| HS Code | 122767 |
| Product Name | SABIC VALOX™ PCR PBT T1N830 |
| Material Family | Polybutylene terephthalate (PBT) |
| Recycled Content Type | Post-consumer recycled (PCR) |
| Reinforcement | 30% glass fiber |
| Density G Cm3 | 1.53 |
| Tensile Modulus Mpa | 9500 |
| Tensile Strength At Break Mpa | 120 |
| Elongation At Break Percent | 2.5 |
| Flexural Modulus Mpa | 8500 |
| Flexural Strength Mpa | 180 |
| Notched Izod Impact 23c Kj M2 | 8 |
| Hdt 0 45mpa C | 220 |
| Hdt 1 8mpa C | 200 |
| Melting Point C | 225 |
| Mold Shrinkage Flow Percent | 0.3 |
| Mold Shrinkage Crossflow Percent | 0.9 |
| Water Absorption 24h Percent | 0.05 |
| Ul94 Flame Rating | HB |
| Volume Resistivity Ohm Cm | >1E15 |
| Dielectric Constant 1mhz | 3.5 |
As an accredited SABIC VALOX™ PCR PBT T1N830 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PCR PBT T1N830 is supplied in 25 kg moisture-barrier foil-lined bags, palletized for industrial storage and transport. |
| Container Loading (20′ FCL) | SABIC VALOX™ PCR PBT T1N830 resin is palletized, secured, and loaded into a 20-foot FCL container for export shipment. |
| Shipping | SABIC VALOX™ PCR PBT T1N830 is shipped as dry resin pellets in moisture-resistant bags, boxes, or octabins. Transport in clean, dry, ventilated containers at ambient temperature, protected from moisture, contamination, and direct sunlight. It is generally not classified as dangerous goods; follow the SDS and local regulations. |
| Storage | Store SABIC VALOX™ PCR PBT T1N830 in a cool, dry, well-ventilated area, protected from direct sunlight, heat, moisture, and ignition sources. Keep containers tightly closed and palletized, away from oxidizers, acids, and bases. Avoid dust generation and static buildup. Do not store outdoors or in damp conditions. Follow first-in/first-out rotation and applicable SDS/local regulations. |
| Shelf Life | Shelf life is typically 24 months when stored dry and cool in original unopened packaging, protected from moisture and contamination. |
In thin-wall connector and terminal cavity applications where the UL yellow card for T1N830 governs flame retardance, the resin is processed on all-electric injection moulding machines with screw diameters between 25 mm and 35 mm and L/D ratios of 20 to 25. Pre-drying in a desiccant hopper at 120 °C for 2–4 h to 0.02% moisture is mandatory because ester hydrolysis at melt temperatures above 250 °C reduces molecular weight and causes intermittent connector latch fracture. The melt temperature window is held at 250–270 °C, the mould at 60–90 °C, and holding pressure is adjusted to maintain a screw cushion of 1–2 mm. For multi-cavity hot-runner tools with valve-gated drops, fill-to-pack switch-over by cavity pressure is set at 400–600 bar; this setting is derived from short-shot studies on PBT connector housings rather than a universal machine recommendation. The use of regrind is typically limited to 20 wt% of the same PCR grade, with the feed stream screened to remove ferrous contamination before blending. End products include automotive engine-compartment connectors, terminal position assurance blocks, and modular connector shells where dimensional tolerance across 24-cavity moulds is maintained at ±0.05 mm. Because PCR feedstocks can shift melt viscosity by ±5% between lots, the filling-to-packing transfer on connector housings with 0.4 mm snap arms must be re-tuned after each silo change. Compliance is verified against IEC 60695-2-12 glow-wire ignition at final wall thickness, UL 94 V-0 as applicable to the minimum thickness in the UL yellow card, and ISO 527-2 tensile modulus when PCR content affects weld-line strength.
Engine-compartment relay housings and sensor bodies moulded from T1N830 are sensitive to screw-back pressure because the PCR fraction can carry low-level polyolefin or label residue that lowers melt homogeneity. Screw rotation with back pressures of 5–10 bar and screw surface speeds below 0.3 m/s is used to avoid unmelted flake in thin wall sections. The pre-drying requirement is identical: 120 °C for 3–4 h to 0.02% residual moisture, but for relay housings with metal insert moulding, the insert preheat temperature is set to 110–130 °C to reduce differential shrinkage at the PBT-to-brass interface. Mould temperature is biased toward the upper limit of 80–90 °C to force PBT crystallization, because post-mould crystallinity below 35% can cause creep in snap-fit relay covers. The finished components are checked for dimensions after 24 h at 23 °C and 50% RH, as moisture uptake at the surface can swell PBT by 0.1–0.2%. In engine compartment testing, relay housings are subjected to thermal cycling from −40 °C to 150 °C according to automaker specifications, often referencing ISO 16750-4. The resin’s dry-as-moulded tensile strength is sufficient for ultrasonic welding of cover and base, but welding amplitude must be kept below 10 µm at 20 kHz to avoid melt ejection from the energy director. Assembled products include automotive relay boxes, glow plug sensor housings, and pressure sensor bodies in which over-moulded pins require PBT to achieve leakage-free encapsulation.
When T1N830 replaces virgin PBT in appliance control enclosures and small appliance bases, the moulding facility must re-certify glow-wire performance because PCR-derived pigments and residual label inks can alter the carbon black distribution that otherwise stabilizes tracking resistance. The formulation is a single-resin system without glass fibre, but a PBT-based masterbatch is used at 2–4 wt% for dark colours; higher masterbatch loadings can depress impact strength and reduce melt flow length. Pre-drying is conducted at 110–120 °C for 2–4 h in a desiccant dryer with a dew point of −40 °C or lower. Melt temperatures of 255–265 °C are paired with a cold-runner screw with a compression ratio of 2.5:1 to preserve PCR melt stability over residence times not exceeding 5 min. Amine-containing purging compounds are avoided because they accelerate ester cleavage at processing temperatures and create surface streaks. Cavity filling is sequenced through two-stage injection: the first stage fills 95% of the cavity at moderate velocity, and the second stage packs the part at lower pressure to prevent valley lines around bosses. Parts are ejected only after the mould is cooled to 70 °C or below; early ejection from a hotter mould can produce post-mould warpage in base plates with wall thickness transitions from 1.2 mm to 2.5 mm. End products include washing machine control panels, steam iron shells, and small kitchen appliance bases where the final part must satisfy IEC 60335-1 glow-wire testing at 750 °C or higher depending on the end-product standard. Dimensional inspection is anchored to ISO 294-4 for shrinkage and ISO 178 for flexural modulus, which for unfilled PBT is typically near 2 500 MPa but must be verified on the actual PCR lot.
Terminal blocks for DIN-rail control cabinets made from T1N830 demand tracking resistance and flame retardance at visible surfaces. The PCR feed stream introduces variability in residual metal and paper fibre; therefore, a magnetic separator and 60 µm screen pack are installed in the material conveying line before the dryer. Processing uses a melt temperature of 260–270 °C and a mould temperature of 70–80 °C, with injection speeds deliberately reduced to 50–70 mm/s along the main runner to prevent jetting in cavities with metal screw-clamp inserts. Holding pressure is set between 300 bar and 500 bar based on gate-seal time determined by weight stabilization; early gate freeze leads to sink marks at the terminal recesses. The mould is a two-plate cold-runner design with tunnel gates, because hot-runner valve pins are more difficult to purge when PCR particles accumulate in the pin bushing. Finished terminal blocks, feed-through connectors, and fuse terminal bases are tested for comparative tracking index under IEC 60112; unfilled PBT typically meets CTI 400 V but the specific PCR lot should be re-qualified. Glow-wire ignitability is assessed at the final wall thickness under IEC 60695-2-12, and flammability is confirmed under UL 94 at the minimum rated thickness. A compliance matrix for low-voltage terminal block use is presented below.
| Standard / test method | Property evaluated | Condition | Typical acceptance for unfilled PCR PBT |
|---|---|---|---|
| UL 94 | flammability | minimum Yellow Card thickness | V-0 at that thickness |
| IEC 60695-2-12 | glow-wire ignitability | 750 °C, 2 s | no ignition |
| IEC 60112 | tracking resistance | solution A, 600 V max | CTI 400 V typical |
| IEC 60947-1 | terminal block creepage | pollution degree 3 | no tracking failure |
| ISO 178 | flexural modulus | 23 °C, 2 mm/min | 2 500 MPa typical |
In LED light engine housings and driver enclosures where T1N830 sits adjacent to aluminium heat sinks operating near 90–110 °C, long-term ageing must be separated from short-term heat deflection. The material’s short-term performance is measured by ISO 75-2 HDT at 0.45 MPa, which for unfilled PBT is typically in the range of 150–165 °C, but this value does not predict oxidative embrittlement over 50 000 h. Instead, the part designer uses the UL 746B relative thermal index for the specific PCR grade and colour; published data for this specific PCR configuration may be limited, so prior qualification on virgin PBT is not directly transferable. Processing for light engine parts requires a nitrogen-purged hopper if ambient RH exceeds 60%, and melt residence time is capped at 4 min at 265 °C because the PCR fraction can contain trace metals that catalyse thermo-oxidative degradation. Mould temperature is set to 90 °C to maximize crystallinity and reduce post-cracking around screw bosses. Ejection is delayed until parts cool below 80 °C; thin-wall lenses are not moulded from this grade, only the housing, driver tray, and reflector base. The finished components undergo IEC 62471 photobiological safety evaluation only as part of the assembled luminaire, not at resin level. UV exposure at the housing surface is often evaluated via ISO 4892-2 with xenon-arc weathering for 500 h; chalking or colour shift beyond ΔE 5 may require an opaque cover design. The use of T1N830 in this application is limited to non-optical structural parts, and direct contact with silicone-based thermal greases should be validated because low-viscosity silicones can migrate into PBT and alter surface resistivity.
Directly in circuit-protection base plates and miniature circuit breaker housings, T1N830 is evaluated for arc ignition resistance rather than simple flame spread. The moulded part must maintain flatness over a 100 mm length with a total indicated runout below 0.1 mm, because warped bases prevent secure assembly of moving contacts. The tool is typically a 2+2 stack-turning mould with cold-runner sub-gates, and the resin is dried to 0.015% moisture or less using a desiccant dryer at 120 °C for 4 h. Barrel temperature profile is ascending from 240 °C at the feed throat to 265 °C at the nozzle; decompression after screw retract is set to 2–4 mm to prevent drool from the open nozzle. Injection velocity is profiled with an initial rapid fill of 80–100 mm/s into the main runner and a slower 20–30 mm/s traverse across the arc chamber wall, which reduces shear heating in the thin section. PCR-derived particles larger than 40 µm must be screened out because they tend to concentrate at the gate land and can create surface voids visible after silver plating. The arc chamber region is assessed for glow-wire ignition at 960 °C under IEC 60695-2-12 only if the end-product specification requires unattended appliance protection; otherwise 750 °C ratings apply. Unreinforced T1N830 is not normally specified for the 960 °C glow-wire category; it is more commonly used for 750 °C end-product categories. Electrical endurance tests are performed under IEC 60898-1 for miniature circuit breakers and IEC 60947-2 for moulded-case switches, with the PBT base plate acting as insulation between live parts.
Small DC motor brush card holders and coil formers moulded from T1N830 use the resin’s high flow to fill long, thin flow paths around brass inserts, but surface defects are controlled by selecting a mould temperature at the lower limit of 60–70 °C. Lower mould temperature reduces crystallization rate at the wall, allowing the material to pack rib features before freeze-off; however, it also reduces dimensional stability if parts are ejected too early. Ejector pins are placed on flat surfaces only, because PCR grades with slightly higher gel content can tear at rib root locations if the part is short-shot during ejection. Mould release is provided by stearate-based external release agents sprayed at intervals of 50–100 shots for initial trials, but production runs use a self-releasing PBT formulation with no external release. The resin is processed at 250–260 °C with screw back pressure of 3–7 bar; higher back pressure raises melt temperature and promotes hydrolysis, leading to a drop in melt viscosity that appears as short shots in the brush holder’s 0.5 mm snap features. Incoming lot MFR is checked via ISO 1133-1 at 250 °C and 2.16 kg; a shift greater than ±10% triggers barrel temperature compensation. Finished parts are tested for dielectric strength under IEC 60243-1 at 2 kV across terminal separation, and for insulation resistance under IEC 62631-3-1 after 48 h conditioning at 85 °C and 85% RH. The end product is a motor brush card that positions carbon brushes within a commutator assembly; dimensional accuracy of the brush slot is inspected at ±0.03 mm using a vision measurement system after annealing at 120 °C for 2 h to stabilize PCR-induced post-mould shrinkage.
Competitive SABIC VALOX™ PCR PBT T1N830 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
In the polybutylene terephthalate (PBT) portfolio, the injection-molding material SABIC VALOX™ PCR PBT T1N830 is a post-consumer recycled grade whose alphanumeric designation is the purchase-order identifier for raw-material qualification. The product is specified where a semicrystalline engineering resin with a fast crystallization rate and a documented recycled-content position is required. The designation alone does not disclose filler content, melt volume-flow rate, or recycled mass fraction; those values are fixed in the SABIC material letter, batch certificate, and UL card. Because the PCR stream can introduce ester-based contamination and viscosity drift, incoming lots are evaluated under ISO 1133-1:2022 and residual moisture testing. The following sections address processing constraints, application conditions, and the grade’s technical position relative to virgin and reinforced VALOX PBT counterparts.
Residual moisture in PBT is a processing hazard above 0.02 wt% because hydrolytic chain scission accelerates at melt temperatures in the 240–270 °C band. Unfilled VALOX PBT processing guides direct dehumidified drying with a dew point no higher than −30 °C and inlet air temperature between 110 °C and 120 °C for 3–4 h. For T1N830, recycled feedstock may carry higher surface moisture or volatile residues; the dryer residence time should be verified by hopper-level calibration and return-air temperature monitoring. A closed-loop loader with an insulated hopper is required. Wet pellets produce surface silver streaks, lower extrusion pressure, and elevated tetrahydrofuran odor at the mold split line. The moisture limit is not a recommendation; it is the boundary between stable screw plastication and degradation-driven viscosity loss.
High-volume connector and sensor-body molding on an all-electric injection machine with a general-purpose screw of 18:1 to 22:1 L/D generally uses a barrel profile starting at 240 °C and ending no higher than 270 °C. The nozzle is set between 250 °C and 265 °C unless hot-runner thermal loads require a narrower band. Mold temperature is held at 60–93 °C to allow sufficient crystallization before ejection. Below 60 °C, thin-wall parts may develop a quenched skin with lower modulus and higher shrinkage anisotropy; above 93 °C, ejection can become difficult and cooling time increases. T1N830-specific melt and mold settings are to be derived from the supplier’s processing datasheet. Published data for this specific configuration is limited; therefore these values are general unfilled PBT practice and are not a substitute for a validation run.
When a valve-gate hot-runner is used, the melt encounters a second thermal residence unit beyond the barrel. For a recycled PBT grade such as T1N830, the hot-runner manifold should be balanced to within ±5 °C of the nozzle setpoint to avoid low-viscosity channels that preferentially fill and starve other cavities. At temperatures above 270 °C, PBT degradation produces tetrahydrofuran, carboxylic acid end groups, and colored low-molecular-weight species. Extended residence in a hot runner can reduce melt pressure loss while simultaneously lowering tensile elongation at break. A gate-bubble or blush defect, especially during recycled lot startup, is not automatically a moisture problem; it may indicate local overheating in the hot gate or a dead zone in the manifold. Mold-fill analysis should include residence-time mapping, not just pressure-drop mapping.
In thin-wall applications, screw speed and injection velocity act as secondary melt heaters. For unfilled PBT, shear heating can raise the melt front temperature by 10–15 °C at high injection velocities. Screw speed is typically limited to 100–200 rpm and back pressure to 0.3–0.7 MPa to avoid excessive frictional heat in the plastication zone. For PCR T1N830, lot-dependent viscosity shifts require short-shot purge evaluations after each batch change. A short shot should not show jetting or frothy vent flow; if it does, the melt temperature is over the safe band for the material.
Mechanical release values should be obtained on dry-as-molded specimens because moisture conditioning changes tensile yield and flexural modulus. The standard framework uses ISO 527-1 and ISO 527-2 for tensile properties, ISO 178 for flexural properties, ISO 180 or ASTM D256 for notched Izod impact, and ISO 294-4 for mold shrinkage. Datasheet values for T1N830 are not reproduced here because the grade-specific datasheet and UL card are the controlled technical documents. If a datasheet figure is not available, data from unfilled PBT counterparts cannot be substituted directly for structural calculations; an incoming-lot verification must be performed at the application temperature and wall thickness.
Electrical connector programs select PBT when cyclic humidity exposure must be tolerated with lower moisture uptake than polyamide 66. Typical PBT equilibrium moisture uptake under 23 °C and 50% RH is below 0.2 wt%, whereas PA66 under the same conditions takes up approximately 2.5 wt%. The material is nevertheless notch-sensitive, and cold-impact testing is required if the connector is handled or installed below −20 °C. T1N830 may be evaluated for connectors if the recycled-content lot passes high-humidity preconditioning, thermal cycling, and post-test continuity checks. The choice between T1N830 and a virgin VALOX grade is often made after measuring connector wall thickness and gate area; if the PCR lot shows wider melt volume-flow rate variation, the cavity-fill balance of a multi-cavity tool may shift enough to alter critical contact pin retention.
For environmental reporting and regulatory review, the PCR-content claim must be supported by chain-of-custody documentation. The table lists the standards and directives that are applied to the material in electrical, electronic, and industrial applications.
| Standard / Directive | Clause or Designation | Application to T1N830 |
|---|---|---|
| ISO 1133-1:2022 | Determination of melt volume-flow rate | Used to verify incoming lot MVR consistency before molding; T1N830-specific test temperature and load must be read from the grade datasheet. |
| ISO 527-1 / ISO 527-2 | Tensile properties | Used to measure yield stress and elongation at break on dry-as-molded specimens; values are not comparable after moisture exposure. |
| ISO 178 | Flexural properties | Used for flexural modulus measurement; specimen conditioning must match datasheet conditions. |
| ISO 180 / ASTM D256 | Notched Izod impact | Used for impact comparison; PBT is notch-sensitive and low-temperature impact should be verified at application temperature. |
| UL 94 | Flammability class | The applicable class and thickness are grade- and color-specific; a UL card for T1N830 should be confirmed. |
| RoHS Directive 2011/65/EU | Annex II restricted substances | Needed for electrical/electronic component compliance; only the supplier certificate confirms lot-specific status. |
| REACH Regulation (EC) No 1907/2006 | Candidate List SVHC | Needed to verify that recycled feedstock does not introduce candidate substances above reporting limits. |
| ISO 14021:2016 | Environmental labels and declarations | Applies to PCR-content claims and requires chain-of-custody data. |
Compared with a petrochemical-only general-purpose VALOX PBT, T1N830’s main difference is the recycled feedstock origin and the associated lot-to-lot viscosity control. Virgin PBT typically has a narrow intrinsic-viscosity distribution; post-consumer PBT may contain trace polycarbonate, PET, or additive residues that alter nucleation, crystallization temperature, and melt viscosity. Against glass-filled VALOX grades, the unfilled or low-modulus position of T1N830 means it is not suitable for load-bearing brackets where glass-reinforced flexural modulus measured under ISO 178 and heat-deflection temperature measured under ISO 75-2 are required; mold shrinkage is also higher and more anisotropic without glass. Against flame-retarded PBT grades, T1N830’s UL 94 classification, comparative tracking index under IEC 60112, and colorability must be confirmed on the recycled lot because halogen-free or brominated additive packages are grade-specific. The production-scale decision cannot be made from the family name alone; it requires a side-by-side validation of the actual T1N830 batch against the incumbent material.
For elevated-temperature service, the heat-deflection temperature of unfilled PBT typically falls below 80 °C under 1.8 MPa using ISO 75-2/A, whereas continuous-use temperature is determined by aging rather than short-term heat deflection. Flame-retardant-enhanced grades are required where glow-wire ignition temperature under IEC 60695-2-11 exceeds the unfilled polymer’s capability. Published data for T1N830 elevated-temperature performance is limited; electrical insulation applicators should request the UL Yellow Card and not rely on PBT family values.
Flow-length data obtained on a spiral tool is a relative, geometry-dependent output that cannot substitute for mold-fill validation on the production tool. For a recycled PBT lot, short-shot trials are more informative than a datasheet melt volume-flow rate because they capture gate freeze, hot-runner pressure drop, and cavity thickness effects simultaneously. Published data for this specific configuration is limited; a validation run should include cavity-pressure sensors at both the gate and end-of-fill.
Operational boundaries include minimized hopper exposure above 60% RH, no drying above 130 °C to avoid pellet sticking and oxidative discoloration, and no contact with strong alkaline mold-release agents that accelerate surface hydrolysis. When conveying dried T1N830 over long distances, dried-air or vacuum conveying should be used rather than ambient air at high humidity. Recycled feedstock can contain trace metals from labels and sorting; a magnet and fine mesh filtration should be designed into compounding or regrind return loops. The use of regrind from sprues and runners is generally possible for unfilled PBT, but the ratio must be controlled by melt-flow verification under ISO 1133-1:2022. Published data for the effect of PCR content on high-temperature electrical properties is limited; therefore comparative tracking index under IEC 60112 and dielectric strength under IEC 60243-1 should be tested at the maximum service temperature rather than extrapolated from virgin PBT databases.