| HS Code | 783484 |
| Density | 0.944 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.18 g/10 min |
| Tensile Yield Strength | 23 MPa |
| Elongation At Break | ≥600% |
| Flexural Modulus | 1000 MPa |
| Vicat Softening Temperature | 125 °C |
| Environmental Stress Cracking Resistance | ≥1000 h |
| Oxidation Induction Time | ≥20 min |
| Carbon Black Content | 2.0-2.5% |
| Moisture Content | ≤0.1% |
| Bulk Density | 0.55 g/cm³ |
| Ash Content | ≤0.1% |
| Mrs Classification | PE80 |
As an accredited Shanghai Jinfei HDPE HHM-TR144 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Shanghai Jinfei HDPE HHM-TR144 is packaged in 25 kg multiwall bags, with 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Shanghai Jinfei HDPE HHM-TR144, 25 kg bags, palletized, shrink-wrapped, securely stowed for ocean export. |
| Shipping | Shanghai Jinfei HDPE HHM-TR144 is a high-density polyethylene grade supplied in 25 kg woven bags, stacked on pallets, shrink-wrapped. It ships as non-hazardous general cargo in clean, dry containers, protected from moisture, sunlight, and heat. Standard ocean or truck transport is suitable with stable stacking and clear labeling. |
| Storage | Store Shanghai Jinfei HDPE HHM-TR144 in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep material in original sealed bags or containers, on pallets, off the floor, and away from moisture, dust, oils, and other contaminants. Maintain stable temperature, avoid excessive stacking, use first-in, first-out rotation, and follow local regulations. |
| Shelf Life | Shanghai Jinfei HDPE HHM-TR144 has a typical shelf life of 24 months under dry, cool, sealed storage away from sunlight. |
In the high-molecular-weight HDPE blown film segment, Shanghai Jinfei HDPE HHM-TR144 is processed on high-stalk extrusion lines rather than conventional low-stalk LDPE lines. The resin is supplied as a granular, high-molecular-weight, high-density polyethylene with density in the 0.946 g/cm³ to 0.950 g/cm³ class under ISO 1183-1 and a 21.6 kg melt flow rate below 10 g/10 min under ISO 1133-1. These values place it in the film-grade HMW-HDPE category where bubble stability and melt strength determine usable gauge. For T-shirt grocery sacks, converters meter 10 parts to 20 parts of clean in-house edge trim regrind per 100 parts of virgin resin. Pigmentation is achieved with 4 parts to 6 parts of a 50% color masterbatch for opaque or tinted film. A silica-based antiblock masterbatch is added at 1 part to 2 parts to prevent film-to-film blocking, and erucamide slip masterbatch at 0.5 part to 1.0 part lowers coefficient of friction. The formulation is conveyed through a grooved-feed single-screw extruder with L/D between 24:1 and 30:1, using a die gap of 0.8 mm to 1.5 mm for 10 µm to 25 µm final gauge. Blow-up ratios are held between 3:1 and 5:1. Frost line height is maintained between 500 mm and 900 mm in a high-stalk bubble configuration. Melt temperature is controlled between 190 °C and 220 °C, and excursions above 230 °C are avoided to limit oxidative degradation. Mechanical properties are tested according to ASTM D1709 for dart drop, ASTM D882 for tensile yield and break, ASTM D1922 for Elmendorf tear, and ASTM D1894 for coefficient of friction. Food-contact compliance for grocery sacks intended for direct produce contact is typically verified against FDA 21 CFR 177.1520 and GB 9685-2016 where applicable. End products include die-cut T-shirt bags, produce roll bags, and light-duty merchandise bags. The process is sensitive to ambient air turbulence; a ±5 °C fluctuation in room air temperature can move the frost line enough to alter thickness profile.
Institutional can liner film made from HHM-TR144 is commonly compounded with 15 wt% to 30 wt% of a C4-LLDPE having density 0.918 g/cm³ to 0.922 g/cm³ to raise dart impact and Elmendorf tear. The LLDPE reduces melt strength and can destabilize the high-stalk bubble if it is dosed above 30 wt%. Carbon black masterbatch containing 40% carbon black is metered at 5 parts to 6 parts per 100 parts of resin to produce 2.0% to 2.5% final carbon black for opacity and UV resistance. The blown film line is configured with a 100 mm to 300 mm die, die gap of 1.2 mm to 2.0 mm, and blow-up ratio of 2.5:1 to 3.5:1. Internal bubble cooling is used to stabilize frost line height between 400 mm and 700 mm. Melt temperature is held at 195 °C to 215 °C. Film thickness for can liners ranges from 20 µm to 40 µm, with heavier service liners at 50 µm to 60 µm. Dart impact is measured under ASTM D1709, and tear resistance is measured under ASTM D1922; converter specifications vary by end-user drop test and liner fill weight. For non-food refuse contact, mechanical and chemical safety are demonstrated through REACH (EC) No 1907/2006 and RoHS Directive 2011/65/EU. End products include star-sealed can liners, flat-pack trash bags, and drawstring refuse sacks. The main failure mode on high-output lines is bubble chatter when LLDPE content exceeds 25 wt% and frost line height is not compensated; this appears as alternating thick and thin bands in the collapsed film. Processors therefore limit LLDPE to 20 wt% for high-speed lines and adjust internal bubble cooling air temperature rather than raising extruder speed.
Blown film for frozen food packaging and cereal liners is formulated with tighter additive ceilings than retail sack film. The resin is processed without recycled content in most food-contact structures. Slip is limited to 300 ppm to 800 ppm erucamide or 500 ppm to 1000 ppm behenamide. Silica antiblock is maintained at 1000 ppm to 2000 ppm. These concentrations are low enough to satisfy overall migration limits under EU 10/2011 for general food contact, while retaining film opening properties on high-speed form-fill-seal equipment. Melt temperature is kept between 190 °C and 205 °C to reduce oxidative degradation products that can create off-odour. The bubble is run in high-stalk geometry with blow-up ratio 3:1 to 4:1 and frost line height 600 mm to 900 mm. Die gap is typically 1.0 mm to 1.5 mm for 20 µm to 50 µm finished film. The film is tested for migration according to EN 1186-1 and for sensory carry-over on sensitive food simulants. FDA 21 CFR 177.1520(c) 2.1 covers polyolefin resins used as food contact articles at room temperature and below. GB 9685-2016 governs additive positive lists for China-bound packaging. The end products include frozen vegetable bags, ice cream overwrap film, cereal liner tubes, and bakery tissue replacement film. The processing limitation is that melt temperatures above 210 °C increase gel specks and odour-causing oxidation products; screens should be checked after each shift when running high-slip food film.
| Regulatory/Test Domain | Standard Designation | Verification Requirement |
|---|---|---|
| EU food contact | EU 10/2011 | Overall migration per EN 1186-1; limit 10 mg/dm² |
| US food contact | FDA 21 CFR 177.1520(c) 2.1 | Resin identity and extraction limits per regulation |
| China additive compliance | GB 9685-2016 | Specific migration limits per additive positive list |
| Coefficient of friction | ASTM D1894 | Film-to-film kinetic and static COF |
For heavy-duty industrial liners at 60 µm to 150 µm, the gauge itself shifts the conversion line away from high-stalk thin-gauge geometry. The extruder is typically a 65 mm to 90 mm grooved-feed single-screw machine with L/D 24:1 to 30:1. Die gap is widened to 1.6 mm to 2.5 mm, and blow-up ratio is reduced to 1.8:1 to 2.5:1 to maintain thick-film bubble stability. Frost line height is lowered to 300 mm to 500 mm. Carbon black masterbatch is added at 5 parts to 6 parts per 100 parts of HMW-HDPE to obtain 2.0% to 2.5% carbon black for UV stabilization. Clean edge trim and post-industrial reprocessed film are introduced at 10 wt% to 25 wt%, but higher regrind increases gels and bubble instability. A fluoropolymer processing aid is dosed at 300 ppm to 800 ppm when extruder head pressure exceeds 60 MPa or when melt fracture appears at the die lip. No slip agent is used for stacked liners because low coefficient of friction can cause pallet slippage. The finished film is tested for dart impact under ASTM D1709, puncture resistance under ASTM D4833, and tear under ASTM D1922. End products include drum liners, compactor bags, FIBC inner liners, and waste containment films. The operational boundary is that carbon black dispersion must be checked under ISO 18553; undispersed carbon black acts as a stress concentration site and reduces puncture resistance.
Thin-gauge rollstock for produce bags and wicket-mounted packaging is run with a die gap of 0.8 mm to 1.1 mm and a blow-up ratio of 4:1 to 5:1. The high-stalk bubble is extended to 600 mm to 1000 mm frost line height to develop machine-direction orientation and load-bearing capacity in films as thin as 8 µm to 15 µm. A narrower molecular weight distribution in the resin maintains melt strength under this long-stalk geometry. The formulation is kept lean: 1 part to 2 parts of silica antiblock masterbatch, 0.5 part to 1.0 part of slip masterbatch, and 2 parts to 3 parts of color masterbatch. Regrind is limited to 10 wt% or less because thin-gauge bubbles tolerate fewer gel particles before film breaks occur. Extruder temperatures are set from 190 °C at the feed zone to 210 °C at the die. Oscillating haul-off or reversing winders are used to spread thickness variation. The film is tested under ASTM D882 for tensile, ASTM D1709 for dart impact, and ASTM D1922 for tear. Food-contact grades for produce bags are verified under FDA 21 CFR 177.1520 and EU 10/2011 where required. End products include perforated produce rollstock, dry-cleaning protective film, and thin-gauge textile packaging. The main process failure is bubble snap at the frost line when ambient air temperature varies by more than ±3 °C; closed-loop air ring temperature control is required for stable production.
Competitive Shanghai Jinfei HDPE HHM-TR144 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Shanghai Jinfei HDPE HHM-TR144 is a high-density polyethylene pipe compound designated for pressure piping in buried water, gas, and industrial fluid networks. The resin is evaluated under ISO 12162:2009 within the PE100 class, which requires a minimum required strength of 10.0 MPa at 20°C for a 50-year service life when tested under ISO 9080:2012. This classification separates it from lower hydrostatic design basis resins such as PE80 and from high-flow high-density polyethylene grades used in injection molding or film, which lack the slow crack growth resistance required for long-term pressure service. Grade-specific density, melt flow rate, tensile, impact, and hydrostatic data are batch-dependent; the manufacturer’s certificate of analysis and third-party batch certification should be used for acceptance decisions. The technical envelope described below is derived from public PE100 pipe-compound requirements and production-scale practices rather than a single proprietary datasheet, because published data for HHM-TR144 in some large-diameter configurations is limited.
The designation HHM-TR144 consists of a manufacturer-specific HDPE pipe-grade code. The prefix HHM is used in certain Chinese polyethylene plants for high-density pipe compounds, while TR144 denotes a product variant. The ISO PE100 classification is not encoded directly in the designation; therefore, specification engineers should verify that the grade appears on an approved list for the relevant water or gas standard. In Chinese water-supply projects, this includes GB/T 13663.2-2018; for gas, GB 15558.1. The grade is typically supplied as natural or black compound with carbon black dispersion meeting ISO 4427 and ISO 4437 requirements for weathering resistance. The table below is a screening matrix for PE100 pipe compounds, not a batch certificate for HHM-TR144.
| Property | Test method | Class requirement or acceptance window |
|---|---|---|
| Density | ISO 1183-1:2019 | 0.949–0.953 g/cm³ |
| Melt flow rate | ISO 1133-1:2022 at 190°C, 5 kg | 0.10–0.20 g/10 min |
| Tensile yield stress | ISO 527-2:2012 | ≥ 22 MPa |
| Elongation at break | ISO 527-2:2012 | ≥ 350% |
| Charpy notched impact strength at 23°C | ISO 179-1:2010 | ≥ 20 kJ/m² |
| Charpy notched impact strength at -30°C | ISO 179-1:2010 | ≥ 10 kJ/m² |
| Slow crack growth resistance | ISO 13479:2009 | ≥ 500 h at 80°C, 4.0 MPa |
| Oxidation induction time at 200°C | ISO 11357-6:2018 | ≥ 20 min |
| Carbon black content | ISO 6964:2019 | 2.0–2.5 wt% for black pipe compound |
For incoming quality control, HHM-TR144 is typically assessed for density and melt flow rate because these parameters indicate batch-to-batch variation and can shift extrusion output, wall thickness, and fusion behavior. The manufacturer-specific suffix TR144 does not replace the PE100 designation; both should be verified on the technical datasheet before material substitution.
Pipe extrusion of PE100-class high-density polyethylene such as HHM-TR144 typically occurs on grooved-barrel single-screw extruders with an L/D ratio of 30:1 or greater. The grooved-feed section generates high conveying forces that are required for low-MFR, high-molar-mass HDPE; screw compression ratios in the range 2.5:1 to 3.5:1 are typical for pipe-grade compounds. Production-scale behavior on bimodal PE100 resins of similar melt flow and density shows that barrel set temperatures are commonly held at 180°C in the feed zone, 200°C in the compression zone, and 210°C in the metering zone. Melt temperature at the die entry should not exceed 230°C, because thermo-oxidative degradation accelerates rapidly above this threshold and produces gel particles that appear as surface defects in the pipe wall. During line stoppages, residence time at temperatures above 220°C should be kept below 10 min. Screw backpressure is typically maintained between 15 MPa and 25 MPa to homogenize the melt and to stabilize output; however, published data for HHM-TR144 specifically in this pressure range is limited, so start-up trials should record melt-pressure variance before locking the process window.
Moisture control for HDPE pipe compounds is often underestimated. Although HDPE has low equilibrium moisture absorption, condensation on cold granulate can occur in humid production halls. When storage relative humidity exceeds 60%, hopper drying at 80°C for 2 h is recommended before extrusion. Surface moisture introduced into the feed throat can be converted to steam in the compression zone, producing microvoids and internal roughness in thick-walled pipe. The die land length ratio should be at least 10:1 and preferably 12:1 to reduce melt fracture at high output; die-lip exit temperatures below 210°C increase the risk of sharkskin, particularly on thin-wall SDR 17 and SDR 21 pipe. Vacuum calibration with segmented spray cooling is used to stabilize dimensions and to control sag in diameters above 315 mm. For solid-wall pipe in SDR 11 or SDR 17, line speed is normally governed by heat removal from the pipe wall and by wall-thickness tolerance rather than by extruder throughput. Gravimetric feeding, melt-temperature sensing at the adapter, and melt-pressure monitoring before the screen changer are standard controls because a batch-to-batch melt flow rate shift of 0.02 g/10 min can produce measurable changes in screw motor load and output stability.
The broad molecular weight distribution of PE100-class compounds such as HHM-TR144 produces pronounced shear thinning at extrusion shear rates between 100 s⁻¹ and 1000 s⁻¹. This behavior permits higher output on grooved-barrel extruders than the low melt flow rate would imply, but it also narrows the temperature window for stable, melt-fracture-free operation. Die swell is generally higher than that of unimodal HDPE, so sizing sleeve clearance and haul-off speed must be adjusted during start-up. In-plant regrind from trimmings and off-spec pipe should not exceed 10% by weight unless the resulting compound is re-validated by long-term hydrostatic testing under ISO 9080:2012, because slow crack growth performance is sensitive to molecular weight distribution and to the presence of degraded regrind.
In buried potable-water service, HHM-TR144 is evaluated against ISO 4427-2:2019 and, in China, GB/T 13663.2-2018. The PE100 class permits a design stress of 8.0 MPa at 20°C for water when the overall service coefficient is 1.25, yielding pressure ratings of 16 bar for SDR 11, 10 bar for SDR 17, and 6.4 bar for SDR 26. Pipe stiffness values decrease with higher SDR, so buried installations in high-traffic zones may require a compacted sand pad or geogrid support; the pipe itself remains flexible and responds to soil load by deflecting rather than by brittle failure. For gas distribution, HHM-TR144 is evaluated under ISO 4437-2:2014 and GB 15558.1. Gas service adds the requirement for resistance to rapid crack propagation, often assessed by the full-scale small-scale steady-state test ISO 13477:2008 at temperatures of 0°C or lower, and by full-scale testing under ISO 13478:2007 for critical pressure assignment. The material is also used in industrial slurry and drainage lines where the high molar mass and toughness of PE100 resins provide better abrasion resistance than PE80, but chemical compatibility with aggressive streams must be confirmed under ISO/TR 10358. Swelling, environmental stress cracking, and oxidative attack are possible with aromatic hydrocarbons, concentrated acids, and strong oxidizers at elevated temperatures.
Jointing of HHM-TR144 pipe is performed by butt fusion under ISO 21307:2017 or by electrofusion under ISO 12176-2:2012. The high molecular weight of PE100 pipe grades does not prevent fusion, but it requires tight control of interfacial pressure and melt bead geometry. Cold welds are a documented field failure mode; they cannot be detected by visual inspection alone and are caused by insufficient melt interface temperature or contamination. For municipal water networks, HHM-TR144 pipe is commonly joined by butt fusion to produce a monolithic system that eliminates mechanical leak points under differential ground settlement. Coiling of HHM-TR144 pipe is practical in diameters up to 160 mm; larger diameters are supplied in straight lengths because residual bending stresses can reduce long-term hydrostatic performance.
Published data for HHM-TR144 in diameters above 800 mm is limited. Designers should not linearly extrapolate small-diameter hydrostatic data to large-diameter pipes without full-scale cone or burst tests. In large-diameter pressure applications, the critical failure modes shift from ductile bursting to rapid crack propagation and slow crack growth from stress concentrations at wall-thickness variations; therefore, batch-specific hydrostatic tests and full-scale tests are required for municipal trunk mains and gas transmission lines.
Substituting HHM-TR144 for a PE80 compound changes the hydraulic design basis. Under ISO 12162:2009, PE80 carries a minimum required strength of 8.0 MPa, while PE100 carries 10.0 MPa. At the same overall service coefficient of 1.25, the design stress rises from 6.3 MPa to 8.0 MPa. This permits a thinner wall at a given pressure rating, reducing material consumption and increasing internal bore for gravity-assisted drainage. The trade-off is a narrower processing window and greater sensitivity to regrind-induced degradation.
| Parameter | PE80 class | PE100/HHM-TR144 class |
|---|---|---|
| MRS per ISO 9080:2012 | 8.0 MPa | 10.0 MPa |
| Design stress at 20°C, C=1.25 | 6.3 MPa | 8.0 MPa |
| SDR 11 pressure rating | 12.6 bar | 16 bar |
| SDR 17 pressure rating | 8 bar | 10 bar |
Compared with North American PE4710 materials classified under ASTM D3350-21, the ISO PE100 classification is not directly interchangeable. PE4710 uses a hydrostatic design basis at 23°C and 60°C with cell classification values for density, melt index, flexural modulus, tensile strength, and environmental stress-crack resistance. HDPE HHM-TR144 may satisfy PE4710 performance in many respects, but dual-listing requires independent testing under ASTM D2837 and ASTM D3350-21; published data for this specific configuration is limited. The substitution should be evaluated against pipe stiffness, rapid crack propagation resistance, and local installation codes before specification change.
In comparison with unimodal high-flow HDPE grades used for injection molding or thin-wall containers, HHM-TR144 has a much lower melt flow rate, typically below 0.20 g/10 min at 190°C/5 kg. This limits the material’s suitability for complex injection-molded fittings and for extrusion processes requiring high-speed melt flow; instead, fittings for HHM-TR144 pipe networks are often produced from compatible high-flow PE100 or PE80 electrofusion compounds that meet the same long-term standard requirements. The low melt flow rate improves melt strength during pipe extrusion but increases shear heating; therefore, extruder temperature set points and screw speed must be derived from melt-temperature measurements rather than barrel temperature settings alone.
For gas transmission and large-diameter water trunk mains, the critical property is not short-term tensile strength but resistance to rapid crack propagation. Small-scale Charpy impact tests under ISO 179-1:2010 provide a quality-control indicator, but they do not replace full-scale testing. The small-scale steady-state test ISO 13477:2008 pressurizes a pipe section at low temperature and measures the arrest of a rapid crack. HHM-TR144, as a PE100 pipe compound, is expected to be formulated for arrest toughness, but published data for this specific configuration is limited; therefore, full-scale validation on the actual pipe diameter and wall thickness is required when the operating temperature falls below 0°C or when the diameter exceeds 315 mm. Failure to conduct full-scale testing can result in catastrophic line failure because a propagating crack can run for hundreds of metres before arrest if the material toughness is insufficient. The same concern applies when high-speed impact from excavation equipment or third-party damage initiates a crack in pressurized pipe.
Operational boundaries for HHM-TR144 storage and processing require protection from ultraviolet radiation for extended outdoor exposure. PE100 pipe compounds are commonly protected with carbon black or with hindered amine stabilizer packages, but black compounds remain preferred for above-ground storage exceeding 12 months. The material should not be combined with amine-based anti-static concentrates or oxygenated process oils because these additives can shorten oxidation induction time under sustained thermal load. Avoid contact with strong oxidizing acids such as concentrated nitric acid at temperatures above 40°C, and avoid aromatic solvents such as benzene and toluene, which induce swelling and reduce hydrostatic strength. When joining HHM-TR144 pipe by butt fusion, interfacial pressure should be controlled according to ISO 21307:2017 with bead geometry verified by production tests; deviations from the specified fusion pressure can lead to cold welds that are not detectable by visual inspection alone.
For batch-to-batch consistency, incoming resin should be tested for melt flow rate and density; oxidation induction time may be measured by ISO 11357-6:2018 to detect stabilizer depletion. Published data for HHM-TR144 specific to oxidation induction time and rapid crack propagation are limited; critical pressure-pipe projects should require batch certificates covering full ISO 9080:2012 validation and not rely on nominal grade identity alone.