Shandong Yulong Hdpe Hd Tr144

Shandong Yulong HDPE HD-TR144

    • Product Name: Shandong Yulong HDPE HD-TR144
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 440409
    Density 0.944 g/cm³
    Melt Flow Rate 0.18 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield ≥24 MPa
    Tensile Strength At Break ≥30 MPa
    Elongation At Break ≥600%
    Flexural Modulus ≥1000 MPa
    Notched Izod Impact Strength ≥200 J/m
    Vicat Softening Point ≥120°C
    Heat Deflection Temperature ≥70°C
    Environmental Stress Cracking Resistance ≥1000 h
    Shore D Hardness 60
    Water Absorption ≤0.01%
    Melting Point 130-135°C
    Crystallinity ≥70%
    Bulk Density ≥0.50 g/cm³
    Ash Content ≤0.05%
    Moisture Content ≤0.05%
    Thermal Conductivity 0.4 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2×10⁻⁴ /°C
    Dielectric Constant 2.3
    Dielectric Strength 20 kV/mm
    Volume Resistivity >10¹⁶ Ω·cm
    Chemical Resistance Excellent

    As an accredited Shandong Yulong HDPE HD-TR144 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Shandong Yulong HDPE HD-TR144 is typically packaged in 25 kg PP woven bags, with 1,000 kg jumbo bags also available.
    Container Loading (20′ FCL) 20′ FCL loading for Shandong Yulong HDPE HD-TR144: typically 25 MT in 25 kg bags, unpalletized, subject to final packing.
    Shipping Shandong Yulong HDPE HD-TR144 is typically shipped in 25 kg PP woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport as non-hazardous cargo in clean, dry trucks or containers. Store cool, dry, ventilated, away from moisture, sunlight, and heat. Keep packaging sealed.
    Storage Store Shandong Yulong HDPE HD-TR144 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizing agents. Keep original bags/containers tightly closed and palletized. Prevent moisture, dust, oil, and chemical contamination. Avoid prolonged UV exposure and excessive stacking. Maintain clean handling areas, control static, and follow local regulations and supplier SDS recommendations.
    Shelf Life Shandong Yulong HDPE HD-TR144 has a shelf life of 24 months when stored cool, dry, ventilated, and away from sunlight.
    Application of Shandong Yulong HDPE HD-TR144

    Where HD-TR144 is introduced into municipal pressure pipe extrusion, the first processing limit is not melt flow stability but the maintenance of a homogeneous gel-free melt at the die entry. A high-molecular-weight HDPE of this type is typically processed on a single-screw extruder with a 30:1 to 33:1 L/D ratio and a barrier screw, with barrel zones from 180 °C to 220 °C and the adaptor/die held between 200 °C and 215 °C. Lower melt temperatures, particularly below 190 °C, increase die swelling and produce surface melt fracture that is not corrected by haul-off speed alone; higher temperatures above 230 °C accelerate thermo-oxidative chain scission and reduce the slow crack growth resistance measured by ISO 13479 notched pipe testing. The extrusion line should use vacuum sizing with calibrated sleeves and a closed-loop water temperature system maintained at 15–25 °C; the melt pressure before the screen changer should remain within 10–25 MPa as a practical window for preserving high output without excessive shear heating. These parameters are line-specific and must be confirmed against the HD-TR144 certificate of analysis; the ranges above represent the normal operating envelope for high-molecular-weight HDPE pressure-pipe extrusion.

    Compounding for potable water pipe uses a carbon black masterbatch at 2.0–2.5 wt% to provide ultraviolet stabilization, and where extended outdoor storage is specified an antioxidant masterbatch is added at 0.05–0.15 wt% only after lot-specific oxidation induction time data is reviewed under ISO 11357-6. For gas distribution grades, in-house regrind is limited to ≤10 wt% because higher levels broaden the molecular weight distribution and shift the hydrostatic design basis. The finished pipe is converted into SDR 11 and SDR 17 pressure pipe for potable water mains, industrial water lines, and gas distribution networks under ISO 4427, EN 12201, ISO 4437, ASTM D3350, and NSF/ANSI 61.

    Standard / Test MethodApplication Requirement
    ISO 4427-2PE100 pipe dimensions and material designation for water supply
    ISO 9080Long-term hydrostatic strength regression for MRS classification
    ISO 13479Notched pipe slow crack growth resistance
    ASTM D3350HDPE cell classification for PE4710 pipe-grade resin
    NSF/ANSI 61Potable water contact health effects
    ISO 4437Gaseous fuel distribution pipe systems

    What Controls Carbon Black Dispersion and Thickness Uniformity in HD-TR144 Geomembrane Sheet?

    Flat-die extrusion of HD-TR144 into geomembrane roll stock is not governed solely by the resin melt index but by the ability of the compounding step to develop carbon black dispersion without creating microgels that later initiate stress cracking at the edge of a welded seam. A masterbatch addition of 2.0–3.0 wt% carbon black is typical, with the exact ratio set by the requirement in GRI-GM13 that the sheet maintain 2.0–3.0 wt% total carbon black content after letdown; the base resin should not be combined with low-molecular-weight waxes at more than 0.1 wt% because die lip plate-out becomes visible within 4–6 h of continuous running. The downstream process uses a flat die with automatic lip adjustment, a three-roll stack held at 70–90 °C, and beta or X-ray thickness scanning; sheet thickness is typically 1.5–3.0 mm, and the on-line tolerance window is maintained at ±10% of nominal thickness to meet ASTM D5199 nominal thickness control.

    Compliance for waste containment geomembrane liners is verified under GRI-GM13, ASTM D1505 density, ASTM D1238 melt flow rate, ASTM D638 tensile properties, ASTM D1004 tear resistance, and ASTM D4833 puncture resistance. Terminal products include single- and double-textured HDPE geomembrane liners for landfill cells, heap leach pads, and industrial ponds.

    During accumulator-head blow molding of HD-TR144 into 220 L L-ring drums, the first process adjustment is the parison programming curve for the shoulder and chime sections, not for the cylinder wall alone. The resin is processed at a melt temperature of 180–210 °C with a die gap of 2.5–7.0 mm, blow pressure of 0.6–0.9 MPa, and mold cooling water at 8–15 °C; shot capacity on accumulator machines for 220 L drums typically requires a clamp force of 1,000–3,000 kN. The formulation is usually limited to a UV/color masterbatch at 0.5–2.0 wt%, and any post-consumer regrind is restricted to ≤30 wt% when the finished container must pass UN 1H1 or UN 1H2 drop and stacking tests. For food-contact configurations, the compound and colorant must meet FDA 21 CFR 177.1520 and, where applicable, EU 10/2011 overall migration limits. Terminal output includes 220 L closed-head drums, 1,000 L IBC inner bottles, and 20–60 L jerry cans for industrial chemical packaging.

    If a Vacuum-Forming Corrugator Is Used for HD-TR144 Stormwater Pipe

    When HD-TR144 is run on a vacuum-forming corrugator, the dominant process variable is the vacuum differential across the mold blocks because the polymer must be drawn into the corrugation ribs before the outer wall solidifies. A carbon black masterbatch at 2.0–2.5 wt% is standard for outdoor weatherability, and a fluoropolymer processing aid at 0.02–0.05 wt% can be used to reduce die build-up; in-house regrind from edge trim and start-up scrap should not exceed 20 wt% to avoid reducing rib stiffness. Extrusion temperatures are maintained at 190–220 °C, vacuum levels at −0.03 to −0.06 MPa, and corrugator mold block speed is set to match the haul-off rate so that the formed rib height remains within the dimensional tolerance required by ASTM F2306 and AASHTO M294 for 100–600 mm diameters. Terminal products are double-wall corrugated drainage pipe, stormwater culverts, and subsurface retention/detention piping. Compliance includes ASTM F2306, AASHTO M294, and EN 13476-3 where European specifications apply.

    Cable Duct Extrusion: Wall Thickness Uniformity Under UL and NEMA Conduit Requirements

    HD-TR144 can be converted into corrugated or smooth-wall HDPE conduit where the line must control wall thickness at the inside radius of coiling bends. The formulation for outdoor-exposed cable duct uses carbon black at 2.0–2.5 wt%, and the extrusion process relies on a vacuum calibration tank with closed-loop water temperature at 15–25 °C and an ultrasonic wall-thickness scanner downstream. Screw speed and melt temperature are set within 180–220 °C; the die and calibration sleeve dimensions are adjusted to maintain an ovality below 1.5% for coilable duct diameters up to 200 mm. Compliance verification includes UL 651A, NEMA TC 7, and ASTM D3485 for smooth-wall coilable polyethylene conduit, while underground power cable duct often references NEMA TC 7 dimensional schedules and flammability limits. Terminal products are high-density polyethylene electrical conduit, telecommunications duct, and fiber-optic innerduct. For corrugated cable duct, the same resin may be run on a corrugator under conditions similar to those for drainage pipe, but published data for this specific configuration is limited and should be validated on the target line.

    Free Quote

    Competitive Shandong Yulong HDPE HD-TR144 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Shandong Yulong HDPE HD-TR144 is a high-density polyethylene pellet grade supplied for melt conversion on continuous extrusion and injection-moulding lines. The identification string HD-TR144 places the material within the high-density class defined by ISO 1872-1:2018; resins in this class are specified as having a density above 0.940 g/cm³ when measured after annealing under ISO 1183-1:2019. The operative specification boundary for any delivered lot is the certified batch certificate, not a generic trade listing. Lot-specific values for melt mass-flow rate at 190 °C/2.16 kg, tensile yield stress, and density are measured by ISO 1133-1:2022, ASTM D638-14, and ISO 1183-1:2019, respectively. Where published trade data conflicts with the batch certificate, the batch certificate controls.

    Conversion routes for HD-TR144-class materials include pressure pipe extrusion, solid-wall and corrugated drainage pipe, blow moulding of industrial containers, and thick-section profile extrusion. The grade is generally selected when the finished article must combine long-term hydrostatic strength, slow crack growth resistance, and stiffness retention. On production lines, the material is processed on grooved-barrel extruders with screw lengths of 30:1 to 36:1 or on injection-moulding machines with sufficient clamp force for the projected area. Melt temperature during pipe extrusion is maintained between 190 °C and 220 °C; injection moulding uses a wider window of 210 °C to 250 °C. These temperature windows are starting points for process validation and are not substitutes for the supplier’s lot-specific guidance.

    Material Identity, Specification Boundary, and Lot Release Framework

    The specification framework for HD-TR144 is best read across three layers: base resin properties, delivered compound state, and converted article performance. Base resin density is measured under ISO 1183-1:2019. Melt flow is reported as both mass-flow rate and volume-flow rate under ISO 1133-1:2022 and ISO 1133-2:2020. Mechanical properties are usually determined on compression-moulded sheets prepared under ISO 293:2004; tensile yield stress and elongation at break are tested under ASTM D638-14, flexural modulus under ASTM D790-17, and Charpy notched impact under ISO 179-1:2010. The short-term tensile data have limited value for pressure-pipe qualification. Long-term hydrostatic strength is evaluated by regression analysis under ISO 9080:2022, and the minimum required strength classification is assigned under ISO 12162:2009.

    Additive stabilisation is assessed by oxidation induction time under ISO 11357-6:2018. For black pressure-pipe formulations, carbon black content and dispersion are checked under ISO 6964:2019 and ISO 18553:2002. Density shifts within the HDPE class, for instance from 0.950 g/cm³ to 0.955 g/cm³, can alter short-term tensile yield stress and flexural modulus, but the slow crack growth response is governed more strongly by molecular weight distribution and tie-chain density. Therefore, a single density or melt-flow value is insufficient to define the grade; the molecular architecture, additive package, and conversion history must be considered together.

    Compliance and test framework for HD-TR144-class high-density polyethylene
    Property or compliance domain Primary standard or regulation Application-linked note
    Density and classification ISO 1183-1:2019, ISO 1872-1:2018 Confirms HDPE class above 0.940 g/cm³
    Melt mass-flow rate ISO 1133-1:2022 Measured at 190 °C/2.16 kg
    Tensile yield stress and elongation ASTM D638-14 Compression-moulded specimen
    Flexural modulus ASTM D790-17 Stiffness ranking
    Charpy notched impact ISO 179-1:2010 Toughness screening
    Environmental stress crack resistance ASTM D1693-15 Stress-cracking comparison
    Long-term hydrostatic strength ISO 9080:2022, ISO 1167-1:2006 Pressure-pipe qualification
    Carbon black content and dispersion ISO 6964:2019, ISO 18553:2002 Black pipe compound
    Thermal stability ISO 11357-6:2018 Oxidation induction time
    Food contact FDA 21 CFR 177.1520, EU Regulation 10/2011 If declared for the supplied formulation

    What Processing Parameters Govern Stable Extrusion of HD-TR144?

    Stable extrusion is governed by pressure control, melt-temperature uniformity, and the avoidance of melt fracture in the die land. On single-screw grooved-barrel extruders with 30:1 to 36:1 L/D, the grooved feed zone generates high conveying pressure and requires a barrier screw with distributive mixing elements to limit melt-temperature spikes above 230 °C. Die-head pressure for high-molecular-weight HDPE is higher than for unimodal film grades of the same melt-flow rate; back-pressure should be recorded at constant screw speed to separate screw-wear drift from lot-to-lot viscosity change. Melt temperature at the die entry is maintained between 190 °C and 220 °C for pipe extrusion, with the lower band used for thicker walls and higher melt strength. When output surpasses the critical shear rate, sharkskin or stick-slip melt fracture may appear. Die-lip chromium carbide treatment or a fluoropolymer processing aid at 200 to 600 mg/kg may reduce surface defects, but only after hydrostatic testing under ISO 1167-1:2006 confirms that surface defect initiation has been controlled.

    For injection moulding, a general-purpose polyolefin screw with a compression ratio near 2.5:1 to 3.5:1 and a shot size between 25% and 75% of barrel capacity is used. Melt temperature is set between 210 °C and 250 °C; lower temperatures reduce flow length, whereas higher temperatures increase energy use and degradation risk. Thick sections are cooled until ejection temperature is below the heat deflection temperature of the resin, and tool temperature is controlled between 10 °C and 40 °C. At shutdown, the machine is purged with a lower-viscosity polyolefin to reduce black-speck formation in stagnant hot-runner melt. Processing aid dosage, screw speed, and back-pressure settings should be re-established after any pellet change or shutdown to maintain dimensional consistency.

    Pressure pipe qualification from HD-TR144-class resin is performed at system level rather than on resin short-term tests alone. Pipes are subjected to sustained internal pressure at 20 °C and 80 °C under ISO 1167-1:2006 and ISO 1167-2:2010, with regression analysis under ISO 9080:2022 used to establish the lower predictive limit. For gas-distribution pipe, rapid crack propagation resistance is evaluated at low temperature under ISO 13477:2008. The slow crack growth response of a bimodal resin is generally superior to a unimodal material of equal density and melt flow, but weld-line orientation, wall-thickness distribution, and extrudate swell shift the stress state in the installed pipe. In corrugated drainage and cable ducting, melt-strength and swell consistency control corrugation depth; die-temperature variation of more than ±5 °C can produce visible wall-thickness changes. The die gap and calibration vacuum are therefore adjusted after any change in melt temperature or screw speed, not solely after dimensional feedback.

    When HD-TR144 Replaces a Unimodal HDPE in Pipe and Profile Extrusion

    When HD-TR144 replaces a unimodal HDPE of similar density on an existing pipe line, the operator should anticipate changes in die-head pressure, torque, melt temperature, and extrudate swell before dimensional changes appear. The replacement grade may have a bimodal molecular weight distribution with a higher high-molecular-weight fraction; this increases zero-shear viscosity and die swell relative to a typical unimodal material. Grooved-barrel extruders with 30:1 to 36:1 L/D are recommended because the positive feed pressure allows lower melt temperature and reduces shear heating. Die-head pressure at constant screw speed may be higher, and barrel temperatures should be reset to keep the melt between 190 °C and 220 °C. Raising output by screw speed alone is not advised because melt-fracture onset in bimodal HDPE often occurs at lower shear rates than in unimodal grades, and die-lip fouling increases if melt temperature falls below 180 °C. Dimensional control depends on thermal shrinkage and calibration; the vacuum tank and sizing sleeve positions must be re-centred because extrudate swell at the die exit changes the initial tube diameter.

    Mechanical property differences between HD-TR144 and a generic unimodal HDPE are most apparent in long-term tests, not short-term tensile values. Under ASTM D1693-15, a bimodal pipe-grade material may resist environmental stress cracking for longer than an equivalent density and melt-flow unimodal material; the exact improvement depends on stress concentration, notch depth, and test temperature. Under ISO 16770:2019, full-notch creep test failure time is used to rank slow crack growth resistance. A replacement grade is not accepted solely on higher density and flexural modulus because these values can mask a loss in tie-chain density if the molecular weight distribution and comonomer placement are not correct. Trials should include notched pipe tests under ISO 13479:2022 and full-scale hydrostatic tests under ISO 1167-1:2006 before lot-for-lot substitution is approved.

    Comparative behaviour: HD-TR144-class bimodal HDPE versus conventional unimodal HDPE at equivalent density
    Evaluation domain Unimodal HDPE reference HD-TR144 observed shift Test method or equipment
    Melt flow at 190 °C/2.16 kg Higher for same density Lower ISO 1133-1:2022
    Die swell and die-head pressure Lower Higher Grooved-barrel extruder, 30:1 L/D
    Slow crack growth Lower resistance Higher resistance ISO 16770:2019
    Notched pipe failure time Earlier Later ISO 13479:2022
    Rapid crack propagation Higher susceptibility Lower susceptibility ISO 13477:2008
    Flexural modulus at equal density Similar Similar to slightly higher ASTM D790-17
    Melt fracture onset Later Earlier within typical pipe outputs Visual or die-pressure measurement

    Thermal Degradation Pathways and Additive Stabilisation Limits

    Thermal degradation in HD-TR144 follows the standard polyolefin oxidative pathway: hydroperoxide formation, radical propagation, chain scission, and, in the presence of oxygen, carbonyl formation. The practical consequence is a reduction in melt viscosity, a shift in melt-flow rate, and surface oxidation of extrudate if barrel residence time is excessive or melt temperature exceeds 250 °C. Oxidation induction time under ISO 11357-6:2018 provides a comparative measure of stabiliser package efficiency, but it does not guarantee long-term thermal performance at service temperature. For pressure-pipe compounds, the thermal stabilisation system must withstand extrusion at 190 °C to 230 °C without consuming the antioxidant reserve needed for service life. Repeated recycling of in-house regrind above 20 wt% should be validated by melt-flow stability, tensile yield stress, and hydrostatic tests; uncontrolled regrind addition can shift the molecular weight distribution because of shear-induced chain scission and reduce slow crack growth resistance.

    Storage and handling boundaries also affect degradation. The resin is not hygroscopic, but surface moisture from outdoor storage or condensation can produce surface defects during extrusion. If storage relative humidity remains above 60%, drying in a desiccant hopper dryer at 80 °C for 2 h to 4 h is applied before processing. Prolonged exposure to ultraviolet light degrades unprotected HDPE; if the supplied grade does not contain carbon black or a UV stabiliser package, outdoor storage should be limited. Incompatibility with certain additives should be checked before blending: strongly alkaline or amine-based masterbatches can destabilise the base polymer or consume the antioxidant package, and flame-retardant systems may alter melt stability. Compatibility is verified by oxidation induction time and melt-flow retention after compounding.

    Compliance must be confirmed at the supplied formulation level. For food-contact use, the base resin may fall under FDA 21 CFR 177.1520 for olefin polymers, but the finished article must meet any applicable migration limits under EU Regulation 10/2011 with its amendments. For drinking-water pressure pipe, system standards such as EN 12201 and national approvals control the installation, not the resin alone. For electrical conduit and cable ducting, heavy-metal restrictions under the RoHS Directive 2011/65/EU and REACH candidate-list screening may apply. These requirements depend on colourants, carbon black, and processing aids; a natural resin may comply while a colour-compounded version may not. The grade should be stored in dry, closed conditions and away from prolonged UV exposure unless UV stabilisation is declared.

    On production-scale twin-screw compounding lines and pipe extrusion lines, batch-to-batch variance in bimodal HDPE is detected by monitoring die pressure, melt temperature, and post-extrusion melt-flow rate. A melt-flow shift of more than ±0.05 g/10 min can indicate a reactor transition or blending error and should be investigated before pressure-pipe production. Pellet size distribution is checked under ASTM D1921-18, and dust content is controlled to prevent feeding defects in vacuum hopper loaders. In blown-film and sheet conversion, melt strength and draw-down limits are controlled through air-ring design and chill-roll temperature, not by excessive melt temperature. Published data for this specific configuration is limited; production validation remains the controlling step for any new application of Shandong Yulong HDPE HD-TR144.

    Top