| HS Code | 734500 |
| Polymer Base | Polybutylene terephthalate (PBT) |
| Reinforcement | Unreinforced |
| Flame Retardancy | Flame retardant |
| Hydrolysis Resistance | Hydrolysis resistant |
| Density | 1.31 g/cm3 |
| Melt Volume Rate | 10 cm3/10 min (260°C/2.16 kg) |
| Tensile Modulus | 2600 MPa |
| Tensile Stress At Yield | 55 MPa |
| Tensile Strain At Break | 50% |
| Flexural Modulus | 2400 MPa |
| Flexural Strength | 85 MPa |
| Notched Izod Impact Strength | 5 kJ/m2 (23°C) |
| Heat Deflection Temperature At 1 8 Mpa | 60°C |
| Heat Deflection Temperature At 0 45 Mpa | 150°C |
| Ul94 Flammability Rating | V-0 at 0.75 mm |
As an accredited SABIC VALOX™ Unreinforced PBT HR326 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ Unreinforced PBT HR326 is supplied in 25 kg moisture-barrier bags, palletized and stretch-wrapped for shipping. |
| Container Loading (20′ FCL) | SABIC VALOX™ Unreinforced PBT HR326 loaded in a 20-foot FCL container, palletized and secured for safe sea transport. |
| Shipping | SABIC VALOX™ Unreinforced PBT HR326 is shipped as non-hazardous polymer pellets in moisture-barrier bags, lined boxes, or octabins. It is not regulated for transport. Store in a cool, dry area away from direct sunlight and ignition sources; consult the SDS for handling guidance. |
| Storage | Store SABIC VALOX™ Unreinforced PBT HR326 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep original bags or containers tightly closed to prevent water absorption and contamination. Use first-in, first-out stock rotation. Avoid prolonged storage in humid conditions; dry material before processing if recommended by the manufacturer. |
| Shelf Life | Typically indefinite when stored dry and cool in original sealed packaging, protected from moisture, heat, and direct sunlight. |
Under-hood connector bodies and sensor carriers molded from unreinforced PBT are subjected to continuous thermal soak at 85°C and 85% RH in qualification protocols such as IEC 60068-2-30 Db variant cycling and SAE USCAR-2 humidity exposure. In this environment, standard unreinforced PBT loses tensile strength through ester hydrolysis, with fracture initiating at knit lines and sharp corners where residual stress and crystallinity gradients are highest. HR326 is selected for its hydrolysis-resistant molecular structure, but component survival is not a resin property alone; it depends on drying protocol, tool temperature, and regrind management. Production-scale use typically begins with desiccant drying at 120°C for 3–4 h to residual moisture ≤ 0.02% per ISO 15512, with dryer dew point maintained at ≤ -40°C and closed feed throat to prevent moisture re-uptake when ambient relative humidity exceeds 60% RH. The formulation is 100 parts HR326 predried resin, 1.0–2.0 wt% carbon black or color masterbatch, and clean dry regrind at 10–20 wt%; regrind is reduced to ≤ 10 wt% when the part must survive 1,000 h of 85°C/85% RH aging because repeated thermal history narrows molecular weight distribution and accelerates moisture ingress at flow fronts. Avoid unneutralized amine-containing color concentrates; residual amines catalyze ester hydrolysis at processing temperatures. Injection molding is run on a 20:1–24:1 L/D general-purpose screw with barrel zones at 240–255°C, nozzle at 250–260°C, mold at 75–85°C, injection velocity 80–120 mm/s, hold pressure 55–70 MPa, and melt residence above 265°C limited to 5 min. Terminal parts include engine sensor housings, transmission range sensor carriers, EGR valve connector bodies, and camshaft position sensor housings. Published multiyear continuous hot-glycol immersion data for this specific HR326 configuration are limited; component-level pressure-cycling validation remains required before use in direct liquid-cooled housings.
In laundry and dishwashing appliances, pump covers and flow-restrictor bodies are exposed to oscillating water temperature from 20°C to 95°C and detergent solution pH between 8 and 10. The replacement of glass-filled PBT with unreinforced HR326 in these parts removes the capillary path along glass-fiber bundles that delivers water directly to the resin matrix, a known failure mode in hot-water pump bodies after 1,500–2,000 h of intermittent duty. Compliance is typically evaluated under IEC 60335-1 for leakage current and glow-wire ignition, UL 746B for relative thermal index, and IEC 60529 for ingress protection. In production, the formula is 100 parts HR326 dried to residual moisture ≤ 0.02% per ISO 15512; white masterbatch addition is held at 1.5–2.5 wt% and silicone-based processing aid at 0.2–0.4 wt%, with regrind capped at 15 wt% because wet-heat aging accelerates chain scission of previously hydrolyzed regrind. Molding is performed with melt at 255–265°C, mold at 80–90°C to force higher surface crystallinity, hold pressure 60–80 MPa, and cooling time of 25–35 s for a 2.0 mm nominal wall. The resulting terminal parts are condensate pump housings, drain pump covers, flow-meter bodies, and steam generator sensor floats.
Miniature relay bobbins with wall sections between 0.45 mm and 0.80 mm exhibit process hysteresis if regrind content is increased beyond a defined threshold, because the unreinforced PBT melt loses shear-thinning character when the molecular weight distribution is narrowed by repeated extrusion-history thermal exposure. The shear-heating limit in an 8-cavity or 16-cavity hot-runner tool becomes the controlling variable: a 22–28 mm diameter screw with high recovery speed will locally push melt through sub-0.30 mm gate lands at shear rates approaching 10,000 s⁻¹, raising melt temperature at the gate by 10–15°C above the set barrel value. If nozzle setpoint is 250°C, gate melt may approach 265°C; if regrind exceeds 20 wt%, the viscosity shift causes short-shot or weld-line brittleness in the bobbin flange. The permissible regeneration ratio is therefore limited to 10–15 wt% for bobbin walls below 0.60 mm, with 100 parts HR326 predried to ≤ 0.02% moisture, 0.5–1.0 wt% laser-marking masterbatch, and no external mold release because surface residues interfere with subsequent coil winding adhesion. Barrel zones are run at 245–255°C, hot runner manifold at 250–260°C, mold at 70–90°C, injection speed 150–250 mm/s, and back pressure 2–4 MPa. The component is verified under IEC 61810-1 for electromechanical relay endurance, UL 1446 for insulation systems, UL 94 HB for flammability, and IEC 60112 for comparative tracking index. Terminal products include PCB relay bobbins, contactor coil formers, timer base plates, and solenoid actuation bases.
In brushed universal motor tools, power tool trigger housings and brush-card frames are injection molded from unreinforced PBT where dimensional stability under transient heating from current-carrying contacts is more critical than structural load-bearing performance. The trigger housing must maintain contact separation distance after repeated thermal excursions from 60°C to 120°C at the contact bridge; HR326 is processed with 100 parts predried resin, 1.0–2.0 wt% color masterbatch, 0.5–1.0 wt% carbon black masterbatch for UV-laser marking, and 0.2–0.5 wt% metal stearate internal mold release. Regrind is limited to 20 wt% for wall sections above 1.0 mm, but for thin snap-fit arms below 0.80 mm the regrind fraction is reduced to 10 wt% because impact strength at the gate area drops when orientation from repeated processing causes anisotropic shrinkage. The molding window uses melt temperature 250–260°C, mold temperature 65–80°C, hold pressure 50–65 MPa, and fill speed 100–150 mm/s to avoid jetting at the flat contact base. Component compliance follows IEC 62841-1 for motor-operated hand-held tools, UL 746B for thermal aging, and UL 94 HB for material flammability. The terminal articles are variable-speed trigger housings, brush-card frames, reverse-switch chambers, and microswitch bases.
Across 16-cavity sensor carrier molds, sequential valve gating is programmed so that the flow front from gate 1 does not merge with gate 2 at the O-ring groove; if the fronts meet at a seal surface, the resultant weld line creates a moisture ingress path under IP67 validation per IEC 60529. HR326 is predried at 120°C for 4 h to ≤ 0.02% residual moisture; the formulation uses 100 parts HR326, 1.0–1.5 wt% color masterbatch, 0.1–0.3 wt% ethylene bis-stearamide processing aid, and clean regrind not exceeding 15 wt% to hold shot-to-shot viscosity constant. The downstream injection molding process operates with a 30 mm screw, melt at 250–260°C, mold at 75–85°C, fill speed 120–180 mm/s, and hold pressure 55–70 MPa. Gate seal time is set at 0.4–0.7 s after fill to avoid overpacking thin castellations that locate the printed circuit board. Compliance of the finished carrier is assessed under IEC 61010-1 for electrical safety of industrial control equipment, IEC 60068-2-30 for damp heat, and ISO 527-2 for tensile properties. Terminal products include inductive proximity sensor carriers, photoelectric sensor housings, flow-meter sensor bodies, and level switch floats.
Competitive SABIC VALOX™ Unreinforced PBT HR326 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ HR326 is an unreinforced polybutylene terephthalate (PBT) injection-molding resin supplied in pellet form. The grade is positioned for applications in which an unfilled PBT must retain snap-fit ductility and dielectric integrity after exposure to hot, humid air or intermittent condensation. Physical data reported for the resin include a density of 1.30–1.32 g/cm³ under ASTM D792 and water absorption after 24 h at 23°C of 0.08% under ASTM D570. Because the compound is unfilled, mold shrinkage in the flow direction is typically 1.4–1.8% under ASTM D955, which is higher than shrinkage for glass-reinforced PBT and therefore affects cavity dimensions, gate placement, and cooling-channel layout in multi-pin connector housings.
The short-term property values in Table 1 represent typical ranges for unfilled hydrolysis-resistant PBT. They are not lot-specific guarantees and should be checked against the current SABIC datasheet and the UL Yellow Card file number. The absence of glass fiber in HR326 reduces abrasive wear on barrels and screws and permits lower melt pressure during filling of thin sections below 0.8 mm.
| Property | Standard | Typical value or range |
|---|---|---|
| Density | ASTM D792 | 1.30–1.32 g/cm³ |
| Tensile stress at yield | ASTM D638, Type I, 50 mm/min | 50–55 MPa |
| Tensile strain at break | ASTM D638 | >200% |
| Flexural modulus | ASTM D790 | 2200–2500 MPa |
| Flexural strength | ASTM D790 | 80–90 MPa |
| Notched Izod impact at 23°C | ASTM D256 | 25–40 J/m |
| Heat deflection temperature at 1.82 MPa | ASTM D648 | 54–60°C |
| Vicat softening temperature, Rate B/120 | ASTM D1525 | 175–185°C |
| Water absorption, 24 h at 23°C | ASTM D570 | 0.08% |
| Mold shrinkage, flow direction | ASTM D955 | 1.4–1.8% |
| Dielectric strength | ASTM D149 | 16–18 kV/mm |
| Volume resistivity | ASTM D257 | 1.0 × 1015 Ω·cm |
| UL flame class | UL 94 | HB |
The unfilled composition places HR326 among the lower-viscosity PBT materials used for thin-wall electrical encapsulation, where glass-free flow behavior permits filling of complex connector geometries without fiber-induced anisotropic shrinkage. The short-term heat deflection temperature under 1.82 MPa remains in the region of 54–60°C; the material is therefore not a substitute for glass-reinforced PBT in load-bearing housings requiring continuous elevated-temperature stiffness. Electrical values for unfilled PBT, including comparative tracking index under IEC 60112, are typically favorable for low-voltage connectors, but final values should be obtained from the active datash sheet and the UL Yellow Card.
Because the terephthalate ester linkage in PBT is the primary reactive site for hot-water degradation, the hydrolysis-resistant formulation modifies the degradation pathway rather than the base polymer architecture. The hydrolysis reaction proceeds by autocatalytic carboxylate end-group formation; reported apparent activation energy values for unfilled PBT hydrolysis often fall in the 70–100 kJ/mol range. This means degradation accelerates steeply above 85°C, and a hydrolysis-resistant package can shift the failure time but cannot eliminate the reaction. In humid environments above 85°C, standard unfilled PBT grades lose tensile elongation at break over several hundred hours. Automotive qualification programs commonly require 85°C/85% RH exposure for 1000 h with retention of snap-fit insertion force, dielectric strength, and visual surface integrity. Published data for HR326 in openly available datasheets is limited, but the HR suffix identifies the grade as one of the hydrolysis-stabilized VALOX™ materials selected for humid underhood packaging.
Resistance is not absolute. Continuous immersion in pressurized hot water above 85°C or exposure to alkaline solutions with pH greater than 10 remains outside the intended envelope because ester hydrolysis is base-catalyzed. The grade should not be combined with amine-based additives or water-soluble metal salt corrosion inhibitors in regrind, because these ingredients can accelerate chain scission during melt processing and reduce molded-part toughness. End-group analysis by titration or chromatographic detection of degradation products is not routinely used on production lines; instead, notched Izod impact retention and tensile elongation after aging serve as practical indicators of hydrolysis damage.
For chemical contact in underhood environments, screening should be conducted under ASTM D543 immersion protocols using the actual production fluid, because fuel and coolant packages vary by OEM. Unfilled PBT generally withstands mineral oil, unleaded gasoline, and diesel at moderate temperatures below 60°C; however, brake fluid, methanol-blended fuels, and hot ethylene glycol/water mixtures above 100°C can plasticize or degrade the polyester. The hydrolysis-resistant package of HR326 does not confer resistance to those media. Ultraviolet exposure also embrittles unfilled natural PBT; black or UV-stabilized versions are required for outdoor connectors unless the part is fully shielded. If flame retardance is required, a non-halogenated V-0 unreinforced PBT grade should be specified instead, because HR326 carries an HB classification and must not be used where a V-0 rating is required without additional shielding.
On injection molding machines with screws of L/D 20:1–24:1, HR326 is processed with a barrel profile of 240–260°C from feed to nozzle and a mold temperature of 66–93°C. The unfilled melt exhibits pronounced shear-thinning; published data for unfilled PBT generally place apparent viscosity below 100 Pa·s at shear rates above 1000 s-1 and 250°C. This low viscosity enables thin-wall filling but also increases flash risk on equipment with marginal clamp force. For a 2.0 mm plaque, the projected-area clamp force should not be less than 4.0 kN/cm²; thin-wall connector housings may require 6.0 kN/cm² or more depending on flow length and injection speed.
Drying before processing is mandatory. Desiccant drying at 121°C for 3–4 h to a pellet moisture content below 0.02% is standard; a dryer dew point of −40°C or lower is recommended. At plant relative humidity above 60%, open hoppers and unheated transfer lines can reintroduce surface moisture within minutes. Production-scale failures observed on injection lines include splay, viscosity loss, weld-line delamination, and intermittent gate-stringing when barrel residence time exceeds 5 min at 260°C. Shot-to-shot moisture variation at or above 0.03% is usually detected first as reduced notched Izod impact and degraded tensile elongation in molded test bars. Nozzle drool is controlled by decompression after screw recovery, typically 3–5 mm depending on nozzle diameter; excessive decompression causes air entrapment and bubble defects.
Mold temperature below 60°C is not recommended because underdeveloped crystallinity produces excessive post-mold shrinkage and gloss variation. Differential scanning calorimetry per ISO 11357-3 can be used to confirm crystallization behavior; unfilled PBT typically shows a melt crystallization exotherm near 190°C during cooling at 10°C/min. Gate dimensions should be at least 50% of wall thickness to avoid premature gate freeze, and hold pressure should be maintained until the gate seals. For unfilled PBT, hold times below 0.5 s per mm of wall thickness may produce sink marks and shrinkage voids in boss areas and snap-fit roots. High-speed injection with profiled velocity is preferred for connectors with living hinges or snap-fit tabs. Regrind levels up to 20 wt% are used on production lines when hydrolytic stability after molding is critical, provided the regrind is dried and free of oil contamination; each additional heat cycle reduces molecular weight and elongation at break.
In underhood connector applications, selection is made after thermal-humidity cycling rather than short-term tensile data alone. HR326 is used in relay sockets, sensor housings, junction boxes, and terminal blocks where the design operates within the unfilled PBT thermal envelope and requires lower moisture absorption than polyamide 66. PBT absorbs approximately 0.08% moisture after 24 h under ASTM D570; polyamide 66 typically absorbs several percent, which can shift dielectric performance and dimensional pitch in multi-cavity connectors. The hydrolytic stabilization of HR326 delays surface-cracking and tensile elongation loss after intermittent condensation exposure relative to general-purpose unfilled PBT; initial tensile stress at yield, flexural modulus, and heat distortion temperature remain in the typical unfilled PBT range.
Compared with a 30% glass-fiber-reinforced PBT grade, HR326 has lower flexural modulus, lower heat distortion temperature, higher mold shrinkage, and higher elongation. The unfilled grade is not appropriate for large load-bearing housings requiring continuous stiffness at temperatures above 120°C; those designs are commonly assigned to reinforced PBT or PBT/ASA blends. Conversely, HR326 is preferred for complex cavities with long, thin-walled snap-fit geometry where fiber orientation in reinforced grades produces anisotropic shrinkage, warpage, and reduced living-hinge fatigue life. Molded components produced in HR326 should be dimensionally checked after 48 h post-mold conditioning because crystallinity continues to develop after ejection; parts measured immediately will not represent final as-molded dimensions.
Electrical and electronic qualification generally requires creepage resistance under IEC 60664-1, dielectric strength under ASTM D149, comparative tracking index under IEC 60112, and hydrolytic aging under an OEM-specific 85°C/85% RH protocol. Users should obtain the current UL Yellow Card for final flame class, relative thermal index, and electrical RTI values. REACH and RoHS declarations are supplied through the material documentation system of the supplier. For injection molding plants, lot-to-lot viscosity variation should be monitored by melt flow rate testing under ISO 1133-1 at 250°C and 2.16 kg; a shift outside the supplier’s specified range indicates moisture uptake, thermal degradation, or incorrect drying.