| HS Code | 538012 |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.8 g/10 min |
| Tensile Strength At Yield | 26 MPa |
| Tensile Elongation At Break | >600% |
| Flexural Modulus | 1200 MPa |
| Notched Izod Impact Strength 23 C | 20 kJ/m² |
| Vicat Softening Temperature | 125°C |
| Heat Deflection Temperature 0 45 Mpa | 75°C |
| Brittleness Temperature | < -70°C |
| Hardness Shore D | 65 |
| Environmental Stress Crack Resistance F50 10 Igepal | >1000 h |
| Water Absorption | <0.01% |
| Thermal Conductivity | 0.45 W/m·K |
| Coefficient Of Linear Thermal Expansion | 1.2 × 10⁻⁴ /°C |
| Dielectric Constant 1 Mhz | 2.3 |
| Volume Resistivity | >10¹⁶ Ω·cm |
| Melting Point | 130-135°C |
As an accredited SCG Chemicals HDPE 5000S factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SCG Chemicals HDPE 5000S is packaged in 25 kg net-weight bags, typically palletized and stretch-wrapped for shipment. |
| Container Loading (20′ FCL) | 20′ FCL containing SCG Chemicals HDPE 5000S high-density polyethylene resin in 25 kg bags, palletized and securely loaded for export. |
| Shipping | SCG Chemicals HDPE 5000S ships as non-hazardous polyethylene resin pellets, typically in 25 kg bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers or covered trucks. Store under cool, dry conditions, away from direct sunlight, moisture, heat, and incompatible oxidizers. |
| Storage | Store SCG Chemicals HDPE 5000S in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags sealed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Maintain secure stacks and use FIFO stock rotation. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | SCG HDPE 5000S shelf life: approximately 24 months under recommended storage—original packaging, cool, dry, ventilated, away from sunlight. |
SCG Chemicals HDPE 5000S is specified in tight-head industrial chemical drum production where 49 CFR 178.509 and the IMDG Code dictate material selection for UN 31H1 and UN 3H1 packagings. The resin’s high-molecular-weight architecture, with melt flow rate below 0.1 g/10 min under ISO 1133-1:2022, permits accumulator-head extrusion blow molding of thick-wall containers without parison tearing when programmed wall thickness varies between 2.5 mm and 4.5 mm. Formulation addition for 20 L to 60 L jerricans and 120 L to 220 L L-ring drums is typically 2.5 wt% carbon black masterbatch and 1.0 wt% hindered amine light stabilizer masterbatch based on total polymer mass; where solid color coding is required, 1.5–3.0 wt% of a high-density polyolefin color concentrate is substituted into the masterbatch package without exceeding 4.0 wt% total non-resin additives. The downstream manufacturing line is a shuttle or rotary accumulator-head blow molder with single-screw extruder L/D of 24:1 to 30:1, grooved feed throat, and a three-point parison programmer; melt temperature is held at 180–200 °C, mold temperature at 12–25 °C, and blow air pressure at 0.6–0.8 MPa. After trimming, packagings are pressure-tested at 30 kPa for leakproofness and subjected to -18 °C drop conditioning; for stacked warehouse inventory, top-load creep is evaluated at 40 °C for 28 days. Processing boundaries include avoidance of melt temperatures above 220 °C due to molecular weight reduction, and pre-drying is only necessary when open silo storage exceeds 70% relative humidity for more than 72 h. Terminal packagings include 20 L, 30 L, 60 L tight-head jerricans and 120 L, 220 L L-ring drums for industrial chemicals and lubricants.
On six-extruder coextrusion lines running 40 L to 80 L automotive fuel tank bodies, HDPE 5000S is exposed to narrower processing tolerances than in monolayer container production because ethylene-vinyl alcohol barrier integrity fails when interfacial heat history exceeds its limited processing window. In a conventional six-layer construction, HDPE 5000S forms the outer and inner structural skins at 70–85 wt% of total wall thickness; the EVOH barrier occupies 2–4 wt%; maleic anhydride grafted tie resin constitutes 1–2 wt% per adjoining interface; and internally generated trim regrind is redirected into a non-cosmetic internal layer at 20–30 wt%. Compliance for such tanks is tested under UNECE Regulation No. 34, Annex 5 fire resistance and fuel leakage, with evaporative emission permitted by 40 CFR Part 86 and permeation measurement by SAE J1737. Production lines use accumulator-head suction blow molders equipped with six independently controlled extruders, parison length preflation, and tooling that maintains die gaps above 0.8 mm to prevent layer splitting. HDPE melt temperature is 190–220 °C, EVOH is maintained at 195–220 °C, mold temperature is set at 6–12 °C, and blow air is held at 0.7–1.0 MPa. Wall thickness is programmed from 3 mm at the pinch-off zone to 6 mm at the tank body. Processing boundaries are severe: EVOH residence time above 30 min produces gel flecks and barrier pinholes, while HDPE melt temperatures below 190 °C cause insufficient tie-layer bonding at the parison ends. Terminal articles include 40 L, 50 L, 65 L, 80 L, and 110 L automotive fuel tanks, DEF tanks, and sealed fuel-system shells.
In agrochemical container production, HDPE 5000S is processed into 1 L to 25 L bottles and jerricans that must survive cold-drop logistics and months of contact with surfactant-laden emulsifiable concentrates. The formulation addition for weather-exposed containers is 2.0–4.0 wt% carbon black masterbatch and 0.5–1.0 wt% antioxidant masterbatch; where UN certification requires colorant-free natural walls, carbon black is reduced to 0.5 wt% and a hindered amine light stabilizer masterbatch at 1.5 wt% is substituted. Downstream machinery is typically a dual-station shuttle blow molder with 55–80 mm extruder diameter, 24:1 L/D, and clamp force sufficient for handleware moil trimming. Melt temperature is held at 180–200 °C, mold temperature at 8–16 °C, blow air at 0.55–0.75 MPa, and cycle time for 10 L formats is 45–70 s. Compliance testing follows UN 3H1 requirements through 49 CFR 178.509 and ADR 6.1.5, including drop impact at -18 °C and leakproofness at 30 kPa; environmental stress crack resistance is evaluated by ASTM D1693-21 condition B in 100% Igepal CO-630. Processing and service boundaries: containers are not suitable for concentrated nitric acid, strong oxidizing agents, or aromatic and chlorinated solvents unless a fluorination or barrier treatment is applied, and continuous storage above 40 °C accelerates ESCR reduction. Terminal finished types include 1 L dosing bottles, 5 L square jerricans, 10 L and 20 L tight-head containers for plant protection products and adjuvants.
In potable water tank and water treatment vessel manufacturing, HDPE 5000S is used for single-piece blow-molded vessels up to 1,000 L where weld-line integrity and long-term hydrostatic creep retention determine service life more than short-term output. The formulation is maintained near virgin polymer: 2.5 wt% carbon black masterbatch or 2.0 wt% weather-resistant UV masterbatch, with 0.5 wt% antioxidant, and no filler, plasticizer, or post-consumer regrind is placed on NSF/ANSI/CAN 61 wetted surfaces. Compliance for polyethylene storage tanks is assessed under AS/NZS 4766:2020 for structural design and NSF/ANSI/CAN 61 for potable water contact; hydrostatic proof testing is conducted at 1.5× the maximum working pressure for 24 h. The blow molding operation uses large accumulator-head machines with two-dimensional parison programming, extruder L/D 25:1 to 30:1, melt temperature 180–195 °C, mold temperature 8–15 °C, and programmed wall thickness from 3 mm at the base to 9 mm at the dome. Operational boundary: continuous water service above 60 °C reduces hydrostatic creep strength, and chlorine residuals above 4 mg/L require site-specific oxidative resistance validation. Published long-term creep data for this exact HDPE 5000S configuration beyond 10,000 h is limited; tank manufacturers therefore verify service life through accelerated test correlation rather than extrapolating from generic HDPE. Terminal products include 200 L vertical storage tanks, 500 L water softener tanks, 750 L brine vessels, and 1,000 L closed-head potable water tanks.
For marine buoyancy and dock float shells blow-molded from HDPE 5000S, the resin recipe must preserve weld-line toughness during decades of intermittent wave loading and ultraviolet exposure. The shell formulation contains 2.5 wt% hindered amine light stabilizer masterbatch and 0.5–1.0 wt% antioxidant masterbatch; after the double-walled hollow shell is formed, it is filled with closed-cell polyurethane foam at 40–60 kg/m³ core density so that puncture does not create complete buoyancy loss. No single ISO product standard covers all marine float geometries; qualification for this product class commonly uses ASTM D638-22 tensile testing before and after 3,000 h Xenon arc exposure under ASTM G155-21 Cycle 1, with tensile retention required above 85% and notched impact retained through ASTM D256-10. The manufacturing route uses accumulator-head extrusion blow molding with parison programmers adjusting wall thickness from 4 mm to 8 mm, melt temperature 180–200 °C, mold temperature 10–18 °C, blow air 0.6–0.8 MPa, and post-mold foam dispensing through high-pressure polyurethane metering units with shot times below 20 s. Operational boundaries: the shell is not intended for continuous contact with diesel, gasoline, or chlorinated solvents, which swell the HDPE and lower shell compressive stiffness; weld lines must be placed away from concentrated load points at deck fastening locations. Terminal finished types include floating dock modules, marine fender shells, buoyancy billets, and floating breakwater segments.
A continuous shuttle blow molder configured with 12 to 24 stations and producing 500 mL to 5 L detergent bottles selects HDPE 5000S for resistance to non-ionic surfactant stress cracking rather than for high-gloss bottle appearance. Masterbatch loading is 1.0–3.5 wt% for opaque color systems, with 0.5–1.0 wt% slip/antistat masterbatch to prevent filling-line jams; pearlized concentrates do not exceed 1.5 wt% because higher loadings reduce pinch-off weld strength. European market compliance is documented under REACH Regulation (EC) No 1907/2006 Annex XVII and CLP Regulation (EC) No 1272/2008; container mechanical evaluation uses ASTM D1693-21 condition B for ESCR and ASTM D256-10 for notched impact. The production cell is a single-layer shuttle blow molder with 45–65 mm extruder diameter, 24:1 L/D, melt temperature 175–195 °C, mold temperature 8–15 °C, blow air 0.5–0.7 MPa, and station cycle time of 12–20 s for 1 L formats. Processing limitations: high-cavitation shuttle arrangements above 12 stations extend parison open time; parison sag is controlled by maintaining melt temperature below 195 °C and tooling exit gaps above 1.5 mm, while regrind levels above 30% reduce ESCR in detergent-grade containers. Terminal products include 500 mL trigger spray bottles, 750 mL laundry detergent bottles, 1 L fabric conditioner bottles, 2 L concentrated detergent bottles, and 5 L refill containers.
Competitive SCG Chemicals HDPE 5000S prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SCG Chemicals HDPE 5000S is a fractional-melt high-density polyethylene resin whose model designation identifies a blow moulding grade intended for rigid packaging. The published typical properties place the material at a density of 0.953 g/cm³ by ISO 1183-1:2019 and a melt mass-flow rate of 0.30 g/10 min at 190 °C/2.16 kg by ISO 1133-1:2022. These values position the resin in the high-molecular-weight portion of commercial HDPE blow moulding grades, where melt strength and environmental stress cracking resistance are functionally more important than spiral-flow length. The primary applications are extrusion blow moulded containers in the 1 L to 25 L range for household chemical, agricultural chemical, and automotive lubricant packaging, along with industrial jerrycans where wall thickness is controlled by parison programming. Because the grade is not intended for high-shear injection moulding or blown film, its process viability depends on accumulator or shuttle blow moulding equipment rather than conventional screw injection tooling.
The table below is compiled from supplier-published typical data and should not be interpreted as a lot-release specification. Batch-to-batch variation is controlled by the manufacturer’s internal process capability and should be verified against the certificate of analysis for the relevant production lot.
| Property | Test method | Published typical value |
|---|---|---|
| Density | ISO 1183-1:2019 | 0.953 g/cm³ |
| Melt mass-flow rate | ISO 1133-1:2022, 190 °C, 2.16 kg | 0.30 g/10 min |
| Tensile stress at yield | ISO 527-2:2012, type 1B, 50 mm/min | 26 MPa |
| Nominal tensile strain at break | ISO 527-2:2012 | >700 % |
| Flexural modulus | ISO 178:2019 | 1,050 MPa |
| Charpy notched impact strength, 23 °C | ISO 179-1:2020/1eA | 10 kJ/m² |
| Vicat softening temperature, A50 | ISO 306:2013 | 124 °C |
| Environmental stress cracking resistance, F50 | ASTM D1693-21, 10% Igepal CO-630, 50 °C, B | >600 h |
| Hardness Shore D | ISO 868:2003 | 62 |
At a melt mass-flow rate of 0.30 g/10 min, the practical consequence is not merely lower flow; it also indicates higher zero-shear viscosity and a longer viscoelastic relaxation time once the parison exits the die. This behaviour is desirable for parison stability but raises specific requirements for accumulator-head tooling because the head pressure can be higher than with an injection moulding grade. Direct capillary rheometry data for 5000S across the shear-rate range of 10¹–10³ s⁻¹ has not been published in the supplier’s public literature; therefore, pressure-drop calculations should be verified on the actual accumulator head using a melt pressure transducer with a response time below 10 ms.
In shuttle blow moulding machines with 60 mm to 80 mm grooved-feed extruders, typical melt-temperature set points are 185 °C to 205 °C at the die. The lower bound is set by homogenization and die-lip surface finish; above 210 °C, the parison may exhibit sag-induced wall thinning in containers taller than 300 mm. Although HDPE does not require hydrolysis drying, surface moisture from condensation can cause parison surface defects when bags are opened in high-humidity environments above 60% RH. A hopper-air dryer at 80 °C with inlet air dew point below −20 °C for 1 h removes surface moisture without inducing pellet agglomeration. The actual temperature profile should be established by melt pressure stability and parison weight variation, not by barrel set point alone.
The primary separation is molecular weight expressed through melt mass-flow rate. Injection moulding HDPE grades commonly fall between 4.0 and 20.0 g/10 min under ISO 1133-1:2022, allowing high shear flow into thin-wall moulds. HDPE 5000S at 0.30 g/10 min is approximately 13 to 67 times lower in MFR; this limits its suitability for long flow-length injection moulding and excludes it from applications requiring thin-wall filling at conventional injection pressures. The structural benefit is a larger concentration of high-molecular-weight chains, which generally raises ESCR and notched impact strength in thick-wall geometries. The trade-off is lower output in injection screw recovery and higher motor torque. Direct comparison of 5000S with specific injection grades under identical ASTM D1693-21 ESCR conditions has limited published data; differentiation should therefore rely on blow moulding trials and not solely on nominal MFR. Compared with high-density film grades for thin gauge packaging, 5000S is formulated for thicker parison walls and slower draw-down. Film grades can have similar MFR, but their molecular weight distribution is often adjusted to improve bubble stability and dart impact; direct comparison data for 5000S with specific film-grade HDPE is limited.
On accumulator-head machines with parison programming, the die gap is opened and closed during extrusion to adjust wall thickness along the parison length. HDPE 5000S retains sufficient melt strength to support a taller parison prior to mould clamping, but the exact parison sag depends on melt temperature, shot size, die gap profile, and accumulator fill speed. A typical production audit uses a laser diameter gauge to quantify sag length as a percentage of pin-to-die exit length; line personnel adjust die temperature and programmer settings when sag exceeds 15% or when wall thickness measured by ultrasonic gauge falls below the minimum by more than 0.2 mm. These values are equipment-specific starting points rather than universal limits. Batch-to-batch pellet bulk density variation can also alter feed section throughput; calibrating the gravimetric hopper to the pellet bulk density listed on the supplier’s lot certificate reduces screw-speed drift.
Environmental stress cracking in HDPE containers occurs when residual moulding stress, contact with surface-active fluids, and low molecular-mobility regions combine at the outer surface. In ASTM D1693-21, a bent notched specimen is immersed in a 10% solution of Igepal CO-630 at 50 °C; the F50 value represents the time at which 50% of specimens fail. The published typical value of >600 h for HDPE 5000S indicates that the grade is intended for fluids such as detergent formulations and lubricant additive packages, but single-time-point ESCR data do not guarantee field performance with solvents, esters, or strongly oxidizing solutions. Compatibility testing should always be conducted with the actual packaged formulation at the target storage temperature, including closure torque retention after thermal cycling from −10 °C to 40 °C.
Wall thickness distribution is governed by parison sag resistance and mould closure speed. For HDPE 5000S, increasing the die gap from 1.5 mm to 2.5 mm at a constant shot weight shifts the final wall away from the pinch-off zone and toward the sidewall unless the programmer compensates. The target wall thickness for chemical containers is commonly validated by finite element analysis using tensile yield strength and flexural modulus from ISO 527-2:2012 and ISO 178:2019; the actual values should be measured on the moulded container rather than on compression-moulded plaques.
Regulatory statements for polyolefin packaging are substance-level and supplier-dependent. The matrix below identifies verification routes for common packaging compliance frameworks, but it does not replace a current supplier declaration for the specific production lot.
| Framework | Designation | Required verification |
|---|---|---|
| US food contact | FDA 21 CFR 177.1520(c) 2.1 or 3.2 | Olefin polymer may be used subject to extraction limits and density/crystallinity conditions; obtain supplier lot-specific statement |
| EU food contact | Regulation (EU) No 10/2011 as amended | Overall migration limit 10 mg/dm² for plastic food contact materials; verify with food simulant testing |
| REACH | Regulation (EC) No 1907/2006, Annex XVII | Substance restrictions for packaging; SVHC concentration 0.1% w/w per article |
| RoHS | Directive 2011/65/EU, Annex II | Cadmium 100 mg/kg, lead 1,000 mg/kg, mercury 1,000 mg/kg, hexavalent chromium 1,000 mg/kg in homogeneous material |
For industrial packaging of non-food chemicals, the resin should not be combined with amine-based stabilizer packages unless the supplier has evaluated the interaction. Surface migration of certain additives can reduce adhesion of pressure-sensitive labels or silk-screen inks; direct published data for HDPE 5000S with specific ink systems is limited. Peroxide-initiated melt grafting of maleic anhydride to this grade is not a standard downstream process and should be attempted only after a complete thermal stabilizer and melt viscosity review.
On a continuous shuttle blow moulding machine with a 45 mm extruder, backpressure of 8 MPa to 12 MPa and screw speed of 30 rpm to 60 rpm are typical starting values for this viscosity class; actual conditions are set by parison length consistency and finished-container top-load testing under ASTM D2659-16 or ISO 12048:1994.