| HS Code | 143992 |
| Polymer Type | PBT with 30% glass fiber |
| Filler Content | 30% glass fiber |
| Density | 1.53 g/cm3 |
| Melt Volume Rate | 8 cm3/10 min at 250°C/2.16 kg |
| Tensile Modulus | 10000 MPa |
| Tensile Strength At Break | 120 MPa |
| Elongation At Break | 2.5% |
| Flexural Modulus | 9000 MPa |
| Flexural Strength | 180 MPa |
| Notched Izod Impact | 80 J/m |
| Unnotched Izod Impact | 500 J/m |
| Heat Deflection Temperature 0 45mpa | 220°C |
| Heat Deflection Temperature 1 8mpa | 200°C |
| Molding Shrinkage Flow | 0.2-0.5% |
| Water Absorption | 0.07% |
| Flame Rating | UL94 HB |
As an accredited SABIC VALOX™ PBT+GF30% 4031 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT+GF30% 4031 supplied in 25 kg moisture-barrier bags, packed on pallets for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with SABIC VALOX™ PBT+GF30% 4031 in palletized bags, securely stowed, sealed, and ready for export. |
| Shipping | SABIC VALOX™ PBT+GF30% 4031 is supplied as glass-fiber-reinforced PBT pellets in moisture-barrier bags or octabins, palletized. Ship dry, covered, at ambient temperature, away from direct sunlight and moisture. Normally non-hazardous for transport; follow local regulations and keep packaging sealed until use. |
| Storage | Store SABIC VALOX™ PBT+GF30% 4031 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers tightly closed in original packaging. Protect from moisture, dust, and contamination, and follow first-in/first-out stock rotation. Consult the SDS for detailed local storage requirements. |
| Shelf Life | SABIC VALOX™ PBT+GF30% 4031 typically has a 24-month shelf life when stored dry, in unopened original packaging at moderate temperatures. |
Desiccant hopper drying at 120 °C for 3–4 h to a residual moisture content below 0.02% is the first process control point for SABIC VALOX™ 4031 before automotive under-hood connector housings are injection molded. The material is a 30% glass-fiber-reinforced polybutylene terephthalate grade, and moisture above that threshold reduces molecular weight during melt processing, producing surface splay and lower weld-line strength. On a production line with a 24-to-48-cavity hot-runner tool, typical barrel settings from feed to nozzle are 245 °C, 250 °C, 255 °C, and 260 °C, with nozzle melt temperature held at 260 °C ± 5 °C. Mold temperature is controlled at 80–100 °C. If mold temperature drops below 60 °C, surface resin freezes before fiber orientation completes, producing dull patches and increased post-molding shrinkage variation. If melt temperature exceeds 275 °C or residence time exceeds 5 min, thermally degraded polymer can deposit on gas vents and reduce weld-line integrity. These limits are observed during multi-hour runs on 120 t to 180 t clamp-force injection machines fitted with 22:1 L/D general-purpose screws.
The connector domain exploits the balance between stiffness and thermal distortion resistance. Representative mechanical values for 30% glass-reinforced PBT are tensile stress at break near 120 MPa measured per ISO 527-2, flexural modulus near 9 000 MPa per ISO 178, and heat deflection temperature close to 215 °C at 1.8 MPa per ISO 75-2/Af. These are not substitutes for the production certificate; the current SABIC datasheet must be checked for exact lot values. In engine bay use, the connector body must maintain terminal retention during thermal cycling from −40 °C to 150 °C. Material-level thermal aging is commonly assessed according to ISO 527-2 after exposure, but automotive connector validation follows USCAR-2, which includes mechanical shock, vibration, and temperature-humidity cycling. The grade is typically rated UL 94 HB at a specified thickness. If thicker wall sections are used, the heat extraction rate changes and a different mold temperature profile may be needed.
Gate position and weld-line placement dominate terminal retention. A gate placed at the narrow pin-retention side creates a weld line at the rear face of the connector body; that weld line can become the initiation point for pin insertion cracking during harness assembly. Flow leadership in the tool is adjusted by varying local steel thickness or by adding flow channels in the runner, not by raising melt temperature above 270 °C. Pin inserts are preheated to 120–150 °C to reduce thermal shock when melt arrives. Inserted pins made of brass or phosphor bronze are preferred because their thermal expansion is closer to the surrounding plastic than aluminium pins. The terminal product includes engine-bay sensor connectors, transmission control unit headers, and powertrain control module sockets.
The limiting parameter in high-voltage busbar carrier molding is the differential thermal contraction between copper conductors and the 30% glass-filled PBT matrix. Copper expands at roughly 17 ppm/K, whereas glass-reinforced PBT can exhibit linear thermal expansion of 30–35 ppm/K in the flow direction and higher in the transverse direction. When melt at 255–265 °C contacts cold copper, the polymer freezes quickly at the conductor edge, leaving a quench layer with high residual stress. Production tools therefore preheat copper busbars to 120–180 °C before insertion. Copper edges are radiused rather than shear-cut square because sharp edges act as notch concentrators during thermal shock. The molding machine is configured with low screw backpressure, typically 0.5–1.0 MPa measured hydraulic, and a slow initial injection velocity to avoid jetting at the conductor interface. Published data for this specific configuration is limited, particularly for thick copper cross-sections above 4 mm; process developers confirm acceptable interface adhesion by sectioning parts and examining the copper-polymer boundary under reflected-light microscopy.
Electrical clearances for busbar carriers are evaluated against IEC 60664-1. Creepage and clearance distances are determined by working voltage and pollution degree, not by the material’s UL rating alone. Comparative tracking index is tested per IEC 60112, and the value shown on the material datasheet must be used for design calculation. A shallow zone exists for material handling if the granulate is not dried properly; busbar carriers with wall thickness above 3 mm can trap volatiles during filling, causing voids at the conductor reverse side. These voids reduce partial discharge inception voltage, so pressure-holding stages are extended until gate freeze-off. The terminal product is an encapsulated busbar carrier in a battery management distribution unit, where the PBT serves as the dielectric spacer and dimensional seat for bolted interconnects. The operational boundary is clear: if the carrier is exposed to condensing moisture at voltages above 60 V DC in a pollution degree 3 environment, the design requires a sealed cover or a hydrolysis-resistant grade not inferred from this material designation.
Gate position, not glass loading alone, determines the balance class of an axial cooling fan hub molded from VALOX 4031. A single-edge gate produces a high degree of fiber alignment parallel to flow, which increases tangential stiffness but can create an out-of-balance condition after ejection. In a multi-cavity hot-runner tool with a central ring gate, the material fills the hub first and the blade cavities last, placing the weld line at the blade trailing edge. Mold temperature is held between 80 °C and 100 °C, and fill speed is kept moderate to prevent glass fiber separation at the blade leading edge. After ejection, parts are placed on a contour fixture until enthalpy relaxation is complete, because immediate free-standing cooling leads to hub warpage below 0.15 mm on the shaft seat diameter. Dimensional inspection uses a coordinate measuring machine at 23 °C ± 2 °C after conditioning per ISO 291. Balance quality is evaluated per ISO 14694 for fan assemblies, usually at G 6.3 or tighter depending on rotor speed. The terminal product includes cooling fan frames for telecom rectifier trays and industrial variable-frequency drives.
The shallow zone is the material mixing step: no compounding or additive incorporation is required. The granulate is loaded directly into the hopper dryer and then into the molding machine. Any regrind use is limited to 20% by weight and must be dry-blended with virgin material to avoid lot-to-lot fiber length reduction. The key incompatibility is with hydrocarbon-based release agents; if an external mold release is used, an alcohol-compatible grade is selected to prevent loss of adhesion at the hub metal-insert interface. Long-term dimensional stability is affected by maximum service temperature; above 140 °C, continuous exposure can result in progressive post-shrinkage, and the fan hub seat diameter may drift beyond the press-fit tolerance.
In appliance control housing production, the material is seldom the limiting process variable; the failure point is usually the snap-fit geometry and the gate vestige. A 30% glass-reinforced PBT housing with a snap arm requires the gate placed away from the arm root because the fiber orientation at the gate freezes in a stress concentration. Molders use a mold temperature of 80 °C and a melt temperature of 255 °C. The terminal product is a relay base or igniter control housing for gas-fired heating appliances. Continuous service is limited to dry enclosures at or below 130 °C; if the housing sits adjacent to a hot-gas plenum, the grade must be evaluated against IEC 60695-2-11 glow-wire ignition requirements, and if the result does not meet the appliance standard, a flame-retarded PBT or another polymer class is required.
At wall thicknesses below 0.8 mm, the injection pressure required to fill an ignition coil bobbin rises sharply, and glass-fiber breakage becomes a dominant cause of molded-in stress. For a bobbin with a winding length of 35 mm and a core pin diameter of 12 mm, filling is completed in 0.2–0.4 s, with peak injection pressure between 80 MPa and 120 MPa. The sprue and runner are designed with a diameter larger than 4 mm to avoid excessive shear heating. Mold temperature is held at 100 °C, not lower, to maintain a thin frozen layer and to reduce the pressure gradient along the core pin. The core pin is lubricated with a high-temperature mold release at start-up only; continuous application is avoided because it can degrade dielectric strength. After molding, bobbins are annealed at 120 °C for 1 h to relieve orientation stress before winding. The wire tension during winding must be limited, typically below 5 N for 0.2 mm enameled copper wire, because the thin bobbin flange can fracture from hoop stress. The dielectric strength of the molded bobbin is tested per ASTM D149 under oil.
The processing window for this geometry is narrow. A melt temperature above 270 °C generates flash at the split line, while a temperature below 245 °C produces short shots in the bobbin flange. Barrel residence time is limited to 4 min. Screw recovery speed is set low enough to ensure glass-fiber distribution but high enough to maintain cycle time; otherwise, the charging phase produces non-uniform fiber content between the first and last cavities. The terminal product is an ignition coil bobbin for small-displacement spark-ignition engines. Published data for this exact thin-wall configuration is limited, so process validation relies on cross-sectioning a first-article bobbin and measuring fiber orientation at the flange-to-body transition.
Power tool motor support frames molded from VALOX 4031 are usually admitted into production after impact tests on the final assembly, but the raw material itself is characterized by notched Izod impact values measured per ISO 180/1A. For 30% glass-filled PBT, notched Izod is typically lower than unfilled ductile PBT, so the design must avoid sharp internal corners at the bearing seat and at the fan-baffle attachment bosses. The tool builder specifies a minimum internal radius of 0.5 mm and local wall thickness of at least 1.5 mm around screw bosses. Molding is done with a melt temperature of 250–260 °C and a mold temperature of 80 °C. The terminal product is a gearbox support frame in a corded hand-held power tool. If the frame is exposed to transmission oil at elevated temperature, the material must be confirmed for oil resistance under the specific oil formulation, because glass-filled PBT can undergo stress cracking in contact with certain ester-based lubricants. The exact compatibility statement belongs to the material datasheet and application-specific oil immersion testing per ISO 175.
Competitive SABIC VALOX™ PBT+GF30% 4031 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PBT+GF30% 4031 is a short-glass-fiber-reinforced polybutylene terephthalate injection molding compound with a nominal glass loading of 30 wt%. Under ISO 1043-1:2011, the material designation is PBT+GF30. Molded density is generally reported in the 1.52–1.56 g/cm³ range under ISO 1183-1. Tensile modulus values for this glass-reinforced PBT class commonly fall between 8,500 MPa and 10,000 MPa when tested to ISO 527-2/1; notched Charpy impact values measured under ISO 179-1/1eA are usually in the 6–9 kJ/m² band. The grade is positioned as a general-purpose 30% glass-filled PBT without halogenated flame-retardant loading. Flame classification should be verified against the current SABIC UL file at the specified thickness; many unfilled and glass-reinforced PBT grades of this class are listed as UL 94 HB at 0.75 mm. Published datasheet values are typical and are not specification limits.
The primary departure from unfilled PBT is the large increase in stiffness and heat distortion resistance at the expense of melt flow and isotropic shrinkage. Unfilled PBT typically displays tensile modulus in the 2,400–2,700 MPa range under ISO 527-2/1 and heat distortion temperature under 1.8 MPa near 50–60°C when measured to ISO 75-2/Af. At 30 wt% short glass, tensile modulus rises to 8,500–10,000 MPa and HDT/A values move into the 195–210°C band. Flexural modulus under ISO 178 also shifts from approximately 2,200–2,500 MPa for unfilled PBT to 7,000–8,000 MPa for the reinforced compound. These differences make PBT+GF30% 4031 better suited to structural housings, gear carriers, motor end shields, and pump components where deflection under load must remain low.
Compared with lower-glass PBT grades, the 30% reinforcement level reduces mold shrinkage and changes orientation-induced distortion. Unfilled PBT can show flow-direction shrinkage of 1.5–2.0% under ISO 294-4, while 15% glass-filled PBT generally falls near 0.6–0.9%. At 30 wt% glass, flow-direction shrinkage commonly registers between 0.3% and 0.6%, with transverse shrinkage often 0.7–0.9%. The anisotropy is not benign: fiber orientation produced during cavity fill creates a shrinkage differential that must be addressed through gate placement, wall-thickness uniformity, and controlled mold temperature. Compared with impact-modified 30% glass PBT formulations, the 4031 designation should be expected to provide a higher modulus but lower notched impact retention; buyers should compare notched Charpy values under ISO 179-1/1eA rather than relying on filler level alone.
| Property | Test method | 30% GF PBT class | Unfilled PBT | 15% GF PBT |
|---|---|---|---|---|
| Density, 23°C | ISO 1183-1 | 1.52–1.56 g/cm³ | 1.30–1.32 g/cm³ | 1.41–1.44 g/cm³ |
| Tensile modulus | ISO 527-2/1 | 8,500–10,000 MPa | 2,400–2,700 MPa | 4,800–5,500 MPa |
| Flexural modulus | ISO 178 | 7,000–8,000 MPa | 2,200–2,500 MPa | 4,000–4,700 MPa |
| Notched Charpy, 23°C | ISO 179-1/1eA | 6–9 kJ/m² | 3–5 kJ/m² | 4–7 kJ/m² |
| HDT/A, 1.8 MPa | ISO 75-2/Af | 195–210°C | 50–60°C | 160–180°C |
| Molding shrinkage, flow | ISO 294-4 | 0.3–0.6% | 1.5–2.0% | 0.6–0.9% |
On production-scale injection molding lines, PBT+GF30% 4031 requires closed-loop desiccant drying to avoid hydrolysis of the polyester backbone. The target melt moisture content is below 0.02% by weight, measured by Karl Fischer titration to ISO 15512:2019. Hopper dryer setpoints of 110–120°C with a dew point at or below -20°C and residence time of 3–4 h are standard practice on 60–100 kg/h throughput cells. Inadequate drying is observed as splay, silver streaking, and loss of tensile strength at the gate rather than as a uniform melt-temperature defect. Melt temperature at the nozzle should be maintained between 250°C and 270°C. Sustained periods above 270°C or residence time beyond 8 min promote thermal degradation, which can reduce load-bearing capacity and generate volatiles. Mold temperature should not be treated as a minor variable; mold surface temperatures between 60°C and 100°C are required, with the upper half of that range improving crystallization and reducing post-mold shrinkage in thick sections. Cavity fill speeds should be sufficient to prevent freeze-off in ribs thinner than 0.8 mm, while excessive shear in hot-runner drops can mechanically degrade the glass strands and reduce tensile modulus.
| Parameter | Recommended range | Equipment or test condition |
|---|---|---|
| Drying temperature | 110–120°C | Desiccant dryer, dew point ≤ -20°C |
| Drying time | 3–4 h | Closed-loop hopper, target moisture < 0.02% |
| Melt temperature | 250–270°C | Nozzle thermocouple |
| Mold temperature | 60–100°C | Mold surface thermocouple |
| Back pressure | 0.3–0.7 MPa | Hydraulic gauge pressure |
| Screw L/D | 20:1–24:1 | General-purpose, compression 2.0:1–2.5:1 |
| Maximum residence time | < 8 min | At maximum melt temperature |
The structural benefit of 30% glass fiber is strongly dependent on fiber orientation frozen into the cavity. At knit lines, glass fibers do not cross the flow fronts in the same density as they align in the primary flow path; weld-line tensile strength in short-glass PBT can fall to 40–60% of the unreinforced-flow value. Published data for SABIC VALOX™ PBT+GF30% 4031 under multi-gate tensile specimens is limited, but the mechanism is well established for short-glass polybutylene terephthalate. Gate placement should therefore locate weld lines away from boss pull-out loads, snap-fit hinges, or bearing shoulders. Where weld lines are unavoidable, tensile testing on molded plaques under ISO 527-2/5 using a single gate versus double-gated tool is preferable to relying on nominal datasheet strength. Orientation also produces anisotropic creep and thermal expansion behavior; measured coefficient of linear thermal expansion in flow direction is typically lower than transverse expansion. Parts requiring roundness after annealing should be checked at 120°C for post-mold distortion because locked-in orientation relaxes progressively above the glass transition of the PBT matrix.
Applications for PBT+GF30% 4031 include electrical terminal blocks, relay bases, coil bobbins, motor brush holders, appliance handle structural frames, power tool housings, and underhood automotive brackets where exposure is intermittent up to 140°C. Electrical performance should be anchored to the relevant material datasheet and part test plan: dielectric strength under IEC 60243-1 is commonly reported in the 18–24 kV/mm range for 3.0 mm plaques, and volume resistivity measured to IEC 60093 is generally above 1E15 Ω·cm at 23°C. These values do not constitute electrical safety ratings for finished parts; creepage and clearance requirements under IEC 60664-1 remain geometry-dependent. The product resists aliphatic hydrocarbons, gasoline, mineral oils, greases, and many neutral aqueous solutions at room temperature, but continuous exposure to hot water, steam, strong acids, or strong bases above 60°C can hydrolyze the ester backbone and must be excluded from use. Where long-term hydrolysis resistance is required, a heat-stabilized or hydrolysis-resistant PBT grade should be specified instead of a general-purpose 30% glass material.