Sabic Valox Pbt Gf30 Medical Hx420hp

SABIC VALOX™ PBT+GF30%-Medical HX420HP

    • Product Name: SABIC VALOX™ PBT+GF30%-Medical HX420HP
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 165770
    Grade Name SABIC VALOX™ PBT+GF30%-Medical HX420HP
    Material Type Polybutylene terephthalate (PBT)
    Melt Volume Rate Cm3 10min 10–20 (250 °C/2.16 kg, typical)
    Tensile Modulus Mpa 9000–10000
    Tensile Strength At Break Mpa 110–130
    Elongation At Break Percent 2–3
    Flexural Modulus Mpa 8500–9500
    Notched Izod Impact 23c J M 70–90
    Heat Deflection Temperature 1 8mpa C 190–200
    Vicat Softening Temperature C 205–215
    Mold Shrinkage Flow Percent 0.2–0.5
    Water Absorption 24h Percent 0.06–0.08
    Processing Method Injection molding

    As an accredited SABIC VALOX™ PBT+GF30%-Medical HX420HP factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ PBT+GF30%-Medical HX420HP is packaged in 25 kg moisture-barrier bags on pallets with lot traceability.
    Container Loading (20′ FCL) 20′ FCL container loaded with SABIC VALOX™ PBT+GF30%-Medical HX420HP in original sealed packaging, palletized and secured for safe ocean transport.
    Shipping SABIC VALOX™ PBT+GF30%-Medical HX420HP is typically shipped as non-hazardous polymer pellets in sealed moisture-barrier bags or containers. Keep dry, clean, and protected from direct sunlight, extreme temperatures, and contamination. Use standard ambient transport; follow the SDS and applicable local regulations.
    Storage Store SABIC VALOX™ PBT+GF30%-Medical HX420HP in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, moisture, and incompatible materials. Keep in original sealed packaging until use to prevent contamination and moisture pickup. Use first-in, first-out stock rotation. Follow local regulations and the safety data sheet for additional handling and storage requirements.
    Shelf Life Shelf life is typically 24 months from date of manufacture when stored in original sealed packaging under dry, ambient conditions.
    Application of SABIC VALOX™ PBT+GF30%-Medical HX420HP

    Automatic injector mechanisms and pen injector dose-setting systems that use SABIC VALOX™ PBT+GF30%-Medical HX420HP in load-bearing internal frames require particulates, extractables, and leachables control appropriate for transient skin contact or indirect patient contact. The compound is processed as supplied; downstream formulation changes are limited to 0.2–0.5 wt% color masterbatch and, where validated by the device master record, 20 wt% maximum regrind of the same HX420HP lot stream. Injection molding on all-electric machines with a screw L/D ratio of 20:1–22:1 and a shut-off nozzle is conducted at melt temperatures of 250–270°C, mold temperatures of 80–100°C, and injection speeds of 80–150 mm/s to orient glass fibers along high-stress ribs and snap-fit levers. Pre-drying at 120°C for 3–4 h to a moisture content below 0.02% is mandatory because residual moisture above this threshold hydrolyzes ester linkages during plastication, causing melt flow rate shifts and gate-area embrittlement. Terminal components include autoinjector chassis frames, trigger buttons, dose dial rings, and cartridge retention ribs that are verified under design-specific actuation forces in the range 25–100 N after ethylene oxide sterilization cycles. Compliance is anchored to ISO 10993-5:2009 for cytotoxicity, USP <88> Class VI for biological reactivity, FDA 21 CFR 177.1660 for poly(tetramethylene terephthalate) resin requirements, and ISO 10993-17:2023 for toxicological risk assessment when device contact duration exceeds transient classification.

    Surgical reload frames where glass-fiber orientation controls staple alignment

    In surgical stapler reload housings and laparoscopic device frames, HX420HP is selected for flexural modulus in the range 8,500–9,500 MPa measured per ISO 178:2019, dimensional stability under autoclave or low-temperature hydrogen peroxide gas plasma sterilization, and resistance to enzymatic cleaning solutions. The upstream 30% glass-fiber content is fixed; downstream addition is limited to 0.05–0.2 wt% external mold release or 0.5–1.0 wt% polytetrafluoroethylene masterbatch only in validated low-friction cartridge follower applications, because higher solid loadings reduce weld-line strength below design limits. Molding uses a sequential valve-gated hot-runner tool with two to four gates; melt temperature is maintained at 255–270°C and mold surface temperature at 90–110°C to delay PBT crystallization and allow fiber orientation into thin ribs and staple pocket walls. The processing window is deliberately narrow: if melt residence time exceeds 5 min at 270°C, thermal degradation reduces relative viscosity and shifts the part-weight failure mode from short shot to flash at the parting line; if mold temperature drops below 85°C, weld-line stiffness in the cartridge retention features can fall by more than 15% compared with 100°C processing, a difference measurable with ISO 178:2019 flexural tests on excised weld-line specimens. Terminal finished parts include reload cartridge outer housings, anvil support frames, firing trigger levers, and laparoscopic jaw frames that are subjected to 100–200 repeated sterilization cycles. Compliance relies on ISO 10993-1:2018 biological evaluation planning, ISO 10993-10:2010 skin sensitization testing, USP <88> Class VI, and cleaning-agent resistance screening per ASTM D543-20 against sodium hypochlorite, ortho-phthalaldehyde, and peracetic acid at clinically relevant concentrations; lot-to-lot tensile testing under ISO 527-1:2019 and ISO 527-2:2012 is maintained in the device technical file.

    Control pointStandard / designationApplication boundary
    Biological evaluation endpointISO 10993-1:2018Surface-contacting device with repeated exposure
    CytotoxicityISO 10993-5:2009L929 fibroblast extract method
    Skin sensitizationISO 10993-10:2010Clinically relevant extract vehicle
    Biological reactivityUSP <88> Class VISystemic injection, intracutaneous, implantation
    Chemical compatibilityASTM D543-20Mass and visual change after 24 h at 23±2°C
    Flexural modulus after moldingISO 178:2019Lot-control range per device master file

    What Limits Hydrolytic Stability in Reusable Nebulizer Compressor Housings?

    Reusable compressor-type nebulizer systems use HX420HP for upper housings, filter caps, and nebulizer reservoir retainers because these parts experience intermittent contact with water, pharmaceutical solutions, and cleaning agents at 35–50°C but are not intended as primary drug-contacting surfaces. The as-delivered compound is molded without further filler addition; downstream color masterbatch is held at 0.3–0.5 wt%, and carbon black masterbatch at 0.1–0.3 wt% is permitted only for non-clear parts where laser marking contrast is required. Production uses injection molding machines sized so that shot weight consumes 40–70% of barrel capacity; melt temperature is 240–260°C and mold temperature is 70–90°C to reduce cycle time while maintaining acceptable crystallinity. Pre-drying is enforced at 120°C until Karl Fischer moisture measurement confirms less than 0.02% water; wet-resin barrel temperatures above 260°C accelerate autocatalytic chain scission, which is a known limitation for PBT in steam and high-humidity service. Field observations on production lines indicate that gate blush and silver streaks appear in parts molded from resin dried for less than 2 h at 110°C; such parts are typically rejected for visible housing surfaces. Terminal finished parts include compressor top housings, filter covers, medication cup holders, and carrying-handle mounts for respiratory therapy devices. Compliance is referenced to ISO 10993-5:2009 and USP <88> Class VI for skin-contact components, IEC 60601-1:2005+A1:2012 for electrical medical equipment safety, and cleaning-agent compatibility testing per ASTM D543-20 for detergent and disinfectant exposure; steam autoclave performance should be verified under ISO 17665-1:2006, because hydrolytic retention at 121°C is more severe than low-temperature chemical sterilization. Alkaline or amine-based sterilants are not recommended for repeated high-temperature exposure because nucleophilic attack on ester bonds accelerates molar-mass reduction; if such disinfectants are required, tensile retention after 100 wipe cycles must be measured per ISO 527-1:2019.

    On benchtop clinical chemistry and immunoassay analyzer platforms, SABIC VALOX™ HX420HP is used for sample carousel gears, reagent bottle carriers, and cartridge docking plates where dimensional tolerance across 10–40°C laboratory ambient and exposure to dilute acids, surfactants, and lipid residues must not shift pitch diameters or backpressure in aspirate/dispense manifolds. The upstream 30% glass-fiber content is not modified; downstream formulation is constrained to 0.05–0.1 wt% of a non-silicone mold release masterbatch and, where black parts are specified, 0.2–0.4 wt% carbon black masterbatch, because higher siliconized release levels can transfer to sealing faces and alter fluidic seal contact angles. Molding is performed with a two-plate hot-runner tool, injection speed 100–150 mm/s, packing pressure 60–80 MPa, and mold temperature 80–100°C; gate locations are placed at the centroid of thick bosses rather than at flow edges to prevent jetting and knit lines across the manifold plane. In process development, differential shrinkage between 0.4–0.6% in the flow direction and 0.8–1.0% in the transverse direction must be compensated by iterative mold steel adjustments, because a mismatch greater than 0.05 mm across a 150 mm cartridge interface can cause incomplete reagent cartridge seating and sample aspiration faults. Terminal finished products include sample carousels, reagent rotor plates, wash-head brackets, and optical cuvette carrier frames. Compliance is verified by ISO 10993-5:2009 for cytotoxicity when the part is patient-indirect, ISO 13485:2016 clause 7.5.2 for validated production processes, FDA 21 CFR 177.1660, and dimensional inspection via ISO 1101:2017 geometric product specification where datum targets are defined on sealing surfaces.

    When patient monitor enclosures must meet IEC 60601-1 flammability and cleaning-agent resistance

    Medical electrical equipment housings, including patient monitor rear shells and portable ultrasound cart chassis panels, can be molded from HX420HP when the design requires higher stiffness than unfilled PBT or polycarbonate/ABS blends and when repeated cleaning with quaternary ammonium disinfectants is specified by the hospital infection-control protocol. The flexural modulus of the 30% glass-fiber-reinforced grade is on the order of 8,500–9,500 MPa; unfilled PBT typically falls near 2,500–3,000 MPa, and general-purpose PC/ABS falls near 2,300–2,600 MPa, so the grade permits thinner wall sections and lower mass in structural enclosures if moldability constraints are met. Downstream formulation addition is limited to 0.3–0.5 wt% color masterbatch; where electrostatic discharge control is required, 0.5–1.0 wt% conductive carbon masterbatch may be considered but must be balanced against impact toughness because excess carbon black reduces notched Izod impact values under ASTM D256-10 by 10–20% compared with natural glass-filled PBT. Injection molding of large-area housing parts uses a hot-runner tool with sequential valve gating and clamp force calculated at roughly 0.4–0.6 tonnes/cm² of projected area; melt temperature is 245–265°C, mold temperature is 70–90°C, and fill time is kept below 2 s for thin-wall sections of 1.5–2.2 mm to avoid premature solidification before fiber orientation is established. Weld lines at ventilation slots and cable-management openings are a known failure site: if the melt-front temperature falls below 245°C at the converging fronts, flexural strength at that location may fall below 60% of the nominal value measured on an ISO 178:2019 flexural specimen. Terminal finished components include patient monitor rear enclosures, tilt/swivel stands, battery compartment frames, and ultrasound cart structural panels. Compliance is anchored to UL 94 V-0 at the specified wall thickness as certified by the resin supplier’s UL Yellow Card, IEC 60601-1:2005+A1:2012 clause 11.3 for enclosure mechanical strength and heat resistance, ISO 10993-5:2009 for accessible skin-contact surfaces, and ASTM D543-20 for disinfectant compatibility using wipes based on 0.5% hydrogen peroxide or 70% isopropyl alcohol; flame-retardant additive selection must not introduce substances restricted under EU 2011/65/EU RoHS Annex II.

    Free Quote

    Competitive SABIC VALOX™ PBT+GF30%-Medical HX420HP prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ PBT+GF30%-Medical HX420HP is a 30% glass-fibre reinforced polybutylene terephthalate injection-moulding resin supplied under SABIC’s Healthcare product policy. The grade combines a semicrystalline PBT ester matrix with a nominal 30% by mass chopped-glass-fibre reinforcement, increasing tensile strength, flexural modulus, and heat deflection temperature compared with unfilled medical PBT formulations. The material is specified for precision injection-moulded components in medical and diagnostic devices where structural rigidity, dimensional stability, chemical resistance, and intermittent elevated-temperature exposure are required. The HX420HP designation places the product within the VALOX 420 engineering thermoplastic family while adding healthcare-specific change management, document control, and biocompatibility-related documentation support.

    The polyester backbone of PBT is produced from terephthalic acid or dimethyl terephthalate and 1,4-butanediol. In the melt state, ester linkages are vulnerable to hydrolysis, and the presence of 30% glass fibre raises melt viscosity and shear heating but does not confer resistance to water-induced chain scission. The grade therefore requires closed-loop drying and careful residence-time control in injection moulding. Moisture levels above approximately 0.02% before plastication can reduce molecular weight, lower tensile elongation, and produce brittle failure in load-bearing sections, even when the moulded surfaces appear acceptable.

    Application areas for this grade include structural frames and housings for diagnostic instrumentation, internal chassis components for respiratory devices, surgical handpiece bodies, pump and fluid-handling support structures, and other metal-replacement components where repeated exposure to cleaning agents, dimensional stability, and creep resistance are required. The glass-fibre content makes the grade suitable for enclosures that must maintain tolerances under mechanical load, but impact-loaded components such as snaps and clips should be analysed at the weld-line region.

    What Limits the Processing Window for 30% Glass-Fibre Medical PBT?

    Melt temperature at the nozzle is typically held between 250 °C and 270 °C. Below this range, the high glass-fibre content increases melt viscosity and can produce short shots or poor fibre wet-out; above 270 °C, thermal degradation of the PBT matrix accelerates and the risk of surface splay, yellowing, and loss of impact strength increases. Mould temperature is commonly set from 60 °C to 90 °C. The lower boundary supports faster cycle times but may produce underdeveloped crystallinity and lower dimensional stability, while the upper boundary improves crystallinity and surface finish at the cost of longer cooling time and higher total energy input.

    Pre-drying is performed in a desiccant dryer with a dew point at or below -30 °C. A drying temperature of 120 °C to 130 °C for 4 h is typical for material that has been exposed to ambient conditions. Open containers and hopper transfer lines must be sealed or continuously purged with dry air, because regrind and virgin granules can reabsorb moisture quickly in environments above 60% relative humidity. If the resin is received in sealed bags, drying can sometimes be omitted; if bags are punctured or stored in humid conditions above 60% relative humidity, pre-drying becomes mandatory. A hopper dryer without desiccant cannot reliably reduce moisture below the threshold of 0.02% in many high-humidity facilities. Dew-point monitoring at the hopper inlet, not just at the dryer outlet, is recommended because distribution lines can leak ambient air.

    Injection moulding machines used for glass-fibre reinforced PBT require wear-resistant barrel, screw, and check-ring surfaces. The chopped glass fibres increase abrasion, and unhardened screws can show measurable wear in continuous production. A general-purpose screw with an L/D ratio between 18:1 and 24:1 and a compression ratio near 2.5:1 is used for melt homogeneity; back pressure is kept moderate, typically 0.3 MPa to 0.7 MPa, to avoid excessive glass-fibre breakage. High back pressure reduces fibre length and lowers final tensile strength, while insufficient back pressure can produce non-uniform fibre distribution and inconsistent shrinkage.

    Residence time in the barrel is a critical threshold variable. At barrel temperatures above 260 °C, cumulative residence times beyond 8–10 min can degrade the polyester matrix and produce black specks, splay, and impact loss. During production interruptions, the barrel temperature should be reduced or the screw rotated in purge mode. Regrind from glass-filled PBT lowers fibre length and should be limited to 20% or less in critical medical applications unless process capability studies demonstrate acceptable mechanical performance. Glass fibres shorten during each melting cycle, so regrind use increases the variability of tensile strength and impact toughness.

    Moisture content is not linearly related to property loss. Below 0.02%, hydrolysis is minimal; between 0.02% and 0.05%, molecular weight decreases progressively; above 0.05%, surface defects and brittle fracture can occur abruptly. This threshold behaviour explains why visual inspection of pellets is insufficient and why moisture analysis by Karl Fischer titration or an equivalent calibrated method is specified at incoming inspection.

    Mould filling is affected by the anisotropic flow of glass fibres. The fibre orientation follows the flow front, producing higher tensile properties along the flow direction and lower properties transverse to flow. Shrinkage is similarly anisotropic: longitudinal flow shrinkage is commonly in the range of 0.3% to 0.5%, while transverse shrinkage is higher and can reach 0.6% to 1.0% depending on gate geometry and wall thickness. Weld lines formed downstream of holes or multi-gate layouts contain disrupted fibre orientation and are typically the weakest locations in a moulded part. Tool designs that reposition weld lines away from loaded ribs or snap-fit features are preferred over raising melt temperature or injection speed alone.

    Mechanical and Thermomechanical Response Under Tensile and Flexural Loading

    The table below summarizes representative values reported for 30% glass-fibre reinforced PBT medical grades of the VALOX family. These values are not a substitute for the active certificate of analysis and should be verified for each lot, particularly where device dimensions are linked to creep or fatigue behaviour.

    PropertyTest standardTypical range
    DensityISO 11831.53–1.56 g/cm³
    Tensile stress at breakISO 527-2105–120 MPa
    Tensile elongation at breakISO 527-22–3%
    Flexural strengthISO 178160–190 MPa
    Flexural modulusISO 1786,000–7,600 MPa
    Notched Izod impact at 23 °CISO 180/1A8–10 kJ/m²
    Heat deflection temperature at 1.82 MPaISO 75-2/A200–215 °C
    Melt mass-flow rate at 250 °C and 2.16 kgISO 11338–15 g/10 min

    Compared with unfilled PBT, the 30% glass-fibre network raises tensile stress at break from approximately 55 MPa to more than 105 MPa, while flexural modulus increases by approximately a factor of three. The same reinforcement reduces elongation at break from above 30% to the 2–3% range, so the material is selected for structural rigidity rather than for snap-fit deflection or high-strain energy absorption. The combination of high modulus and relatively low notched impact means that sharp corners, internal gate vestiges, and abrupt wall-thickness transitions act as failure initiation sites under drop or impact loading.

    Creep resistance of glass-reinforced PBT is superior to unfilled PBT, but the creep modulus remains temperature-dependent and load-level dependent. Applications that carry continuous load above 80 °C should be evaluated under ISO 899-1 because the matrix begins to soften as the glass transition temperature of PBT, typically 45 °C to 60 °C, is exceeded. The glass fibre continues to carry load above the glass transition, but creep deflection increases and dimensional recovery may be incomplete after sustained loading.

    Chemical Resistance, Sterilization, and Hydrolytic Boundaries

    PBT offers resistance to dilute acids, aliphatic hydrocarbons, alcohols, glycols, and many halogen-free cleaning agents at room temperature. Strong bases, strong oxidizing acids, phenols, cresols, and certain chlorinated solvents can attack the polyester matrix and must be excluded. Environmental stress-cracking evaluations are typically performed under ISO 22088 or ASTM D543 when the device is exposed to disinfectants, lipids, or cleaning agents.

    Gamma sterilization at dose levels from 25 kGy to 50 kGy may produce colour shift and measurable reductions in tensile elongation because of chain scission in the PBT matrix. If gamma processing is required, the effect on mechanical performance must be evaluated on finished devices under ISO 11137. Ethylene oxide sterilization is generally less aggressive to PBT; however, residual limits are controlled under ISO 10993-7. Steam autoclave exposure at 121 °C introduces water into the polymer at elevated temperature and accelerates hydrolysis. Published data for repeated steam sterilization of this specific 30% glass-filled medical configuration is limited, and cyclic autoclave use is not recommended for load-bearing components unless extensive application-specific testing demonstrates acceptable molecular weight retention and impact strength after maximum cycle count.

    Biocompatibility Documentation and Supply-Chain Controls

    SABIC healthcare grades are controlled through a formulation lock and a documented change-management process. The supplier may provide regulatory statements that support evaluation of the grade as a component material, but these statements do not replace final device biocompatibility testing under ISO 10993-1.

    Regulatory or handling itemStandard or reference
    Biocompatibility evaluationISO 10993-1, ISO 10993-5, ISO 10993-10
    Ethylene oxide residual controlISO 10993-7
    Radiation sterilization validationISO 11137
    Ethylene oxide sterilization validationISO 11135
    Moist heat sterilization validationISO 17665-1
    Food-contact reference regulationFDA 21 CFR 177.1660, EU 10/2011
    RoHSDirective 2011/65/EU
    REACHRegulation (EC) No 1907/2006

    A production-scale bottleneck associated with this grade is lot-to-lot melt viscosity variation if the glass fibre length distribution shifts during compounding. Twin-screw extrusion with controlled screw speed, feed rate, and side-stuffer glass addition is used to preserve fibre length and dispersion. Incoming lots should be checked for melt mass-flow rate and moisture content, and a moulding trial is warranted when any component is subjected to creep or fatigue because fibre orientation in the tool may differ from the isotropic laboratory specimen.

    When the HX420HP Specification Replaces a Standard Glass-Filled PBT in a Device Program

    Substitution of a standard 30% glass-filled PBT with HX420HP is not solely a material-data change. The healthcare grade provides the same mechanical foundation but adds supplier-controlled change notification, medical-grade documentation, and regulatory support appropriate to device risk management. A change from a standard grade to a healthcare grade may reduce regulatory documentation burden when the base chemistry is similar, but it does not eliminate the need for engineering equivalence assessment. Moulded parts should be re-qualified for critical dimensions because slight changes in moulding viscosity, mould release, or additive package can alter shrinkage and warp.

    Compared with a 20% glass-fibre PBT, the 30% grade gives higher flexural modulus and improved creep resistance but lower flowability and increased anisotropy. Gates and runners sized for 20% glass may need to be enlarged or pressures raised. Compared with an unfilled medical PBT, the reinforced grade provides a step change in stiffness and heat deflection; however, the ductility decrease and weld-line sensitivity require design changes such as thicker ribs with larger radii rather than deeper ribs.

    Compared with amorphous medical resins such as polycarbonate or polycarbonate blends, the PBT matrix offers better resistance to hydrocarbon-based lubricants, alcohols, and many cleaning agents, but it has lower practical impact strength and greater hydrolytic sensitivity. The semicrystalline nature gives lower mould shrinkage and better chemical resistance, yet the 30% glass reinforcement can produce warpage if cooling is non-uniform. In multi-cavity tools, cavity-to-cavity variation in glass orientation may be observed when runner balancing is not maintained.

    Weld-line tensile strength in glass-fibre reinforced PBT is commonly lower than bulk tensile strength because fibre orientation is disrupted at the weld plane; the reduction is design-dependent and must be measured on the actual tool. When a standard glass-filled PBT is converted to HX420HP, the same weld line limitation persists, and the healthcare-grade change does not address the physical weakness.

    Top