Sabic Valox Unreinforced Pbt 310se0

SABIC VALOX™ Unreinforced PBT 310SE0

    • Product Name: SABIC VALOX™ Unreinforced PBT 310SE0
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 667961
    Density 1.31 g/cm3
    Melt Volume Rate 250c 2 16kg 12 cm3/10min
    Mold Shrinkage Flow 1.8-2.0 %
    Tensile Modulus 2500 MPa
    Tensile Stress At Yield 55 MPa
    Tensile Strain At Break 50 %
    Flexural Modulus 2400 MPa
    Flexural Strength 85 MPa
    Notched Izod Impact 23c 35 J/m
    Hdt 0 45mpa 150 C
    Hdt 1 8mpa 55 C
    Vicat Softening Temperature B50 165 C
    Ul94 Flame Rating V-0 at 0.75 mm
    Dielectric Strength 17 kV/mm
    Volume Resistivity >1E15 ohm·cm
    Comparative Tracking Index 600 V

    As an accredited SABIC VALOX™ Unreinforced PBT 310SE0 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ Unreinforced PBT 310SE0 is supplied in 25 kg moisture-barrier, foil-lined bags, palletized for industrial handling.
    Container Loading (20′ FCL) Packed in 25 kg bags, palletized and loaded into a dry 20′ FCL container for secure, stable transport.
    Shipping SABIC VALOX™ Unreinforced PBT 310SE0 is typically shipped as solid thermoplastic resin pellets in sealed moisture-barrier bags or containers, palletized. Protect from moisture, heat, contamination, and UV. Usually not regulated as dangerous goods; follow SDS and local transport regulations.
    Storage Store SABIC VALOX™ 310SE0 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers tightly closed and use original packaging to prevent moisture pickup and contamination. Avoid prolonged high humidity; dry material before processing if specified. Maintain good housekeeping and follow local regulations and SDS guidance.
    Shelf Life Shelf life is typically 24 months when stored dry, in original sealed packaging, below 50°C, away from sunlight and moisture.
    Application of SABIC VALOX™ Unreinforced PBT 310SE0

    Across IEC 60999-1 low-voltage terminal blocks, the insulating body that clamps a stranded copper conductor is direct-gated in a 32-cavity cold-runner mold. VALOX™ 310SE0 is injection molded at 100 wt% without glass reinforcement because glass-filled PBT warps around tin-plated brass inserts and reduces conductor clamp force after thermal cycling. The compliance foundation is IEC 60999-1:1999 for screwless-type clamping units, UL 1059 for terminal blocks, and IEC 60947-7-1 for DIN rail-mounted blocks; the material’s flame-retardant listing is checked against UL 94 V-0 at 0.71 mm rather than relying on a generic PBT datasheet. The formulation addition ratio is 100 phr virgin resin; cold-runner regrind is added at 15 phr maximum after closed-loop drying at 120 °C to a dew point of −30 °C and a moisture content below 0.02 %. The downstream production process uses a 25:1 L/D general-purpose screw without compression mixing pins to limit adiabatic shear heating. Melt temperature is held at 245–260 °C, mold temperature at 60–80 °C, injection velocity is profiled from 60 mm/s to 25 mm/s at the gate, and holding pressure is 55–70 MPa for 4 s/mm of wall thickness. The processing boundary is set by halogenated flame-retardant decomposition: if barrel residence exceeds 5 min at 260 °C or the hot-runner temperature exceeds 265 °C, gas evolution at the check ring causes short shots and the mold surfaces show acidic deposit. Terminal finished articles include feed-through terminal blocks, disconnect terminal blocks, and PE grounding terminal blocks with rated cross-sections from 1.5 mm² to 35 mm².

    How Does Ultrasonic Welding Redistribute Flame Retardant at Relay Housing Joint Lines?

    Three-dimensional mold flow analysis across a relay base and cover set indicates an injection pressure drop of 22 MPa when the cover wall is reduced from 1.2 mm to 0.8 mm; published data for this specific configuration is limited, but production trials show gas voids near the coil pin if the shot weight exceeds 70 % of barrel capacity. The resin is charged at 100 wt% VALOX™ 310SE0; a non-blooming ester mold-release additive is not pre-compounded in the pellet but metered as a 0.3 wt% masterbatch at the machine throat after the desiccant drying hopper. Compliance is anchored to IEC 61810-1 for electromechanical elementary relays and IEC 60335-1 end-product glow-wire provisions; the grade is specified only after the customer’s UL file transfer accepts UL 94 V-0 at 0.71 mm. The downstream production process uses a 40:1 L/D barrier screw with vacuum venting at −0.09 MPa, melt temperature 250–265 °C, mold temperature 70 °C, and hot-tip valve gates to prevent stringing. The housing is not post-cured. The cover is ultrasonically welded to the base at 20 kHz with a 35 µm joint interference; the energy director is molded into the cover to keep the flame-retardant skin layer intact on the external joint face. Batch-to-batch variance in weld joint strength is monitored by a 30 N spring-loaded shear test on every 12-hour shift. Terminal products include PCB power relays, interface modules, and HVAC compressor relay sockets intended for pollution degree 2 installations.

    When IEC 60335-1:2020 clause 30.2.3 governs unattended appliance control housings carrying a current above 0.2 A, the insulating material must pass an end-product glow-wire test at 850 °C, and the unfilled PBT grade is chosen because it removes glass fiber orientation-induced post-mold warpage that can shift a rotary selector shaft bore centerline by 0.15 mm across a 90 mm span. No separate flame-retardant masterbatch is used; the addition ratio is 100 phr VALOX™ 310SE0. If a color masterbatch is run for appliance brand matching, the let-down is limited to 2.0 wt% and is pre-dried together with the virgin resin at 120 °C for 4 h. The downstream production process uses a 200 t injection molding machine with a 22 mm diameter screw, 20:1 L/D, and a cold sprue bushing. Melt temperature is held at 250 ± 5 °C because wider excursions liberate halogenated decomposition products that corrode the mold; mold temperature is set to 65 °C, and holding pressure is applied until the gate freezes at 3.5 s. The mold is vented to 0.02 mm at the perimeter and 0.01 mm at the parting line inserts. Terminal finished articles include washing machine rotary program switch housings, air conditioner display boxes, and refrigerator defrost timer bodies. Operator handling is restricted to closed-loop granulate feed after two consecutive runs show black specks at 0.5 mm² or larger in the transparent control window, which indicates flame-retardant package breakdown in the barrel.

    Automotive Cabin Connector Bodies, USCAR-2 Mechanical Keying, and Vibration-Proof Latch Retention

    Automotive OEM harness drawings for cabin unsealed connectors reference USCAR-2 and the OEM’s thermal shock profile from ISO 16750-4:2023. The molding feed is 100 phr VALOX™ 310SE0 because unfilled PBT retains sufficient flexural modulus at 23 °C for latch function but does not undergo brittle fracture in the −40 °C cold-shock test when the cantilever latch is designed with a 1.2 mm root radius. Heat stabilizer masterbatch is not normally added because cabin ambient temperatures remain below 85 °C at the connector bulk, while UV-stabilized color masterbatch at 2–3 wt% is used only for upper instrument panel exposed parts. The downstream production process is a 24-cavity hot-runner mold with individually controlled valve-gate tips on a 120 t press. Injection speed is profiled to 55 mm/s at the latch and 30 mm/s at the terminal slot to avoid jetting; melt temperature is 245–255 °C, mold temperature 70–80 °C, and back pressure 0.4 MPa to homogenize the flame-retardant package without excessive shear. After molding, the bodies are subjected to 100 % functional keying pin insertion force tests and sample lot vibration testing per USCAR-2. Terminal products include instrument panel cluster connectors, HVAC actuator sensor connectors, and body control module connector bodies.

    In self-ballasted LED driver enclosures that carry SELV outputs below 120 V DC but sit adjacent to a live printed circuit board, UL 8750 requires the enclosure polymer to maintain the flammability rating after lead-wire insertion and screw-boss torquing. VALOX™ 310SE0 is loaded at 100 wt%; sprue and runner regrind is added at 10 wt% only after hot-air drying at 120 °C for 3 h and magnetic filtering to remove metallic fines. The compliance foundation is UL 8750, UL 94 V-0 at 0.71 mm, and IEC 60695-10-2 ball-pressure at 125 °C. The downstream production process is single-cavity cold-runner molding on a 90 t machine with a 25 mm screw, 22:1 L/D, and a mixing nozzle; barrel temperatures from feed to nozzle are profiled at 240 °C, 250 °C, 255 °C, and 250 °C. If peak injection pressure exceeds 110 MPa, the screw is purged because flame-retardant gas displacement at the check ring causes short shots. Terminal products include LED driver end caps, fluorescent lamp holder bodies, and emergency lighting battery housings.

    Electrical Contact Carrier Molding in Unreinforced PBT Under High-Cycle Arc Erosion of Power Tool Switches

    Electrical contact carrier molding in power tool switches is evaluated by IEC 61058-1 and UL 1054; the polymer sits below a moving copper contact and must hold its creep dimension after 100,000 switching cycles. VALOX™ 310SE0 is charged at 100 phr without glass reinforcement because glass fibers become conductive dust when the contact arc erodes the polymer surface. Formulation loading is 100 phr virgin; 0.5 wt% of fine polytetrafluoroethylene powder is added only when the customer requires a lower coefficient of friction on the trigger guide, and this addition is pre-blended in a low-speed ribbon blender before drying. The downstream production process is insert molding of brass contact rivets in an 8-cavity family mold on a 100 t press, with the parting line vented to 0.015 mm and core pins cooled by beryllium copper inserts. Melt temperature is 250 °C, mold temperature 75 °C, screw speed 80 rpm, and cushion is held at 3–5 mm to maintain a consistent check ring seal. The molding operator monitors nozzle pressure decay: if the curve transitions from exponential to linear within 2 s, the non-return valve is worn and residual flame-retardant package can back-flow. Terminal products include variable-speed drill switch housings, angle grinder trigger housings, and orbital sander switch bodies.

    Free Quote

    Competitive SABIC VALOX™ Unreinforced PBT 310SE0 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ Unreinforced PBT 310SE0 is an unfilled polybutylene terephthalate compound carrying a UL 94 V-0 flame-retardant classification at 0.71 mm wall thickness. The absence of glass or mineral reinforcement distinguishes the grade from filled VALOX flame-retardant PBT products, altering shrink anisotropy, surface appearance, and mechanical stiffness. Published datasheet values identify a density of 1.41 g/cm³ per ISO 1183-1, tensile stress at break of 58 MPa per ISO 527-2/50, flexural modulus of 2600 MPa per ISO 178, and notched Izod impact at 23°C of 4 kJ/m² per ISO 180/1A. These mechanical indicators position 310SE0 below 30% glass-reinforced V-0 PBT grades in stiffness and above them in elongation, while the unfilled morphology provides lower directional shrinkage and reduced fiber-induced warpage in thin-wall electrical components.

    PropertyTest methodPublished typical value
    DensityISO 1183-11.41 g/cm³
    Tensile stress at breakISO 527-2/5058 MPa
    Tensile strain at breakISO 527-2/5020%
    Flexural modulusISO 1782600 MPa
    Notched Izod impact, 23°CISO 180/1A4 kJ/m²
    Heat deflection temperature, 1.8 MPaISO 75-2/Ae70°C
    Heat deflection temperature, 0.45 MPaISO 75-2/Be150°C
    Mold shrinkage, flow directionISO 294-41.6–2.0%
    Flame ratingUL 94V-0 at 0.71 mm

    What limits the processing window when running V-0 unreinforced PBT in hot-runner tooling?

    The principal processing risk is hydrolytic degradation of the polyester backbone when residual moisture exceeds 0.02% before plastication. Drying is specified at 120°C for 3–4 h in a desiccant dryer with inlet air dew point between -20°C and -40°C. Central drying systems on production-scale injection molding lines are operated with regeneration cycles below 220°C; higher regeneration temperatures can discolor pellets and reduce melt stability. Barrel temperature profiles are typically set from 240°C to 260°C, with nozzle temperature controlled to 250°C and melt temperature measured at the nozzle between 250°C and 265°C. Mold temperature is maintained between 60°C and 90°C, with the lower range favoring cycle time and the upper range improving surface gloss and crystalline uniformity.

    Residence time at melt temperature must remain below 5 min. In hot-runner tooling, the flame-retardant additive package can generate acidic degradation by-products if held above 270°C, leading to viscosity reduction, gas evolution, and surface splay. Hot-runner manifolds require balanced flow channels without dead spots, and integral valve gates are preferred over thermal gates in multi-cavity connector tools because they limit stagnant melt volume. Screw specifications for a general-purpose injection unit include an L/D ratio of 20:1 to 25:1 and a compression ratio of 2.0:1 to 2.5:1. Screw surface speed is held at 0.2–0.4 m/s to avoid frictional heating, and back pressure is set at 0.5–1.0 MPa hydraulic. Clamp force calculations for thin-wall electrical connectors typically require 0.6–0.8 kN/cm² projected area; published data for this specific configuration is limited when wall sections exceed 2.0 mm and should be confirmed by cavity-pressure trials.

    Processing parameterSet point or rangeOperational note
    Drying temperature120°CDesiccant dryer, 3–4 h
    Residual moisture<0.02%Karl Fischer measurement
    Melt temperature at nozzle250–265°CMeasured by pyrometer
    Mold temperature60–90°CHigher for gloss and crystallinity
    Screw L/D ratio20:1–25:1General-purpose constant taper
    Compression ratio2.0:1–2.5:1Non-blocking feed section
    Screw surface speed0.2–0.4 m/sLimits shear heating
    Back pressure0.5–1.0 MPaHydraulic circuit
    Residence time<5 minAt melt temperature
    Regrind ratio≤20%Dried, uncontaminated regrind only

    Production-scale failure modes observed on injection molding machines with hot-runner valve gates include gate stringing when nozzle temperatures drift below 245°C, and local delamination on connector ribs when mold temperatures vary by more than ±5°C across the cavity. These defects are process-related rather than intrinsic to the compound, but they occur more readily in unreinforced V-0 PBT than in glass-filled PBT because the unfilled melt has lower thermal conductivity and lower mechanical green strength at ejection. Ejection is typically initiated when part surface temperature falls below 80°C.

    Electrical terminal carriers, relay housings, switch frames, and bobbins represent the principal application field for 310SE0 because the material combines V-0 ignition resistance with high flow and a smooth unfilled surface. In terminal blocks designed under IEC 60664-1, the published comparative tracking index of 250 V under IEC 60112 supports creepage-distance calculations only when the printed circuit board environment is classified as pollution degree 2 or lower. The grade is not a substitute for high-CTI grades in severe pollution environments. Published volume resistivity is on the order of 10¹⁵ Ω·cm under IEC 60093, and dielectric strength for 3.2 mm specimens is reported near 20 kV/mm under IEC 60243-1, but these values should be re-verified at end-product thickness and humidity because condensation can reduce surface resistance by orders of magnitude.

    Comparative dielectric, weld-line strength, and shrinkage anisotropy against glass-filled PBT

    The mechanical differentiation between 310SE0 and a 30% glass-reinforced flame-retardant VALOX PBT grade is substantial. Glass-filled V-0 PBT grades typically publish tensile strengths greater than 100 MPa, flexural modulus above 8000 MPa, and heat deflection temperatures above 200°C at 1.8 MPa. In comparison, 310SE0 reports 58 MPa tensile stress at break, 2600 MPa flexural modulus, and 70°C HDT/A. The unfilled grade therefore cannot be substituted into snap-fit designs originally sized for glass-filled PBT without increasing section thickness or adding ribs. Conversely, glass-filled PBT can introduce anisotropic warpage in rectangular connectors because fiber orientation follows flow direction. 310SE0 exhibits flow-direction and cross-flow shrinkage both in the 1.6–2.0% range, whereas reinforced grades may show cross-flow shrinkage up to 0.8% and flow-direction shrinkage below 0.3%, producing non-uniform thermal contraction and dimensional deviation.

    Weld-line strength is another process-related distinction. In glass-filled PBT, flow fronts meeting at weld lines show fiber alignment parallel to the weld plane, which reduces tensile strength at the weld by 40–60% relative to the unreinforced matrix. The unfilled 310SE0 retains higher weld-line elongation because there are no reinforcing fibers to orient at the knit line, although the absolute strength remains lower than the filled grade. For thin-wall relay bobbin flanges, the unfilled grade can therefore tolerate less aggressive gate placement and still avoid flange cracking at pin insertion. Mold-filling trials on two-plate cold-runner tools with 0.8 mm nominal wall and pin gate diameters of 0.6–0.8 mm have shown that short shots occur at melt temperatures below 248°C when flow length exceeds 120 mm. Under the same tooling, increasing melt temperature to 260°C restores complete filling but raises the risk of flash if vent depths exceed 0.02 mm.

    When thin-wall relay bases replace thermoset polyester in unattended appliances

    In unattended appliance components such as relay bases and terminal strips, the flammability requirement is often UL 94 V-0 at 0.75 mm or thinner. 310SE0 is classified V-0 at 0.71 mm, which permits wall-stock reduction compared with V-0 grades rated only at 1.5 mm. The reduction in wall thickness lowers shot weight and cycle time, but it also reduces mechanical stiffness at the base. Because flexural modulus is 2600 MPa, the base may require an additional center rib of 1.2–1.5 mm thickness to maintain contact pressure on relay terminals. Published data for specific contact-force retention after thermal aging at 120°C is limited; qualification programs typically measure contact insertion force after 1000 h at 85°C/85% RH rather than relying solely on datasheet values.

    The flame-retardant package in 310SE0 is not halogen-free; the grade should not be represented as meeting halogen-free material declarations under IEC 61249-2-21. Electrical equipment manufacturers requiring halogen-free connector materials must select a different product. The material has a risk of mold deposit formation at vent pins when melt residence times exceed 5 min or when nozzle temperatures exceed 270°C. Vent cleaning intervals on 8-cavity relay base tooling have been observed at 40,000–60,000 shots under normal processing; contaminated vents reduce gas escape and promote burn marks at fill ends.

    Colorability is another operational variable. 310SE0 is available in natural and black; custom colors are typically produced by compounding with pigment concentrates at the press. Liquid color carriers can shift ignition resistance and should be verified on 0.71 mm plaques per UL 94 after addition. If the color concentrate carrier is a low-viscosity polyolefin, tensile stress at break may fall below 50 MPa and HDT/A may drop. Validation is performed by molding 0.71 mm test bars and conducting vertical burn testing after 168 h of conditioning at 23°C/50% RH. Regrind levels above 20% can reduce notched Izod impact below 3 kJ/m² and increase lot-to-lot melt viscosity variation, particularly if the regrind is sourced from degating scrap that has experienced additional residence time.

    Contamination with polyamide or glass-filled PBT regrind must be prevented. Polyamide contamination can produce visible delamination and gas generation during melt processing because of incompatibility and moisture absorption in nylon. Glass-filled PBT contamination alters shrink isotropy and can clog small gate inserts. On production lines with shared drying hoppers, a material changeover procedure should include purging with a low-MFI polypropylene or acrylic purge compound followed by 15–20 min of fresh 310SE0 flush at 250°C before molding finished parts. Verification includes melt-flow retention at 250°C under 2.16 kg load and UL 94 vertical burn retention on 0.71 mm specimens.

    Top