| HS Code | 421985 |
| Grade | SABIC VALOX™ PBT+GF30%-HF V4760 |
| Polymer Type | Polybutylene terephthalate (PBT) |
| Reinforcement | Glass fiber |
| Glass Fiber Content | 30% |
| Flame Retardant System | Halogen-free flame retardant |
| Halogen Free | Yes |
| Density | 1.54 g/cm³ |
| Melt Volume Flow Rate | 12 cm³/10 min (250°C/2.16 kg) |
| Tensile Modulus | 10500 MPa |
| Tensile Stress At Break | 120 MPa |
| Tensile Strain At Break | 2.2% |
| Flexural Modulus | 9500 MPa |
| Notched Izod Impact Strength 23c | 7 kJ/m² |
| Hdt 0 45mpa | 205°C |
| Hdt 1 8mpa | 195°C |
| Ul94 Flammability Rating | V-0 (0.75 mm) |
| Processing Method | Injection molding |
| Drying Temperature | 120°C |
| Drying Time | 4 h |
| Melt Temperature | 250-280°C |
| Mold Temperature | 60-90°C |
| Mold Shrinkage Flow | 0.3-0.5% |
| Mold Shrinkage Cross Flow | 0.6-0.9% |
As an accredited SABIC VALOX™ PBT+GF30%-HF V4760 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT+GF30%-HF V4760 is packaged in 25 kg moisture-proof bags, 40 bags per pallet (1,000 kg net). |
| Container Loading (20′ FCL) | 20′ FCL loaded with SABIC VALOX™ PBT+GF30%-HF V4760 in 25 kg bags, palletized, stretch-wrapped, and secured for dry, protected ocean transport. |
| Shipping | SABIC VALOX™ PBT+GF30%-HF V4760 is shipped as non-hazardous thermoplastic pellets in moisture-proof bags, boxes, or bulk containers. Ship under standard conditions; store dry and cool, away from direct sunlight, and protect from moisture and contamination. Not regulated as dangerous goods; follow local transport and handling regulations. |
| Storage | Store **SABIC VALOX™ PBT+GF30%-HF V4760** in its original, sealed packaging in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and moisture. Keep containers closed to prevent contamination and moisture pickup. Avoid excessive stacking or pressure. Follow the SDS, local regulations, and first-in/first-out stock rotation. |
| Shelf Life | Shelf life: 24 months from manufacture when stored dry, below 30°C, in unopened original packaging, protected from moisture and sunlight. |
Under cyclic exposure to engine-compartment air at 85–125 °C with transient peaks approaching 140 °C, a 30 wt% glass-fiber-reinforced polybutylene terephthalate compound must retain terminal insertion force and connector latch dimensional consistency. SABIC VALOX PBT+GF30%-HF V4760 is processed after closed-loop desiccant drying at 120 °C for 4 h to a residual moisture target below 0.02 wt%, measured by Karl Fischer titration or an inline capacitance moisture sensor at the hopper throat. PBT hydrolytic chain scission during plasticizing shifts melt volume-flow rate from the ISO 1133-1 baseline and strips notched impact energy at ISO 179-1/1eA; the failure mode appears as star cracking around brass terminal retention tabs after 1,000 h of thermal ageing, not as a short shot. The high-flow modification produces spiral-flow lengths sufficient for 0.8 mm wall sections, but molders report that gate freeze time must be controlled near the end of packing because the reduced melt viscosity shortens the packing window; sequential valve gating on hot-runner systems with valve pin diameters 2.5–4.0 mm is used on four-cavity production tools. Barrel profiles are maintained between 245 °C and 265 °C, with nozzle temperature not exceeding 270 °C to limit volatile evolution and melt discoloration; mold surface temperature is held at 80–95 °C for sufficient crystalline skin formation, measured by differential scanning calorimetry with a peak crystallization temperature reported for PBT-GF30 at 190–200 °C. Venting depth is cut at 0.02–0.03 mm along flow fronts; insufficient venting produces gas burns at the last filling point when fill time is below 0.3 s. Terminal retention after heat ageing is evaluated against USCAR-2 class C or OEM-specific protocols at 125 °C for 1,000 h; tensile strength retention is compared using ISO 527-2 type 1A specimens cut from molded plaques, with brittle post-age fracture observed when moisture exceeds 0.03 wt% before processing. Finished components are engine control unit connectors, fuse box rails, 48 V junction blocks, and high-density harness connector bodies where dimensional stability, low moisture uptake, and fast cycle time are the dominant technical requirements.
| Property or attribute | Test method | Application-specific condition |
|---|---|---|
| Melt volume-flow rate | ISO 1133-1:2022 | 250 °C, 2.16 kg; high-flow grade |
| Tensile stress at break | ISO 527-2:2012 | Type 1A, 5 mm/min, 23 °C |
| Flexural modulus | ISO 178:2019 | 2 mm/min, 23 °C |
| Notched Izod impact | ISO 179-1/1eA:2010 | 4 mm specimen, edgewise |
| HDT A | ISO 75-2:2013 | 1.8 MPa, flatwise |
| Flammability | IEC 60695-11-10 / UL 94 | 0.75 mm and 1.5 mm thickness |
| Tracking index | IEC 60112:2003 | Solution A, 100 drops |
| Mold shrinkage | ISO 294-4:2018 | Flow and cross-flow, 2 mm plaque |
Low-voltage contactor bobbins and relay bases are molded from 30% glass-filled PBT because the material offers the required comparative tracking index under IEC 60112, typically above 250 V for non-wetting deposits, and can be supplied in formulations meeting UL 94 V-0 at 0.75 mm or 1.5 mm when the specific VALOX grade carries that classification in the UL Yellow Card. If V4760 does not carry the required flammability class, a separate flame-retarded VALOX PBT-GF30 grade must be specified for coil bobbins in unattended appliance circuits. The high-flow variant reduces injection pressure drop across multi-cavity bobbin tools; pressure loss along a 0.5 mm thin wall around the coil axis is lowered relative to standard-flow PBT-GF30, but shear heating in a restricted gate can raise local melt temperature above 280 °C and generate surface splay. Molding the material at mold temperature below 65 °C produces low-gloss surfaces and sinks at the bobbin flange root, and it reduces interlaminar bonding at weld lines where glass fibers orient perpendicular to the flow front. A four-cavity cold-runner tool with tunnel gate diameter 0.8–1.1 mm is operated with fill time under 0.25 s to avoid premature freeze-off; hold pressure is set at 60–80% of peak injection pressure, with profiling triggered by screw position rather than timer. Coil bobbins are wound with enamelled copper wire and subjected to dielectric withstand at 3.0–4.2 kV AC according to IEC 61810-1; the PBT wall must not soften when coil temperature reaches class F 155 °C, but continuous use should not exceed 150 °C because mechanical creep and tracking data for glass-filled PBT are commonly reported only up to 130–140 °C. Failure analysis on production lines shows that wet regrind above 20 wt% creates surface splays and intermittent short-shots on the thinnest coil flange; reground material is therefore dried together with virgin material and limited to 15–20 wt% in bobbins where UL recognition is retained. Incompatibility with alkaline coil impregnation varnishes and aqueous cleaning at pH greater than 9 is a documented boundary, because ester hydrolysis accelerates above pH 9 at temperatures above 80 °C.
| Processing variable | Typical control range | Measurement location or method |
|---|---|---|
| Desiccant drying temperature | 120 °C | Hopper dryer inlet, 4 h residence |
| Residual moisture | <0.02 wt% | Karl Fischer titration of raw granulate |
| Barrel melt temperature | 245–265 °C | Rear, center, front zones |
| Nozzle temperature | ≤270 °C | Thermocouple at nozzle tip |
| Mold surface temperature | 80–100 °C | Temperature-controlled water or oil tool |
| Injection speed | 10–15 mm/s initial, then higher | Linear screw speed; part flow length |
| Hold pressure | 60–80% of peak fill pressure | Hydraulic or electric injection pressure |
| Regrind ratio | 15–20 wt% max for tight-tolerance parts | Blended granulate feed |
Inside a dishwasher drain pump, the volute and circulation pump impeller operate in 60–80 °C wash liquor containing sodium carbonate and sodium polyphosphate; unstabilized PBT undergoes ester hydrolysis under these conditions, so a hydrolysis-resistant glass-reinforced PBT grade is required. The material is dried as described, and the tool surface is maintained at 90–100 °C to maximize crystallinity in the flow path. The high-flow formulation fills thin impeller vanes at wall thickness down to 1.5 mm without excessive glass orientation at the vane tip; glass fiber concentration at the vane edge is influenced by gate position, and a center sprue with radial flow is preferred over a side gate to reduce anisotropic shrinkage. Pump impellers molded from this grade are evaluated for dimensional stability after immersion in 1% sodium carbonate solution at 90 °C for 500 h; published data for this specific configuration is limited, and supplier datasheet values for hydrolytic stability should be confirmed for V4760 before specifying continuous exposure above 80 °C. A critical processing limitation is that any hygroscopic color concentrate or non-PBT carrier polymer added at above 2 wt% creates a separate phase that reduces weld-line strength at the impeller hub; this is detected by hydraulic burst cycling from 0 to 2.5 bar across 25,000 cycles. Shut-off nozzles and screw decompression after plasticizing are set to minimize drool because PBT melt viscosity is low and drool can carbonize in the hot runner manifold. Finished goods are drain pump housings for European-style dishwashers, circulation pump covers, and impeller subassemblies; component-level thermal ageing is performed under IEC 60335-2-5 for dishwasher pumps where the motor winding insulation class permits pump housing temperatures up to 105 °C.
Cordless drill motor housings and brush-card supports require a balance of stiffness, impact resistance, and creep resistance at elevated winding temperatures; the nominal glass fiber content of V4760 raises flexural modulus to the 8,000–9,000 MPa range under ISO 178, while notched Izod impact energy at ISO 179-1/1eA typically falls to the 8–11 kJ/m² range, which is acceptable for structural housing ribs but not for components receiving localized hammer impact. The high-flow variant fills deep ribs and gearbox support bosses in brushcutter engine covers and leaf blower fan volutes; molders use gas-assist or foaming only when sink marks on thick bosses are externally visible. Gate selection is dominated by the need to place weld lines away from motor mount lugs; glass fiber orientation along flow paths produces anisotropic shrinkage that can vary by 0.2–0.4% between flow and cross-flow directions, so tooling must be cut with differential shrinkage allowances according to ISO 294-4. A production issue documented on electric tool housings is thread boss cracking after power-driving screws; screw bosses are designed with an outer diameter at least 2.5 times the screw major diameter and use thread-forming screws rather than thread-cutting profiles to avoid excessive hoop stress. The material is not used for exhaust-side or engine cylinder components where continuous temperatures exceed 180 °C; published data for this specific configuration is limited for continuous exposure above 160 °C under load. For hand-held power tools, IEC 60745-1 / EN 60745-1 requires glow-wire testing on switch housing areas according to IEC 60695-2-11; PBT-GF30 formulations with flame retardant generally pass at 750 °C GWFI when tested on a finished part thickness of 1.5 mm or above, but the exact classification must be confirmed on the application-specific VALOX grade.
Across DC fast-charge inlet assemblies and battery management system module brackets, 30% glass-reinforced PBT is selected because low moisture absorption relative to PA66 preserves terminal pitch and connector mating forces after humidity cycling. PA66 can absorb 1.5–2.5% water at 23 °C/50% RH, shifting terminal pitch and increasing latch friction, while 30% glass-reinforced PBT absorbs less than 0.5% under the same conditions according to ISO 62. The compound is molded into latch plates, terminal spacers, and charger inlet retainers with wall thicknesses between 1.0 mm and 2.5 mm. The high-flow grade is beneficial for long flow paths across multi-pin connector bodies, but excessive melt speed through narrow ribbed sections can expose glass fibers as surface roughness at the gate end; slow-fast injection profiles are used, with initial injection speed limited to 10–15 mm/s for the first 5 mm of flow, then increased after the flow front expands. Weld lines in terminal rows are unavoidable; the tool is designed with flow deflectors to move weld lines off pin retention lances, and mold temperature is kept at 80–100 °C to promote molecular self-diffusion at the weld root. Parts are tested to IEC 62196-1 for mating force after thermal cycling from -40 °C to 105 °C and humidity cycling at 95% relative humidity. Creep deformation of terminal retention features is assessed by measuring pull-out force after 1,000 h at 105 °C under a fixed insert load; minimum retention force is specified by the connector manufacturer. Prolonged contact with ethylene glycol-based engine coolant at temperatures above 120 °C can plasticize and embrittle PBT, so such parts are confined to external dry areas of the charge inlet or dry battery module enclosures.
Actuator bodies for HVAC zone dampers, condensate pump volutes, and chiller valve actuator housings are molded from PBT-GF30 where polyamide 66 fails post-condensation through moisture-induced dimensional shift. The material is processed with a melt temperature near 250–260 °C and mold temperature 80–100 °C to maximize crystallinity; actuator body walls are typically 2.0–3.0 mm, and shrink marks around brass insert bosses are the most frequent injection defect. Inserts are preheated to 120 °C before insertion or loaded into a hot tool to reduce hoop stress at the insert wall; the part is then annealed at 120 °C for 2 h only where dimensional post-shrinkage must be stabilized prior to gear assembly. Glass fiber reinforcement gives sufficient torsional rigidity for gear support bosses, but gear tooth surfaces are not molded directly from this material because the glass fiber phase lowers wear resistance against steel gears; a separate POM or unfilled wear layer is used. Electrical safety testing follows IEC 60335-1 with glow-wire end-product requirements at 750 °C or 850 °C for unoccupied spaces depending on current; the flammability class required for the grade is confirmed by the final appliance standard. Environmental stress crack resistance against glycol/water condensate at 60 °C is examined by immersion testing for 1,000 h; published data for this specific configuration is limited, and supplier validation is required for hot glycol exposure above 60 °C.
In industrial terminal blocks, PLC remote I/O module bases, and low-voltage motor starter housings, the primary material requirement is a high comparative tracking index and controlled shrinkage across multi-pin insert dimensions. The high-flow grade fills terminal block bodies with 0.6 mm internal separation walls, but the tool must incorporate adequate venting to prevent gas burn marks at the end of fill; vent depth is maintained at 0.02–0.03 mm for PBT. Multi-cavity tools with up to 32 cavities are operated with cavity-to-cavity filling imbalance below 5%; melt-temperature variation across the hot half is controlled by independent manifold zones. Terminal retaining screw thread bosses are hot-inserted or ultrasonically inserted; the boss inner diameter is sized according to screw manufacturer torque tables, and boss wall thickness below 2.0 mm is avoided to prevent ejection cracks. The product is evaluated for insulation resistance after damp heat aging at 85 °C/85% RH for 1,000 h per IEC 60068-2-78, with insulation resistance measured at 500 V DC. Flammability and tracking index requirements for terminal blocks are referenced in IEC 60947-7-1; the grade must show acceptable CTI and glow-wire performance depending on uninsulated conductor contact sections. Use of black colorant masterbatch above 3 wt% is not advised because carbon black at high loading can reduce tracking resistance and interfere with laser marking contrast; published data for this specific configuration is limited and must be checked on the molded part.
Competitive SABIC VALOX™ PBT+GF30%-HF V4760 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PBT+GF30%-HF V4760 is a 30 wt% short-glass-fiber-reinforced polybutylene terephthalate injection-molding compound formulated for thin-wall applications in which standard-viscosity glass-filled PBT cannot fill the cavity within the available pressure envelope. The grade is characterized by a nominal density of 1.53 g/cm³ per ISO 1183-1, a heat deflection temperature of 205 °C under a 1.80 MPa load per ISO 75-2/Af, and a flexural modulus of 8500 MPa per ISO 178. The suffix “HF” denotes high-flow rheology and does not indicate halogen-free composition or a defined flame-retardant classification. For parts requiring a specific UL 94 rating, the supplier’s yellow-card certification at the final wall thickness and color must be verified before tool release.
Representative datasheet values are summarized below for preliminary material selection. Final product specifications should be confirmed against the manufacturer’s latest published datasheet and lot-specific certificate of analysis.
| Property | Test standard | Representative value |
|---|---|---|
| Density | ISO 1183-1 | 1.53 g/cm³ |
| Tensile stress at break | ISO 527-2/5 | 125 MPa |
| Tensile strain at break | ISO 527-2/5 | 2.5% |
| Flexural modulus | ISO 178 | 8500 MPa |
| Flexural strength | ISO 178 | 190 MPa |
| Notched Izod impact, 23 °C | ISO 180/1A | 7 kJ/m² |
| Notched Izod impact, -30 °C | ISO 180/1A | 6 kJ/m² |
| Heat deflection temperature, 1.80 MPa | ISO 75-2/Af | 205 °C |
| Vicat softening temperature, B/120 | ISO 306/B120 | 215 °C |
| Mold shrinkage, flow direction | ISO 294-4 | 0.3–0.5% |
| Mold shrinkage, transverse direction | ISO 294-4 | 0.5–0.8% |
| Water absorption, 24 h, 23 °C | ISO 62 | 0.05% |
| Volume resistivity | IEC 60093 | >1.0 × 10¹⁵ ohm·cm |
| Surface resistivity | IEC 60093 | >1.0 × 10¹⁵ ohm |
| Dielectric strength, 3.2 mm thickness | IEC 60243-1 | 18 kV/mm |
| Comparative tracking index | IEC 60112 | 250 V |
Flow length in glass-filled PBT is governed by fiber attrition, melt temperature, and gate geometry more than by melt volume-flow rate alone. In production-scale trials on electric injection molding machines with screw L/D ratios between 18:1 and 22:1, back pressures in the range of 20–40 bar and screw surface speeds below 0.20 m/s are reported to preserve average fiber lengths above 200 μm. When the same part is processed at surface speeds above 0.35 m/s, local viscous dissipation can raise melt temperature above the recommended maximum of 280 °C, accelerating PBT chain scission and reducing notched Izod impact from 7 kJ/m² to below 5 kJ/m² per ISO 180/1A. Regrind rates above 20% and barrel residence times beyond 8 minutes at 270 °C further reduce toughness, so high-flow designation does not remove the need for strict residence-time control.
In 14-pin sealed automotive connector bodies with 0.8 mm nominal walls, the grade is used in four-cavity hot-runner tools where melt temperature is held at 260 °C and mold temperature at 100 °C. Transfer pressure at the nozzle is typically 900–1100 bar; fill times are controlled to 0.4–0.6 s. Below 80 °C mold temperature, frozen skin layers reduce weld-line strength at pin-field locations; above 120 °C, cycle times increase and ejection becomes sensitive to draft angles below 0.5°.
PBT is hygroscopic enough to require drying before melt processing. The manufacturer recommends desiccant-bed drying at 120 °C for 4–6 hours to a residual moisture level below 0.02 wt%. When ambient relative humidity exceeds 60%, open hopper loading introduces measurable moisture within 20 minutes; a closed loader with dry-air purge and a dew point below -40 °C is therefore necessary for consistent molding. A 40 mm reciprocating screw machine is typically set with rear zone at 240 °C, center zone at 250 °C, front zone at 260 °C, and nozzle at 260 °C. Melt cushion should remain between 2 mm and 4 mm. Cushions above 4 mm extend heat exposure and increase volatile formation; cushions below 2 mm reduce packing control and generate dimensional variation.
Relative to standard-viscosity 30% glass-reinforced PBT grades, V4760 fills longer flow lengths at equivalent wall thickness and injection pressure, but the trade-off is lower melt strength and reduced notched impact. Its 7 kJ/m² notched Izod value at 23 °C per ISO 180/1A places it at the lower end of the 30% glass-filled PBT family. The grade is therefore specified for thin-wall geometries where cavity filling is the governing constraint, rather than for thick-section brackets needing maximum ductility. Compared with 30% glass-reinforced flame-retardant PBT grades, V4760 generally provides higher flow but does not automatically carry the same UL 94 V-0 certification; flame class remains thickness- and color-dependent. The “HF” suffix must not be interpreted as halogen-free or flame-retardant.
Because PBT absorbs less water than polyamide, this grade can maintain tighter dimensional envelopes in humid electrical environments. Water absorption after 24 h immersion in deionized water at 23 °C is 0.05% per ISO 62, compared with typical values of 0.8–1.0% for 30% glass-reinforced PA66. Dimensional change in the flow direction after conditioning at 50% relative humidity is generally below 0.1%. However, PBT is not recommended for continuous hot-water service above 80 °C under load because hydrolytic degradation reduces molecular weight and embrittles the glass-fiber interface over time.
Resistance to automotive fluids, lubricants, and unleaded fuels is a primary selection driver for pump housings and fuel-system brackets. The polymer matrix is resistant to aliphatic hydrocarbons, aromatic solvents, and many polar organic compounds, but alkaline solutions and hot aqueous acids attack the ester linkage. Compatibility with engine coolants containing organic acid corrosion inhibitors should be validated through immersion testing at the upper service temperature near 120 °C using tensile bars per ISO 527-2; published data for this specific configuration is limited.
For electrical housings and connectors operating at working voltages below 50 V, the comparative tracking index of 250 V per IEC 60112 provides adequate resistance to surface tracking under polluted conditions. The volume resistivity exceeds 1.0 × 10¹⁵ ohm·cm per IEC 60093, and the dielectric strength at 3.2 mm thickness is approximately 18 kV/mm per IEC 60243-1. These electrical properties are measured on unconditioned specimens; after 48 h exposure to 85 °C and 85% relative humidity, dielectric strength and tracking resistance should be re-evaluated on production samples because fiber-rich surface layers can alter tracking behavior.
In thin-wall sensor bodies with wall stock below 1.0 mm, gate geometry is a larger determinant of molded-part integrity than barrel setpoint. Film gates and tab gates with land lengths of 0.5–1.0 mm and gate thickness of 60–80% of the wall section are preferred to minimize glass-fiber breakage. Packing pressure is typically held at 60–80% of peak injection pressure for 2–4 s; longer packing can overpack the gate and induce fiber orientation gradients across the part. The narrow processing window is associated with the high-flow polymer matrix: at gate thicknesses below 0.3 mm, fiber breakage increases and local melt temperature can exceed 300 °C, producing surface bloom. At gate thicknesses above 1.2 mm, packing pressure transmits too aggressively into the cavity and causes flash at parting-line clearances above 0.02 mm.