| HS Code | 709200 |
| Density | 1.31 g/cm³ |
| Reinforcement | Unreinforced |
| Tensile Strength At Yield | 50 MPa |
| Tensile Elongation At Break | 50 % |
| Flexural Modulus | 2100 MPa |
| Notched Izod Impact At 23 C | 6 kJ/m² |
| Notched Izod Impact At 40 C | 2 kJ/m² |
| Heat Deflection Temperature At 0 45 Mpa | 150 °C |
| Heat Deflection Temperature At 1 82 Mpa | 55 °C |
| Vicat Softening Temperature | 160 °C |
| Water Absorption | 0.08 % |
| Molding Shrinkage | 1.5-2.0 % |
| Melt Temperature | 240-260 °C |
| Mold Temperature | 40-80 °C |
As an accredited SABIC VALOX™ Unreinforced PBT 315 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ Unreinforced PBT 315 is packaged in 25 kg moisture-resistant bags, palletized for safe industrial storage and transport. |
| Container Loading (20′ FCL) | SABIC VALOX™ Unreinforced PBT 315 in 25 kg bags, palletized and loaded into a 20′ FCL for stable, efficient shipment. |
| Shipping | SABIC VALOX™ Unreinforced PBT 315 is shipped as non-hazardous thermoplastic PBT resin pellets in sealed moisture-barrier bags, boxes, or bulk containers. Store dry and cool; avoid moisture, contamination, and prolonged heat. It is not regulated for transport under DOT, IMDG, or IATA unless the SDS or local regulations state otherwise. |
| Storage | Store SABIC VALOX™ Unreinforced PBT 315 in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, and moisture. Keep containers tightly closed, labeled, and in original packaging to prevent contamination. Avoid prolonged high humidity; use dry conditions or desiccant if required. Do not store near incompatible chemicals. Follow local regulations and the Safety Data Sheet. |
| Shelf Life | SABIC VALOX™ Unreinforced PBT 315 has no fixed shelf life; store dry and cool, and use within the manufacturer-recommended period. |
For miniature terminal blocks and DIN-rail carrier bases, SABIC VALOX™ Unreinforced PBT 315 is processed after desiccant drying at 120 °C for 4 h to a residual moisture content below 0.02 wt%. The resin is injected on all-electric or servo-hydraulic machines with screw L/D ratios of 20:1 to 24:1 and a compression ratio of 2.5:1 to 3.0:1; barrel temperatures are set from 240 °C at the feed throat to 255–265 °C at the metering zone. The mould temperature is held at 80–90 °C because lower temperatures generate a less crystalline surface layer and produce inconsistent insertion force on metal screw terminals. A published typical tensile stress at yield of 55 MPa under ISO 527-2 and a flexural modulus of 2350 MPa under ISO 178 are used as incoming lot-control references. The terminal carrier is filled through a cold runner with a heated sprue bushing; gate diameter is kept at 0.8–1.2 mm for wall thicknesses of 1.5–3.0 mm to avoid jetting. Hold pressure is set to 50–70 MPa after cavity pressure transfer at 40–55 MPa, and hold time is 4–6 s for a 2.0 mm wall. Regrind from sprues and runners is limited to 20 wt% because higher addition rates reduce notched Izod impact measured under ISO 180/1A and narrow the processing window. The moulded parts are conditioned for 48 h at 23 °C and 50% relative humidity before screw insertion torque is measured. The finished terminal block is evaluated under IEC 60947-7-1 for insulation coordination and under IEC 60112 for comparative tracking index; the material carries a comparative tracking index of 600 V when tested with standard solution A. This enables creepage distance calculations under IEC 60664-1 for rated voltages up to 250 V in pollution degree 2 environments.
On high-cavitation tools, the most common failure mode is not short shot but weld-line embrittlement at the junction of two flow fronts around a terminal bore. Increasing melt temperature to 270 °C improves weld-line strength but shortens the permissible residence time. The material should not remain in the barrel above 270 °C for longer than 5 min; longer residence produces a visible yellow shift and lowers melt viscosity due to ester-bond scission. In production monitoring, melt viscosity is checked by ISO 1133-1 at 250 °C with a 2.16 kg load, and the lot is rejected if the melt volume-flow rate shifts more than 15% from the reference value. Tool venting channels are ground to a depth of 0.02 mm and a width of 3–6 mm to remove volatiles; vacuum venting is applied when sink marks appear on ribs thicker than 2.8 mm. The terminal product is a moulded DIN-rail terminal block housing with insert-moulded brass clamp plates, used in control cabinets where dimensional stability and tracking resistance are the controlling material properties.
For automotive door connectors and seat-position sensor shells, VALOX 315 is submitted to terminal retention-force testing under SAE/USCAR-2. The test is performed on a universal test machine at a displacement rate of 100 mm/min after thermal cycling from -40 °C to 85 °C. Because unreinforced PBT 315 retains a tensile elongation at yield of around 3–4% under ISO 527-2, the snap-fit tabs and terminal locking lances do not fail in brittle mode at ambient temperature. The processing boundary appears when recycled sprues and runners exceed 25 wt% of the blend. At that level, the melt viscosity curve shifts because the recycled fraction carries additional thermal history; melt flow measured by ISO 1133-1 can increase by 10–20% after three regrind cycles. This is significant in thin-wall connector shells with wall thickness from 0.8 mm to 1.2 mm, where the cavity pressure at switchover falls and the gate freezes later. The result is a wider retention-force distribution and occasional fall-out of terminal pins during harness assembly. A hot runner with valve-gated drops is used for the shell, and the manifold is sized to keep residence time below 15 s per shot. The recommended processing regime is melt temperature 250–265 °C, mould temperature 80 °C, and injection velocity 100–150 mm/s. Cavity pressure transducers control switchover at 60–70 MPa. The finished connector is conditioned per ISO 291 before retention force is measured. The material meets the chemical resistance requirements of automotive cabin exposure, but the design should avoid contact with brake fluid and strong alkaline cleaners, which soften the unreinforced polyester.
The terminal product is a door-latch actuator connector or seat occupancy sensor connector. In this use, the connector body is placed outside the engine compartment, so the underhood 125 °C continuous-use class is not required. If the same geometry is used underhood, published data for unreinforced PBT 315 in that specific configuration is limited; a heat-stabilized or glass-reinforced PBT grade should be evaluated under ISO 75-2 at 1.82 MPa and IEC 60068-2-14 thermal shock.
In washing machine inlet-valve bobbins and solenoid coil formers, VALOX 315 is processed with a hot-tip gate or pin gate placed on the bobbin flange. The main purpose of the material in this component is to survive the winding of enameled copper wire and the subsequent varnish bake at 120 °C for 2 h. The coil former must not distort during the bake; the heat deflection temperature under 0.45 MPa is 154 °C under ISO 75-2, and the Vicat softening temperature is 175 °C under ISO 306. The tool is a four-cavity cold runner, with a runner diameter of 4 mm and a pin gate of 0.6 mm. A colour masterbatch containing 2 wt% titanium dioxide and 0.2 wt% carbon black in a PBT carrier is metered at 1–2 wt%; no external nucleating agent is used because mould temperature is close to 80 °C. Regrind is permitted to 15 wt% only from non-plated parts, because any contamination by copper dust from winding changes the melt thermal stability. The bobbin is moulded at 250–260 °C melt temperature with back pressure 0.4 MPa and screw speed 60–80 rpm. After ejection, the parts are annealed at 130 °C for 1 h to stabilize the crystalline fraction and to reduce creep during the varnish bake. The finished coil former is evaluated under UL 1446 as part of the electrical insulation system; the material alone does not carry a system temperature class. The terminal product is a solenoid bobbin for a cold-water inlet valve used in domestic washing machines and dishwashers.
Field production of bobbins in high-cavity tools frequently encounters coil-former flange cracking during terminal pin insertion. This is not a material limitation if the notch radius of the pin socket is below 0.2 mm; a minimum radius of 0.3 mm and a pin-hole draft angle of 0.5° are specified to prevent cold-tool brittleness. If pin insertion is done on an automated line at 23 °C, the parts are removed from sealed packaging only after reaching ambient temperature; PBT moulded parts stored below 10 °C exhibit lower impact resistance and should be brought to 23 °C before assembly. The processing window for this component is wide, so only a single sentence is needed for the mixing step: the masterbatch is tumble-blended with virgin pellets for 20 min at 20 rpm.
Thin-wall automotive blade-fuse holders with wall thickness 0.7–1.0 mm require high melt flow to fill without short shots, but the processing window for unreinforced PBT 315 above 270 °C is narrow. The principal risk is thermal degradation of the ester bond, which occurs fastest at the screw tip and the hot runner dead spots. For this application, the barrel is set from 245 °C in the feed zone to 270 °C at the nozzle only when the injection shot mass is 40–60% of the rated barrel capacity. The residence time is kept below 5 min, and the melt cushion is controlled at 2–4 mm. The tool is a 32-cavity valve-gated hot runner with manifold temperature 255–265 °C; the gate insert is made of beryllium-free copper alloy to avoid local overheating. Injection velocity is raised to 200–300 mm/s to fill the thin web before solidification. Switchover is set by cavity pressure at 55–65 MPa; holding pressure is 60–80 MPa for 1.0–1.5 s. After ejection, the fuse holder is checked for dimensional stability according to the drawing, and warpage is measured on a flatness fixture. The material is not exposed to temperatures above 100 °C in the vehicle interior; therefore the unreinforced grade is acceptable. Compliance is tested under IEC 60127-6 for fuseholders and under IEC 60695-2-11 glow wire at 650 °C for the accessible insulation parts. The terminal product is a low-profile multi-fuse holder for passenger-car instrument panels.
When the melt temperature exceeds 270 °C, carbon black in dark colours catalyses oxidation; if a black fuse holder lot shows a ΔE colour shift greater than 1.5 against the standard plaque, the hot runner temperature is reduced by 5 °C increments and the nozzle is inspected for hot spots. The purging compound is run after every 500 shots on such high-temperature tools to remove charred particles that deposit on the screw root. A release agent is not applied to the mould for this component, because silicone-based mould releases migrate to the surface and reduce print adhesion for laser marking. The marking system is a 1064 nm fiber laser with a pulse width of 200 ns, which provides contrast on the unreinforced PBT surface without breaching the insulation wall. These process boundaries define the use of VALOX 315 in fuse carriers where high flow and thin-wall filling conflict with thermal stability.
Because E26/E27 LED lamp bases must retain a threaded metal shell, survive an automated screwing operation, and keep their inner diameter after thermal loading from the LED driver, the unreinforced PBT 315 compound is pre-dried at 120 °C to 0.015 wt% moisture and moulded at 250 °C melt and 85 °C mould. The wall thickness around the thread is 2.0 mm; the gate is located at the center of the base to provide radial flow and minimize weld lines on the load-bearing thread. The mould shrinkage of 1.8–2.2% is compensated in the thread profile, and the part is annealed at 120 °C for 2 h after ejection. Without annealing, post-mould crystallization can reduce the inner diameter by 0.1–0.2% over the first 48 h, causing excessive torque when the metal shell is threaded in. The insertion torque for the shell is set at 0.8–1.2 N·m; below 0.8 N·m, the shell may rotate during lamp removal. The material’s comparative tracking index of 600 V under IEC 60112 is relevant because the nearest live pin spacing is below 3 mm in some compact GU10 designs. Flammability is assessed under UL 94; the unreinforced grade carries a HB rating, but for the lamp base the more critical requirement is glow-wire performance under IEC 60695-2-11. Published data for this specific configuration is limited, and a flame-retardant PBT is used when the luminaire standard requires 750 °C glow-wire ignition resistance without flame. The finished lamp base is subjected to IEC 60838-1 torque and thermal endurance tests. Regrind is limited to 10 wt% and is excluded entirely for white parts to avoid yellowing. The terminal product is a GU10 lamp holder body for LED retrofit lamps.
In condensing gas furnace condensate pumps, volutes and drain pans are evaluated in hot, wet environments that sit at the service limit of standard unreinforced PBT. VALOX 315 has low moisture absorption at 23 °C, typically 0.08% after 24 h under ISO 62, but above 60 °C in neutral water the ester linkage undergoes gradual hydrolytic chain scission. A pump volute that operates with condensate at 50 °C and drains between cycles can be moulded successfully from this grade; continuous immersion above 60 °C is an operational boundary because the material loses tensile elongation and the screw bosses eventually crack. The tooling is a single-cavity cold runner with a fan gate of 1.5 mm thickness; the wall thickness of the volute is maintained at 2.0–2.5 mm. Melt temperature is 250–260 °C, and mould temperature is 80 °C. A hydrolysis-resistant masterbatch containing 0.5–1.0 wt% of an epoxide or carbodiimide stabilizer in PBT carrier is sometimes metered at the press; because the additive must be uniformly dispersed, a mixing section screw with a L/D of 20:1 to 24:1 and a back pressure of 0.6–0.8 MPa are required. The use of such a masterbatch is validated by measuring melt viscosity stability over 20 min at 250 °C in an ISO 1133-1 test. The parts are not used in contact with amine-based corrosion inhibitors, strongly alkaline boiler treatment chemicals, or hot glycol mixtures, because these substances accelerate stress cracking in unreinforced polyester. The terminal product is a condensate pump volute for high-efficiency gas furnace condensate, tested under IEC 60335-2-40 for abnormal operation and leakage current.
Competitive SABIC VALOX™ Unreinforced PBT 315 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
VALOX™ 315 is an unreinforced polybutylene terephthalate (PBT) injection-molding grade supplied by SABIC. The “315” model designation identifies a general-purpose unfilled polyester formulated without glass fiber, mineral filler, or flame-retardant additives. The absence of reinforcement produces a smooth surface, near-isotropic mold shrinkage, and lower melt viscosity than filled PBT compounds, but it also places the material in a lower stiffness and lower heat-deflection class. Under ISO 1183, the density is 1.31 g/cm³. The polymer is semicrystalline; the melting point is near 225 °C and the glass-transition temperature of unfilled PBT is commonly reported between 45 °C and 60 °C by dynamic mechanical methods. The product is not a flame-retardant compound; the published flammability classification is UL 94 HB at 1.5 mm. Because the ester backbone is sensitive to hydrolytic chain scission, predrying to below 0.02 % residual moisture is an essential production control rather than an optional preparation step.
The grade is processed on conventional reciprocating-screw injection molding machines. Production-scale settings are typically validated with clamping forces between 400 kN and 1500 kN for small electrical parts, and with a general-purpose screw having an L/D ratio of 20:1 to 22:1. Because PBT crystallizes rapidly, mold temperature and cooling time control the crystalline layer thickness, frozen-in orientation, and shrinkage after demolding. In comparison with amorphous resins such as polycarbonate or polycarbonate blends, VALOX 315 provides higher chemical resistance to fuels and oils but a narrower wet-service boundary due to the ester linkage.
The property shifts between VALOX 315 and filled or modified PBT grades are most visible in tensile modulus, heat deflection temperature, and shrinkage anisotropy. A representative 30 % glass-fiber-reinforced PBT with the same base chemistry typically exhibits a tensile stress at yield near 120 MPa and a flexural modulus near 8000 MPa under ISO 527-2/50 and ISO 178. VALOX 315 is reported at approximately 55 MPa tensile stress at yield and 2400 MPa flexural modulus. The unreinforced grade retains higher elongation at break and lower density, but its HDT/A at 1.82 MPa is near 55 °C, while glass-reinforced PBT commonly exceeds 190 °C. The unfilled grade also exhibits mold-shrinkage values from 1.5 % to 2.2 % across flow and transverse directions under ISO 294-4; glass-reinforced PBT can drop below 0.5 % in the flow direction and remain above 1.0 % in the transverse direction, creating anisotropic warpage in large flat parts. For parts requiring flatness and surface finish, VALOX 315 is therefore specified over glass-filled grades despite its lower load-bearing capability.
Compared with flame-retardant PBT compounds, VALOX 315 does not contain a halogenated or phosphorus-based flame-retardant package. The UL 94 classification remains HB, while V-0 grades use additive systems that can alter melt viscosity, density, and color stability. Compared with impact-modified PBT, the unreinforced general-purpose grade has lower notched impact strength; a notched Izod value near 4 kJ/m² under ISO 180/1A is typical, whereas impact-modified PBT can exceed 25 kJ/m² but with lower flexural modulus and greater creep under load.
Table 1. Published typical values for VALOX 315; lot-specific data and the current manufacturer’s datasheet remain controlling.
| Property | Test standard | Published typical value |
|---|---|---|
| Density | ISO 1183 | 1.31 g/cm³ |
| Tensile stress at yield | ISO 527-2/50 | 55 MPa |
| Tensile strain at break | ISO 527-2/50 | > 20 % |
| Flexural modulus | ISO 178 | 2400 MPa |
| Heat deflection temperature, 1.82 MPa | ISO 75-2/A | 55 °C |
| Heat deflection temperature, 0.45 MPa | ISO 75-2/B | 155 °C |
| Notched Izod impact, 23 °C | ISO 180/1A | 4 kJ/m² |
| Volume resistivity | IEC 60093 | 1 × 1015 Ω·m |
| Dielectric strength | IEC 60243-1 | 17 kV/mm |
| Comparative tracking index | IEC 60112 | 600 V |
| Flammability at 1.5 mm | UL 94 | HB |
| Mold shrinkage | ISO 294-4 | 1.5–2.2 % |
Table 2. Comparative class-level property shifts for unfilled, glass-filled, and impact-modified PBT.
| Property | VALOX 315 unreinforced | 30 % glass-reinforced PBT | Impact-modified PBT |
|---|---|---|---|
| Density, ISO 1183 | 1.31 g/cm³ | 1.50–1.55 g/cm³ | 1.22–1.26 g/cm³ |
| Tensile stress at yield, ISO 527-2 | 55 MPa | 120–130 MPa | 35–45 MPa |
| Flexural modulus, ISO 178 | 2400 MPa | 8000–9000 MPa | 1500–2000 MPa |
| HDT/A, ISO 75-2/A | 55 °C | 190–220 °C | 45–55 °C |
| Notched Izod, ISO 180/1A | 4 kJ/m² | 7–10 kJ/m² | 25–45 kJ/m² |
| UL 94 at 1.5 mm | HB | HB or V-0 depending on flame package | HB |
These comparative values are class-level data from public PBT literature, not guaranteed substitutions for a specific grade; exact comparisons require current datasheets and chemical-resistance declarations from the manufacturer.
In melt processing, the pellets are predried in a desiccant dryer at 120 °C for 3 h to 4 h until residual moisture is below 0.02 %. The dryer inlet air should have a dew point no higher than -30 °C. Pellets left in open hoppers in a molding shop above 60 % relative humidity can regain enough moisture to produce splay, silver streaks, and a measurable drop in tensile stress at yield. The barrel profile is typically set with the rear zone at 230 °C, center zones between 240 °C and 250 °C, and the nozzle at 250 °C to 260 °C. The maximum melt temperature is regarded as 270 °C; above this level the polyester undergoes thermal degradation with liberation of tetrahydrofuran and formation of carboxyl end groups, and the melt viscosity falls while mechanical properties deteriorate.
Residence time is a more critical variable than set-point temperature. At melt temperatures above 250 °C, total heated-barrel residence time should be kept below 5 min. Hot-runner systems with dead spots or unmelted pellets in low-flow channels are a known cause of black speck formation and intermittent part contamination on production equipment. Valve-gated hot runners are preferred over open hot runners because they reduce drool and allow hot-runner channel pressure to be held during pack; however, the gate temperature must not exceed 270 °C.
Mold temperature is set between 65 °C and 85 °C to obtain a sufficient crystalline fraction. At mold temperatures below 40 °C, the supercooled melt freezes before crystallization completes; the part may pass short-term dimensional checks but later shrink further when exposed to service temperatures near the HDT/A. At mold temperatures above 95 °C, ejection becomes more difficult because the unfilled grade has lower hot stiffness and the part may stick on polished cores. Injection speed is set fast enough to fill thin walls before freeze-off; for wall thickness below 1.5 mm, values from 80 mm/s to 120 mm/s are common. Hold pressure is established by gate seal; typical values are 40 MPa to 70 MPa. Back pressure is held at 0.5 MPa to 2 MPa to avoid excessive shear heating. Melt-volume-flow rate under ISO 1133-1 at 250 °C and 2.16 kg is the standard flow parameter used in mold-filling simulation; class-level data for unreinforced PBT injection grades typically fall between 10 cm³/10 min and 25 cm³/10 min, but drying state and lot-to-lot variation can shift the measured value.
Electrical and electronic components are a principal application field. The material is used in relay bobbins, terminal blocks, connector housings, sensor carriers, motor brush holders, and switch internals. In these designs, volume resistivity is approximately 1 × 1015 Ω·m under IEC 60093, and dielectric strength measured on a 3.2 mm plaque is near 17 kV/mm under IEC 60243-1. The comparative tracking index under IEC 60112 is 600 V, which permits the material to be used in compact creepage-distance designs only after the clearance and creepage requirements of IEC 60664-1 are calculated with the actual working voltage, pollution degree, and insulation material group. The absence of glass fiber eliminates exposed fiber ends on molded surfaces, which can be a concern in low-voltage switching because conductive dust and carbonized debris can settle along fiber troughs.
Under continuous electrical load, the temperature rise of the contact or coil must be considered. The unreinforced grade has an HDT/A of approximately 55 °C; if the part is clamped by a terminal screw or pressed by a spring, softening and creep at the bearing surface can reduce contact pressure. This limitation is more severe in VALOX 315 than in glass-reinforced PBT. Published data for arc resistance under ASTM D495 for this exact unfilled grade is limited; qualification under the actual switching current, opening speed, and contact gap is required for arcing contacts.
The service boundary is governed by hydrolysis of the ester linkage. In continuous hot-water contact above 80 °C, tensile strength falls as molecular weight is reduced; the part may fail by surface cracking after repeated thermal cycling. The material is not recommended for pressurized hot-water or steam service, and it is not a replacement for hydrolytically stabilized PBT grades or polyphenylene sulfide in cooling-system components. Strong aqueous bases and amine-containing cleaning agents attack the polyester through ester cleavage or aminolysis; hot alkaline degreasing solutions, epoxy amine hardeners, and repeated contact with strongly basic flux residues should be avoided. Chlorinated solvents and concentrated sulfuric acid are not compatible under stress; the resulting swelling and stress cracking can reduce notched impact strength below the published value.
Resistance to fuels, diesel, hydraulic oils, and aliphatic hydrocarbons is good at room temperature and under unstressed immersion; this makes the grade suitable for oil-tolerant electrical housings and fuel-system connectors only if the temperature remains below the softening boundary and the housing is not under continuous flexural load. For outdoor exposure, unfilled natural PBT degrades by surface chalking and loss of elongation under ultraviolet radiation; UV-stabilized or carbon-black-filled grades are used when the part is exposed to direct sunlight. The unreinforced 315 grade is therefore specified for indoor electrical and electronic applications, short-term oil contact, and dry mechanical parts rather than exterior or hot-fluid service.
In dry mechanical parts such as gears, cams, rollers, and pump housings, the unfilled grade offers low noise and low coefficient of friction relative to glass-filled PBT, but the absence of fiber reinforcement reduces wear resistance under high pressure–velocity conditions. Published wear factors for this exact grade are limited; end-use testing on the actual counterface and lubrication condition is necessary. The grade is also used in appliance components where dimensional repeatability, surface gloss, and resistance to cooking oils at moderate temperature are required, but it is not suitable for direct contact with heating elements above the published HDT/A.