Shanghai Jinfei Hdpe Hhmtr 210hs

Shanghai Jinfei HDPE HHMTR-210HS

    • Product Name: Shanghai Jinfei HDPE HHMTR-210HS
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 834642
    Polymer Type High-density polyethylene (HDPE)
    Density 0.949 g/cm³
    Melt Flow Rate 0.20 g/10 min (190°C/5 kg)
    Melting Point 130 °C
    Tensile Yield Strength ≥23 MPa
    Elongation At Break ≥600%
    Flexural Modulus ≥1000 MPa
    Vicat Softening Temperature ≥120 °C
    Brittleness Temperature ≤-70 °C
    Environmental Stress Crack Resistance ≥1000 h
    Oxidative Induction Time ≥20 min
    Carbon Black Content 2.0-2.5%
    Long Term Hydrostatic Strength Mrs 10.0 MPa

    As an accredited Shanghai Jinfei HDPE HHMTR-210HS factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Shanghai Jinfei HDPE HHMTR-210HS is supplied in 25 kg woven bags, palletized, or 1,000 kg jumbo bags for bulk shipment.
    Container Loading (20′ FCL) Shanghai Jinfei HDPE HHMTR-210HS 20′ FCL loading: 25 kg bags, 1000 bags, 25 MT net; palletized options available.
    Shipping Shanghai Jinfei HDPE HHMTR-210HS ships as a non-hazardous high-density polyethylene resin. Use sealed 25 kg bags or jumbo bags. Keep dry, cool, ventilated, away from sunlight, moisture, and ignition sources. Maintain original packaging and labels; handle with care. No UN hazard class or special transport documentation is required.
    Storage Store Shanghai Jinfei HDPE HHMTR-210HS in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags closed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and high stacking. Follow local regulations and manufacturer/supplier SDS recommendations.
    Shelf Life Shelf life is typically 24 months when stored cool, dry, well-ventilated, sealed, and away from direct sunlight in original packaging.
    Application of Shanghai Jinfei HDPE HHMTR-210HS

    For potable water pressure pipe, Shanghai Jinfei HHMTR-210HS is assessed against the long-term hydrostatic strength classification of ISO 9080:2012 and ISO 12162:2017; a PE100 grading requires the regression curve to maintain a minimum required strength of 10 MPa at 20 °C for 50 years when the lower confidence limit is applied. On a production-scale single-screw extruder with a grooved feed section and an L/D of 33:1 to 37:1, the melt temperature at the die head is held at 190 °C to 220 °C for natural compound; the screen changer differential pressure should not exceed 8 MPa because higher shear creates local melt-temperature spikes that alter die swell uniformity and inner-wall gloss. An SDR 11 solid-wall pipe operating at 16 bar must pass the hydraulic acceptance test of ISO 1167:2019 at 20 °C under a hoop stress of 12.0 MPa for at least 100 h, and the resin lot should also show a ductile failure in the notched pipe test of ISO 13479:2022 at 80 °C; any brittle crack earlier than the specified regression limit indicates insufficient slow crack growth resistance. Surface moisture from outdoor silo storage at relative humidity above 60% should be removed with a desiccant hopper dryer at 70 °C for 2 h or by dry-air conveying below 0.01% moisture, because melt-phase moisture volatilisation produces splay and microvoids at the inner pipe wall. External lubricant additions above 0.1% by mass should be avoided unless qualified, as plate-out on the vacuum calibration sleeve alters the friction coefficient and produces cyclic wall thickness marks. For drinking-water contact, the finished pipe must meet the migration limits of the applicable national code, commonly NSF/ANSI/CAN 61 in North America or the water-contact requirements invoked through EN 12201-1:2011 in the EU project specification.

    Representative HMW-HDPE property envelope applicable to HHMTR-210HS; values are class-typical and not a lot certificate.
    PropertyTest methodControl window
    Melt flow rate, 190 °C/5 kgISO 1133-1:20220.20 to 0.35 g/10 min
    DensityISO 1183-1:20190.948 to 0.955 g/cm³
    Tensile yield strengthASTM D638-14≥ 23 MPa
    Elongation at breakASTM D638-14≥ 600 %
    ESCR, 100% Igepal, F50ASTM D1693-21> 1000 h
    Carbon black content, UV-stabilised pipeASTM D1603-142.0 to 2.5 % by mass

    Which Variables Govern Butt Fusion Bead Reversal in PE100 Pipeline Construction?

    Butt fusion joining of HHMTR-210HS pipes under field conditions changes the failure criterion from pipe-body long-term strength to the interfacial weld zone. On a 250 mm SDR 11 pipe, the heating plate must be set to 210 °C with a tolerance of ±10 °C, and the bead-up pressure should be held at 0.15 MPa until the initial bead height is 1.0 mm to 1.5 mm; subsequent closure and cooling follow ISO 21307:2017 procedure. The most frequent field rejection mode is cold fusion caused by plate temperature falling below 205 °C on exposed sites, so the fusion machine must be shielded and the plate surface checked with a pyrometer before each joint. Failed joints from production records often show double-bead formation with the inner bead narrower than 2 mm, which indicates insufficient melt displacement at the interface; the approved geometry is verified destructively by ISO 13953, where the fracture must propagate in the pipe wall rather than along the weld line. After welding, hydrostatic testing of the string is performed according to ISO 1167 or the project specification, and the joined section is typically held for 24 h at 1.5 times the service pressure before burial. In high-UV construction areas, the pipe surface should be protected until backfill; sustained exposure beyond 12 months without carbon black or stabiliser coverage may reduce weld peel strength because oxidation lowers molecular weight at the outer skin.

    Fluorine Barrier Chemistry in Coextruded HDPE Fuel Tank Shells

    When HHMTR-210HS is diverted into automotive fuel tank blow moulding, the accumulator-head machine should be sized so that the shot volume does not exceed 65% of the head capacity; larger shots increase residence time and can generate gel particles from the high-molecular-weight tail. The melt is processed at 200 °C to 220 °C, and parison programming is set to hold a minimum wall thickness of 3.0 mm at the pinch-off and 2.5 mm in the sidewall, because the permeability of the finished shell is inversely related to local thickness. Post-mould surface fluorination at 2% to 5% elemental fluorine in nitrogen for 30 s to 180 s creates a 0.5 µm to 5 µm surface layer that reduces hydrocarbon permeability to the emission limits of EPA 40 CFR Part 86 and CARB LEV III for the complete fuel system; the barrier is validated on the finished tank by a sealed housing evaporative determination test, not by resin specification alone. The principal failure mode on production-scale fluorination lines is inconsistent fluorine concentration at the pinch-off seam, where residual mould release or trimming debris masks the surface; therefore the pre-fluorination washing step must be monitored for conductivity and the bath temperature controlled to 40 °C to 60 °C. Additives used in HHMTR-210HS must be screened for fluorination compatibility: migratory slip agents and unsaturated fatty acid amides can reduce the reaction depth and cause post-fluorination yellowing, so any additive package change requires requalification of the permeation result.

    Landfill liner service shifts the governing failure mechanism from yield stress to slow crack growth at the sheet fusion seam. HHMTR-210HS extruded into 1.5 mm or 2.0 mm geomembrane sheet must satisfy the single-point notch resistance of ASTM D5397 at 50 °C; a minimum transition time of 500 h is commonly required before brittle crack propagation occurs, and the ESCR of the base resin in 100% Igepal at 50 °C should exceed 1000 h under ASTM D1693-21. On a flat-die sheet line, automatic gauge control must keep thickness variation within ±5% of nominal, since wedge-welded seam peel strength under GRI GM19 fails in a peel mode when the two sheets differ by more than 0.2 mm. The most common field defect on installed liners is not sheet rupture but seam opening from improper fusion temperature; the wedge welder must be set to 400 °C to 450 °C and the seam surface prepared by planing to remove the oxidised skin immediately before welding. For leachate contact containing aromatic hydrocarbons or high total dissolved solids, prequalification should include immersion in the project-specific liquid for 30 days at 40 °C because the stress crack resistance shift cannot be predicted from ESCR alone.

    UN 3H1/L1.0 Stacking Compression and Solvent Crack Resistance

    Under UN 3H1/L1.0 certification for free-standing rigid plastics jerricans, a blow moulding formulation based on HHMTR-210HS must pass the stacking, drop, and hydraulic pressure tests of the UN Recommendations on the Transport of Dangerous Goods, Part 6, for the packing group and liquid specific gravity declared in the type approval. A 20 L jerrican is typically drop tested at -18 °C from the applicable height for the relative density of the filling liquid, and then internally pressured to the test pressure specified for the packaging class; any seam or pinch-off failure is cause for rejection. The blow moulding line should be operated with an accumulator shot ratio below 1.5:1 and a mould temperature of 10 °C to 25 °C, because the pinch-off weld is the critical shear zone and must achieve a uniform flash thickness. For aromatic solvent or agrochemical formulations, the resin selection is driven by ASTM D1693-21 ESCR in 100% Igepal at 50 °C; lots that fall below 1000 h F50 show stress whitening at the handle weld zone within the first six months of storage. Post-mould dimensional checks are made after 24 h conditioning at 23 °C and 50% relative humidity, because high-molecular-weight HDPE continues to shrink in the first day after moulding and a container measured too early can pass a capacity test that it later fails.

    When HHMTR-210HS Is Extruded Through a Spiral-Wound Large-Diameter Pipe Die

    When spiral-wound large-diameter pipe is produced from HHMTR-210HS, the load-bearing strip is extruded on a 30:1 single-screw extruder at a melt temperature of 180 °C to 210 °C and wound around a rotating steel mandrel; the inter-helical weld is formed with a hot air welding shoe set to 350 °C to 450 °C, but the controlling parameter is the measured weld-root temperature, which must exceed 180 °C for molecular diffusion across the helix interface. Published data for HHMTR-210HS in this specific structured-wall configuration is limited compared with solid-wall pipe datasets, so the fabricator must verify ring stiffness to ISO 9969 and creep ratio to ISO 9967 on the full pipe rather than extrapolating from raw material tensile yield. The limiting failure mode is not short-term burst but inter-turn delamination under sustained soil load; therefore a welded seam that exhibits incomplete bead removal or a root gap below 0.5 mm should be sectioned and tested before the mandrel is released. If the strip compound contains recycled HDPE or a regrind fraction above 10%, the ESCR and slow crack growth values must be re-established because the high-molecular-weight fraction of HHMTR-210HS may be diluted below the threshold required for a ductile response in the helical weld.

    Free Quote

    Competitive Shanghai Jinfei HDPE HHMTR-210HS prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Shanghai Jinfei HDPE HHMTR-210HS is identified as a high-density polyethylene resin whose model designation places it within the producer’s HHMTR series. The suffix “HS” is interpreted in producer technical correspondence as a modifier for stiffness-related performance, but the controlling document for each lot is the Shanghai Jinfei certificate of analysis. Published third-party dossiers containing a full ISO 9080 long-term hydrostatic strength dataset for this specific configuration are limited. Consequently, numerical values supplied below are class-typical expectations for high-density polyethylene with density 0.945–0.955 g/cm³ and melt mass-flow rate 0.2–0.7 g/10 min at 190 °C/2.16 kg. They are not a substitute for the producer’s lot-specific certificate, safety data sheet, or revision-controlled technical datasheet.

    The resin is typically considered for extruded pressure pipe, technical profiles, and rigid sheet where slow crack growth resistance, high melt strength, and dimensional stability are required. Because the producer has not made a complete comparative dataset publicly available for all HHMTR-series grades, direct quantitative separation from HHMTR-210, HHMTR-210H, or other nearby designations requires a written producer comparison against ISO-conforming specimens. The processing environment, stabilizer package, and molecular architecture interact with condensation-controlled hopper feed and screw design in ways that can alter observed output and surface finish across otherwise equivalent lines.

    What Standardized Verification Points Should the Producer’s Certificate Address?

    For a grade positioned in this HDPE class, incoming quality verification is normally anchored to ISO 1183-1 for density, ISO 1133-1:2022 for melt mass-flow rate, ISO 527-2 for tensile yield stress, ISO 178 for flexural modulus, and ISO 179-1/1eA for Charpy notched impact strength. Environmental stress crack resistance may be reported under ASTM D1693 or ISO 22088-3, depending on the target market. Oxidative induction time, when specified, is assessed under ISO 11357-6. The certificate should state the test method revision, conditioning period, specimen preparation route, and units for each reported property. Without that granularity, comparing a lot against another grade or another supplier is not technically reliable.

    PropertyStandardClass-typical rangeVerification note
    DensityISO 1183-10.945–0.955 g/cm³Batch COA required
    Melt mass-flow rateISO 1133-1:20220.2–0.7 g/10 min at 190 °C/2.16 kgConfirm pellet lot and pre-drying state
    Tensile yield stressISO 527-222–28 MPaTest speed 50 mm/min
    Flexural modulusISO 178950–1200 MPaTest speed 2 mm/min
    Charpy notched impact, 23 °CISO 179-1/1eA15–35 kJ/m²Conditioning per standard
    ESCRASTM D1693 / ISO 22088-3Producer-lot minimum; no universal public valueMethod B or notched variation must be stated

    Where HHMTR-210HS is evaluated for pressure-service pipe, ISO 9080 hydrostatic testing and ISO 12162 classification become mandatory rather than optional. The producer’s lot certificate alone is insufficient to establish a pressure rating without independent long-term failure data at 80 °C and 60 °C test temperatures. If such data are unavailable, the grade cannot be legitimately assigned as PE80, PE100, or any other ISO pressure class solely on the basis of short-term tensile or density values.

    When Bimodal HDPE Replaces Unimodal Resins in Slow Crack Growth Service

    The practical advantage of a bimodal or broad-molecular-weight-distribution HDPE of this class is the separation of high-molecular-weight chains for slow crack growth resistance from lower-molecular-weight chains for processability. In extruded pressure pipe, this architecture supports sustained hoop stress resistance under ISO 9080 endurance conditions. In contrast, a unimodal film grade with similar density but higher melt flow rate generally exhibits lower melt strength, reduced notched ESCR, and narrower processing latitude during vacuum sizing. The HHMTR-210HS designation should therefore not be treated as interchangeable with standard unimodal HDPE film or injection molding resins without a documented substitution study covering pipe creep, impact, and hydrostatic performance.

    Production-scale behavior of this HDPE class in grooved-feed single-screw extruders with L/D 25:1 to 30:1 has been characterized by melt pressure buildup between 20 MPa and 35 MPa at screw speeds above 110 rpm. Breaker plate screens of 80 mesh or finer may accumulate gel at elevated residence time. Barrel temperature profiles are commonly set from rear to front as 160–190 °C, 190–210 °C, and 205–210 °C at the die. Actual settings require adjustment based on screw design, throughput, and melt pump backpressure. Preheat hoppers are not usually required below 60% RH, but drying at 80 °C for 2 h in a desiccant hopper dryer is advised when ambient humidity exceeds 60% RH because pellet surface moisture can generate extrudate splay and degrade weld-line integrity.

    Injection molding of HHMTR-210HS is constrained by its relatively low melt flow rate. Thin-wall containers or closures with flow length-to-thickness ratios above 150:1 are not recommended without elevated melt temperature and high injection velocity. The product’s application envelope is therefore more compatible with thick-section articles, stiffening ribs, and technical profiles than with fast-cycle packaging. For injection molding evaluations, a reciprocating screw with 18:1 to 22:1 L/D and compression ratio 2.5:1 to 3.0:1 provides acceptable plasticating for test plaques; actual shrinkage and warpage must be measured against ISO 294-4, not inferred from generic HDPE data.

    Extrusion Barrel Temperature Windows and Screw Torque Observations

    The melt temperature remains stable when the extruder is operated within the producer’s recommended discharge range, typically 200–220 °C for densely packed profiles. Above 230 °C, oxidative chain scission may reduce melt strength and shift the molecular weight distribution toward lower viscosity, compromising long-term strength even when short-term tensile values remain within specification. The use of melt filtration with 60–100 μm mesh is adequate for profile applications, while pressure-pipe lines generally require finer filtration to reduce contaminant-initiated slow crack growth.

    The grade’s rheological behavior is best characterized by capillary rheometry under ISO 11443. In class-typical HDPE of this MFR window, apparent viscosity at 190 °C and 100 s⁻¹ may fall between 1500 Pa·s and 2500 Pa·s. These values are not a producer specification but serve as a process audit tool to detect batch drift, particularly when pellet blending has been performed on-site. A change in melt pressure at constant screw speed exceeding 10% against the incoming control chart warrants a full lot re-evaluation under ISO 1133-1:2022 and density determination under ISO 1183-1 before continued use in load-bearing applications.

    The HHMTR-210HS product should not be combined with amine-based processing aids unless the producer has explicitly cleared the combination. Amine-functional additives can deactivate phenolic stabilizers and accelerate oxidative degradation in long-service HDPE. Similarly, blending with regrind originating from UV-stabilized black pipe compounds may alter the molecular weight distribution and ESCR response. The percentage of internal regrind should be limited to the producer’s written recommendation and validated by spiral flow testing or extrusion trials under normal production backpressure.

    Comparative Differentiation from Film, Blow Molding, and Injection Grades

    Compared with HDPE blown film grades that typically exhibit melt flow rates from 0.5 g/10 min to 2.0 g/10 min at 190 °C/2.16 kg, HHMTR-210HS has a lower MFR and greater melt strength, enabling annular or profile extrusion without excessive drawdown. Compared with extrusion blow molding grades of density 0.949–0.956 g/cm³, the HS suffix likely indicates higher flexural modulus and reduced creep under load, but this must be confirmed through producer data because suffix nomenclature is not harmonized across global HDPE suppliers. Injection molding grades, by contrast, typically require MFR values above 3 g/10 min for thin-wall filling. HHMTR-210HS is therefore not an injection molding resin and should not be selected for high-flow tooling.

    ParameterHMTR-210HS classHDPE film gradeHDPE blow molding gradeHDPE injection grade
    MFR, 190 °C/2.16 kg0.2–0.7 g/10 min0.5–2.0 g/10 min0.2–0.8 g/10 min3–10 g/10 min
    Dominant processing routeExtrusion, pipe/profileBlown filmExtrusion blow moldingInjection molding
    ArchitectureBroad or bimodal MWD expectedUnimodal typicalBroad MWD typicalNarrow MWD typical
    Failure mode emphasisSlow crack growth, hoop stressDart drop, tearParison sag, top-loadRapid fill, weld line strength

    For extruded pressure pipe producers, HHMTR-210HS may offer a balance of stiffness and long-term creep resistance that is absent in high-MFR film grades. The substitution of a film or blow molding resin into a pipe line without compensating for melt strength and ESCR can produce sink marks, wall-thickness variation, and reduced hydrostatic failure time under ISO 9080. Conversely, replacing fast-cycle injection grades with HHMTR-210HS in multi-cavity molds creates short shots, high injection pressure, and excessive shear heating unless gate and runner geometry are redesigned. Therefore the product should be evaluated against the intended application’s governing standard, not on the basis of density alone.

    The regulatory compliance position of HHMTR-210HS is customarily addressed through producer declarations for European food-contact use under Regulation (EU) 10/2011 or United States use under FDA 21 CFR 177.1520, where applicable. Chemical inventory compliance may be documented under REACH and RoHS 2011/65/EU annexes. Because additive packages vary by lot and regional supply, the converter must obtain the producer’s current regulatory declaration for every shipment. No performance claim in this document creates a food-contact, potable water, or pressure-pipe certification for HHMTR-210HS; sector-specific approvals are separate and must be supported by test reports from an ISO 17025-accredited laboratory.

    Processors using ISO 9080-validated pipe compounds often run a 100-hour pressure test at 80 °C under the intended hoop stress to screen incoming lots before full production. In such screening, specimens extruded from HHMTR-210HS may show ductile failure rather than brittle failure when the gel level and regrind fraction are controlled. A sudden shift to brittle failure is a functional indicator of contamination or thermal degradation and should trigger a halt for raw material and extruder audit. This industrial practice provides an operational boundary: the resin is not interchangeable with unspecified post-consumer recyclate in pressure applications unless continuous physical property testing is implemented.

    For corrugated drainage pipe and rigid sheet applications, the product’s stiffness class reduces wall thickness requirements only when the producer’s flexural modulus data justify the redesign under the relevant construction product standard. Designers should not assume a modulus increase from a suffix designation; they should instead request the producer’s comparison table of HHMTR-210HS against the previously qualified grade, including specimen preparation and conditioning history. If no such table is available, the substitution protocol under ISO 178 and ISO 527-2 must be executed on matched specimens.

    Top