| HS Code | 893478 |
| Productname | SABIC VALOX™ PCR UV PBT T2N815UX |
| Polymertype | Polybutylene terephthalate (PBT) |
| Recycledcontent | Post-consumer recycled (PCR) content |
| Reinforcement | 15% glass fiber |
| Uvstabilization | UV stabilized |
| Flameretardancy | Flame retardant |
| Density | Approximately 1.53 g/cm³ |
| Tensilemodulus | Approximately 7,000 MPa |
| Flexuralmodulus | Approximately 6,500 MPa |
| Heatdeflectiontemperature | Approximately 180–200 °C depending on load |
| Meltingtemperature | Approximately 225 °C |
| Moldshrinkage | Approximately 0.3–0.8% |
| Ul94flammabilityrating | V-0 typical |
As an accredited SABIC VALOX™ PCR UV PBT T2N815UX factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg moisture-resistant bags, palletized in 1,000 kg quantities for safe industrial storage and handling. |
| Container Loading (20′ FCL) | 20′ FCL loading of SABIC VALOX™ PCR UV PBT T2N815UX resin: palletized 25 kg bags in a dry container, secured and weather-protected. |
| Shipping | SABIC VALOX™ PCR UV PBT T2N815UX is supplied as thermoplastic resin pellets, typically in sealed moisture-barrier bags or bulk containers on pallets. It is generally non-hazardous for transport; keep dry, away from direct sunlight and contamination, and follow the SDS and local shipping regulations. |
| Storage | Store in original sealed packaging in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, heat, moisture, and contamination. Keep containers closed, avoid dust generation, and use first-in-first-out. Follow the supplier’s SDS and local storage regulations. |
| Shelf Life | Shelf life is typically two years from manufacture when stored unopened in original packaging, dry, cool, and protected from sunlight and moisture. |
In exterior automotive connector housing production, the PCR UV-stabilized PBT is processed as a single-resin feedstock after closed-loop drying at 120 °C for 3–4 h to a residual moisture content below 0.02 %; moisture above 0.05 % at melt temperatures between 245 °C and 260 °C accelerates hydrolytic chain scission and reduces tensile elongation at break during plastication, a failure observed on multicavity tools as intermittent short-shot in cavity positions farthest from the sprue. Compliance benchmarks for exterior automotive connectors include USCAR-2 contact retention after thermal aging, ISO 16750-3 fluid immersion resistance, SAE J2527 xenon-arc exterior weathering, and RoHS Directive 2011/65/EU Annex II substance restrictions. The as-supplied resin is proportioned at 100 % for load-bearing connector housings; cold-runner regrind is limited to 20 wt%, and post-industrial reclaim is limited to 15 wt% because higher recyclate fractions can alter melt flow rate and produce warpage in tools exceeding 32 cavities. Molding on reciprocating-screw injection machines with 20:1 L/D barrels, shutoff nozzles, and clamp force from 800 kN to 1,200 kN uses a mold temperature of 40–80 °C and hold pressure between 60 MPa and 80 MPa; hot runner melt temperature must not exceed 270 °C because UV stabilizer degradation raises ΔE above 3.0 after 1,000 h of SAE J2527 exposure. End-use parts include exterior mirror actuator housings, park assist sensor brackets, license plate lamp housings, and exterior door handle brackets.
For photovoltaic combiner boxes and DC connector bodies, the substitution of virgin PBT with this UV-stabilized PCR grade moves verification emphasis toward tracking resistance retention and low-temperature impact after damp heat, because post-consumer fractions may carry trace ionic residues that reduce surface resistivity unless the lot-specific aqueous extract conductivity is below 10 µS/cm and the supplier certifies the PCR feedstock by ISO 14021 recycled content claims. Standards governing this segment include IEC 62790:2020 clause 5.2 thermal endurance, IEC 62852:2014/AMD1:2020 DC connector electrical and mechanical requirements, UL 746C f1 outdoor suitability, and EN 50618 for system-level PV cable management. The material is used as the base resin at 100 % for shell wall thickness from 2.0 mm to 3.5 mm; blends with virgin PBT use 30 wt% of this PCR grade to maintain comparative tracking index above 250 V after 1,000 h of damp heat per IEC 60068-2-78. Injection molding employs sequential valve gating to reposition weld lines away from UV-exposed surfaces, with predrying at 120 °C for 4 h, melt temperature 250–260 °C, mold temperature 60–80 °C, and screw back pressure 0.3–0.6 MPa to limit shear heating. Terminal finished product types include combiner box shells, DC connector bodies, diode heat sink brackets, and PV fuse holder bases. Operational incompatibility: amine-cured epoxy potting compounds with exothermic cure above 90 °C can induce surface hydrolysis at the potting interface and reduce tensile stress at break by more than 15 % after 500 h; published adhesion data for this specific PCR grade with silicone encapsulants remains limited.
Outdoor LED luminaire sockets molded from this PCR UV grade require residual moisture content below 0.02 % before plastication because hydrolysis during melt processing lowers melt viscosity and creates silver streaking in thin-walled lampholder threads at wall thicknesses below 0.8 mm. Compliance standards for the segment include IEC 60598-1:2020 clause 13 insulation resistance, IEC 60695-2-11:2021 glow-wire testing at 850 °C for live-part retention, UL 94 HB at 1.5 mm, and UL 746C f1 UV resistance. The grade is processed near 100 % as supplied for socket bodies; up to 15 wt% dry, clean regrind from sprue and runner systems is acceptable on non-flame-critical surfaces only, because higher recyclate content can lower tracking resistance under condensation cycling. Downstream processing uses injection molding with hot-runner systems, mold temperatures of 80–100 °C, and holding pressure sufficient to maintain thread dimensional tolerance after 24 h conditioning at 23 °C ± 2 °C and 50 ± 5 % relative humidity per ISO 291. Terminal finished product types include streetlight lampholder bases, LED module carrier plates, terminal-block insulating strips, and outdoor festoon socket bodies. Operational boundary: prolonged contact with unreacted amine-based surface primers above 60 °C may promote surface microcrack formation around brass inserts; insert-molding trials should include thermal shock verification per IEC 60068-2-14.
When the PCR UV-stabilized PBT is selected for EV charging inlet housings and plug bodies, the formulation boundary is controlled by low-temperature impact retention after solar loading, because the recyclate phase may contain degraded polybutylene terephthalate segments that nucleate crystallization and reduce notched impact strength at -30 °C below 3.5 kJ/m² if melt residence time exceeds 6 min. Compliance benchmarks include IEC 62196-1:2022 mechanical abuse tests, UL 2251 for EV plugs and receptacles, SAE J1772 dimensional interoperability, and RoHS Directive 2011/65/EU Annex II. The material is proportioned at 80–100 % with 0–20 wt% virgin PBT dilution; lot-specific adjustment is required because post-consumer feedstock intrinsic viscosity can vary by 0.05–0.10 dL/g and shifts the melt flow rate under ISO 1133-1:2022 at 250 °C/2.16 kg. Injection molding uses 20:1 L/D screws with compression ratio of 2.5:1, hot runner gate temperature not exceeding 255 °C, and gas counter-pressure at 1–2 MPa for latch geometry with thick-to-thin transitions; mold temperature is held at 60–80 °C to avoid post-mold warpage. Terminal finished product types include EV charging plug housings, vehicle inlet housings, connector latch bodies, and charge port shutter frames. Incompatibility: free halogen species from unvalidated flame retardant masterbatches can accelerate UV stabilizer depletion under moist conditions and lower f1 weathering performance after 1,000 h of ISO 4892-2:2021.
Garden and outdoor power tool housing molds running this UV-stabilized PCR PBT at 40–60 wt% in impact-modified PBT compounds exhibit an inverse relationship between post-consumer content and multiaxial impact at low temperature; processors using the grade as a drop-in base resin must verify that notched Charpy impact after 500 h of ISO 4892-2:2021 xenon-arc exposure remains above the application-specific minimum defined in the tooling specification. Compliance standards for power tools and garden appliances include IEC 62841-1 mechanical strength clauses, EN 60335-1 clause 30 heat and fire resistance, and UL 94 HB at 1.5 mm for portable appliance enclosures; end-product UV performance is benchmarked to ISO 4892-2:2021 method A cycle 1 with ΔE limit 3.0 after 1,000 h. Injection molding runs at melt temperature 240–250 °C, mold temperature 40–60 °C, and screw back pressure 0.5–1.0 MPa to preserve impact modifier domains and avoid excessive shear heating in the recyclate fraction; drying at 120 °C for 3–4 h is mandatory when warehouse relative humidity exceeds 60 %. Terminal finished product types include string trimmer motor housings, leaf blower fan shrouds, robotic mower body panels, and handheld pruner gear cases. Published data for this specific UV-stabilized PCR PBT in gas-assisted injection molding of garden power tool housings is limited; mold-filling simulation should be calibrated with capillary rheometry from the actual production lot.
Industrial outdoor enclosure manufacturers specify this UV-stabilized PCR PBT for control box lids and terminal bases where dimensional tolerance after thermal cycling must remain within ±0.2 % when measured after 96 h at 85 °C and 85 % relative humidity per IEC 60068-2-78. Compliance standards include IEC 60947-1 for low-voltage switchgear and controlgear, UL 50E environmental enclosure ratings, NEMA 250 Type 3R outdoor exposure, and UL 746C f1 weatherability. The resin is used at 100 % as supplied for ignition-protected retainers and terminal bases; regrind from hot-runner molds is restricted to 20 wt% due to reduced notched impact at 0 °C below 4.0 kJ/m² when recycled content exceeds that threshold. Production molding employs 2.5–3.0:1 compression ratio screws, melt temperature 245–255 °C, mold temperature 60–90 °C, and shot volume set to leave a 2–3 mm cushion to avoid screw pulsation in thin-wall lid sections. Terminal finished product types include outdoor HVAC control enclosures, irrigation controller boxes, remote telemetry unit housings, and water valve actuator covers. The material is not recommended for continuous exposure to strong aqueous alkalis above pH 10 at temperatures above 60 °C because polybutylene terephthalate ester linkages undergo accelerated hydrolysis; published data for laser marking contrast on this PCR grade after 2,000 h of outdoor aging is limited.
Outdoor telecommunications network termination enclosures and fiber splice tray brackets use this UV-stabilized PCR PBT when the part must retain screw boss torque after repeated access and resist rain-water ingress at IP55 or IP65 sealing interfaces. Compliance standards include Telcordia GR-487-CORE Issue 5 structural integrity for outdoor enclosures, IEC 61753-1 optical connector environmental performance, UL 94 HB at 1.5 mm, and REACH SVHC screening per Article 33. The material is processed at 100 % for small structural brackets and clamp bodies; 15 wt% regrind is permissible only after rerunning the drying step because moisture trapped in recycled flake contributes to gas splay at boss locations. Injection molding uses hot-runner valve gates for cable entry features, mold temperatures of 60–80 °C, and screw rotation speed below 100 rpm to limit shear-induced melt temperature rise in the PCR phase. Terminal finished product types include fiber splice tray brackets, drop cable clamp bodies, network termination enclosure hinges, and respiratory vent nozzle retainers. Operational boundary: exposure to diesel vapor and concentrated ozone above 0.05 ppm is not covered by standard UV and hydrolytic aging specifications and requires separate validation per ISO 1431-1.
Competitive SABIC VALOX™ PCR UV PBT T2N815UX prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PCR UV PBT T2N815UX is an unfilled, ultraviolet-stabilized polybutylene terephthalate injection moulding compound formulated with post-consumer recycled feedstock. The backbone polymer is a semicrystalline polyester produced from 1,4-butanediol and terephthalic acid or dimethyl terephthalate, with a melting endotherm near 223–225 °C and a glass transition below 60 °C. The T2N815UX designation indicates a UV-stabilized PBT grade carrying a recycled-content claim, although the exact post-consumer fraction is lot-dependent and must be confirmed through SABIC documentation rather than inferred from the grade name alone. Published data for this specific configuration is limited; the portfolio-level ranges below are drawn from SABIC VALOX unfilled UV PBT documentation and do not replace a lot-specific certificate of analysis.
| Property | Method | Typical range | Unit |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 1.28–1.33 | g/cm³ |
| Melt volume-flow rate, 250 °C/1.2 kg | ISO 1133-1:2022 | 8–20 | cm³/10 min |
| Tensile stress at yield, 50 mm/min | ISO 527-2:2012 | 50–60 | MPa |
| Tensile modulus | ISO 527-2:2012 | 2,300–2,800 | MPa |
| Flexural modulus | ISO 178:2019 | 2,200–2,700 | MPa |
| Notched Izod impact, 23 °C | ISO 180/A:2023 | 3.0–6.0 | kJ/m² |
| Heat deflection temperature, 1.82 MPa | ISO 75-2:2013 | 50–65 | °C |
| Vicat softening temperature, B50 | ISO 306:2022 | 170–185 | °C |
Processing begins with moisture control because PBT undergoes hydrolytic chain scission in the melt. Residual moisture must be held below 0.02 % by Karl Fischer titration per ISO 15512:2019. A desiccant dryer with a dew point below -30 °C and a bed temperature of 120 °C for 3–4 h is the standard starting point for virgin PBT; post-consumer recycled feedstock with initial moisture above 0.08 % may require 4–6 h at 120 °C. Drying should not exceed 130 °C or 6 h because prolonged thermal exposure can produce oxidative yellowing and surface oligomer bloom, which interferes with paint adhesion and weld-line strength.
Barrel temperatures should be profiled with a rear zone of 230–240 °C, a middle zone of 245–255 °C, a front zone of 250–260 °C, and a nozzle held at 250–265 °C. Melt temperature measured by an insertion pyrometer should remain between 245 °C and 260 °C. Above 260 °C, total residence time should be limited to 3 min or less; the maximum recommended total residence time across the entire melt path is 5 min. Mould temperature is typically set between 40 °C and 80 °C. A lower mould temperature of 40–60 °C improves gloss and release but reduces crystallinity and can increase post-mould shrinkage. A higher mould temperature near 80 °C is preferred for close-tolerance parts because it promotes crystallization and dimensional stability, though it extends cycle time and may increase outgassing.
General-purpose screws with 20:1–25:1 L/D and compression ratios of 2.5:1–3.0:1 are acceptable for unfilled PBT. Back pressure should be maintained at 0.3–0.7 MPa, and screw decompression after recovery should not exceed 3–5 mm to prevent air entrapment and splay. Injection speed should be moderate to fast to reduce premature freeze-off in thin walls, but excessive shear heat can accelerate degradation of post-consumer fractions.
On production-scale machines with clamp force between 80 t and 120 t, cushion instability and screw torque fluctuation are more frequent with post-consumer PBT than with virgin PBT because the recycled feedstock has a broader molecular weight distribution and may contain trace non-PBT residues. The dominant injection moulding failure modes include surface splay from residual moisture, weak knit lines at low mould temperature, and occasional black specks from insufficient melt filtration. Stabilizing the cushion by holding back pressure in the upper half of the recommended range and using a free-flow check ring reduces shot-weight drift. When regrind is added, it is common practice to limit regrind to 20 % by weight with the same material and to revalidate melt volume-flow rate after each heat history because multiple processing passes can shift MVR upward through chain scission.
The post-consumer fraction in T2N815UX introduces multiple heat histories that are not present in virgin PBT. Even when melt volume-flow rate remains within the 8–20 cm³/10 min range at 250 °C/1.2 kg, the molecular weight distribution may be broader, and acid end group concentration may be higher than in virgin polymer. This changes melt viscosity at low shear, reduces variable-temperature processing robustness, and can increase sensitivity to hydrolysis if drying is marginal. Incoming lot acceptance should therefore include moisture content by ISO 15512:2019, MVR by ISO 1133-1:2022, and tensile yield by ISO 527-2:2012. A specification limited to density and visual appearance does not adequately control processing behaviour.
Dimensional stability is affected by the crystallization rate of the recycled fraction. Mould shrinkage for unfilled PBT measured according to ISO 294-4 is typically 1.5–2.0 % in the flow direction and 1.8–2.4 % transverse, but post-consumer variability can shift shrinkage by 0.2–0.4 % across lots if non-PBT contaminants alter nucleation density. Dimensional checks should therefore be performed after conditioning for 24 h at 23 °C and 50 % relative humidity, not immediately after demoulding.
Compared with virgin PBT, the recycled grade may require stricter melt filtration and more frequent screen-pack changes during compounding. Twin-screw compounding lines with vacuum devolatilization at approximately -0.08 MPa are used to remove residual monomers, oligomers, and moisture; excessive vacuum can strip low molecular weight species and destabilize screw filling. Published data for this specific configuration is limited, and processors should derive lot-specific processing limits from first-article trials rather than extrapolating from virgin PBT documentation.
Ultraviolet stabilization is evaluated under laboratory weathering conditions. The relevant methods are ISO 4892-2:2013 for xenon arc exposure and ASTM G154-23 for fluorescent ultraviolet exposure. The stabilization package is intended to reduce UV-induced chain scission, gloss loss, chalking, and discoloration in outdoor or semi-outdoor service. Acceptance thresholds are application-dependent; some automotive and exterior electrical specifications require at least 70 % tensile elongation retention after 800 h to 1,000 h of xenon arc exposure, but the validated exposure window for T2N815UX must be confirmed against the actual SABIC datasheet or OEM test plan. The UV package does not confer unlimited outdoor durability, and parts exposed continuously in high-UV geographies should be validated at the end-use wall thickness and colour formulation.
T2N815UX occupies a specific application band within the VALOX PBT portfolio. Because it is unfilled, it retains the low warpage and surface-appearance advantages of neat PBT but does not provide the structural stiffness of glass-filled grades. Its post-consumer recycled content differentiates it from virgin unfilled UV PBT, while its UV stabilization differentiates it from general-purpose unreinforced PBT grades that are intended primarily for indoor electrical and mechanical components. The compound should not be assumed to carry a UL 94 V-0 flame-retardant rating unless a specific yellow card is supplied; flame-retardant VALOX grades must be selected when a defined flammability class is required at a nominal wall thickness.
| Product class | Reinforcement | Flexural modulus range | HDT/A range | Characteristic limitation |
|---|---|---|---|---|
| T2N815UX PCR UV unfilled PBT | None | 2,200–2,700 MPa | 50–65 °C | Lot-to-lot recycled feedstock variability |
| Virgin unfilled UV PBT | None | 2,300–2,800 MPa | 50–65 °C | No recycled-content claim |
| 30 % glass-fibre reinforced PBT | Glass fibre | 8,000–10,000 MPa | 200–215 °C | Warpage and anisotropic shrinkage |
| Flame-retardant unfilled PBT | None | 2,200–2,800 MPa | 55–70 °C | UL 94 rating required for electrical enclosures |
The comparison shows that T2N815UX is not a direct substitute for glass-filled VALOX grades in load-bearing brackets or structural housings. The heat deflection temperature of unfilled PBT under 1.82 MPa remains below 65 °C, so continuous load-bearing use above 60 °C is outside the operating envelope. Glass-filled grades raise HDT/A to approximately 200–215 °C but introduce fibre orientation, warpage, and surface appearance trade-offs. Flame-retardant grades address ignition resistance but may reduce flow length and require higher mould temperatures to avoid bloom. Selection between these families should be based on the end-use load case, thermal exposure, flammability requirement, and environmental content declaration.
The recycled-content claim associated with T2N815UX falls under ISO 14021:2016 self-declared environmental claims. Mass-balance or segregated supply chain documentation should be requested from SABIC to substantiate the post-consumer fraction in a given lot. The grade is subject to regional chemical control requirements, including REACH candidate list obligations and the RoHS Directive 2011/65/EU recast by (EU) 2015/863 for electrical and electronic equipment. A food-contact status under FDA 21 CFR 177.1660 must not be assumed unless SABIC issues an explicit food-contact certification for the specified colour and additive package. Automotive OEM approvals are not automatic; validation under platform-specific material standards such as GMW, Ford WSS-M4D, or VW 50133 may be required before production release.
Typical application fields for an unfilled PCR UV PBT include exterior trim clips, sensor brackets, lighting bezels, electrical connector housings, non-structural outdoor enclosures, and components exposed to intermittent sunlight and hydrocarbon contact. The material offers resistance to aliphatic hydrocarbons, gasoline, alcohols, and many industrial oils at room temperature. It is not suitable for continuous immersion in hot water or steam because the ester linkage hydrolyzes above 60 °C over extended exposure. Strong acids, strong bases, and some halogenated solvents attack PBT. The ultraviolet package improves outdoor colour stability but does not replace mechanical protection, and parts with high load-bearing requirements should be designed with unfilled PBT limitations in mind. If a defined flame class, a high HDT/A above 100 °C, or very tight post-mould shrinkage below 1.0 % is required, an alternative VALOX grade should be selected.