| HS Code | 295348 |
| Polymer Type | PBT |
| Reinforcement | 30% glass fiber |
| Flame Retardant | Yes |
| Hydrolytic Stabilization | Yes |
| Density | 1.53 g/cm³ |
| Tensile Modulus | 10000 MPa |
| Tensile Strength At Break | 120 MPa |
| Elongation At Break | 2% |
| Flexural Modulus | 9500 MPa |
| Flexural Strength | 180 MPa |
| Notched Izod Impact At 23c | 60 J/m |
| Charpy Notched Impact At 23c | 6 kJ/m² |
| Hdt At 0 45mpa | 210 °C |
| Hdt At 1 8mpa | 200 °C |
| Ul94 Flammability Rating | V-0 at 0.8 mm |
| Mold Shrinkage | 0.2-0.6% |
| Water Absorption 24h | 0.06% |
| Melting Temperature | 225 °C |
| Thermal Conductivity | 0.24 W/m·K |
| Coefficient Of Linear Thermal Expansion Flow | 2.5E-5 1/°C |
As an accredited SABIC VALOX™ PBT+GF30%-Hydrolytic-FR V4860HR factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ V4860HR PBT+GF30% hydrolytic-FR resin supplied in 25 kg moisture-barrier bags, palletized for industrial shipment. |
| Container Loading (20′ FCL) | 20′ FCL loaded with palletized 25 kg bags of SABIC VALOX™ PBT+GF30%-Hydrolytic-FR V4860HR, shrink-wrapped, secured, and kept dry. |
| Shipping | SABIC VALOX™ PBT+GF30%-Hydrolytic-FR V4860HR ships as a non-hazardous solid in sealed moisture-barrier bags or boxes on pallets. Keep dry and protect from heat, sunlight, and contamination. Handle per SDS; no special transport classification unless local regulations specify otherwise. |
| Storage | Store SABIC VALOX™ V4860HR in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture pickup and contamination. Avoid dust generation. Segregate from strong oxidizers and incompatible chemicals. Use adequate ventilation and follow local regulations and the supplier’s SDS for detailed storage and handling requirements. |
| Shelf Life | Typically 24 months in original sealed packaging, stored dry below 30°C, away from sunlight and moisture; verify with SABIC datasheet. |
In engine-compartment connector housings, VALOX™ PBT+GF30%-Hydrolytic-FR V4860HR is processed on reciprocating-screw injection moulding machines with screw L/D ratios of 20:1 to 22:1 and compression ratios of 2.5:1 to 3.0:1. The granulate is dried in a desiccant dryer at 120 °C for 4 h until residual moisture falls below 0.02% by Karl Fischer titration. Melt temperature is maintained between 250 °C and 270 °C, and barrel residence time above 6 min at the upper limit is avoided because it produces brown streaking and a measurable loss in tensile strength under ISO 527-2. Mould temperature is held at 80 °C to 90 °C to stabilise crystallinity and reduce post-mould shrinkage in latch bosses. Underhood exposure combines glycol-water coolant splash, hot oil mist, road salt aerosol, and peak air temperatures above 125 °C on turbocharged gasoline direct-injection platforms. Verification follows USCAR-2 connector performance requirements, with thermal shock from −40 °C to 150 °C and humidity exposure according to ISO 16750-4. Hydrolytic stabilisation shifts the observed field failure mode from brittle latch fracture toward mechanical wear at the retention interface. Contact retention force after ageing still requires validation on production-tooled parts because glass fibre length distribution after plastication influences anisotropic shrinkage in thin latch walls. A cavity-pressure integral control during hold pressure is used to keep latch bore roundness within 0.03 mm across batch runs. Amine-based mould release agents are excluded from the process because they can accelerate ester exchange and reduce molecular weight in PBT.
In electric vehicle supply equipment built to IEC 62196-1 and IEC 62196-3, the contact carrier separates live DC pins from the handle surface and performs both electrical insulation and mechanical retention. Flame-retardant classification is assessed under UL 94 at the minimum production wall thickness, not solely on a standard plaque. For connector sets rated above 60 V DC, creepage distances are determined according to IEC 60664-1, and the tracking index measured under IEC 60112 determines required spacing between adjacent terminals. VALOX™ V4860HR is dried to below 0.02% moisture before plastication because residual moisture hydrolyses PBT at barrel temperatures above 260 °C, causing surface splay and reduced weld-line strength at the pin roots. The melt is processed at 250 °C to 270 °C with a mould temperature of 80 °C to 90 °C to maintain pin-to-pin dimensional stability. Insert moulding of pre-tinned copper pins creates anisotropic glass fibre orientation around each pin, so mould filling simulation is performed on the production tool geometry before pin location is locked. Regrind content above 10% or concentrated colour masterbatch may lower the tracking index, requiring a screening plaque test under IEC 60112 before lot release. The material provides flame retardancy without shifting the harness assembly process; however, contact retention force after thermal cycling and damp heat is product-dependent and must be verified on moulded assemblies.
In dishwasher circulation pump housings where the pump motor is integrated into the wetted enclosure, the hydrolytic stabilisation package is the primary selection criterion. The material is dried to below 0.02% moisture and moulded at 250 °C to 270 °C. Long-term exposure to 60 °C to 90 °C water containing oxygen-based detergents can attack the glass fibre/matrix interface if moulded-in stress exceeds the critical stress for environmental stress cracking. Gate locations are placed away from impeller hub fillets, and packing pressure is used to prevent sink marks in thick boss sections. Published data for this exact pump housing configuration is limited, so service life estimates require component-level testing in the final plumbing assembly.
At terminal pitch below 2.54 mm, connector walls between adjacent cavities may drop to 0.40 mm or less. In a 30% glass-filled PBT, fibre orientation near the cavity surface creates differential shrinkage between flow and cross-flow directions. Shrinkage is measured according to ISO 294-4; flow-direction values in this filler class commonly fall between 0.25% and 0.50%, while cross-flow values may reach 0.60% to 0.90%, but tool-specific values must be confirmed on production parts. The mould is run at 90 °C to promote uniform crystallite formation and stabilise post-mould dimensions. Pin retention force is validated by pull-out testing after thermal ageing, with acceptance limits defined by the end-use automotive or industrial specification. Weld lines at cavity bottoms are unavoidable in multifinger pin rows. Raising melt temperature to 265 °C to 270 °C with a fast injection speed reduces visible weld-line depth but increases fibre attrition. Running at the lower melt-temperature boundary shortens flow length and raises cavity-pressure demand. The practical processing window therefore narrows to approximately ±5 °C for thin-wall tools with hot runners. Dimensional capability studies are performed on the production machine to separate material shrinkage from tool-temperature variation.
Terminal blocks in assemblies built to IEC 60947-7-1 are tested as complete articles. The insulating housing must resist glow wire ignition under IEC 60695-2-12 and flame spread under IEC 60695-2-13. Many designs specify a glow wire flammability index of 960 °C, but published data for this specific configuration is limited because the test result depends on wall thickness and the thermal mass of the inserted copper or aluminium current bar. Where screw clamps are installed, residual hoop stress can initiate stress cracking in contact with cleaning solvents or humidity. VALOX™ V4860HR is moulded with a hold-pressure profile that fills thick screw bosses without overpacking the thin web between adjacent circuits. Dimensional inspection follows ISO 294-4, and creepage distances are verified against IEC 60664-1. In pollution degree 3 installations, tracking index under IEC 60112 is a critical input for spacing calculations. Regrind addition above 10% or uncontrolled colour masterbatch can shift tracking classification; a plaque test under IEC 60112 is therefore run before production release. The grade should be evaluated with the final terminal assembly because material performance alone does not satisfy end-product glow wire testing.
Photovoltaic DC connector bodies and junction box covers installed behind modules are exposed to ultraviolet radiation, thermal cycling from −40 °C to 90 °C, and condensing humidity. Flame retardancy is required under IEC 61730-1 and UL 373 because DC arcs can initiate polymer combustion. External surfaces are typically pigmented black; unpigmented natural resin is not suitable for long-term ultraviolet exposure. Hydrolytic stabilisation slows chain scission that can cause microcracking and loss of dielectric strength across the wall. Drying to 0.02% moisture and moulding at 80 °C improve the dimensional stability of snap-fit covers over service life. When threaded inserts are installed, low insertion speed is specified to reduce tensile stress around the boss. Published data for specific ultraviolet retention of this exact grade should be requested from the resin producer’s technical datasheet before outdoor qualification.
Busbar support insulators in low-voltage switchgear are constrained between copper conductors and a steel backplate. During a short-circuit event, the copper bar heats rapidly above 200 °C and expands, imposing compressive and shear stresses on the polymer insulator. A 30% glass-reinforced flame-retardant PBT is used when the design electrical withstand requirement is 600 V to 1000 V AC or DC. The polymer part is not a fuse; it maintains creepage distance during the first clearing cycles until the upstream protective device opens. Moulded-in stress around press-fit brass inserts is the dominant failure mechanism, and it may appear only after thermal cycling between −20 °C and 130 °C. Insert bosses are designed with a minimum wall thickness of 1.5 times the insert diameter, and insertion is performed by heat staking or ultrasonic insertion after moulding rather than cold press fit. The material is processed at the upper end of the melt-temperature window to reduce viscosity and fill long flow lengths between ribs, but hold pressure is limited to prevent glass-orientation-induced warpage. Tracking resistance and ignition resistance are tested under IEC 60112 and IEC 60695-2-12. A reduction in tracking index after 1000 h of damp heat ageing is a known risk for mineral-filled flame-retardant systems. The hydrolytic stabilisation package in V4860HR is intended to limit that reduction, but final performance must be validated on aged production parts from the actual switchgear assembly.
Competitive SABIC VALOX™ PBT+GF30%-Hydrolytic-FR V4860HR prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ V4860HR is a hydrolytically stabilized, 30% glass-fiber-reinforced polybutylene terephthalate injection-molding compound carrying a flame-retardant package. The grade is positioned for electrical, appliance, and automotive components that must retain mechanical integrity after exposure to heat, water vapor, and intermittent condensation while satisfying a UL 94 V-0 flammability classification at the thicknesses recorded in the current UL Yellow Card. The 30% by weight glass-fiber reinforcement raises flexural modulus, tensile strength, and heat deflection temperature relative to unreinforced PBT, while the hydrolytic stabilization package slows molecular-weight loss caused by ester hydrolysis in hot-wet service conditions.
The base polymer is a semicrystalline aromatic polyester with a melting point near 225 °C and a glass transition temperature in the 45–60 °C range. Hydrolytic degradation in PBT proceeds through chain scission of ester linkages; the resulting reduction in molecular weight leads to surface chalking, loss of tensile strength, and increased notch sensitivity before mechanical failure. In hydrolytically stabilized grades, carboxylic acid end-group concentration is reduced and hydrolysis-resistant additives are dispersed during compounding, which retards the autocatalytic hydrolysis reaction. Supplier-specific additive chemistry is proprietary, but the effect is evaluated by tensile retention after aging at 85 °C and 85% RH under ISO 527-2 or by accelerated pressure-cooker exposure. Melt flow for this class of 30% glass-fiber-reinforced flame-retarded PBT, measured at 250 °C with 5 kg according to ISO 1133-1, is generally reported in the 8–15 g/10 min interval; the current SABIC datasheet remains binding for process-window calculations.
Relative to a standard 30% glass-filled PBT without flame retardancy, V4860HR has higher density because of the flame-retardant solids and, in thin-wall tools, a shorter flow length. Published property envelopes place the density in the 1.64–1.68 g/cm³ interval under ISO 1183-1, tensile stress at break between 120 and 135 MPa under ISO 527-2/5, flexural modulus between 8,500 and 10,000 MPa under ISO 178, and heat deflection temperature HDT/A between 195 °C and 215 °C at 1.8 MPa under ISO 75-2. Table 1 summarizes the representative property envelope for design calculations.
| Property | Test method | Representative value or range |
|---|---|---|
| Density | ISO 1183-1 | 1.64–1.68 g/cm³ |
| Tensile stress at break | ISO 527-2/5 | 120–135 MPa |
| Tensile strain at break | ISO 527-2/5 | 2.0–3.0% |
| Flexural modulus | ISO 178 | 8,500–10,000 MPa |
| Flexural strength | ISO 178 | 175–195 MPa |
| Charpy notched impact at 23 °C | ISO 179-1/1eA | 6.5–9.0 kJ/m² |
| Heat deflection temperature HDT/A at 1.8 MPa | ISO 75-2 | 195–215 °C |
| Volume resistivity | IEC 60093 | ≥1 × 10¹⁴ Ω·cm |
| Surface resistivity | IEC 60093 | ≥1 × 10¹³ Ω |
The addition of an effective flame-retardant package to a 30% glass-filled PBT modifies several mechanical and electrical characteristics. Melt viscosity increases relative to unfilled PBT and non-FR glass-filled grades, which reduces flow length in thin ribs and snap-fit geometries. Impact strength is lower than that of impact-modified PBT grades; the notched Charpy values shown in Table 1 place V4860HR in the rigid, notch-sensitive region of glass-reinforced PBT compounds. The hydrolytic stabilization package does not eliminate hydrolysis, but it shifts the effective service envelope by retaining molecular weight longer under humid heat. Published data for this specific configuration under simultaneous 85 °C/85% RH aging and applied electrical stress is limited, so component validation should include application-specific temperature, humidity, and voltage cycling rather than relying solely on generic datasheet comparisons.
In dry-as-molded comparisons, a non-flame-retardant 30% glass-filled PBT may exhibit tensile strength in the same high-strength band and a somewhat higher comparative tracking index because it lacks FR fillers and synergists. However, after hot-wet exposure, a non-hydrolytically stabilized grade undergoes faster molecular-weight loss and surface degradation. The V4860HR designation is therefore selected when a V-0 rating and resistance to hot-humid aging are simultaneous requirements. The trade-off is that processing must be tightly controlled because the hydrolytic stabilization package and flame-retardant solids produce a narrower thermal window during compounding and injection molding than a standard 30% glass-filled PBT.
V4860HR must be dried before melt processing. A desiccant-bed or molecular-sieve dryer with a dew point no higher than -40 °C and a drying temperature of 120 °C for 2–4 h is specified in standard molding guidance for this class. Moisture above 0.02% by weight accelerates hydrolysis during plastication and produces splay, reduced tensile strength, and loss of Charpy impact. In molding shops above 60% RH, dried pellets should be conveyed in sealed hoppers or consumed within a defined holding time; unprotected exposure can exceed acceptable moisture limits within 30 min under atmospheric humidity. Avoid uncontrolled addition of basic or amine-bearing additives because these additives can alter the hydrolysis equilibrium or catalyze transesterification, confounding both the hydrolytic stabilization and flame-retardant packages.
The recommended melt temperature is 250–270 °C at the nozzle, with barrel settings increasing from the feed zone toward the nozzle. A screw compression ratio of 2.5:1 to 3.5:1 and a screw length-to-diameter ratio of 20:1 to 25:1 are standard for glass-reinforced PBT. Injection pressure at the screw tip commonly falls in the 100–140 MPa range, with hold pressure at 60–80 MPa depending on gate dimensions and wall thickness. Cavity pressure in the 40–70 MPa range is typical for this filler class during pack and hold; required clamp force is then selected from projected area and expected cavity-pressure distribution. Mold temperature should be held between 60 °C and 90 °C to obtain uniform crystallization and minimize post-mold dimensional change. Residence time at melt temperature must remain below 5 min; longer heated residence degrades the flame-retardant package and releases acidic residues that can corrode tool surfaces and accelerate polymer chain scission.
The 30% glass-fiber reinforcement makes the melt abrasive. Production-scale screw and barrel wear on repeated runs is reduced by specifying bimetallic barrels, hardened screw flights, and wear-resistant check rings. Hot-runner manifolds should avoid dead spots and abrupt changes in melt-channel diameter. Regrind addition is generally limited to 20% by weight for retention of the UL 94 certification; higher regrind ratios can reduce effective hydrolytic resistance by introducing additional thermal history and carboxylic acid end groups.
In automotive underhood applications, the material is used for ignition-coil housings, sensor bodies, connector shells, and relay covers where intermittent hot-air exposure, road-salt spray, and engine-bay humidity coexist with a requirement for electrical insulation and flame resistance. In appliance applications, the material is specified for pump housings, terminal blocks, and steam-exposed control components that require rigidity, low creep, and resistance to condensation. The 30% glass-fiber reinforcement supplies the stiffness needed to hold pin alignment in multi-cavity connectors; the hydrolytic stabilization package addresses the longer wet-ageing demands seen in sealed or semi-sealed enclosures. Component design must respect the grade’s notch sensitivity and low elongation at break. Snap-fit strain in glass-filled PBT should generally remain below 0.8% for long-term creep resistance; actual allowable strain depends on corner radius, gate position, and local wall thickness.
Standard 30% glass-filled PBT without hydrolytic stabilization is often adequate for dry electrical enclosures and short-term underhood exposure. The decisive difference appears when a connector housing is subjected to high ambient moisture, thermal cycling above the glass transition of PBT, and a flame-retardant requirement in the same part. In those conditions, standard grades lose surface quality and tensile strength earlier than hydrolytically stabilized grades, while unmodified PBT cannot maintain the required V-0 classification. V4860HR addresses this combination by balancing the chemistry of the hydrolysis-resistant system with 30% glass-fiber reinforcement and the FR package. The material should not be considered suitable for continuous immersion in hot water or pressurized steam above 95 °C, and prolonged contact with alkaline solutions can still attack the PBT backbone. Acidic or glycol-containing automotive fluids should also be evaluated before part release because they can accelerate ester hydrolysis or stress cracking in glass-reinforced PBT.
Table 2 identifies the standard attachments commonly referenced for a flame-retarded glass-filled PBT of this class. Final compliance claims must be confirmed against the current SABIC certification documents and the final part wall thickness, not from representative web summaries alone.
| Regulation or standard | Test designation or clause | Relevance |
|---|---|---|
| UL 94 | IEC 60695-11-10 | V-0 classification at listed specimen thicknesses |
| IEC 60112 | Method A | Comparative tracking index for electrical insulation |
| IEC 60093 | Volume and surface resistivity | Electrical insulation resistance |
| IEC 60695-2-12 | Glow-wire flammability index | Fire safety for unattended appliances |
| IEC 60695-2-13 | Glow-wire ignition temperature | Ignition resistance at elevated temperature |
| RoHS 2011/65/EU | Annex II and delegated amendments | Restricted-substance conformity at homogeneous material level |
| REACH 1907/2006/EC | SVHC candidate list | Supply-chain communication duties |
| ISO 11469 | Marking | Polymer identification marking for recycling |
For hot-runner systems, thermal gate temperature should remain within the melt-temperature window and the hot-drop volume should be minimized to avoid extended heated residence. The grade is not recommended for prolonged service in pressurized steam above 95 °C, strong alkaline solutions, or aggressive glycol-containing fluids under high tensile load; for those environments, semi-aromatic polyamides, PPS, or other hydrolysis-resistant polymers should be assessed.