Sabic Valox Pcr Pbt T2nv8090

SABIC VALOX™ PCR PBT T2NV8090

    • Product Name: SABIC VALOX™ PCR PBT T2NV8090
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 895674
    Productname SABIC VALOX™ PCR PBT T2NV8090
    Polymertype Polybutylene terephthalate (PBT)
    Recycledcontent Post-consumer recycled (PCR)
    Thermoplasticclass Semi-crystalline engineering thermoplastic polyester
    Processingmethod Injection molding
    Moisturesensitivity Hygroscopic; requires drying before processing
    Density Approximately 1.30–1.55 g/cm³ depending on grade formulation
    Meltmassflowrate Grade-specific; confirm with manufacturer data sheet
    Tensilemodulus Approximately 2,400–8,000 MPa depending on reinforcement
    Tensilestrengthatbreak Approximately 45–120 MPa depending on reinforcement
    Elongationatbreak Approximately 2–50% depending on reinforcement
    Flexuralmodulus Approximately 2,200–8,000 MPa depending on reinforcement
    Notchedizodimpactstrength Grade-specific; confirm with manufacturer data sheet
    Heatdeflectiontemperature Approximately 60–210°C depending on reinforcement and load
    Vicatsofteningtemperature Approximately 170–210°C depending on formulation
    Waterabsorption Low; typical PBT behavior
    Moldingshrinkage Approximately 0.2–2.5% depending on reinforcement and processing
    Chemicalresistance Good resistance to many oils, greases, and solvents
    Electricalinsulation Good electrical insulating properties typical of PBT

    As an accredited SABIC VALOX™ PCR PBT T2NV8090 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ PCR PBT T2NV8090 is supplied in 25 kg moisture-barrier bags, palletized for industrial handling and storage.
    Container Loading (20′ FCL) SABIC VALOX™ PCR PBT T2NV8090 is loaded in a 20′ FCL container, palletized and secured, observing weight and packaging limits.
    Shipping SABIC VALOX™ PCR PBT T2NV8090 ships as non-hazardous solid resin pellets in sealed 25 kg bags or octabins. Keep dry and clean, protected from moisture, contamination, and direct sunlight. Use standard freight; follow the SDS, packaging integrity checks, and local transport regulations.
    Storage Store SABIC VALOX™ PCR PBT T2NV8090 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and incompatible chemicals. Keep containers closed and protect from moisture and dust. Avoid static buildup and follow safe stacking limits. Use original packaging; consult the SDS and local regulations for specific requirements.
    Shelf Life SABIC VALOX™ PCR PBT T2NV8090 typically has a 24-month shelf life when stored dry in unopened original packaging.
    Application of SABIC VALOX™ PCR PBT T2NV8090

    For thin-wall connector insulators molded from SABIC VALOX™ PCR PBT T2NV8090, the drying sequence is the first limiting variable. Desiccant-bed drying at 120°C for 4 h with a dew point below -30°C reduces residual moisture to less than 0.02% by mass when verified by ISO 15512 Method A. On a 50-t hydraulic injection molding press with a 35 mm three-zone screw and 20:1 L/D ratio, the melt profile from feed throat to nozzle is set at 240°C, 250°C, 255°C, and 260°C, with actual melt temperature confirmed by needle pyrometer rather than inferred from barrel thermocouples. Injection velocity is maintained between 180 mm/s and 260 mm/s for wall sections of 0.8 mm to 1.2 mm; velocities below this range promote flow hesitation at the terminal pin array, while higher velocities generate shear heating sufficient to produce color shift in the PCR fraction. Holding pressure is applied at 65 MPa to 85 MPa for 2.5 s to 4 s, with gate freeze confirmed by part-weight stabilization rather than timer setting. Back pressure is held at 4 bar to 8 bar and screw recovery speed at 90 rpm to 120 rpm. Terminal products are multi-pin industrial connector insulators and relay sockets requiring UL 94 V-0 at the minimum thickness declared on the SABIC Yellow Card, with creepage and clearance audited under IEC 60664-1 for pollution degree 2 environments.

    What Processing Window Avoids Gate Stringing in Terminal Block Inserts?

    On multi-cavity tooling for low-voltage terminal blocks, a two-stage injection profile is used with T2NV8090 to avoid gate stringing and insert displacement. The first stage fills the runner and gate land at 220 mm/s; the second stage packs the part at 55 MPa to 75 MPa depending on cavity balance. Brass and phosphor-bronze terminal inserts are preheated to 90°C before placement. If insert temperature falls below 70°C, the PCR PBT freezes prematurely at the insert interface, producing stress concentrations that are detectable by polarization microscopy around the crimp zones. This is a known batch-scale failure mode because after 48 h, cracks propagate from insert corners during vibration testing under IEC 60947-1. For wall sections above 1.0 mm, holding time is extended by 0.5 s per additional millimeter of nominal wall. Melt temperature at the nozzle is limited to 260°C; prolonged residence above 300 s at this temperature causes a measurable reduction in melt viscosity and a shift in electrical tracking resistance. Compliance for DIN rail terminal blocks includes a comparative tracking index above 250 V per IEC 60112 when creepage distances fall below 2.0 mm for pollution degree 2. Batch records should retain the lot-specific melt volume-flow rate measured under ISO 1133-1:2022 at 250°C and 2.16 kg. RoHS Directive 2011/65/EU Annex II and REACH Regulation EC No 1907/2006 SVHC declarations are verified against the supplier certificate for each production lot because recycled feedstock origin can change with supplier sourcing.

    In automotive interior harness retainers operating at discontinuous 85°C peaks, the relevant failure mode of T2NV8090 is not short-term heat deflection but hydrolytic chain scission during hot-moisture exposure. Published data for this specific PCR configuration under OEM long-term heat-aging protocols is limited; qualification must therefore be run on molded plaques per ISO 188 at 120°C for 500 h rather than inferred from PBT homopolymer databases. The primary degradation sequence begins with residual ester hydrolysis, increases carboxyl end-group concentration, and leads to brittle fracture during clip insertion after hot-dry exposure. Amine-based heat stabilizers and free amine additives accelerate this chain-scission pathway in hot-moisture service and should be excluded from the formulation unless a specific end-of-life thermal oxidation test has been passed. Moldex3D or Moldflow filling studies should place the weld line away from the snap-fit root because weld-line strength in recycled PBT is more variable than virgin PBT. The post-mold shrinkage allowance for wiring harness retainers is 1.7% to 2.1% in the flow direction and 1.8% to 2.2% cross-flow when measured after 48 h at 23°C and 50% relative humidity under ISO 294-4. Terminal products include harness retainers, connector backshells, and sensor brackets for cabin and engine-compartment bulkheads where dimensional tolerance is governed by clip retention force rather than cosmetic appearance.

    If a Non-Aesthetic Structural Frame Is Transferred from Virgin PBT to T2NV8090

    If a non-aesthetic structural frame inside a small appliance is transferred from virgin PBT to SABIC VALOX™ PCR PBT T2NV8090, the substitution is functionally acceptable only where the PCR fraction is not in direct food contact and where surface speck variation does not affect product safety. The grade is not marketed as compliant with FDA 21 CFR 177.1660 or EU Regulation 10/2011 for direct food-contact articles; such use falls outside the documented scope. In electric-heater internal frames and humidifier bases, the load-bearing geometry is designed with trapezoidal ribs rather than uniform wall stock to compensate for melt viscosity shifts caused by PCR feedstock. Gate location is placed at the thickest section of the frame because early freeze-off at thin hinge features produces short shots that are not detected by pressure-drop alarms. Inserted brass bosses are preheated to 80°C to reduce differential shrinkage at the insert perimeter. If boss pull-out force is a specification, testing is conducted per ISO 19220-1 with a crosshead speed of 5 mm/min on conditioned specimens. The post-mold dimensional audit includes a flow-direction allowance of 0.8% to 1.4% for parts stored at 40°C for 72 h before measurement. Recycled-content documentation under ISO 14021 requires lot-specific mass-balance certification, which is particularly relevant when OEM purchasers require evidence of post-consumer resin allocation in product environmental declarations. The terminal products are internal structural frames, air baffles, and mounting brackets that are hidden behind cosmetic fascias and are not direct food-contact surfaces.

    Damp-Heat Exposure, Chain Scission, and Creepage Distance

    Damp-heat conditioning at 85°C and 85% relative humidity is the most severe qualification condition for LED socket housings molded from T2NV8090 because PBT ester linkages undergo autocatalytic hydrolysis once water penetrates the molded surface. Lamp bases and sockets produced under IEC 60238 and IEC 60598-1 are tested after 1,000 h of damp-heat exposure per IEC 60068-2-78. The critical design parameter is not initial tensile strength but the retention of creepage distance after chain scission has reduced surface hardness. For lampholder insulation at 250 V a.c. under pollution degree 2, a creepage distance of 5.0 mm is required for basic insulation; this distance must be maintained after damp-heat exposure and after a subsequent mechanical impact test. T2NV8090 parts stored in humid environments before secondary welding show inconsistent weld-line strength unless pre-drying is applied at 110°C for 3 h. Mold flow analysis places the gate away from the bayonet ring to avoid a weld line crossing the threaded lamp-base seat, which is the highest-stress region during lamp insertion. The recycled PBT feedstock causes wider batch-to-batch variation in melt flow, so a same-run viscosity check under ISO 1133-1:2022 is required before running large cavitation tooling. UL 94 V-0 classification is thickness-dependent; the minimum thickness on the Yellow Card for T2NV8090 must be matched to the thinnest socket wall, usually not below 0.75 mm, and shall not be extrapolated to thinner sections without retesting.

    Standard codeTest conditionApplication trigger
    UL 94 V-0vertical burn at declared minimum wall thicknessconnector insulators, relay sockets, lamp bases
    IEC 60695-2-12750°C glow wire at 1.0 mmunattended appliance structural frames carrying live parts
    IEC 60112comparative tracking index at 100 V to 600 Vlow-voltage switchgear and terminal blocks with reduced creepage
    IEC 60068-2-7885°C and 85% RH, 1,000 hLED sockets and damp-heat-exposed enclosures
    ISO 527-1/-2tensile modulus at 1 mm/minsnap-fit retainers and wiring harness clips
    ISO 178flexural strength at 2 mm/mininternal structural frames with ribbed geometry
    ISO 294-4shrinkage after 48 h at 23°C and 50% RHdimensional audit for insert overmolding

    A different processing route emerges in power-tool brush holders and armature insulators molded from T2NV8090. In these components, the failure mode is not hydrolytic degradation but surface tracking across the arc shield and weld-line fracture under vibration. Mold flow simulation is used to position the weld line outside the brush pocket because a weld line crossing the arc shield is rejected under the mechanical endurance tests of IEC 60745-1. The gate location is placed opposite the brush pocket to produce unidirectional flow orientation that reduces dielectric weak points at the pocket edge. Melt temperature is held at the lower end of the PBT processing window, between 245°C and 255°C, to limit thermal chain scission that would otherwise reduce comparative tracking index. Short-fiber reinforcement is not assumed with T2NV8090; if the application requires tensile modulus above 3,000 MPa, a glass-filled PCR grade must be specified because this resin in its unfilled form is outside the mechanical envelope for high-load motor housings. Inserted carbon-brush holders are preheated to 100°C to minimize differential shrinkage and avoid microcracks around the insert that become tracking initiation sites. The terminal products are brush holders, armature insulators, and trigger housings for hand-held power tools where the molded part is subjected to arc exposure, vibration, and rapid temperature rise from the motor stack.

    Free Quote

    Competitive SABIC VALOX™ PCR PBT T2NV8090 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ PCR PBT T2NV8090 is a polybutylene terephthalate injection-molding grade incorporating post-consumer recycled feedstock. The grade code T2NV8090 denotes a defined viscosity, additive, and color package within the VALOX™ PBT series, while the PCR prefix identifies post-consumer recyclate content. The material is semicrystalline and therefore exhibits molded-in shrinkage, fast crystallization, and a sharp solid-to-melt transition. Because PCR-derived composition can shift melt rheology, thermal-oxidative stability, and part-level shrinkage relative to virgin PBT, incoming inspection should be performed using ISO 1183-1, ISO 527-1/-2, ISO 178, and ISO 75-1/-2. Published data for this specific configuration is limited in secondary literature; the current SABIC product datasheet remains the binding specification for release and quality limits.

    Does T2NV8090 Conform to Unfilled-PBT Benchmarks or a Separate Specification?

    Property characterization for PBT grades is expressed through a small set of standard methods. Density is determined by ISO 1183-1; mechanical performance under short-term tensile loading is determined by ISO 527-1/-2 at 50 mm/min; flexural modulus is measured by ISO 178; heat deflection temperature under 1.80 MPa is measured by ISO 75-1/-2; and melt flow rate is measured by ISO 1133-1:2022 at 250°C under 2.16 kg. For unfilled virgin PBT, these methods generally generate density of 1.30–1.32 g/cm³, tensile stress at break of 50–60 MPa, tensile modulus of 2500–2800 MPa, flexural modulus of 2200–2700 MPa, and heat deflection temperature at 1.80 MPa of 50–65°C. These ranges are not the T2NV8090 specification; they are unfilled-PBT reference bands used to detect PCR-induced deviation. The T2NV8090 datasheet should be used as the binding source for property limits because recycled content may shift notched impact and melt viscosity beyond baseline expectations.

    Property Unit Test method Unfilled PBT reference band T2NV8090 acceptance basis
    Density g/cm³ ISO 1183-1 1.30–1.32 Supplier datasheet
    Tensile stress at break MPa ISO 527-1/-2 50–60 Supplier datasheet
    Tensile modulus MPa ISO 527-1/-2 2500–2800 Supplier datasheet
    Flexural modulus MPa ISO 178 2200–2700 Supplier datasheet
    Heat deflection temperature, 1.80 MPa °C ISO 75-1/-2 50–65 Supplier datasheet
    Melt flow rate, 250°C/2.16 kg g/10 min ISO 1133-1:2022 10–30 Lot-specific; establish baseline
    Moisture at molding wt% ISO 15512 ≤0.02 Production target

    Post-mold shrinkage is affected by PCR-derived nucleation and molecular weight distribution. For unfilled PBT, shrinkage after 24 h under ISO 294-4 typically lies between 1.2% and 2.0% in the flow direction and between 1.5% and 2.2% perpendicular to flow. These reference bands may shift with PCR-derived contaminants or regrind content. Water absorption under ISO 62 at 23°C saturation is generally near 0.4–0.6 wt% for unfilled PBT. Because mold shrinkage controls dimensional qualification, tooling trials should measure cavity-specific shrinkage on a production press using the same gate geometry and packing profile intended for production.

    Injection molding processing with T2NV8090 begins with desiccant drying. A desiccant-bed dryer with dew point ≤ −40°C and air temperature 120°C for 3–4 h is applied to reduce moisture to ≤ 0.02 wt%. Drying time must be extended when ambient relative humidity exceeds 60% or when regrind is added above 20 wt% because post-consumer PBT can carry adsorbed moisture. Barrel temperature profiles are typically set between 240°C and 260°C, with nozzle temperature controlled within 250–260°C. Mold surface temperature is normally held between 40°C and 80°C, depending on crystallization and dimensional requirements; below 40°C the risk of nozzle freeze-off and incomplete crystallinity increases. Screw geometry with L/D 20:1 to 25:1 and compression ratio 2.5:1 to 3.5:1 provides homogeneous melting without excessive residence time. Back pressure is usually maintained at 0.5–1.5 MPa hydraulic, while screw surface speed is kept in the range 0.10–0.25 m/s. Production-scale failure modes observed on injection lines include gas streaking from incomplete moisture removal, black specks from recycled stream contamination, and flow-length variability due to melt flow shifts. These conditions are standard for unfilled PBT, but the PCR grade requires tighter incoming inspection because post-consumer fraction can alter the relationship between barrel setpoint and actual melt viscosity.

    When Recycled PBT Feedstock Shifts Batch Melt Stability Under Heat

    Hydrolytic degradation is the principal process risk when recycled PBT is held in the melt state. Ester linkages react with residual moisture; the reaction proceeds through chain scission and reduces molecular weight, measurable as an increase in melt flow rate and a decrease in tensile elongation. In PBT, moisture above 0.02 wt% at melt temperature 260°C can shift melt flow rate beyond a ±10% process-control envelope within 5 min. Published kinetic constants for this specific PCR distribution are limited, so molding trials should map melt flow rate by ISO 1133-1:2022 at 250°C/2.16 kg against residence times of 2 min, 5 min, 10 min, and 15 min. A change greater than 10% from the qualified baseline indicates a non-reversible shift; material should be purged and drying verification repeated. Twin-screw compounding lines with L/D 40:1 and vacuum venting below 50 mbar are used to strip volatiles from PCR feedstock, but injection molders cannot replicate this devolatilization inside a reciprocating-screw barrel. Antioxidant and hydrolytic stabilizer packages, typically based on hindered phenolic and phosphate systems, are used to suppress chain scission; amine-based additives should be avoided because they can promote discoloration and secondary degradation in PBT. Regrind should not exceed 20 wt% unless lot-specific thermal stability has been confirmed because multiple heat histories lower intrinsic viscosity and increase carboxylic acid end-group concentration.

    Applications for T2NV8090 are evaluated against electrical, mechanical, and thermal standards. Low-voltage connectors, terminal blocks, sensor brackets, appliance enclosures, and interior structural supports fall into the candidate usage envelope where short-term temperature excursions remain below the heat deflection temperature and chemical exposure is limited to non-solvent hydrocarbons. For electrical parts, tracking resistance is screened through IEC 60112; glow-wire ignition and flammability are screened through IEC 60695-2-10 and IEC 60695-2-11; flammability class is verified by UL 94 at the final wall thickness and color. Mechanical robustness of snap-fit geometries is estimated using flexural modulus from ISO 178 and tensile modulus from ISO 527-1/-2. Creep-sensitive applications require time–strain data under ISO 899-1 or internal test protocols; published data for this specific PCR configuration is limited, so application-specific testing is required. Chemical resistance to hot alkaline solutions and zinc chloride road-salt solutions should be validated because PBT can undergo environmental stress cracking under these exposures. If the component must retain dielectric strength after moisture conditioning, IEC 60243-1 breakdown voltage testing should be performed on molded plaques before final tool release. PBT without flame-retardant modification typically does not achieve UL 94 V-0; many unfilled PBT grades are classified HB at 1.5 mm. If the T2NV8090 datasheet lists a V-2 or V-0 rating, that rating applies only to the tested thickness and color. End-use flammability must be re-tested when pigment, regrind, or wall thickness changes.

    Compared with virgin unfilled PBT, T2NV8090 can exhibit wider melt flow and color batch variation because post-consumer feedstock has a broader molecular weight distribution and possible metal or polymer contamination. Glass-filled PBT grades differ in tensile modulus, which is typically above 8000 MPa at 30 wt% glass under ISO 527-1/-2, whereas unfilled grades remain below 3000 MPa. The PCR grade should not be considered a drop-in replacement for glass-filled PBT in load-bearing gear housings or pump bodies unless structural analysis confirms lower modulus and lower creep resistance are acceptable. Compared with PBT/PET blends, T2NV8090 usually exhibits a narrower melting range and faster crystallization if PET content is low; differential scanning calorimetry by ISO 11357-1/-3 records crystallization and melting peaks that can be used to detect blend composition drift. Impact-modified PBT grades differ in notched impact energy; Charpy notched impact under ISO 179-1/1eA may be specified at 23°C and −30°C to separate toughened from unmodified PCR material. The primary differentiation is therefore not a single physical property but the combination of post-consumer content, narrower thermal stability, and a requirement for incoming lot testing. Table 2 summarizes the directional differences without substituting for the T2NV8090 datasheet.

    Attribute T2NV8090 PCR PBT Virgin unfilled PBT Glass-filled PBT Impact-modified PBT/PBT blend
    Recycled content Present Absent Absent Absent or variable
    Bending modulus, ISO 178 Low–moderate Moderate High Moderate
    Melt stability, ISO 1133-1:2022 Lot-dependent Tight Tight Moderate
    Notched impact, ISO 179-1/1eA Low–moderate Low Moderate High
    Candidate application field Nonstructural electrical, enclosures General-purpose Brackets, housings Snap-fit covers, connectors
    Qualification basis Supplier datasheet plus internal lot testing Established datasheet Established datasheet Established datasheet
    Top