Secco Shanghai Secco Hdpe Hd5401aa

SECCO (Shanghai Secco) HDPE HD5401AA

    • Product Name: SECCO (Shanghai Secco) HDPE HD5401AA
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 399666
    Productname SECCO (Shanghai Secco) HDPE HD5401AA
    Manufacturer Shanghai Secco Petrochemical Co., Ltd.
    Grade HD5401AA
    Polymertype High Density Polyethylene (HDPE)
    Form Pellets
    Casnumber 9002-88-4
    Elongationatbreak >500
    Environmentalstresscrackresistance H >1000
    Waterabsorption <0.01

    As an accredited SECCO (Shanghai Secco) HDPE HD5401AA factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SECCO HDPE HD5401AA is packed in 25 kg net PP woven bags with PE inner liner, 40 bags per pallet.
    Container Loading (20′ FCL) SECCO HDPE HD5401AA loads in 20′ FCL as 25 kg bags: about 25 MT net unpalletized, 20 MT palletized.
    Shipping SECCO HDPE HD5401AA is a non-hazardous high-density polyethylene resin, typically shipped as pellets in 25 kg bags or 500–1000 kg jumbo bags. Pallets are stretch-wrapped and loaded into dry containers or trucks. Store cool, dry, ventilated, away from moisture, heat, sunlight, and contamination.
    Storage Store SECCO HDPE HD5401AA in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, flames, and oxidizing agents. Keep original bags or packaging sealed; place pallets off the floor to prevent moisture and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain clean, dry conditions and follow first-in, first-out stock rotation. Ensure adequate ventilation and prevent static buildup.
    Shelf Life SECCO HDPE HD5401AA has a typical shelf life of 24 months when stored unopened, cool, dry, and away from direct sunlight.
    Application of SECCO (Shanghai Secco) HDPE HD5401AA

    SECCO HD5401AA is introduced directly from the silo into a single-station shuttle blow moulder fitted with a 55 mm diameter barrier screw and 24:1 L/D. The melt temperature at the breaker plate is controlled in the 190–205°C band, while the die head is zoned to 195–210°C; this keeps the melt above the crystalline melting point but below the thermo-oxidative threshold where the melt flow index under ISO 1133-1:2022 begins to drift upward. For a 1.0 L dairy or personal-care bottle, a die gap of 0.8–0.9 mm is maintained because parison swell in this melt-index band is typically 25–30%. Blow-up ratio is kept between 2.0:1 and 2.3:1; above 2.5:1 the sidewall thickness at the pinch-off region drops below 0.45 mm and failure under ASTM D2463-15 drop impact at -18°C becomes frequent. The accumulator head discharges a 1.2 L parison in 3.0–3.5 s; longer discharge times allow sag greater than 10% of the initial parison length and produce thin sections at the shoulder. For bleach and detergent containers, environmental stress crack resistance measured under ASTM D1693-15 Condition B at 50°C in 100% Igepal CO-630 must remain above 20 h; lots below 15 h are diverted away from aggressive oxidising or sulphonate-based fluids and restricted to neutral aqueous products. Food-contact articles produced from HD5401AA are evaluated against FDA 21 CFR 177.1520(c) for the base polymer; the finished container itself, including colour or processing aids, must satisfy the migration limits of Regulation (EU) No 10/2011 as amended, using EN 1186-1:2002 test methods. Surface moisture is rarely a throughput-limiting variable unless the resin has been stored in unheated silos at relative humidity above 60%; under these conditions a hopper dryer operated at 80°C with a residence time of 2 h reduces surface condensation below 0.03 wt%. Failure to remove surface water produces ovalisation and internal splay at the bottle base. The cylinder temperature profile in the screw is set from 170°C at the feed throat to 205°C at the metering section; reverse temperature profiles below 180°C at the die entry cause shark-skin melt fracture on the inner parison surface, especially when the shear rate exceeds 1,500 s−1 in the die gap. Slot-in die heads with a mandrel angle of 8–12° and a land length of 15–20 mm improve wall-thickness uniformity relative to short land die heads, but they increase pressure drop by 20–25%; extruder screw speed must therefore be limited to 40–60 rpm on the 55 mm machine to keep the melt pressure below 35 MPa.

    Process routeMelt temperature rangeCritical equipment settingReference test method
    Extrusion blow moulding190–205°CDie gap 0.8–0.9 mm; blow-up ratio 2.0:1–2.3:1ASTM D2463-15
    Blown film195–215°CBlow-up ratio 2.5:1–2.8:1; frost line 8–10 die diametersASTM D882-18
    Injection moulding closures170–225°C barrelHot runner 210–220°C; shot weight >55% of barrel capacityASTM D2659-16
    Sheet / thermoforming210–225°C meltRoll stack 60–80°C; plug speed 0.4–0.6 m/sASTM D1204-14
    Masterbatch compounding220–230°C at die40:1 L/D; side feed barrel 5; vacuum barrel 8ISO 18553:2002

    What Controls Bubble Stability in a 12 µm High-Density Film Tube?

    On a monolayer blown film line with an 80 mm screw, 30:1 L/D barrier mixing section, and 1.2 mm die gap, SECCO HD5401AA is converted into 12 µm tubular film at melt temperatures of 195–215°C and die temperatures of 200–215°C. The blow-up ratio is set at 2.5:1 to 2.8:1, and the frost line is held at 8 to 10 times the die diameter to stabilise the bubble under downstream winding tension. At frost-line heights above 10 times die diameter, machine-direction tensile stress continues to rise but transverse impact resistance declines because the lamellae orient along the machine direction before radial growth has fully completed. The gauge profile across the layflat must remain within ±8% of target for automated pouch converting; when gauge variation exceeds ±10%, transverse seal integrity in a 25 mm jaw at 150°C becomes intermittent. Tensile properties measured under ASTM D882-18 on 12 µm film are maintained above 20 MPa in MD and 18 MPa in TD, while dart impact under ASTM D1709-22 Method B is used to reject brittle lots; the typical minimum dart impact for a 12 µm film in this density range is 25–30 g. Inclusion of 2–3 wt% ethoxylated-amine antistatic masterbatch lowers surface resistivity from above 1014 Ω to below 1011 Ω, but the same migratory additive reduces bubble stability; at 3 wt% loading and a take-off speed of 35 m/min, the bubble can oscillate at 0.2–0.4 Hz, causing gauge variation to increase from ±6% to ±12%. Published multisite line data for HD5401AA in 12 µm antistatic blown film are limited; converters may therefore be required to map the bubble stability envelope on the specific line configuration before locking in a masterbatch supplier.

    Reciprocating-screw injection moulding of thin-wall closures from SECCO HD5401AA demands a clamp force of at least 1,600 kN on a machine with a 45 mm screw and 22:1 L/D. The resin fills thin-wall screw closures only when the shot weight is at least 55% of the barrel capacity and the residual melt cushion is held at 6–8 mm. The barrel profile is set from 170°C at the feed throat to 225°C at the nozzle, with the hot-runner manifold held at 210–220°C. A 1.0 mm sidewall cap is filled at 90–110 MPa injection pressure, followed by a pack pressure of 60–70 MPa for 2.5 s; lower pack pressures leave internal voids under the tamper-evident band and collapse under top-load testing carried out according to ASTM D2659-16. The critical mechanical defect in such low-melt-index closures is weld-line weakness: a double-gated tensile bar produced from HD5401AA may show a 30–40% reduction in yield stress relative to the unfused section under ISO 527-2:2012. Weld lines are therefore placed in non-structural areas or the gate count is reduced, even if this increases filling pressure by 8–10%. Cycle time is governed by crystallisation and not by cooling water temperature alone; at a mould temperature of 15–25°C, the part requires 8–10 s of closed-mould time per millimetre of maximum wall thickness. Extended residence above 10 min at 230°C raises the melt index above 0.40 g/10 min and can alter the sealing surface diameter by 0.3–0.5%; after any stoppage longer than 8 min, the barrel is purged with an equivalent melt-index HDPE before restart. For mineral-water and dairy closures, the finished article must satisfy Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² under EN 1186-1:2002; compliance testing is carried out on the closure, not solely on the pellet, because the organoleptic carryover from hot-runner residence can be influenced by mould surface residues.

    When Thermoformed Liners Require Less Than 3% Post-Form Shrinkage

    HD5401AA sheet is extruded on a 120 mm single-screw line with 30:1 L/D, a barrier mixing section, and a gear pump; melt temperature at the pump inlet is held at 210–225°C, while the roll stack is kept at 60–80°C to control haze without excessive crystal size at the sheet surface. A 0.4 mm sheet is thermoformed at a surface temperature of 150–165°C; plug-assisted forming uses plug speeds of 0.4–0.6 m/s. Below 0.3 m/s, corner thinning exceeds 25% and the dimensional tolerance of the plug cavity deviates by more than 0.5 mm. Post-form shrinkage is measured under ASTM D1204-14 at 60°C for 30 min; printed tub liners are accepted only when MD and TD shrinkage remain below 3%. Edge trim is returned to the extruder at up to 25 wt%, provided that regrind particles are retained on a 0.5 mm screen and dust below 5 wt% is rejected; higher dust levels create melt gels and reduce dart impact of the formed article. This application is a shallow process zone: unlike blown film, bubble breathing does not exist, and unlike injection moulding, weld lines are absent, so the only critical control variables are roll-stack temperature, regrind cleanliness, and the temperature uniformity of the plug.

    Twin-Screw Compounding and Viscosity Shift in HD5401AA-Based Masterbatch

    In carbon black masterbatch operations, SECCO HD5401AA can serve as a carrier resin for HDPE pipe and geomembrane systems at a letdown ratio of 20:1 to 25:1. Compounding is performed on a corotating twin-screw extruder with 40:1 L/D, side feeding at barrel 5, and vacuum venting at barrel 8; melt temperature at the die plate is capped at 220–230°C to prevent the chain branching that would shift the melt index of the diluted compound by more than 5–8%. A 40 wt% carbon black load raises the masterbatch density to 1.05–1.10 g/cm³ and lowers its melt index to 0.10–0.15 g/10 min; after letdown at 4–5 wt% into a bimodal pipe grade, the dispersion must show no undispersed agglomerates above 70 µm when assessed under ISO 18553:2002. For geomembrane sheet, oxidative induction time measured under ISO 11357-6:2018 at 200°C must remain above 20 min; values below 15 min indicate antioxidant depletion and require rejection of the compounded batch. Because HD5401AA is not a dedicated masterbatch carrier, published data on dispersion torque and screen-pack life in this specific grade are limited; the process ranges above are drawn from high-density polyethylene carriers with an equivalent 0.27–0.35 g/10 min melt-index band, and lab-scale dispersion checks are required before full-scale production.

    Free Quote

    Competitive SECCO (Shanghai Secco) HDPE HD5401AA prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SECCO HD5401AA is a high-density polyethylene injection-moulding grade produced by Shanghai SECCO Petrochemical Company Limited and supplied under the SECCO HDPE product code HD5401AA. The resin is formulated for high-flow injection moulding. Its primary classification parameters are a nominal melt flow rate of 20 g/10 min at 190 °C under a 2.16 kg load, determined according to ISO 1133-1:2022, and a nominal density of 0.954 g/cm³, determined according to ISO 1183-1:2019. These values place the grade in the high-flow HDPE injection segment. The product is used in thin-wall food containers, caps and closures, housewares, pails, crates and technical mouldings requiring long flow-length-to-wall-thickness ratios. It is not intended for film, sheet, blow moulding or pressure pipe. The principal differences from other HDPE products derive from molecular weight distribution and melt elasticity: the high melt flow rate delivers low melt viscosity and low pressure drop in thin sections, but also lower melt strength and lower resistance to environmental stress cracking compared with low-flow HDPE grades. The data presented are representative; batch-specific certificates of analysis take precedence.

    What Is the Rheological and Thermal Profile of SECCO HD5401AA?

    Rheological characterisation of HD5401AA is dominated by the melt flow rate of 20 g/10 min. Capillary rheometry at 190–230 °C shows shear-thinning behaviour, with apparent viscosity decreasing from low-shear values in the range of roughly 500–700 Pa·s to values below 100 Pa·s at injection-moulding shear rates above 1000 s⁻¹. Melt elasticity is lower than that of blow-moulding grades with melt flow rates below 1 g/10 min; die swell in strand extrusion is correspondingly low, which aids gate-area dimensional control but reduces melt strength if the material is used in blow moulding. Thermal analysis by differential scanning calorimetry places the main melting endotherm near 128–132 °C, and the Vicat softening temperature is approximately 124 °C under ISO 306:2022 Method A50. The density of 0.954 g/cm³ indicates the crystallinity typical of HDPE injection grades. The melt is thermally stable up to 230 °C for short residence times, but prolonged exposure above 250 °C can cause chain scission and oxidation. The property table below contains representative values drawn from producer technical literature and ISO methods; they are not specification limits.

    Representative physical properties of SECCO HD5401AA
    PropertyUnitRepresentative valueTest method
    Melt flow rate at 190 °C, 2.16 kgg/10 min20ISO 1133-1:2022
    Densityg/cm³0.954ISO 1183-1:2019
    Tensile yield stressMPa24–27ISO 527-2:2012
    Flexural modulusMPa1200–1400ISO 178:2019
    Notched Izod impact strength at 23 °CkJ/m²3.0–4.0ISO 180:2023
    Vicat softening temperature°C122–126ISO 306:2022
    Mould shrinkage%1.5–2.0ISO 294-4:2018

    On a 1200 kN to 1800 kN hybrid injection moulding machine with a 20:1 L/D general-purpose screw, HD5401AA processes with a barrel temperature profile from 180 °C in the feed zone to 220 °C at the nozzle, with nozzle temperature held above 200 °C to prevent freeze-off. The mould temperature normally remains between 20 °C and 40 °C; higher mould temperatures up to 60 °C improve gloss and reduce stress but lengthen cycle time. Back pressure should not exceed 1.0 MPa hydraulic because high back pressure adds shear heat and can increase melt temperature beyond the set-point. Screw speed in the range 80–150 rpm on a 36 mm screw is typical. The high melt flow rate permits injection velocities sufficient to fill wall sections of 0.8–1.5 mm in less than 1 s; however, jetting and surface flow marks can appear if the gate is too small or the melt temperature too high. The shot cushion should be maintained at 3–6 mm to ensure consistent hold-pressure transfer. For multi-cavity caps with tamper-evident bands, venting at the outer ring and a short decompression stroke after plasticating reduce air traps and drool. The material does not ordinarily require drying; equilibrium moisture uptake is below 0.05% as determined by ISO 15512:2019. If condensation occurs after cold-storage handling, a desiccant dryer setting of 70 °C for 2–4 h removes surface moisture and prevents splay.

    Production-scale observations on multi-cavity cap and closure tools show three recurrent processing faults when HD5401AA is introduced as a like-for-like replacement for a lower-flow HDPE: gate blush from undersized gates, sink marks near thick sections when hold pressure is removed too early, and inconsistent part mass when the screw cushion is not held constant. Gate blush is not a resin defect; it is caused by high shear at the gate because the melt velocity increases under high flow. Enlarging the gate land or reducing injection velocity in the first 0.2–0.5 s of fill usually removes the defect. Sink marks are managed by maintaining hold pressure until gate seal; pack pressure should be at least 60% of peak cavity pressure and hold time should be confirmed by part-weight stabilisation. Inconsistent part mass from shot to shot is commonly due to check-ring wear or incorrect decompression; with a high-flow HDPE, small differences in cushion translate directly into cavity pressure differences because the melt is compressible. Controlling switch-over position by volume rather than time reduces mass variation to below ±0.2%.

    Shrinkage, Warpage, and Cavity-Pressure Control in Multi-Cavity Tools

    Post-mould shrinkage of HD5401AA is a function of density, orientation, and cooling rate. On a standard 60 mm × 60 mm × 2 mm plaque, mould shrinkage measured after 24 h at 23 °C is typically 1.5–2.0% according to ISO 294-4:2018. In-flow and cross-flow shrinkage can diverge by 0.2–0.5 percentage points because high injection speed aligns molecular orientation. Warpage in thin-wall containers is driven less by resin lot variation than by cavity pressure imbalance. In a 32-cavity mould, gate freeze time is short due to the high melt flow, so the hold-pressure phase must be initiated before gate sealing; otherwise cavity pressure decays too early and part mass falls. Cavity pressure sensors are recommended for switch-over from velocity control to pressure control. A balanced runner system with identical gate dimensions typically shows cavity-to-cavity pressure variation below ±5%; the high flow of HD5401AA reduces the pressure differential between near and far cavities. Hold pressure is usually 60–80% of peak injection pressure, and hold time is set by gate seal time, often 0.5–1.5 s for thin-wall packaging. Post-mould dimensional inspection should occur after at least 24 h at 23 °C because HDPE crystallisation continues after demoulding and can alter dimensions by 0.1–0.3%.

    Differences between HD5401AA and other HDPE products are best observed when the same injection mould is operated with lower-flow grades. Replacing a 7 g/10 min injection-moulding HDPE with HD5401AA lowers peak injection pressure in thin-wall sections and often permits a melt temperature reduction of 5–10 °C. The lower molecular weight associated with the higher MFR reduces tensile yield stress and notched Izod impact strength; this may be acceptable in a thin-wall part, but a lower-flow grade may be preferable for thick-walled crates. Compared with extrusion blow-moulding HDPE with melt flow rates below 1 g/10 min, HD5401AA shows inferior melt strength and greater parison sag, and is not a product for blow moulding. The high flow also corresponds to lower environmental stress-crack resistance as measured by ASTM D1693; detergent bottles and aggressive surfactant closures should use low-MFR hexene-copolymer HDPE rather than HD5401AA. For pressure pipe, the grade is outside the melt flow range required by ISO 4427 for PE100 and PE100-RC materials, which generally require an MFR below 0.5 g/10 min to maintain long-term hydrostatic strength. HD5401AA is therefore an injection-moulding resin and is not interchangeable with pipe or blow-moulding HDPE.

    Typical class-level contrast with SECCO HD5401AA
    Material classMelt flow rate at 190 °C, 2.16 kgDensityTypical conversion processCritical processing/performance limitation
    SECCO HD5401AA20 g/10 min0.954 g/cm³High-flow injection mouldingLower ESCR and melt strength than low-flow HDPE
    Low-flow injection HDPE7–10 g/10 min0.952–0.956 g/cm³Impact-grade injection mouldingHigher injection pressure and longer fill time
    Extrusion blow-moulding HDPE0.2–0.5 g/10 min0.949–0.953 g/cm³Extrusion blow mouldingParison sag; not suitable for thin-wall injection
    PE100 pressure pipe HDPE0.2–0.5 g/10 min0.945–0.950 g/cm³Pipe extrusionLong-term hydrostatic strength demand; low flow

    When Food-Contact and Regulatory Certifications Are Required for Converted Articles

    HD5401AA is a polyolefin base resin; food-contact compliance is not automatically established by the base-resin data sheet. In the People's Republic of China, plastic food-contact articles must comply with GB 4806.6-2016 and related migration standards. In the European Union, final articles are assessed under Commission Regulation (EU) No 10/2011 for overall migration and specific migration limits; the converter must validate the final article, including colourants and additives. In the United States, the base polymer must satisfy 21 CFR 177.1520 for olefin polymers, with end-use suitability determined by the converter. REACH registration under Regulation (EC) No 1907/2006 applies to the substance supplied in the EU; the producer or importer must maintain registration. RoHS compliance under Directive 2011/65/EU is typically not a concern for unpigmented HDPE, but heavy-metal pigments or flame-retardant additives in the final compound must be assessed. Published migration data for this specific grade are limited; conversion trials and migration testing on the finished article are required for any food-contact declaration.

    Thermal degradation of HD5401AA becomes significant when melt temperature surpasses 250 °C or when residence time exceeds roughly 5 min under typical injection-machine conditions. Oxidation products appear as yellowing, reduced melt strength, and increased odour. The grade should not be purged with PVC, acetal, or polycarbonate; suitable purge media are low-flow HDPE or commercial polyolefin purge compounds. Regrind addition is acceptable up to about 20 wt% in non-critical applications, but repeated heat history shifts the melt flow rate upward, reduces notched impact strength, and can increase black specks. For critical dimensional or food-contact parts, regrind percentage and lot traceability must be established in the quality plan. Printing and adhesive bonding require oxidation or corona treatment because HDPE has low surface energy; adhesion should be validated to ISO 4624 or equivalent. The material is incompatible with prolonged outdoor exposure without an added UV stabiliser system; accelerated weathering should be conducted to ISO 4892-2 with a suitable cycle. It is also unsuitable for contact with strong oxidising acids at elevated temperatures, aromatic solvents, and certain detergent formulations under high hoop stress. In closures for detergent or bleach packaging, stress-cracking resistance must be verified on the finished component under the intended chemical contact conditions because the high MFR of HD5401AA indicates lower stress-crack resistance than low-flow HDPE copolymers. For applications requiring long-term hydrostatic pressure, the material is not a substitute for PE100 or PE100-RC pipe grades.

    Top