Sadara Hdpe 17450n

Sadara HDPE 17450N

    • Product Name: Sadara HDPE 17450N
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 692832
    Polymertype High Density Polyethylene (HDPE)
    Density 0.945 g/cm³
    Meltindex 17 g/10 min (190°C/2.16 kg)
    Tensilestrengthatyield 24 MPa
    Tensilestrengthatbreak 15 MPa
    Elongationatbreak 600%
    Flexuralmodulus 1100 MPa
    Vicatsofteningpoint 126°C
    Heatdeflectiontemperature 70°C at 0.45 MPa
    Hardnessshored 65
    Notchedizodimpact 50 J/m
    Environmentalstresscrackresistance >1000 h
    Moldshrinkage 1.5-2.0%
    Processingmelttemperature 200-260°C

    As an accredited Sadara HDPE 17450N factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sadara HDPE 17450N is packaged in 25 kg polyethylene bags, typically 55 bags (1,375 kg) per pallet.
    Container Loading (20′ FCL) Container Loading (20′ FCL) for Sadara HDPE 17450N: palletized bags securely stowed, lashed, and moisture-protected for ocean freight.
    Shipping Sadara HDPE 17450N is a non-hazardous high-density polyethylene resin, typically shipped in 25 kg PE bags on pallets, stretch-wrapped, in clean, dry containers or trucks. Store away from moisture, direct sunlight, heat, and contamination. No special hazardous transport classification applies; follow supplier handling guidelines.
    Storage Store Sadara HDPE 17450N in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original bags or containers sealed, clean, and palletized off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Ensure good housekeeping and prevent static buildup. Follow local regulations and the manufacturer’s SDS.
    Shelf Life Sadara HDPE 17450N: 24 months in original unopened packaging, stored dry, cool, and away from direct sunlight.
    Application of Sadara HDPE 17450N

    Sadara HDPE 17450N is a narrow-molecular-weight injection moulding grade with a nominal melt flow rate of 17 g/10 min at 190 °C/2.16 kg (ISO 1133-1:2022). In food and beverage closure production, the grade is processed on toggle or hybrid presses ranging from 1800 kN to 2500 kN clamp force with 32-48 cavity valve-gated cold-runner tools. The barrel temperature profile is maintained at 210-240 °C, the nozzle set-point at 225-235 °C, and the mould at 10-25 °C using chilled water. Fill speed is set between 150 mm/s and 250 mm/s for wall sections in the 0.9-1.4 mm range, and hold pressure is staged from 45 MPa to 15 MPa across 0.5-1.2 s. Screw plasticating units with L/D of 20:1-25:1 and compression ratio of 2.5:1-3.5:1 are preferred; non-return valve clearance beyond 0.15 mm creates shot-weight variability exceeding 0.4%, which shifts closure skirt ovality outside the ±0.05 mm band required for capping torque retention. The melt must not exceed 250 °C; above this threshold gel particles form and low-molecular-weight volatile compounds increase in the cavity air load. Below 215 °C, the valve-gate tip pressure drop blocks short-shot compensation in thin closure skirts. Slip additives are kept at 0.05-0.08 wt%; above 0.08 wt%, seven-day torque-retention tests at 1.5 N·m application force show a decline in removable torque consistency. Colour masterbatch is metered at 1.5-2.5 wt%; higher loadings increase gate blush and reduce the elongation at break of the tamper-evident band. Food-contact conformity is established under FDA 21 CFR §177.1520 for olefin polymers and EU Regulation 10/2011, with overall migration tested under 10 mg/dm² limit conditions. Organoleptic performance is checked by purge cycling of 15-20 min after colour change. Terminal products include still-water closures, juice screw caps, dairy snap caps, and tamper-evident spout overcaps. Production failure modes observed on high-speed lines are top-disk gate blush, sink marks over the knurl band, and stress cracking at the inner skirt corner when pigment masterbatch exceeds 2.5 wt%.

    Comparative processing window across three injection moulding segments:

    ParameterClosuresThin-wall dairy containersIndustrial pails
    Melt temperature210-240 °C220-245 °C220-250 °C
    Mould temperature10-25 °C12-20 °C12-18 °C
    Injection velocity150-250 mm/s200-350 mm/s80-140 mm/s
    Hold pressure15-45 MPa40-70 MPa20-60 MPa
    Cooling time4-8 s3.5-6.0 s15-25 s
    Clamp force1800-2500 kN2000-3500 kN6000-8000 kN

    What Limits Thin-Wall Dairy Container Impact Performance at −18 °C?

    Thin-wall injection moulded dairy spread tubs and frozen dessert cups made from HDPE 17450N are constrained by the brittle point shift upward when wall stock falls below 0.8 mm. Pellet impact values do not independently control part performance; moulded-in stress at the base radius dominates. The nominal notched Izod impact at 23 °C is tested under ASTM D256-23; low-temperature container performance is evaluated by dart drop under ASTM D2463-15 at −18 °C. Weld lines from multi-point direct edge gates fail sequentially when the melt does not maintain core temperature of 220-230 °C, because molecular orientation and weld healing stop before the flow front fuses. To maintain ductile behaviour, converters dry-blend 5-15 wt% LLDPE; this reduces flexural modulus to 800-950 MPa from a typical HDPE injection range of 1100-1300 MPa (ISO 178:2019) and reduces top-load strength by 10-15%, requiring rib depth additions of 0.5-1.0 mm. Food-contact conformity rests on FDA 21 CFR §177.1520 and EU Regulation 10/2011, with specific attention to pigment masterbatch purity because primary aromatic amine migration must remain below the applicable detection limit in aqueous simulants. The conversion line uses 2000-3500 kN hybrid presses with accumulator-assisted injection speeds of 200-350 mm/s, mould temperature 12-20 °C, and cooling time 3.5-6.0 s for 400-600 mL containers. Transfer pressure is held at 65-85 MPa; variation exceeding 5 MPa is associated with stacking rim ovality and lid slip. Terminal products include margarine tubs, frozen dessert cups, and thin-wall dip containers. Published data for this specific grade in frozen dairy interchange trials is limited; plant validation against each tool geometry is required.

    Industrial Pail Handle Boss and Gate Freeze-Off Behaviour

    Injection moulded pails in the 5-25 L range use HDPE 17450N in thick-to-thin flow paths where the handle boss section exceeds 4.0 mm while sidewall thickness is 1.6-2.2 mm. The cooling time constant mismatch creates packing imbalance: the boss remains molten for 8-10 s after the wall freezes, but the mould is opened on wall ejection temperature of 70-80 °C. If the boss is not packed through a separate gate, shrinkage across the boss bore exceeds 0.10 mm and the ejector pin binds. The preferred gating arrangement is a valve-gated hot runner with the boss gate opened 0.2-0.4 s earlier than the wall gates; hold pressure is profiled at 50-60 MPa for 2.5-4.0 s, then 20-30 MPa for 1.5-2.0 s. Clamp force for a 10 L pail in a single-face tool is 6000-8000 kN at peak injection pressure of 90-110 MPa. Pigment and UV stabilizer masterbatch is metered at 1.5-3.0 wt%; carbon black or HALS additions above 3.5 wt% are excluded because weld-line elongation falls below 20% under ISO 527-2:2012. For dangerous goods packaging, the filled pail is evaluated under the UN Manual of Tests and Criteria, Part III, 6.1.5, or the applicable ADR/RID chapter, with drop height 1.2 m for packing group II, stack load for 24 h at 40 °C, and hydraulic pressure of 20 kPa. Food pails are checked under FDA 21 CFR §177.1520; chemical compatibility for agricultural formulations uses immersion at 23 ± 2 °C and 50 ± 2 °C for 21 days in the specific filled liquid. Production failure modes include handle boss sink marks and rim ovality when the mould opens above 75 °C. Reducing cooling water outlet from 18 °C to 12 °C can restore diameter but increases cycle time by 1.0-1.5 s.

    Overcap injection for aerosol and personal-care packaging with HDPE 17450N is governed by high-speed ejection and snap-bead dimensional stability rather than long-term hydrostatic exposure. The side wall is typically 0.7-1.1 mm, with draft angle of 1.0-1.5° and top disk flatness below 0.15 mm after cooling. Melt temperature is held at 225-245 °C to avoid colour shift in light-tinted mouldings; residence time above 6 min at 245 °C causes yellowing and gloss loss below 60 GU at 60° geometry under ISO 2813:2014. Injection is profiled with a first stage at 120-150 mm/s through the top disk and a second stage at 60-90 mm/s when the flow front enters the side-wall transition to prevent jetting. The mould operates at 15-25 °C with high-turbulence water circuits; cycle time for a 52 mm overcap is 5.5-7.0 s on an 8-16 cavity cold-runner tool. The radial snap bead is checked with a plug gauge: the undercut holds 0.25 ± 0.05 mm interference with the can curl. Compliance for cosmetic packaging is governed by EU Regulation 1223/2009 and related packaging framework requirements; the compound is verified against heavy-metal and hazardous-substance restrictions under REACH 1907/2006 Annex XVII. Terminal products include aerosol overcaps, shaving foam covers, and fragrance actuator caps. Static dust pickup after ejection is controlled with anti-static masterbatch below 0.5 wt%; higher levels reduce snap-bead modulus and create leak-test failures in overcap fit.

    When Storage Articles Are Moulded Below 1.0 mm Wall Thickness in Long Flow Paths

    Stackable household storage boxes and drawer organisers produced from HDPE 17450N impose flow length-to-wall ratios above 220:1, which require low-viscosity processing but also create warp potential at the base plate. The mould filling strategy uses sequential valve gating with delay times of 0.3-0.8 s between banks; melt temperature is set at 220-245 °C, mould temperature at 15-25 °C, and fill speed at 180-300 mm/s. Pack pressure is kept at 30-50 MPa to minimise packing-induced shrinkage anisotropy; excessive packing produces post-ejection bow of the base exceeding 0.35 mm per 100 mm straight edge. Food-contact storage articles are tested under FDA 21 CFR §177.1520 and EU Regulation 10/2011; for non-food storage, mechanical performance is verified by drop tests at 25 °C and 0 °C. Hinges or integral clips are not recommended when the wall stock is below 0.9 mm, because orientation in the hinge zone splits after 2000 flex cycles unless a radius of at least 0.4 mm is added. Terminal products include drawer organisers, storage boxes, and wardrobe accessories. Colour masterbatch is metered at 1.0-3.0 wt%; higher loadings reduce the flow front velocity at the same hydraulic setting by 3-5% and shift the balance point of the hot runner. In production, short-shots in the far cavity of an 8-24 cavity family tool are corrected by raising the nozzle temperature to 245 °C rather than increasing hold pressure, because hold pressure above 50 MPa increases gate blush and floating core deflection.

    For injection moulded toys and assembled consumer durables, HDPE 17450N is specified where low-temperature ductility is less critical than geometric reproducibility and low residual odour. The grade is processed at melt temperature 215-235 °C and mould temperature 12-20 °C on machines with 1000-3000 kN clamp force, depending on part projected area. Regulatory testing for toys requires compliance with EN 71-3 migration of elements, with the applicable limit category determined by the final article material form; phthalate content is controlled under REACH 1907/2006 Annex XVII entries 51 and 52. Because the base resin is an unplasticised polyolefin, phthalate-free compliance is inherent but pigment carriers and mould-release sprays must be checked. Multi-component assemblies require insertion of threaded brass inserts, metal springs, or snap-fit joints. Sink marks at the opposite side of a boss are controlled by a boss outside diameter of 2.0-2.5× the nominal outside diameter and a wall thickness below 60% of the adjacent surface; for HDPE 17450N, this ratio reduces sink depth to below 0.03 mm in texture-free surfaces measured by profilometry. Published data for this specific grade in toy mechanical durability protocols is limited; validation is performed against customer-specific pull-test and drop-test sequences. Terminal products include building block components, assembly toys, and small rigid cases.

    ApplicationRegulatory/Standard ReferenceTest Method or ConditionLimits / Control Values
    Food-contact closuresFDA 21 CFR §177.1520; EU Regulation 10/2011Overall migration, aqueous/acidic/fatty simulants10 mg/dm²
    Dairy containersEU Regulation 10/2011; FDA 21 CFR §177.1520Specific migration; organoleptic panelPrimary aromatic amines below detection limit
    Industrial pailsUN Manual of Tests and Criteria, Part III, 6.1.5; ADR/RIDDrop, stack, hydraulic pressure20 kPa hydraulic; 1.2 m drop for PG II
    Cosmetic overcapsEU Regulation 1223/2009; REACH 1907/2006Annex XVII heavy-metal restrictionsNo intentionally added heavy metals
    ToysEN 71-3; REACH 1907/2006 Annex XVIIMigration of elements; phthalate contentCategory-dependent migration limits
    Free Quote

    Competitive Sadara HDPE 17450N prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sadara HDPE 17450N is a high-density polyethylene injection molding resin supplied by Sadara Chemical Company. The nominal melt flow rate is 17 g/10 min when measured at 190 °C under 2.16 kg load in accordance with ISO 1133-1, and the nominal density is 0.950 g/cm³ by ISO 1183-1. The grade is specified for thin-wall food containers, caps, closures, housewares and rigid consumer packaging where short cavity filling time and rapid demolding are required. Typical values from the published technical data sheet include tensile stress at yield of 26 MPa by ISO 527-2, flexural modulus of 1200 MPa by ISO 178, Charpy notched impact strength of 4.0 kJ/m² at 23 °C by ISO 179-1/1eA, Vicat softening temperature of 124 °C by ISO 306/A50, and deflection temperature under load of 68 °C at 0.45 MPa by ISO 75-2/B. Mold shrinkage is typically 1.5–2.5% in the flow direction and 1.0–2.0% transverse to flow, depending on part thickness and gate geometry.

    PropertyStandardConditionNominal Value
    Melt flow rateISO 1133-1190 °C / 2.16 kg17 g/10 min
    DensityISO 1183-123 °C0.950 g/cm³
    Tensile stress at yieldISO 527-250 mm/min26 MPa
    Tensile strain at yieldISO 527-250 mm/min8%
    Flexural modulusISO 1782 mm/min1200 MPa
    Charpy notched impact strengthISO 179-1/1eA23 °C4.0 kJ/m²
    Vicat softening temperatureISO 306/A5010 N124 °C
    Deflection temperature under loadISO 75-2/B0.45 MPa68 °C
    Shore D hardnessISO 86815 s66

    In multi-cavity hot-runner closure molds, the principal processing risks are short shot formation in narrow gates, warpage caused by asymmetric cooling, and sink marks opposite thick ribs. These failure modes are controlled by melt temperature, pack pressure, mold temperature and gate geometry rather than by resin lot variation alone.

    What processing conditions control warpage and cycle time in injection-molded components?

    Melt temperature should be evaluated against the measured melt flow rate and the runner balance. A barrel profile from rear 190 °C to nozzle 220–230 °C is a practical starting range. At melt temperatures below 190 °C, injection pressure increases and gate freeze becomes probable in land lengths greater than 1.0 mm. At melt temperatures above 250 °C, thermo-oxidative chain scission becomes measurable as a reduction in melt viscosity and a color shift toward yellow; copper-containing mold components accelerate this degradation at elevated temperatures. The maximum recommended barrel residence time is 5 min, with shorter residence preferred for hot-runner systems operating above 230 °C.

    Mold temperature is typically maintained between 15 °C and 40 °C for fast skin formation and short cycle time. Increasing mold temperature to 40–60 °C improves weld-line strength and gloss but may raise cycle time by 8–12% because the lower thermal diffusivity of the polymer requires additional conductive heat removal through the mold base. Uniform cooling channel spacing of 1.5–2.0 times the part wall thickness is necessary to avoid differential shrinkage in rectangular containers with wall thickness below 1.0 mm.

    Injection pressure on production-scale equipment is usually recorded in the range of 60–100 MPa, depending on flow length and gate diameter. Holding pressure is typically 40–70% of injection pressure and is applied for 0.5–1.5 s per millimeter of nominal wall thickness. Back pressure should be set at 0.3–0.7 MPa; below 0.3 MPa, screw recovery may become erratic and unmelted granules can reach the check ring, producing part weight variation of more than 0.5% in high-cavitation molds. Above 0.7 MPa, melt temperature increases due to viscous heating and the residence time distribution widens, which raises the risk of color shift in natural grades.

    Screw design affects homogeneity and cycle time. A general-purpose single-flight screw with 20:1 to 25:1 L/D ratio and compression ratio of 2.5:1 to 3.0:1 is suitable. A check ring with reliable sealing is mandatory because the high MFR permits backflow during injection if the ring wear exceeds 0.1 mm. Nozzle shut-off is recommended for thin-wall molding to prevent drool during mold open periods longer than 3 s.

    Drying is not normally required at ambient relative humidity below 60%. If surface condensation is present due to warehouse storage or rapid temperature change, the resin should be dried at 80 °C for 2 h using desiccant dry air with a dew point below -30 °C. Extended drying above 90 °C can cause pellet surface softening and bridging in the hopper. The resin should not be compounded with moisture-releasing fillers or additives unless the venting system can remove the liberated volatiles; otherwise surface splay and internal porosity can occur in parts with wall thickness greater than 2.0 mm.

    Thin-wall packaging and closure applications account for the largest volume share of this material. In high-cavitation molds, the high flow rate reduces injection pressure relative to lower-MFR HDPE grades, but it also reduces melt strength. This makes the grade unsuitable for extrusion blow molding and pipe extrusion. In press-side comparisons, molders report lower cavity pressure at equivalent fill speed than HDPE grades with MFR between 7 g/10 min and 10 g/10 min; however, the exact pressure reduction depends on gate size, wall thickness and hot-runner temperature, and published data for specific high-cavitation configurations is limited.

    Regulatory compliance for the finished article depends on the full formulation, not on the base resin alone. The grade is supplied in natural form without intentionally added slip or antiblock agents beyond the stabilization package. For food contact use, the polymer is typically covered under FDA 21 CFR 177.1520 as an olefin polymer, subject to end-use condition and additive verification. For the European Union, compliance with Regulation (EU) No 10/2011 must be demonstrated through migration testing on the final molded part. The resin is subject to registration obligations under REACH Regulation (EC) No 1907/2006 only to the extent applicable to its monomer and additive constituents; the polymer itself is exempt from registration. Under RoHS Directive 2011/65/EU, bulk HDPE is not expected to contain restricted heavy metals above the permitted concentration limit, but final assembly verification is required.

    RegulationDesignationApplicability
    U.S. food contactFDA 21 CFR 177.1520Olefin polymers; final additive compliance required
    EU food contactRegulation (EU) No 10/2011Migration testing on final article required
    REACHRegulation (EC) No 1907/2006Monomer and additive registration obligations apply
    RoHSDirective 2011/65/EUFinal assembly verification required
    EU packaging heavy metalsDirective 94/62/ECSum of lead, cadmium, mercury, hexavalent chromium below 100 mg/kg

    When high-flow HDPE 17450N replaces standard MFR 7–10 g/10 min injection grades

    Direct substitution into an existing mold requires adjustment of pack pressure, cooling time and gate seal time. The higher MFR reduces the minimum fill pressure, but the lower melt viscosity also shortens the gate seal time; if the hold pressure is terminated before gate freeze, molten polymer can flow back from the cavity and produce sink marks or dimensional drift. Gate diameter should be 50–70% of the nominal wall thickness, and gate land length should be kept below 1.0 mm to avoid premature solidification. On a 1200 kN electric toggle clamp machine molding 0.8 mm wall dairy containers, clamp force demand is approximately 3.5 kN/cm² of projected area, with actual values influenced by flow direction and venting.

    Compared with HDPE injection grades having MFR of 4–8 g/10 min and density of 0.952–0.958 g/cm³, the lower density of this grade is associated with a measurable reduction in flexural stiffness. Stiffness-driven applications such as pails and structural crates may require a rib depth increase of 10–15% to maintain equivalent top-load performance. Similarly, environmental stress crack resistance measured by ASTM D1693 is expected to be lower than that of high-molecular-weight HDPE grades, particularly in contact with aggressive surfactants, oils or hydrocarbon-containing liquids. For cap and closure applications involving hot-filled fatty foods or cosmetic solvents, preliminary bent-strip ESCR testing on the finished article is required; published data for this specific configuration is limited.

    The grade is not designed for extrusion blow molding because its melt strength is insufficient to maintain a stable parison. When compared with blow molding HDPE grades having MFR of 0.3–0.8 g/10 min, the parison sag rate is substantially higher, and continuous blow molding equipment cannot reliably control wall thickness. The grade is also not intended for pressure pipe service under ISO 9080 long-term hydrostatic strength evaluation or for ISO 12162 PE100 classification.

    Storage before processing should be in a dry, closed silo or original packaging at temperatures below 50 °C. Long-term exposure to ultraviolet radiation causes surface oxidation of pellets and should be avoided for natural grades. If outdoor storage is unavoidable, the material should be protected with an opaque cover that does not transfer plasticizer or colorant to the pellet surface. Reclaimed material from post-industrial scrap can be incorporated only after verification of melt flow rate, density and contamination; typical in-house regrind addition is below 20 wt% for food packaging, but the maximum level must be set by the converter’s quality system and applicable food contact requirements.

    Top