Sabic Valox Unreinforced Pbt 325

SABIC VALOX™ Unreinforced PBT 325

    • Product Name: SABIC VALOX™ Unreinforced PBT 325
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 832900
    Density 1.31 g/cm³
    Melt Volume Rate 13 cm³/10 min at 260°C/2.16 kg
    Tensile Modulus 2400 MPa
    Tensile Stress At Yield 55 MPa
    Tensile Strain At Yield 4.0 %
    Nominal Strain At Break 50 %
    Flexural Modulus 2300 MPa
    Charpy Notched Impact Strength At 23 C 4 kJ/m²
    Hdt At 0 45 Mpa 150 °C
    Hdt At 1 8 Mpa 50 °C
    Vicat Softening Temperature 175 °C
    Molding Shrinkage 1.7-2.3 %
    Water Absorption 0.08 %
    Volume Resistivity 1E15 ohm·cm
    Dielectric Constant At 1 Mhz 3.2
    Thermal Conductivity 0.2 W/m·K
    Coefficient Of Linear Thermal Expansion 7E-5 1/°C

    As an accredited SABIC VALOX™ Unreinforced PBT 325 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ Unreinforced PBT 325 supplied in 25 kg moisture-barrier bags, palletized and securely wrapped for industrial handling.
    Container Loading (20′ FCL) 20′ FCL container loading of SABIC VALOX™ Unreinforced PBT 325, palletized bags securely stowed and evenly distributed for safe ocean transport.
    Shipping Shipping description: SABIC VALOX™ Unreinforced PBT 325 is supplied as non-hazardous thermoplastic pellets in moisture-barrier bags, lined boxes, or octabins. Store cool, dry, and clean, away from sunlight and contamination. Not regulated for transport; keep packaging sealed until use and follow standard industrial hygiene practices.
    Storage Store SABIC VALOX™ Unreinforced PBT 325 in its original, sealed packaging in a cool, dry, well-ventilated area. Protect from direct sunlight, heat sources, moisture, and contamination. Keep containers closed when not in use and avoid damage or excessive stacking. Follow first-in, first-out stock rotation; if moisture pickup is suspected, dry the resin according to supplier recommendations before processing.
    Shelf Life When stored dry, cool, and in sealed original packaging, SABIC VALOX™ Unreinforced PBT 325 has a shelf life of about 24 months.
    Application of SABIC VALOX™ Unreinforced PBT 325

    In low-voltage terminal block production, SABIC VALOX™ Unreinforced PBT 325 is introduced as the unfilled polybutylene terephthalate phase in connector housings and insulating bases where the design does not require a V-0 flame classification. The compliance framework starts with flammability testing under UL 94 and IEC 60695-11-10; the unfilled grade is typically certified as UL 94 HB, which restricts its use to separated or low-voltage circuits and excludes uninsulated live parts. Electrical insulation properties are evaluated according to IEC 60243-1, molded shrinkage is checked under ISO 294-4, and batch-to-batch melt flow consistency is monitored under ISO 1133-1:2022. In formulation, the neat resin is loaded at 100 wt%; closed-loop regrind is limited to 25 wt% after desiccant drying, and a color masterbatch is metered at 1–2 wt% only when custom pigmentation is required. No flame-retardant masterbatch is added to this grade, because altering the formulation voids the existing UL 94 HB listing unless complete re-certification is performed. Production is carried out on a reciprocating-screw injection molding machine with a shut-off nozzle and a screw L/D ratio of 20:1 to 25:1; the material is pre-dried at 120°C for 3–4 h until residual moisture is below 0.02%. At ambient relative humidity above 60%, open-container handling is restricted and moisture analysis is repeated before start-up. Melt temperature is maintained at 245–260°C, mold temperature at 40–80°C, and total heated residence time below 5 min; when barrel temperatures exceed 260°C, hydrolytic chain scission accelerates and weld-line impact strength decreases. Processing failure modes recorded on production lines include silver streaks, gas splay, black specks from hot-runner dead spots, and nozzle drool during screw retraction. Finished product types include DIN-rail terminal block bodies, relay socket shells, switch actuator bases, and electrical connector insulating housings where live-terminal separation is provided by another barrier.

    Cabin thermal cycling imposes a narrow processing window on unfilled PBT clips

    For automotive interior clip bodies and sensor mounting brackets, VALOX 325 provides a semi-crystalline matrix with sufficient elongation for snap-fit assembly, but the unfilled composition imposes a lower continuous-use temperature ceiling than glass-filled PBT. Compliance is governed by the End-of-Life Vehicles Directive 2000/53/EC Annex II and Regulation (EC) No 1907/2006 REACH; restricted-substance screening follows IEC 62321 methods for heavy metals and specific phthalates. Tensile properties for snap-fit deflection are evaluated under ISO 527-2:2012. The base resin is used at 100 wt%; granulated sprues and runners from the same grade are reintroduced at a maximum 20 wt% after identical drying at 120°C to avoid shifts in melt viscosity. An elastomeric impact modifier of 2–3 wt% is deliberately avoided in this clip segment because it reduces tensile modulus and changes snap-fit deflection forces. Molding is performed on a reciprocating-screw machine with a barrel profile from 240°C at the feed throat to 255°C at the nozzle, with mold temperature held at 70–80°C to increase crystallinity and reduce post-ejection warpage. Cold-mold operation below 40°C results in low crystallinity at thin clip arms and can cause brittle fracture at the gate area; insufficient venting at the end of fill produces diesel-effect burn marks. Continuous exposure above 85°C at the clip root can produce creep and disengagement, so under-hood or high-temperature cabin locations are outside the grade’s operational boundary. External regrind from unknown PBT streams is excluded because it introduces uncontrolled contaminant ions and lowers batch-to-batch consistency. Finished product types include door trim retention clips, wiring harness clip bodies, cabin sensor brackets, and cable guide housings.

    Mechanical keyboard keycap tooling is gated to balance fill velocity against shear heating in thin-wall PBT flow paths. In double-shot and dye-sublimated keycap applications, VALOX 325 is selected as the unfilled base because its semi-crystalline surface receives dye sublimation and secondary shot adhesion without the surface roughness or glass-fiber read-through associated with reinforced PBT. Regulatory compliance is limited to RoHS Directive 2011/65/EU Annex II and REACH Regulation (EC) No 1907/2006; the application has no food-contact requirement, and the grade is not specified for toy or mouth-contact products. The formulation uses 100 wt% virgin unfilled PBT; a color masterbatch is metered at 1–2 wt% for pre-colored keycaps, while dye-sublimated sets are molded in a neutral base and printed after processing. Tooling employs polished cavity surfaces with mirror finish and venting at the end-of-fill boundary to avoid burn marks in wall sections below 1 mm. Melt temperature is held at 245–260°C, mold temperature at 60–80°C to improve surface replication and flatness, and hold pressure is profiled to minimize sink opposite thick bosses. Because unfilled PBT has lower melt stiffness than glass-filled PBT, long keys such as spacebars are molded with a conditioned straightening fixture after ejection to control bowing. Short-shot analysis is used to set gate position when multiple bosses and legends create unbalanced filling. Finished product types include mechanical keyboard keycaps, POS keyboard buttons, and precision switch plungers.

    Does UL 94 HB limit internal appliance housings to low-current circuits?

    In small-appliance and power-tool construction, VALOX 325 is specified for internal brackets, motor end caps, and switch mounts where the part is not an outer enclosure for uninsulated live parts and the appliance insulation system does not require a V-0 polymer. The governing product standard is IEC 60335-1 with applicable national deviations, supplemented by glow-wire testing under IEC 60695-2-11 when the end-product standard requires a 550°C or 650°C glow-wire class. UL 94 HB alone is not acceptable for parts that function as a flame barrier. The resin is used at 100 wt% as the neat polymer; color masterbatch is metered at 1–2 wt%, and clean in-house regrind is limited to 20–25 wt% after infrared moisture analysis confirms less than 0.02% residual water. Production is characterized by high-cavitation injection molds with heated sprue bushings and no hot-runner dead spots; melt temperature is maintained at 245–260°C, mold temperature at 50–70°C, and cycle time is adjusted to allow sufficient crystallization before ejection. Unfilled PBT shows lower melt stiffness than glass-filled PBT, so gas entrapment and flow hesitation in thick-to-thin transitions are controlled by staged injection velocity; delamination on large-area surfaces is prevented by holding mold temperature above 50°C. The material is not specified for continuous contact with boiling water, strong alkaline cleaners, or chlorinated hydrocarbons because environmental stress cracking and hydrolytic degradation reduce long-term creep resistance. Finished product types include power-tool motor end caps, vacuum cleaner internal brackets, small-appliance switch mounts, and domestic appliance cord storage housings.

    When lampholder bodies require creep resistance without reinforced-grade warpage

    Within LED lampholder and driver enclosure components, VALOX 325 is used where service temperature remains below 85°C and the part geometry requires lower anisotropic shrinkage than a glass-reinforced PBT alternative. The applicable product safety framework is IEC 60598-1 for luminaires, with glow-wire testing conducted under IEC 60695-2-11 at the end-product level because the unfilled grade itself is not V-0; RoHS Directive 2011/65/EU applies to lead, cadmium, mercury, and hexavalent chromium in all soldered connections and polymer components. The resin is loaded at 100 wt% as the base polymer; a heat stabilization masterbatch may be introduced at 0.5–1.0 wt% only after aging studies under IEC 60216-1 confirm retained insulation resistance after thermal cycling. No fiber reinforcement is added because the resulting anisotropy degrades lampholder screw-thread flatness and contact alignment. Molding is carried out on a machine with a 20:1 L/D screw, reverse-pull decompression, and a shut-off nozzle to prevent drool from smaller shot weights. Melt temperature is maintained at 245–260°C, mold temperature at 60–80°C, and back pressure is kept below 0.5 MPa to avoid shear overheating in hot-runner drops. During production, hot-runner channels without smooth flow transitions cause black specks and resin degradation; published data for this specific unfilled grade in multi-cavity lampholder tools is limited, so startup short-shot studies are required. Finished product types include G9 lampholder bodies, LED tube end caps, driver housing covers, and sensor photocell housings.

    PLC relay base flatness and the role of 0.02% moisture control

    Industrial control relay bases and PLC terminal sockets require flat pin arrays and dimensionally stable holes for insertion force consistency. VALOX 325 is used unmodified because its unfilled composition avoids the anisotropic shrinkage that creates post-mold warpage when a 15% or 30% glass-fiber grade is substituted. The standards package includes IEC 61810-1 for electromechanical elementary relays, UL 94 HB for insulating plastic parts, and ISO 294-4 for molded shrinkage comparison; RoHS Directive 2011/65/EU and REACH Regulation (EC) No 1907/2006 compliance are validated by supplier declarations or X-ray fluorescence screening according to IEC 62321. Formulation addition ratio is 100 wt% neat resin; closed-loop regrind is allowed at 15–20 wt% from sprues and runners dried at 120°C for 3–4 h to a residual moisture content not exceeding 0.02%. Moisture above this threshold reduces molecular weight during plastication and increases the variability of melt viscosity, producing differential cavity filling and pin-position drift. Molding uses a mold temperature of 70–80°C, a melt temperature of 245–260°C, and a hold-pressure profile that compensates for volumetric shrinkage in thick boss sections surrounding metallic inserts. Weld lines should be positioned away from thin latch features by gate placement; published data on weld-line tensile retention for this exact unfilled grade is limited, so mold trials with short-shot analysis are used to establish acceptable gate positions. Finished product types include relay base plates, PLC module terminal sockets, signal conditioner housings, and DIN-rail adapter bodies.

    Free Quote

    Competitive SABIC VALOX™ Unreinforced PBT 325 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ 325 is an unreinforced polybutylene terephthalate injection-moulding grade supplied in pellet form. It is classified under ISO 11469:2016 as PBT. The grade is not a flame-retardant compound; its flammability rating is HB under UL 94 when tested at the thickness and colour listed on the current UL Yellow Card. Representative physical data include a density of 1.31 g/cm³ under ISO 1183-1:2019 and a melt flow rate of 25 g/10 min at 250 °C under 1.2 kg load using ISO 1133-1:2022. The unreinforced structure provides moderate stiffness, predictable melt filling, and reduced anisotropic shrinkage when compared with glass-fibre-reinforced PBT compounds.

    Material designation and test standard matrix

    Under ISO 11469:2016, the resin is identified as PBT. The product is intended for injection moulding of dimensionally defined parts where the absence of fibrous reinforcement avoids excessive melt viscosity and tool wear. The following supplier-published values are representative data obtained from conditioned specimens at 23 °C and 50 % relative humidity unless otherwise stated. They are not specification limits and must be confirmed against the current product datasheet for the specific colour, thickness, and regrind content.

    PropertyTest methodRepresentative value
    DensityISO 1183-1:20191.31 g/cm³
    Melt flow rate, 250 °C/1.2 kgISO 1133-1:202225 g/10 min
    Tensile stress at yield, 50 mm/minISO 527-2/1A55 MPa
    Tensile strain at breakISO 527-2/1A>100 %
    Flexural modulus, 2 mm/minISO 178:20192300 MPa
    Flexural stress at yieldISO 178:201980 MPa
    Notched Izod impact, 23 °CISO 180/A:20234 kJ/m²
    Notched Izod impact, -30 °CISO 180/A:20233 kJ/m²
    Heat deflection temperature, 0.45 MPa flatwiseISO 75-1/-2154 °C
    Heat deflection temperature, 1.8 MPa flatwiseISO 75-1/-255 °C
    Vicat softening temperature, B/50ISO 306:2022180 °C
    Water absorption, 24 h at 23 °CISO 62:20080.08 %

    Why Does Unreinforced PBT 325 Differ from Glass-Reinforced PBT Grades?

    A 30 % glass-fibre-reinforced PBT typically shows a density near 1.53 g/cm³, a flexural modulus between 7000 MPa and 9000 MPa, and a tensile stress at yield between 120 MPa and 140 MPa. Unreinforced VALOX 325 sits at 1.31 g/cm³, 2300 MPa, and 55 MPa, respectively, under the same standard methods. The lower modulus reduces dimensional constraint at crystalline shrinkage, which is why unreinforced PBT parts can exhibit less warpage than glass-filled equivalents in complex geometries despite a higher linear mould shrinkage. Mould shrinkage for VALOX 325 is typically 1.5 % to 1.9 % under ISO 294-4, while glass-filled PBT may be below 0.5 % in the flow direction but higher transversely.

    In comparison with impact-modified unreinforced PBT grades, VALOX 325 trades low-temperature ductility for higher tensile yield strength and lower creep under sustained load. Impact-modified unreinforced PBT may reach notched Izod values above 10 kJ/m² at 23 °C, whereas VALOX 325 is 4 kJ/m² under ISO 180/A:2023. The grade is therefore appropriate for connectors, relay bases, bobbins, and switch housings where mechanical loads are predominantly static and where predictable dielectric loss characteristics are more important than high-energy impact resistance.

    When Exposure to Hot Water Exceeds 60 °C, Hydrolytic Chain Scission Controls Failure

    The limiting degradation route for unreinforced PBT is ester hydrolysis. Published data for continuous hot-water immersion of this specific configuration is limited, but polyester-based thermoplastics cannot be considered hydrolytically stable in hot-water or steam service above 60 °C without stabiliser packages formulated for that environment. VALOX 325 is unsuitable for continuous contact with pressurised steam or hot aqueous glycol above that threshold unless the final part is validated on production tooling. Strong alkaline solutions, hot chlorinated solvents, and ketones are incompatible and should be excluded from service conditions. Resistance to common hydrocarbons, dilute acids, mineral oils, and many automotive fluids may be adequate at ambient to moderately elevated temperatures, but any application involving immersion should be tested under ISO 175:2010 with the final part thickness.

    Pre-drying is not an optional step. The pellet must be dried in a desiccant-bed dryer at 120 °C for 3 h to 4 h to a residual moisture content below 0.02 %. Higher humidity, damaged bag seals, or storage at RH > 60 % increases the drying burden. Undried material can produce surface splay, gas voids, and molecular-weight loss from hydrolysis in the barrel. A closed-loop hopper dryer with dew point at or below -30 °C is recommended. Regrind ratios above 25 % should be evaluated for melt-flow shift and mechanical property retention before production release; higher regrind fractions can lower elongation at break and narrow the processing window.

    Processing parameters requiring closed-loop control on reciprocating injection machines

    Melt temperature should be maintained between 240 °C and 270 °C, with 260 °C as a typical set-point. Barrel residence time above 5 min at 260 °C can shift melt viscosity and cause yellowing or surface splay. Screw L/D ratios of 18:1 to 22:1 with a general-purpose compression section are sufficient because the grade contains no glass or mineral filler. Shorter screws below 18:1 can produce melt-temperature non-uniformity in thin-wall fills and should be avoided on parts with wall sections below 0.8 mm.

    Mould temperature is a primary variable for crystallinity. If the mould surface temperature falls below 40 °C, the part solidifies too rapidly for complete crystallisation. The result is reduced dimensional repeatability, lower heat deflection behaviour in service, and increased post-mould shrinkage. A mould temperature of 60 °C to 90 °C is preferred for dimensionally controlled electrical components. High-speed injection, with injection pressures typically 70 MPa to 120 MPa, supports thin-wall filling without excessive shear heating. Back pressure between 0.3 MPa and 0.7 MPa and screw decompression of 3 mm to 5 mm reduce melt-temperature fluctuation and nozzle drool. Incoming lots should be screened for melt flow rate under ISO 1133-1:2022; a variation of ±2 g/10 min from nominal is usually within normal production capability but may require adjustment to hold pressure or injection speed on sensitive multi-cavity tools.

    Applications in electrical and electronic systems are the primary use category for VALOX 325. Typical parts include terminal blocks, relay sockets, stator bobbins, capacitor housings, sensor connectors, and low-power switch components. The grade is selected where the higher stiffness of glass-filled PBT is unnecessary and where anisotropic thermal expansion from fibre orientation would distort pin rows or cause connector body warpage. For automotive under-hood connectors requiring resistance to hot hydrocarbon mists, short-term glycol splash, and moderate temperature cycling, VALOX 325 can be considered when the continuous wall temperature remains below the HDT boundary and when the part is not exposed to continuous hot-water or steam condensation above 60 °C. Published performance for long-term thermal ageing in air should be confirmed against the current UL 746B long-term thermal ageing listing for the relevant wall thickness and colour; generic unreinforced PBT grades may show relative thermal indices below 100 °C depending on thickness.

    Regulatory conformance and documented compliance standards

    Compliance status is highly dependent on colour concentrate choice, regrind sourcing, and final article configuration. The following table records the standard framework within which confirmation is required; it is not a substitute for a supplier-issued regulatory certificate for the production lot.

    SchemeStandard or directiveCondition requiring verification
    UL flammabilityUL 94HB at the thickness and colour shown on the current Yellow Card
    EU RoHSDirective 2011/65/EU as recast by (EU) 2015/863Supplier declaration for final colourant and production lot
    EU REACHRegulation (EC) No 1907/2006, Article 33SVHC concentration below 0.1 % w/w in the article as supplied
    Material identificationISO 11469:2016PBT marking for plastics recycling
    Conditioning stabilityISO 291:2008Conditioning at 23 °C and 50 % RH for comparative data
    Top