported by a cooled blow pin or pre-blow at 0.02–0.05 MPa internal air to prevent draw-down. The mold closes at 0.3–0.6 m/s clamp velocity, and blow pressure is set at 0.7–1.0 MPa. Cycle time for a 60 L container is typically 90–150 s depending on wall thickness and cooling water temperature at 8–12 °C. The pinch-off weld must be evaluated for thickness and ESCR. A flash remnant below 2 mm at the mold face indicates insufficient closing force or incorrect die programming. Top load strength is tested by ASTM D2659-16 with a 25 mm/min crosshead speed until deformation of 10%. Drop impact for UN-certified packagings is tested at -18 °C per 49 CFR 178.603 or applicable ADR/RID procedure. HDPE containers that crack at the pinch-off or handle insert show poor melt fusion or excessive regrind. Food-contact grades must satisfy 21 CFR 177.1520(c) olefin polymer requirements and EU Regulation 10/2011 overall migration limits. Converters should obtain lot-specific compliance from the resin supplier.

    When HXM50100CA Is Extruded into Sheet for Thermoformed Pallets and Dunnage

    In sheet extrusion, the resin is fed to a single-screw extruder with a barrier screw and 33:1 L/D, with melt temperature measured at the adapter at 210–240 °C. A flexible-lip flat die with 800–1600 mm width is set to a gap 10–20% greater than target sheet thickness to compensate for draw-down. The melt curtain enters a vertical three-roll polishing stack. Middle roll temperature is maintained at 80–100 °C, bottom roll at 60–80 °C, and top roll at 70–90 °C. Contact roll pressure of 30–60 N/mm of width is required to suppress surface haze and to control thickness tolerance within ±0.05 mm. Sheet of 3–8 mm thickness for thermoformed pallets is wound or cut inline and then reheated to 140–170 °C surface temperature, verified by infrared pyrometer. Sag during heating is the main process conflict. A heater profile with top zone at 220 °C and bottom zone at 200 °C for 90–180 s is common for 5 mm sheet. Thermoforming is performed on a plug-assist machine with aluminum plug temperature controlled at 100–120 °C. Plug displacement is set to 60–80% of cavity depth before final vacuum. Crystallinity after forming is measured by DSC per ISO 11357-3:2018. Excessively rapid quench on the mold wall produces low crystallinity at the surface and increases warpage after demolding. Dimensional stability is evaluated after conditioning at 23 °C ± 2 °C and 50% ± 5% relative humidity for 40 h. Tensile properties of extruded sheet are measured per ISO 527-2:2012, and flexural modulus per ISO 178:2019. Published data for HXM50100CA in thick-gauge thermoforming is limited; converter trials should establish sag time and plug force for the specific cavity geometry.

    Caps and Closures via High-Cavitation Injection Molding

    High-cavitation injection molding of HXM50100CA for caps and closures requires tighter melt flow stability than many large-part applications because cavity filling imbalance in 48–96 cavity tools is amplified by viscosity variation. The resin is processed at 220–250 °C melt temperature with mold water temperature at 10–15 °C to achieve fast cycle time of 5–12 s. Hot-runner valve gates with 0.4–0.8 mm gate diameter deliver shear heating that reduces viscosity at the gate but may cause gate blush if melt temperature exceeds 260 °C. Holding pressure is set by gate freeze time, typically 0.5–1.0 s for a 1.5 mm skirt wall. Cavity pressure sensors are used to maintain 50–70 MPa peak cavity pressure. Torque retention of tamper-evident bands is influenced by shrinkage and demolding. Closures are ejected when mold opening stroke reaches 40–60% of maximum, and cooling time is adjusted to achieve 80 °C average ejection surface temperature. ESCR of closures is tested by ASTM D1693-15 condition B. Tear-off band integrity is evaluated by a tensile test at 500 mm/min. Values below 15 N on a 29 mm closure indicate insufficient melt fusion at the bridge or excessive mold release. Regulatory compliance for beverages requires FDA 21 CFR 177.1520 and EU 10/2011. Converters must verify organoleptic panel results and overall migration at 40 °C for 10 days per EN 1186 parts.

    High-density polyethylene from HXM50100CA can be converted into oriented strapping and monofilament only when the melt flow rate is appropriate for high draw ratios and the molecular weight distribution is sufficiently broad to stabilize water-bath orientation. The extrusion line uses a single-screw extruder with 24:1–30:1 L/D, a metering pump, and a tubular or flat die with 0.3–0.8 mm gap. Melt temperature is kept at 200–240 °C. Water bath quench temperature is controlled at 30–50 °C to set crystallinity before orientation. The quenching distance from die exit to water surface is 10–30 mm. Longer distances cause uncontrolled crystallization and draw resonance. Orientation is performed in a hot-air oven or hot-roller unit at 90–115 °C, with draw ratios of 8:1–12:1. After stretching, annealing at 100–120 °C for 0.5–2.0 s reduces post-extrusion shrinkage. Line breaks on conventional strapping lines occur when melt gels exceed 0.3 mm or when draw ratio exceeds 12:1 at reduced molecular weight. Tensile strength of oriented HDPE strapping is measured by ASTM D882-18. A break strength of 0.35–0.50 N/tex is typical for HDPE of this class, but published data for HXM50100CA in monofilament configuration is limited and converter trials should establish the actual draw curve. Split resistance and fibrillation tendency are assessed by a twist tester. More than 5 fibrils per 100 mm indicates excessive orientation temperature or inadequate blending. UV-stabilized packaging grades require 0.15–0.30 wt% hindered amine stabilizer masterbatch and a minimum 0.5% carbon black masterbatch for outdoor exposure, tested by ISO 4892-2:2013 for 1000 h weathering.

    Free Quote

    Competitive Shanghai Jinfei HDPE HXM50100CA prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Shanghai Jinfei HDPE HXM50100CA is a bimodal high-density polyethylene pressure-pipe extrusion compound supplied as black pellets. The grade is classified under ISO 12162:2009 as PE 100, with a minimum required strength of 10.0 MPa at 20 °C for 50 years. The model designation identifies the Shanghai Jinfei production line and the carbon black-added formulation. Nominal base-resin density is 0.949 g/cm³ when measured by ISO 1183-1:2019; finished compound density is approximately 0.958 g/cm³ because of carbon black. Melt flow rate under 190 °C/5 kg is 0.22 g/10 min using ISO 1133-1:2022, placing the resin in the low-flow, high-molecular-weight region required for large-diameter pressure pipe. Carbon black content is typically 2.0 wt% to 2.5 wt% and is controlled to the dispersion limits of ISO 18553:2002. The lot certificate of analysis, not a generic datasheet, is the controlling document for each silo batch.

    What molecular architecture permits the 10.0 MPa minimum required strength?

    Unlike unimodal PE80 grades produced in a single-reactor chain, HXM50100CA uses a bimodal molecular weight distribution. The low-molecular-weight fraction controls extruder throughput and reduces head pressure at high line speeds; the high-molecular-weight fraction, into which 1-hexene comonomer is preferentially incorporated, generates the tie molecules and entanglement density that resist slow crack growth under sustained hoop stress. The short-chain branching is not randomly distributed; branch-free high-molecular-weight polyethylene crystallizes too densely, reducing tie molecule concentration and accelerating brittle crack propagation. The ratio of high-load melt index under 190 °C/21.6 kg to the standard 190 °C/5 kg melt index is therefore used as a release proxy for the breadth of the molecular weight distribution. This architecture is the basis for reaching the 10.0 MPa lower prediction limit at 50 years rather than the 8.0 MPa threshold of PE 80. In processing, the bimodal distribution provides high melt strength for vacuum calibration of thick-walled pipe without melt fracture at the die lip. Published lot-specific gel-permeation chromatography curves for this exact configuration remain limited; commercial control relies on melt-flow ratios and batch-to-batch capillary rheometry rather than a single polydispersity index.

    When hydrostatic design stress is derived from ISO 9080 regression data

    ISO 9080:2012 uses failure data from ISO 1167-1:2006 hydrostatic tests at 20 °C, 60 °C and 80 °C to extrapolate the lower prediction limit. For HXM50100CA, the 20 °C, 50-year lower prediction limit exceeds 10.0 MPa circumferential stress, satisfying the PE 100 requirement in ISO 12162:2009. The water-service design stress is obtained by dividing the minimum required strength by the service coefficient C = 1.25, yielding 8.0 MPa at 20 °C. Pressure class follows the relation P = 2σs/(SDR − 1). An SDR 11 pipe therefore carries 1.6 MPa at 20 °C, and an SDR 17 pipe carries 1.0 MPa. At 40 °C, the temperature derating factor for PE 100 under ISO 4427-1:2007 is 0.74, reducing the design stress to 5.9 MPa. The extrapolation procedure also requires a knee-free stress-rupture curve; an early ductile-to-brittle transition before 50 years would prevent PE 100 classification. This classification is a material property, not a standalone guarantee for all service conditions: oxidative disinfectants, abrasive slurries, and poorly compacted trench beds impose additional pipe-life reductions that require separate validation.

    Extrusion of HXM50100CA on grooved-feed single-screw machines with 30:1 to 33:1 L/D ratios and screw diameters of 60 mm to 120 mm typically begins with a feed zone at 180 °C, a compression zone at 200 °C, and a metering zone at 220 °C. Melt temperature at the die entry is held at 200 °C to 230 °C; melt temperatures above 240 °C accelerate depletion of the phenolic-phosphite antioxidant package and shorten the measured oxidation induction time at 200 °C. A 100/80/60 mesh screen pack ahead of the breaker plate is common, and melt pressure before the screen changer ranges from 20 MPa to 35 MPa for SDR 11 pipe diameters up to 315 mm on 90 mm screws. Pressure fluctuations greater than ±1.5 MPa at constant screw speed indicate feed bridging, screen blinding, or temperature drift; such fluctuations can produce wall-thickness eccentricity beyond the K3 tolerance class. Vacuum calibration tanks should maintain spray water at 15 °C to 25 °C and a vacuum level of 0.02 MPa to 0.06 MPa depending on pipe diameter. In production-scale extrusion, a common failure mode is gel formation at the die lip when melt temperature exceeds 240 °C or when the screen pack is blinded; these gels appear as localized oxide inclusions in the pipe wall and can initiate slow crack growth. If pellets are stored in an unheated silo and the dew point exceeds the pellet surface temperature by more than 5 K, surface condensation should be removed by drying at 80 °C for 2 h in a desiccant dryer before hopper loading. Batch-to-batch melt flow rate is typically controlled within ±0.02 g/10 min, but release limits should be verified from the certificate of analysis.

    Slow crack growth, rapid crack propagation, and notched pipe testing

    The predominant long-term failure mechanism in pressure pipes is slow crack growth, not short-term ductile burst. HXM50100CA is engineered to shift the failure mode from brittle crack growth to ductile yielding within the 50-year design window. The notched pipe test under ISO 13479:2009 uses a 100 mm external longitudinal notch machined to 15% of wall thickness; test conditions are 80 °C and 4.0 MPa internal pressure. PE 100 resins of this class typically exceed 1000 h before failure, while early-generation PE 80 materials may fail below 500 h under the same conditions. Published lot-specific values for this exact formulation remain limited, so pipe converters should run confirmatory notched pipe tests on the production line. Full-scale rapid crack propagation testing under ISO 13477:2008 is required when the pipe is used for gas distribution or when compressed gases are present; a critical pressure below the operating pressure at the minimum service temperature must be demonstrated. For trenchless installation or pipe jacking, PE 100 classification alone may be insufficient if the bedding imposes point loads or external scratching. In those cases a PE 100-RC resin specified under PAS 1075:2009 may be required; HXM50100CA is not automatically compliant with PE 100-RC without additional full-scale tests.

    For buried water mains, the controlling mechanical properties are hydrostatic design stress and resistance to environmental stress cracking; for exposed pipe, carbon black dispersion under ISO 18553:2002 must not exceed a rating of 3 on the 1–5 scale, and carbon black content is expected to be 2.0 wt% to 2.5 wt% when measured by ISO 6964:2019. Potable water pipes are typically evaluated under GB/T 13663.2-2018 in China and under EN 12201-2:2011 within European conformity systems. In gas distribution, the grade may be evaluated under ISO 4437-1:2015 if the national gas code permits black PE 100; the critical pressure for rapid crack propagation is determined by ISO 13477:2008 at the minimum service temperature. Chemical resistance should be verified in accordance with ISO 4433-1:1997 for the specific service fluid: concentrated oxidizing acids, aromatic hydrocarbons, and chlorinated solvents can swell the amorphous fraction or deplete the antioxidant. Free chlorine in potable water at pH below 6.5 and residual above 1.0 mg/L may accelerate oxidation in the bore layer; pipes operating outside these limits require a case-specific lifetime assessment. Above-ground temporary pipelines rely on carbon black for UV resistance, but prolonged exposure beyond the design service life can embrittle the surface layer, and butt-fusion weld quality after oxidation should be evaluated by bend testing under ISO 13953:2001.

    Oxidation induction time is a release parameter, not a long-term performance guarantee.

    The oxidative stability of HXM50100CA is controlled at the production stage through a phenol-phosphite antioxidant package. The release test is oxidation induction time at 200 °C by ISO 11357-6:2018, with a typical acceptance threshold above 30 min. The value reflects the amount and activity of the stabilizer package in the pellet, but it does not directly predict pipe service life because thermal-oxidative conditions in the field are lower in temperature and operate over decades. Extended storage above 40 °C, exposure to metal fines, or contamination with incompatible polymers can reduce the observed OIT below 20 min. A lot with an OIT below 20 min should not be used for pressure pipe without additional stabilizer masterbatch, because the antioxidant reserve may be insufficient for welding and long-term thermal stability. The material should not be blended with amine-based processing aids or reclaimed material of unknown stabilizer chemistry because antagonist reactions can consume the primary antioxidant.

    Compared with standard PE 80 materials, HXM50100CA permits a design stress of 8.0 MPa instead of 6.3 MPa at 20 °C for water service, corresponding to an approximate 21% reduction in minimum wall thickness for an equal pressure rating and outside diameter. The table lists the key distinctions that downstream pipe manufacturers use for grade selection.

    ParameterTest methodHXM50100CAConventional PE 80 reference
    Minimum required strength, 20 °C, 50 yearsISO 9080:201210.0 MPa8.0 MPa
    Design stress for water, 20 °CISO 4427-1:20078.0 MPa6.3 MPa
    Melt flow rate, 190 °C / 5 kgISO 1133-1:20220.22 g/10 min0.4–0.7 g/10 min
    Base-resin densityISO 1183-1:20190.949 g/cm³0.940–0.950 g/cm³
    Oxidation induction time, 200 °CISO 11357-6:2018>30 min>20 min

    Selection between PE 80 and PE 100 therefore involves an economic trade between lower wall thickness and higher extruder melt pressure. HXM50100CA reduces the wall-thickness penalty through its bimodal shear-thinning behavior, but the final pipe must be qualified on the specific extrusion line.

    Top