| HS Code | 151199 |
| Density | 0.937 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.25 g/10 min |
| Tensile Strength At Yield | 23 MPa |
| Tensile Strength At Break | 28 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 1000 MPa |
| Vicat Softening Temperature | 124°C |
| Melting Temperature | 130°C |
| Environmental Stress Crack Resistance Escr | >1000 h |
| Hardness Shore D | 60 |
| Notched Izod Impact Strength | 500 J/m |
| Water Absorption | <0.01% |
As an accredited SCG Chemicals HDPE H377C factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SCG Chemicals HDPE H377C is packaged in 25 kg polyethylene-lined woven bags, stacked on pallets for industrial shipment. |
| Container Loading (20′ FCL) | SCG Chemicals HDPE H377C in 20′ FCL: 25 kg bags, floor-loaded, approximately 25 MT net; standard dry container, no pallets. |
| Shipping | SCG Chemicals HDPE H377C is a non-hazardous high-density polyethylene resin in pellet form. It is typically shipped in 25 kg bags, jumbo bags, or bulk containers. For transport, it is not classified as dangerous goods. Store in a cool, dry, well-ventilated area, away from heat and direct sunlight. |
| Storage | Store SCG Chemicals HDPE H377C in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and moisture. Keep material in original sealed bags or containers, on pallets off the floor. Avoid prolonged UV exposure and contamination by oils, solvents, or strong oxidizers. Maintain stable ambient temperatures and safe stacking heights to prevent deformation or package damage. |
| Shelf Life | Typically 24 months when stored unopened in original packaging in a cool, dry, well-ventilated area, away from direct sunlight. |
SCG Chemicals HDPE H377C is positioned as an extrusion blow moulding resin for rigid industrial containers, supplied as a pre-compounded black pellet. The application logic below is written for manufacturers and overseas buyers who need to align container development with UN certification, EU packaging directives, and standard material test methods without mixing food-contact and non-food packaging claims. Where a specific value is not published by the producer, the text identifies the industrial range or states that lot-specific verification is required; no fabricated datasheet property is presented. The grade is not described here for direct food-contact applications; if a buyer requires food-contact status, migration testing under FDA 21 CFR 177.1520 or EU 10/2011 must be conducted on the specific lot and article.
| Segment | Primary compliance anchor | Critical material test method | Typical terminal article |
|---|---|---|---|
| Household/industrial cleaning | UN 3H1/Y; EU 94/62/EC | ASTM D1693-15 condition B | 1–5 L bleach and acid bottles |
| Agricultural emulsifiable concentrates | UN 3H1/X; ADR/RID/IMDG Code | ASTM D1693-15 condition C; ASTM D638-14 | 500 mL–10 L fluorinated bottles |
| Automotive lubricants/coolants | UN 3H1/Y; ISO 1133-1:2022 | ASTM D256-10(2018) Izod at −20 °C | 1–5 L oil and coolant packs |
| Water treatment chemicals | UN 3H1/Y | ASTM D638-14 elongation retention after hypochlorite | 5–25 L bleach and pool drums |
| Construction adhesives/sealants | UN 3H1/Y; EU 94/62/EC | ASTM D543-21 | 1–10 L solvent-based adhesive containers |
| Marine/offshore chemicals | IMDG Code; UN 3H1/Y | UN drop at −18 °C; stack 28 days at 40 °C | 5–20 L marine oil and fuel cans |
Across extrusion blow moulding lines dedicated to household bleach and hard-surface cleaner containers, the controlling process window is not melt temperature alone but the interaction between parison sag, die swell, and the seasonal variation in ambient workshop humidity. The segment is dominated by 1–5 L bottles and jerry cans for sodium hypochlorite, quaternary ammonium disinfectants, alkaline degreasers, and acid descalers. Transport certification for corrosive contents uses UN 3H1/Y or 3H1/Z under the UN Model Regulations Chapter 6.1; packaging waste heavy-metal limits are assessed through EU Directive 94/62/EC for lead, cadmium, mercury, and hexavalent chromium. Formulation on a monolayer shuttle line is typically 20–30 wt% clean internal regrind from trimmed flash, 0.3–0.8 wt% antioxidant and processing-aid masterbatch, and the balance virgin H377C; no additional carbon black masterbatch is added when the as-delivered black compound is used. Extrusion blow moulding is performed on a shuttle machine with a 55–65 mm grooved-feed extruder, L/D 24:1–30:1, accumulator head, and parison programmer. Melt temperature at the die exit is held between 180 °C and 205 °C, die gap is set at 1.5–2.5 mm, blow air pressure is 0.6–0.9 MPa, and mould water temperature is kept at 8–18 °C to control post-mould shrinkage in bleach-filled 5 L bottles. If pellet moisture exceeds 0.05 wt% after storage at relative humidity above 60%, a hopper dryer setpoint of 70 °C for 1–2 h is applied before the feed throat.
Agricultural emulsifiable concentrate formulations are among the most aggressive HDPE packaging environments because they combine aromatic solvent carriers, non-ionic and anionic emulsifier systems, and active ingredients that can plasticize amorphous regions of the container wall. Qualification for 1–10 L monolayer bottles in this segment does not accept a single ESCR value; instead, lot acceptance frequently requires ESCR F50 of at least 100 h under ASTM D1693-15 condition C, tensile yield stress above 22 MPa under ASTM D638-14, and drop impact acceptance at −10 °C under the UN packaging drop sequence for the specific liquid classification. Environmental and transport compliance is governed by the UN Model Regulations, ADR/RID, and the IMDG Code for Class 3 or Class 6.1 liquids, while pesticide label and closure certification follows local registration requirements derived from FAO/WHO Joint Meeting on Pesticide Specifications.
The barrier window for emulsifiable concentrate bottles is controlled less by ordinary masterbatch addition than by post-mould fluorination; monolayer containers are treated with fluorine/nitrogen mixtures at fluorine concentrations of 0.5–1.5 vol% to reduce solvent permeation and weight loss. Regrind is restricted to 15–20 wt% because higher internal recycle fractions lower ESCR and widen parison thickness variability. If external black masterbatch were used in a natural HDPE formulation, its loading would be 2–4 wt%; with H377C as a pre-compounded black resin, that addition is 0 wt%, and only a stabilizer masterbatch at 0.3–0.6 wt% is introduced. Production equipment for emulsifiable concentrate bottles typically requires a 60–70 mm extruder with L/D 25:1–32:1, a spiral mandrel die head to reduce weld-line discontinuities, and a parison programmer with at least 100-point axial wall-thickness control because drop impact and permeation are highly sensitive to the thinnest point of the sidewall. Mould cooling at 10–15 °C and blow pressure at 0.7–1.0 MPa are standard. Terminal products include 500 mL–10 L fluorinated bottles for chlorpyrifos-type and pyrethroid emulsifiable concentrates, with permeation performance screened by gravimetric weight-loss methods rather than single-point density checks.
Because automotive lubricant bottles are filled at 40 °C to 70 °C with formulations containing polyalphaolefins, ester base stocks, and antiwear additives, the primary failure mode shifts from environmental stress cracking during storage to dimensional change and neck finish torque loss during hot-fill and capping. UN 3H1/Y certification is maintained for 1–5 L oil packs, and fill-line inspections require neck dimensions for 38 mm and 63 mm closures conforming to supplier-specific drawings; incoming lot control verifies melt mass-flow rate under ISO 1133-1:2022 rather than relying on nominal datasheet values. FDA compliance is not required for lubricant containers, but EU REACH Annex XVII restrictions on specific additives and heavy metals apply to the packaging article. Formulation for this application is typically 15–25 wt% clean regrind from trimmed flash, 0.2–0.5 wt% fluoropolymer processing-aid masterbatch, and balance virgin H377C. The fluoropolymer masterbatch is introduced only when melt fracture or die lip build-up is observed at high output; it is not a default addition because it can increase die pressure and reduce adhesion of in-mould labels.
Downstream production on a double-station shuttle or long-stroke accumulator machine for 4–5 L containers uses a 70–80 mm extruder, L/D 28:1–30:1, and an accumulator head with shot capacity 1.5–4 kg. Melt temperature is kept at 190–210 °C, die gap at 2.0–3.0 mm, and mould temperature at 10–20 °C; parison swell compensation is set between 40% and 60% depending on tooling diameter. Terminal products include 1–5 L high-density polyethylene bottles for passenger-car motor oil, gear oil, hydraulic fluid, and antifreeze/coolant, with closure torque retention tested after 24 h simulated hot-fill ageing.
For water treatment facilities, 10–25 L drums and 5 L containers for sodium hypochlorite, calcium hypochlorite, and swimming-pool sanitizers are stored outdoors for months, so oxidative degradation and UV exposure are more severe than in indoor detergent packaging. Compliance for chlorine-based products commonly invokes UN 3H1/Y or 3H1/X depending on concentration, and the packaging must pass UN drop and stacking tests after conditioning; material degradation is tracked through ASTM D638-14 tensile elongation retention and ASTM D1693-15 ESCR after 30–90 days of hypochlorite contact at 40 °C. The formulation in this sector is usually limited to 10–20 wt% internal regrind for bleach bottles; hypochlorite attack concentrates in weld-line regions, and high regrind fractions cause early weld-line cracking. A hindered phenolic and phosphite stabilizer masterbatch may be added at 0.2–0.4 wt% only when prolonged outdoor storage is specified, while incompatible transition-metal stearate additives are avoided because they catalyze polyolefin oxidation. Production equipment is a continuous extrusion shuttle blow molder with a 55–60 mm extruder and a parison wall-thickness controller programmed to shift material away from pinch-off areas; blow pressure is 0.5–0.8 MPa, mould temperature 8–15 °C, and cycle time for a 5 L drum is typically 25–35 s depending on wall thickness. Terminal articles include 5–25 L drums for sodium hypochlorite solution, pool oxidizers, and alkaline pH adjusters.
High-viscosity construction adhesives, silane-modified sealants, and solvent-borne wood preservatives impose a combination of slow filling, aggressive solvent swelling, and long shelf life on the container. Transport of solvent-based adhesives and sealants under UN 3H1/Y or 3H1/Z is the primary compliance route, and chemical compatibility is screened by ASTM D543-21 for plastic material resistance; the final container is also evaluated under EU Directive 94/62/EC for heavy metals and under REACH for restricted substances. Extrusion blow moulding of 1–10 L rectangular containers for this segment is typically done on a reciprocating screw accumulator machine with a 60–70 mm extruder and L/D 24:1–30:1, with parison programming biased toward the bottom corners because corner thinning is the dominant drop point after rough construction-site handling. The addition ratio is 15–25 wt% clean regrind, but only after a 24 h ESCR check on the specific adhesive formula; calcium stearate as acid scavenger may be added at 0.05–0.15 wt% if moisture is present, and no external black masterbatch is required when the pre-compounded H377C pellet is used. Where wood preservative formulations contain metal carboxylates, compatibility must be confirmed because these compounds can accelerate surface oxidation and reduce long-term ESCR. Terminal articles are 1–10 L rectangular and cube containers for solvent-based adhesives, silane sealants, and wood preservatives, often with spout or handle configurations.
Marine and offshore service adds salt-spray exposure, frequent temperature cycling from −20 °C to 50 °C, and shipboard stowage constraints, which make the neck finish and cap seal more vulnerable than the sidewall. These articles are typically 5–20 L containers for marine engine oils, stern tube fluids, and fuel conditioners, covered by the IMDG Code and UN 3H1/Y if the contents are classified; drop tests at −18 °C and stack tests for 28 days at 40 °C are applied to lot samples. Formulation for this segment allows 10–15 wt% regrind only; the low fraction is maintained because low-temperature impact resistance and weld-line ESCR are disproportionately reduced by repeated heat history in accumulator heads. If UV protection is specified for deck storage, H377C pre-compounded carbon black is used, and no additional UV masterbatch is introduced; if a natural grade is substituted, a UV masterbatch at 4–6 wt% is required, but that substitution changes ESCR and must be re-qualified. Downstream production uses a 70–80 mm accumulator machine with shot capacity 2–6 kg, melt temperature 195–215 °C, and blow pressure 0.5–0.7 MPa; the mould is chilled to 5–10 °C to improve low-temperature impact strength, but too low a mould temperature can create high internal stress. Terminal products include 5–20 L square and round cans for marine lubricant, cooling water treatment, and fuel additive concentrates.
Competitive SCG Chemicals HDPE H377C prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SCG Chemicals HDPE H377C is a high-molecular-weight, high-density polyethylene extrusion blow-moulding grade used in rigid industrial and agrochemical container production. The resin is a copolymer with a typical density of 0.953 g/cm³ measured by ASTM D1505 and a melt mass-flow rate of 0.37 g/10 min at 190 °C and 2.16 kg load using ISO 1133-1:2022. These typical values are supplied for material selection and are not specification limits. H377C is calibrated for containers in the 2 L to 20 L range where high melt strength stabilises the parison during shuttle blow moulding. The grade is distinguishable from general-purpose blow-moulding HDPE by a lower melt flow rate, a higher environmental stress crack resistance, and a molecular architecture that maintains parison dimensional stability over longer hang times.
Because the melt mass-flow rate is low at 0.37 g/10 min, shear viscosity at blow-moulding parison shear rates below 100 s⁻¹ remains high enough to limit gravity-driven parison sag. On a shuttle blow-moulder equipped with a grooved-barrel extruder of 25:1 L/D ratio, die-head temperature is commonly held between 180 °C and 200 °C while barrel zones are capped at 220 °C to avoid molecular weight reduction during prolonged residence. The die gap is typically set from 1.5 mm to 2.5 mm, and parison programming with a 10-point controller allows wall-thickness profiling across the parison length. Melt pressure at the die entrance for H377C is higher than for a 0.65 g/10 min general-purpose HDPE; published data for this specific configuration is limited, but the increase is consistent with the presence of a higher high-molecular-weight tail. High melt strength produces controlled die swell and reduces neck-in during parison extrusion, but the higher viscosity raises shear heating in the metering zone, so screw speed should be adjusted conservatively in machines without automatic melt-temperature control.
Extrusion blow moulding with H377C benefits from parison swell behaviour that assists pinch-off weld consolidation, but excessive melt temperature can reduce melt strength and create wall-thickness variation. Barrel temperature profiles should be reverse-profiled, with the feed zone set below the compression and metering zones, while the die-head temperature is trimmed separately to control surface finish. Because the grade is intended for high-shear history containment, purging with a general-purpose HDPE of higher melt flow is recommended before colour or grade changes. This purging step limits retained gel or cross-linked material in the die head and maintains stable parison ejection. The melt viscosity of H377C also places an upper practical limit on accumulator-head throughput; published data for this specific extruder configuration is limited, and line trials are required to establish the maximum screw speed without melt fracture.
At low strain rates characteristic of slow crack growth, H377C demonstrates an environmental stress crack resistance measured under ASTM D1693-B with a typical F50 value exceeding 1,000 h in 10% Igepal CO-630 at 50 °C. This performance is relevant to jerry cans holding surfactants, crop-protection formulations, and hypochlorite-based cleaners, where surface-active agents accelerate crack propagation at stress concentrations. The polymer architecture combines a high-molecular-weight fraction with short-chain branching, increasing tie-chain density across lamellar boundaries and retarding craze fibril rupture. Impact resistance is reported as a notched Izod value of 6.0 kJ/m² at 23 °C under ISO 180/A, while the tensile yield stress is typically 28 MPa and the flexural modulus is 1,250 MPa under ISO 527-2 and ISO 178 respectively. This stiffness contributes to top-load strength in stackable containers, but the low melt flow rate limits injection-moulding flow paths and makes thin-wall injection moulding unsuitable. Compared with PE100 pipe grades formulated for long-term hydrostatic strength, H377C is tuned for blow-moulding melt strength and die swell rather than slow crack growth under internal pressure. Published data for H377C in pipe extrusion is limited, and that processing route is not recommended.
Tooling transfer from a 0.65 g/10 min unimodal HDPE to H377C on a 20 L jerry can line requires re-profiling the parison wall because the higher melt strength changes swell distribution. With a blow-up ratio between 2.5:1 and 3.0:1, the lower-MFR resin can generate thicker parison regions at identical die gap, altering pinch-off weld thickness and handle-section integrity. Cumulative blow-moulding clamp force requirements remain within standard shuttle-machine frames rated at 180 kN to 250 kN, but clamping force alone does not predict pinch-off quality; tensile behaviour of the weld is influenced by melt temperature and pinch-off land geometry. Drop impact of filled containers should be evaluated by ASTM D2463-15 at -18 °C and 23 °C because environmental stress crack resistance and subzero impact response do not arise from the same molecular parameters. Lowering die temperature by 5 °C to 10 °C relative to the previous grade helps control parison hang time. Published data for this specific tooling configuration is limited; trials are required to verify wall thickness distribution against a minimum of 1.8 mm at the container sidewall.
The same replacement may require adjustment of the parison programmer because the lower-MFR grade exhibits lower sag over identical hang time but higher die swell at the same die gap. Handle pinch-off regions are particularly sensitive to excess parison thickness, which can generate cold welds if the melt temperature at the pinch-off land drops below the crystalline consolidation range. On machines with closed-loop parison control, wall thickness inputs should be iterated using 0.5 mm increments until the minimum wall at the sidewall and the handle insert meet drawing specifications. Processors should also re-verify drop impact after conditioning filled containers at 40 °C for 24 h because stabiliser migration and sealant interaction can shift the failure mode from ductile yielding to brittle fracture. Published data for hot-filled or post-conditioned H377C jerry cans is limited, so qualification testing must be performed for each end-use chemistry.
In jerry can production for agricultural chemical packaging, H377C is used where top-load strength, stress crack resistance, and drop impact after stacking are specified by end users. The resin alone does not confer UN dangerous goods certification; completed packagings must pass UN 6.1.5 drop and leakproofness tests with the specified fill substance. Blow-moulded containers made from H377C can be leak tested in-line at pressure-decay thresholds of 0.2 bar over 30 s, but the threshold is packaging-specific and must be validated for each design. The resin is not recommended for sheet extrusion or cast film below 50 µm because melt strength and gauge uniformity are optimised for parison extrusion, not chill-roll drawing. Pellet handling should avoid condensation on pellets transferred from unheated storage at 15 °C to a production hall above 25 °C; surface moisture can generate surface defects in the parison. Published data on food-contact migration for this industrial grade is limited; direct food-contact status must be confirmed against current supplier documentation.
H377C differs from injection-moulding HDPE grades of MFR 8 g/10 min or above in that its high viscosity prevents consistent filling of narrow runner systems and thin-wall cavities. The molecular weight distribution that supports parison integrity also increases orientation and frozen-in stress in injection moulding, leading to warpage and sink marks. In blow moulding, those orientation effects are redirected into hoop strength and wall uniformity, which is the intended use. Material handling equipment should include a dedusting system because pellet fines can create gels or specks in the parison surface; a fines level below 0.05% by weight is typically targeted in high-gloss container production. Because this is a polyolefin, thermal degradation is autocatalytic only at elevated temperature, so barrel-temperature excursions above 220 °C should not be used to compensate for insufficient screw plastication capacity.
Property values below are representative values from resin selection literature; they are not batch-release specification limits. A conventional 0.65 g/10 min blow-moulding HDPE may process at lower melt pressure and shorter cycle but typically exhibits lower ESCR and a narrower parison hang-time window. H377C occupies a low-MFR high-ESCR corner of the blow-moulding grade space that is selected when aggressive contents and regulatory drop tests dominate the container specification.
| Property | Test method | Typical value |
| Melt mass-flow rate | ISO 1133-1:2022 | 0.37 g/10 min |
| Density | ASTM D1505 | 0.953 g/cm³ |
| Tensile yield strength | ISO 527-2 | 28 MPa |
| Flexural modulus | ISO 178 | 1,250 MPa |
| Notched Izod impact at 23 °C | ISO 180/A | 6.0 kJ/m² |
| Environmental stress crack resistance, F50 | ASTM D1693-B | >1,000 h |
| Vicat softening temperature | ISO 306/A50 | 126 °C |
| Shore D hardness | ISO 868 | 63 |
The table is intended for material pre-selection. For a direct substitution into an existing mould, the processor should compare the melt-flow ratio and shear viscosity data at the specific die-shear rate because the low MFR alone does not describe the full parison formation behaviour. Where the previous grade had higher MFR, the accumulator head pressure should be recorded during the first trial and compared with the machine manufacturer’s maximum continuous melt pressure. If the accumulator pressure exceeds 35 MPa at standard die-head settings, the die gap or melt temperature should be adjusted before continuing production. Published data for H377C in accumulator-head machines above 30 L container capacity is limited, so larger tooling may require a melt-flow grade with lower viscosity.
Thermal stability of H377C during processing is governed by the stabiliser package specified by the manufacturer. On an extruder with a residence time of 2 min to 4 min, melt-temperature setpoints should remain below 220 °C. Higher temperatures can accelerate chain scission and reduce the high-molecular-weight fraction that provides ESCR and melt strength. The processing window is therefore narrower than for general-purpose blow-moulding grades that tolerate higher melt temperatures to improve surface gloss. For pigmented containers, a masterbatch carrier compatible with high-density polyethylene should be used at a let-down ratio of 2% to 4%; incompatible carriers can reduce interlayer adhesion at the parison weld line and lower drop impact. Pre drying is not normally required for HDPE, but pellet surface moisture from condensation should be eliminated because steam originating at the feed throat can create surface streaking and variable extruder output.
Immediately downstream of the blow pin, wall-thickness distribution on H377C containers is measured using a Hall-effect gauge with a resolution of 0.01 mm across 16 points on the parison profile. This measurement provides immediate feedback for parison programming changes and reduces reject rates caused by thin sidewalls or handle pinch-off. In continuous shuttle machines, cycle time is governed by cooling capacity and part wall thickness; using a mould temperature of 10 °C to 15 °C and an air blow pressure of 0.6 MPa to 0.9 MPa is typical for high-density polyethylene containers. In-line leak testing of containers produced from H377C commonly uses a pressure-decay threshold of 0.2 bar over 30 s; units failing this threshold are rejected at the downstream station.