Sabic Valox Unreinforced Pbt 215hpr

SABIC VALOX™ Unreinforced PBT 215HPR

    • Product Name: SABIC VALOX™ Unreinforced PBT 215HPR
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 924744
    Density 1.31 g/cm3
    Melt Volume Rate 16 cm3/10 min at 250 C/2.16 kg
    Water Absorption 0.5%
    Tensile Modulus 2300 MPa
    Tensile Stress At Yield 55 MPa
    Tensile Strain At Yield 5%
    Flexural Modulus 2200 MPa
    Flexural Strength 80 MPa
    Charpy Notched Impact Strength 5 kJ/m2 at 23 C
    Izod Notched Impact Strength 5 kJ/m2 at 23 C
    Heat Deflection Temperature At 0 45 Mpa 150 C
    Heat Deflection Temperature At 1 8 Mpa 60 C
    Vicat Softening Temperature 180 C
    Mold Shrinkage 1.5-2.0%
    Volume Resistivity >1E15 ohm cm
    Dielectric Strength 17 kV/mm

    As an accredited SABIC VALOX™ Unreinforced PBT 215HPR factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg moisture-barrier bags, palletized; SABIC VALOX™ Unreinforced PBT 215HPR packaging supports safe industrial handling.
    Container Loading (20′ FCL) 20′ FCL container loaded with SABIC VALOX™ Unreinforced PBT 215HPR in 25 kg bags on pallets, secured for sea transport.
    Shipping SABIC VALOX™ Unreinforced PBT 215HPR is shipped as non-hazardous PBT resin pellets in sealed bags/boxes or bulk containers. It is not regulated for transport (no UN number, hazard class, or packing group). Store in a cool, dry area; protect from moisture, contamination, and physical damage.
    Storage Store SABIC VALOX™ Unreinforced PBT 215HPR in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and moisture. Keep containers tightly closed and protected from contamination. Avoid prolonged humid exposure; dry material per supplier recommendations before processing. Follow the manufacturer’s SDS and local storage regulations.
    Shelf Life Shelf life is typically 24 months from date of manufacture when stored dry, below 40°C, in original unopened packaging.
    Application of SABIC VALOX™ Unreinforced PBT 215HPR

    In low-voltage switchgear terminal blocks rated for 600 V AC with insulation coordination class III and pollution degree 3, VALOX 215HPR unreinforced PBT is evaluated primarily for creepage distance stability after condensation cycling, not for bulk tensile strength. When the insulating body carries a nominal wall of 0.35 mm to 0.60 mm, the material is processed as a natural resin with a colour masterbatch added at 1.0 to 3.0 wt%. If flame retardancy to UL 94 V-0 is requested, an FR additive package must be tested at the final wall section because unreinforced PBT without flame-retardant modification is not automatically classed as V-0. Drying in a desiccant dryer with a dew point of −40°C and a resin bed temperature of 120°C for 3 to 4 h keeps moisture below 0.02%; hydrolysis during plastication otherwise reduces melt viscosity and weakens weld lines. Injection moulding on a machine with a 32:1 L/D general-purpose screw and a shut-off nozzle uses melt temperatures of 245°C to 260°C, mould temperatures of 60°C to 85°C, and injection velocities of 80 to 150 mm/s for thin-wall filling. Holding pressure is staged to avoid sink marks at pin gates. Compliance for the finished terminal block is assessed under IEC 60664-1:2020 for clearance and creepage distances, IEC 60947-7-1:2020 for terminal block performance, and IEC 60112:2009 for comparative tracking index. The terminal product range includes DIN-rail feed-through blocks, fuse holder bodies, and miniature circuit breaker housing insulators. A processing boundary exists when hot runner manifold temperatures exceed 270°C or melt residence time exceeds 5 min, producing discolouration and a drop in notched impact strength that cannot be released by visual inspection alone.

    What Limits Regrind Loading in 12V Automotive Wire-to-Board Connector Plates?

    Sealed and unsealed wire-to-board connector plates in 12V electrical distribution systems are moulded from high-flow unreinforced PBT where wall stock around the terminal pocket is 0.30 mm to 0.45 mm. Dimensional stability after thermal shock from −40°C to 85°C is evaluated under USCAR-2 performance sequences; ISO 6722:2018 applies to cable-level validation rather than directly to connector body material. Formulation commonly includes a heat stabiliser package and colour concentrate at 1.0 to 4.0 wt%; regrind is limited to 10% to 20% by weight for non-safety-critical connector plates because repeated extrusion history reduces elongation at break and increases susceptibility to latch fracture. The regrind limit is not fixed; it is set after measuring the melt flow rate ratio according to ISO 1133-1:2022 and notched Izod impact according to ISO 180:2023 on 100% regrind versus virgin material. Drying at 120°C to a residual moisture below 0.02% is mandatory; a dew point of −35°C or lower prevents voids in terminal pockets. Moulding uses a 40 mm screw with a 20:1 to 24:1 L/D ratio and a reverse-taper nozzle to avoid drool; melt temperature is held between 245°C and 265°C while mould temperature is set to 70°C to 90°C to achieve sufficient crystallinity for terminal retention force. Terminal finished parts include body-side connector housings, terminal position assurance blocks, and wire dress covers. A recognised operational boundary is continuous exposure to hot water/glycol or under-hood temperatures above 120°C combined with vibration; unreinforced PBT may embrittle at the latch root unless an impact-modified variant is specified. Published data for 215HPR-specific USCAR-2 full sequencing is limited; automotive qualification batches must be run on the intended moulding machine.

    High-cavitation tooling for washing machine timer cam plates and refrigerator defrost timer cams runs in semi-continuous cycles where hot runner balance, not material price, controls acceptance. This application uses the base resin unmodified except for a nucleating agent masterbatch at 0.5 to 1.5 wt% for faster crystallisation and a blue or white colour concentrate at 0.5 to 2.0 wt%. The part must withstand ball pressure testing under IEC 60335-1:2020 and abnormal heat conditions without excessive deformation; heat deflection temperature under 1.82 MPa loading, measured per ISO 75-2:2023, is the primary limiting boundary. Drying uses a desiccant dryer at 120°C for 3 to 4 h to a maximum moisture of 0.02%, especially when regrind levels rise to 25% because degraded fines absorb moisture. Moulding is performed with a 28:1 L/D screw and a hot runner system with manifold temperature set 10°C to 15°C below the nozzle melt temperature of 250°C; clamp force is calculated at 300 to 500 kg/cm² of projected area for multi-cavity tools. Terminal parts include timer cams, rotary selector knobs, relay bases, and solenoid bobbins. The principal failure mode is not tensile yield but post-mould shrinkage after elevated ambient storage; parts measured at 24 h after demoulding can show additional linear shrinkage of 0.05% to 0.12% if crystallisation is incomplete due to a cold mould. Moulders applying uncontrolled regrind above 30 wt% may observe an increase in ejection pin punch-through and inconsistent timing mark depth.

    When Ethylene Oxide Sterilisation Replaces Gamma Cycling for Non-Fluid-Path Diagnostic Housings

    Medical handheld diagnostic housings and test-reader bodies made from high-flow unreinforced PBT are candidates when the part carries no repeated fluid contact and is classified as a non-communicating external component. The grade designation alone does not establish biocompatibility; the final part supplier must run extractables and leachables screening appropriate to the device classification. For gamma-sterilised parts, typical irradiation doses of 25 to 40 kGy can shift colour and reduce tensile elongation at break; post-irradiation testing under ISO 527-2:2012 and yellow index measurement per ASTM D6290-19 is used to bound acceptable dose. Ethylene oxide sterilisation, when selected, avoids some oxidative yellowing but introduces a residual-gas risk controlled by aeration time after the cycle. The processing window uses a desiccant dryer at 120°C for 3 to 4 h and a moisture target below 0.02%; melt temperature is set at 245°C to 260°C and mould temperature at 80°C to 100°C to stabilise snap-fit retention. If the device is to pass repeated autoclaving at 121°C or repeated hot water immersion, unreinforced PBT is generally not the safest choice because hydrolysis embrittlement at the snap arm root occurs before dimensional failure is observable. Compliance is evaluated under ISO 10993-5 for cytotoxicity and ISO 10993-10 for sensitisation and irritation; USP Class VI testing is sometimes requested but must be performed on the finished component and selected sterilisation method. Terminal output covers benchtop analyser bezels, strip reader frames, and battery door inserts. Published data for 215HPR under repeated terminal sterilisation cycles is limited; applications requiring more than 50 ethylene oxide cycles should be revalidated on production tooling.

    Tracking Failure Follows Titanium Dioxide Loading in White LED Lamp Bases

    LED retrofit lamp screw base insulators and GU10 adapter housings are thin-wall components in which the compounded PBT must balance flow into 0.25 mm to 0.40 mm ribs against the need to pass end-product glow-wire and tracking tests. The feed matrix is often supplemented with a white or natural carrier masterbatch at 1 to 3 wt%; titanium dioxide colouring can raise tracking risk, so the final formulation is checked under IEC 60112:2009 at the required proof voltage. A key process requirement is the use of a screw with no dead spots and a residence time below 4 min because black spec formation in white parts is a direct rejection criterion. Drying at 120°C for 3 to 4 h is maintained to 0.02% residual moisture, and the mould temperature is set at 70°C to 90°C while the melt temperature is controlled in a narrow band from 245°C to 255°C. The terminal finished components include E26/E27 lamp base skirts, bayonet lamp holders, and ceiling fan speed regulator housings. When the end-use standard requires a glow-wire ignition temperature of 750°C at 1.0 mm wall thickness, unreinforced PBT may need an FR additive; the base grade alone cannot be assumed to pass without testing at the minimum wall.

    Test standardTest condition or applicationRelevance to unreinforced PBT screw base
    IEC 60695-2-11Glow-wire end-product test, typically 650°C or 750°C depending on unattended status and currentDetermines ignition and self-extinguishing behaviour of the insulating part
    IEC 60112Comparative tracking index under ammonium chloride wettingClassifies resistance to creepage current and surface degradation
    UL 94Minimum thickness classificationProvides vertical burn classification only if FR package is present; otherwise HB is typical

    Hydrolysis-Limited Boundaries in Aqueous Glycol Flow Meter Housings

    Ultrasonic and turbine flow meter register housings in heating circuits operate with continuous fluid temperatures of 60°C to 80°C; this is the boundary where unfilled PBT must be scrutinised for hydrolysis-induced embrittlement. The material is chosen because of low water absorption and resistance to oils, greases, and aliphatic hydrocarbons, but neutral or alkaline aqueous solutions at temperatures above 80°C attack the ester linkage over time; a hydrolysis-resistant additive package or a glass-reinforced alternative may be required in pumped return lines. Formulation for flow meter bodies frequently includes a black colour masterbatch at 1.0 to 2.5 wt% and an antioxidant package for long-term heat ageing; inserts, if any, are brass or stainless steel rather than aluminium to avoid galvanic corrosion at the polymer-metal interface. Moulding of parts with internal threads and transducer pockets uses a 30:1 L/D screw and a decompression-after-screw-return profile to prevent drool from the reverse-taper nozzle; melt temperature is held at 245°C to 260°C, and the mould temperature is set at 65°C to 85°C. Terminal products include flow meter register cups, pump terminal boxes, and sensor housings. Compliance for potable water contact is not inferred from the base resin; final parts for drinking water service must be evaluated to NSF/ANSI 61 or applicable regional certification. The operational limit for continuous hot water exposure is commonly stated as 70°C to 80°C; prolonged excursions above 90°C are not recommended for unreinforced PBT unless the application is short-term and non-load-bearing.

    Free Quote

    Competitive SABIC VALOX™ Unreinforced PBT 215HPR prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ 215HPR is a semicrystalline polybutylene terephthalate (PBT) injection-molding resin supplied without glass or mineral reinforcement. The polymer backbone is formed from 1,4-butanediol and terephthalic acid; the resulting ester repeat unit provides a melting transition near 225 °C and a density reported as 1.31 g/cm³ per ISO 1183-1:2019. The “HPR” suffix identifies a healthcare product documentation package rather than a separate chemical composition. The grade is characterized by a melt volume-flow rate of approximately 19 cm³/10 min at 250 °C under a 2.16 kg load when tested to ISO 1133-1:2022. This places 215HPR among the higher-flow unreinforced PBT materials used for thin-wall injection-molding applications requiring high mold replication, low moisture uptake, and controlled lot documentation.

    Because 215HPR contains no fibrous reinforcement, it does not generate the screw, barrel, check-ring, and nozzle abrasion observed with glass-filled PBT compounds. In comparison with 30 wt% glass-fiber-reinforced PBT grades that commonly exhibit flexural modulus values in the 7–9 GPa range, 215HPR has a flexural modulus reported at 2.4 GPa under ISO 178:2019. The unfilled grade therefore trades elevated load-bearing stiffness for lower anisotropic warpage, improved surface appearance, and reduced tool wear. Compared with a standard-viscosity unreinforced PBT having a melt volume-flow rate near 10 cm³/10 min, the higher MVR of 215HPR reduces injection-pressure demand in long flow paths but may reduce melt strength during open-mold handling.

    PropertyTest MethodTypical ValueUnit
    DensityISO 1183-1:20191.31g/cm³
    Melt volume-flow rate, 250 °C/2.16 kgISO 1133-1:202219cm³/10 min
    Tensile stress at yield, 50 mm/minISO 527-2/1A/5057MPa
    Tensile strain at yield, 50 mm/minISO 527-2/1A/505.5%
    Flexural modulusISO 178:20192400MPa
    Flexural strengthISO 178:201983MPa
    Charpy notched impact strength, 23 °CISO 179-1:2010/1eA3.5kJ/m²
    Heat deflection temperature, 1.80 MPaISO 75-2:2013/Af52°C
    Vicat softening temperature, B/50ISO 306:2013/B50175°C
    Water absorption, saturation, 23 °CISO 62:20080.4%
    Molding shrinkage, flow directionISO 294-4:20181.8%
    Molding shrinkage, transverse directionISO 294-4:20182.0%

    The supplied values are lot- and color-dependent; structural design should use the supplier’s current product datasheet and not rely on single-point typical values for failure-mode or tolerance-stack analysis.

    What limits direct hot-runner processing of 215HPR in multi-cavity thin-wall parts?

    Direct hot-runner processing of 215HPR is governed by moisture control, thermal residence, and crystallization kinetics. PBT undergoes hydrolytic chain scission when melt processing occurs above 0.04 wt% moisture. The resin should be dried in a desiccant-bed dryer with a dew point below −30 °C at 120 °C for 4 h before molding. On production-scale dehumidifying dryers, hopper residence below 2 h at reduced airflow may leave localized moisture pockets; continuous dew point monitoring is required because moisture-related loss of intrinsic viscosity may not be visible as surface splay until the melt reaches advanced hydrolysis. Melt processing should be limited to 245–270 °C cylinder zone settings, with the nozzle held near 260 °C. At melt temperatures above 280 °C, thermo-oxidative degradation increases carboxylic acid end-group concentration and reduces notched impact energy measurable by ISO 179-1:2010/1eA.

    Mold temperature is a critical threshold because PBT crystallizes rapidly only when the tool surface is maintained above 60 °C. Low mold temperatures below 50 °C produce a quenched skin layer with reduced crystallinity, which increases post-mold dimensional change and lowers short-term heat resistance measured by ISO 75-2:2013/Af. In multi-cavity hot-runner tooling with cavity-to-cavity temperature variation greater than 5 °C, the variance in crystallization shrinkage can produce warp and hole-position drift; polymer melt entering a colder cavity continues to flow with lower viscosity after the hotter cavities have frozen, causing imbalanced packing. The recommended mold temperature for 215HPR is 60–90 °C. Thin-wall parts with nominal wall thickness below 1.0 mm typically require the upper end of that range to maintain flow length without sacrificing crystalline fraction.

    Hot-runner channel size should be selected for shear heating of the higher-flow PBT not to exceed 1000 s⁻¹ in the gate region. Valve-gated systems are preferred for direct gates; thermal-gated open nozzles may string when the manifold is held above 260 °C. Because 215HPR solidifies quickly once injected, hold-pressure time must be established by gate-seal measurements rather than by cavity fill alone. In tools with 32 or more cavities and sub-1.0 mm wall sections, injection fill times below 0.5 s are common, and the switch-over from velocity control to pressure control should occur at 95–98% of visual fill to avoid overpacking of the gate-adjacent region.

    When a shut-off nozzle is absent and recovery delay exceeds 60 seconds

    A shut-off nozzle becomes operationally important when the molding cycle is interrupted, for example during label placement, insert loading, or robotic part extraction after a sensor fault. If the reciprocating screw remains idle with melt in the barrel at 260 °C for more than 60 s, the residence distribution broadens: melt near the barrel wall remains longer and begins to oxidize, while melt in the center remains less degraded. With a conventional hydraulic machine using a 40 mm screw and 20:1 L/D barrel, the effective residence time in the compression and metering zones can exceed the nominal cycle time by a factor of 2–5 depending on shot volume. The absence of a shut-off nozzle permits molten PBT to continue drooling from the open nozzle during prolonged recovery; the exposed strand oxidizes and, when retracted, may contaminate the next shot as unmelts or carbonized inclusions.

    The relevant failure boundary is not continuous throughput but cumulative thermal history above 250 °C. For unreinforced PBT, total melt residence should remain below 5 min, and preferably below 3 min, across all interruptions. At barrel temperatures of 270 °C, degradation accelerates because ester pyrolysis and thermo-oxidative chain scission occur simultaneously. The processing window narrows by approximately 5 °C when the barrel is run at the upper limit because the melt-temperature rise from screw recovery can add 10–20 °C at the check ring. Shot weights below 25% of maximum plasticating capacity create a mismatch between screw recovery and barrel residence; in that condition, a smaller screw diameter or a lower melt temperature should be used. If the mold requires long hold times, the barrel temperature should be lowered toward 250 °C and the nozzle temperature reduced to 255 °C to reduce idle degradation.

    Operators can detect early degradation by monitoring nozzle pressure during recovery and by recording gravimetric shot weight over 30 consecutive cycles. A rising shot weight with constant back pressure indicates viscosity loss and may be accompanied by yellowing, acrid odor, and mold deposit formation. To limit oxidation when a shut-off nozzle is not available, the charging stroke can be delayed until 5–10 s before the next injection cycle instead of immediately after screw recovery. The use of nitrogen blanket drying does not eliminate melt oxidation but reduces hopper-side moisture ingress when ambient relative humidity exceeds 60%. Published data for this specific interruption configuration is limited, but the degradation sensitivity of PBT at elevated residence time is well established in polymer processing literature.

    For healthcare device molders, regrind from degraded purgings should not be automatically returned to the feed stream. If regrind is permitted, the maximum recommended addition is 20 wt% of dry, uncontaminated regrind only after verification that notched impact strength and tensile elongation at yield remain within the supplier’s specification limits under ISO 527-2/1A/50 and ISO 179-1:2010/1eA.

    The HPR documentation package is intended to support healthcare application qualification but does not replace final-device biocompatibility evaluation. Typical supplier documentation may include lot-specific statements for USP <87> in vitro biological reactivity, USP <88> Class VI testing, ISO 10993-5:2009 cytotoxicity, and ISO 10993-10:2010 sensitization and irritation. The resin should be specified only as a raw material; the finished device must be assessed under ISO 10993-1:2018 after molding, cleaning, packaging, and terminal sterilization because process additives, mold release, or degradation products may alter biological response.

    Compliance DomainStandard or MethodTypical Lot Acceptance Evidence
    In vitro biological reactivityUSP <87>Supplier certificate
    Systemic toxicity and implantationUSP <88> Class VISupplier certificate
    CytotoxicityISO 10993-5:2009Supplier certificate
    Sensitization and irritationISO 10993-10:2010Supplier certificate
    Device risk assessmentISO 10993-1:2018Finished-device validation file

    Chemically, 215HPR resists many aliphatic hydrocarbons, alcohols, and dilute aqueous cleaning solutions at ambient temperature. It is not recommended for prolonged immersion in hot water above 60 °C, strong mineral acids, concentrated oxidizing agents, or amine-containing environments. Hot aqueous service accelerates hydrolysis of the ester backbone; the rate is temperature-dependent and can reduce tensile elongation before macroscopic cracking appears. Steam autoclave sterilization above 121 °C imposes a similar hydrolytic stress. Makers of reusable medical devices should evaluate dry heat, ethylene oxide, or low-dose irradiation only after validating that the selected sterilization dose does not reduce key mechanical properties below the design allowance. Published data for 215HPR at specific radiation doses is limited; dose mapping and post-irradiation testing are therefore required for each molded configuration.

    Mold-Fill Performance in Thin-Wall Electrical Connectors

    The combination of high flow and unfilled surface quality makes 215HPR a candidate for small electrical connectors, sensor bodies, and diagnostic housings where wall thickness is between 0.8 mm and 1.5 mm. In these geometries, the pressure drop across a long melt-flow path is reduced compared with standard-viscosity PBT. The moderate flexural modulus of 2.4 GPa provides snap-fit retention while avoiding the brittleness and anisotropic shrinkage of highly glass-filled grades. Electrical insulation values for PBT are high; volume resistivity is typically above 1 × 1013 ohm·m and dielectric strength near 17 kV/mm under relevant IEC 62631 and IEC 60243-1 methods. Comparative tracking index values for unreinforced PBT frequently report above 400 V under IEC 60112:2020, but the exact value for a production lot should be verified.

    Mold filling in connectors is not solely a function of melt viscosity. The flow-front solidification rate depends on mold temperature, which controls the thickness of the frozen layer. At 80 °C mold temperature and 1.0 mm wall, spiral-flow length increases substantially relative to a 50 °C tool. Field experience on hydraulic injection machines with clamp force between 800 kN and 1.6 MN indicates that filling a 0.8 mm wall connector body may require injection-specific pressure of 100–140 MPa depending on flow length. The same part in a glass-filled PBT often requires a higher melt temperature to overcome viscosity, but 215HPR can be run at lower melt temperature to avoid thermal degradation. The expected molding shrinkage of 1.8% in flow and 2.0% transverse must be accommodated in pin-retention features, latch seats, and connector alignment bosses.

    Thermo-Oxidative Failure Boundaries and Lot Acceptance in Regulated Molding Cells

    Lot acceptance in regulated production requires more than a certificate of analysis. Incoming resin should be checked for moisture content with a Karl Fischer method or a heated moisture analyzer calibrated for PBT; a moisture level above 0.04 wt% should trigger re-drying before supply to the molding cell. Melt flow verification can be conducted on a small lot sample using ISO 1133-1:2022 at 250 °C/2.16 kg. A lot producing MVR outside the supplier’s specified range may indicate unintended regrind, contamination, or thermal history during compounding. Intrinsic viscosity or solution viscosity measurement is preferred when hydrolysis or oxidative degradation is suspected because MVR alone may not distinguish chain scission from additive-related plasticization.

    During production, the molding machine should be fitted with a temperature probe in the nozzle adaptor rather than relying exclusively on barrel band heaters. The nozzle melt temperature should be recorded at least every 5 min. Melt cushion should remain between 2 mm and 5 mm. A decreasing cushion with constant switch-over position often indicates check-ring leakage or viscosity reduction. In such cases, notched impact test bars should be molded and tested to ISO 179-1:2010/1eA after the tool stabilizes. A drop in notched impact strength below 3.0 kJ/m² from a baseline of 3.5 kJ/m² can indicate thermal degradation even when visual appearance remains acceptable. The processing boundary is therefore statistical, not single-point; lot-to-lot and cycle-to-cycle variation must be controlled within ±5 °C melt temperature and ±5 °C mold temperature to keep crystallinity and degradation within an acceptable design envelope.