| HS Code | 815309 |
| Grade | SABIC VALOX™ PBT+GF17%-FR DR48 |
| Polymer Base | PBT |
| Mold Shrinkage Flow Percent | 0.3-0.5 |
| Mold Shrinkage Cross Flow Percent | 0.6-0.8 |
| Ul94 Rating | V-0 |
As an accredited SABIC VALOX™ PBT+GF17%-FR DR48 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT+GF17%-FR DR48 is packaged in 25 kg moisture-barrier bags, 40 bags per pallet (1,000 kg). |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized bags of SABIC VALOX™ PBT+GF17%-FR DR48, shrink-wrapped, secured, and shipped in a clean, dry container. |
| Shipping | SABIC VALOX™ PBT+GF17%-FR DR48 is typically shipped as non-hazardous solid pellets in moisture-barrier bags, lined sacks, or octabins on pallets. Keep dry, cool, and contamination-free. Follow the SDS and local transport regulations; no special hazardous shipping classification is normally required. |
| Storage | Store in a cool, dry, well-ventilated area in original, sealed containers. Protect from direct sunlight, moisture, heat, sparks, open flames, and static discharge. Keep away from strong oxidizers and other incompatible materials. Avoid dust formation and maintain good housekeeping. Use first-in, first-out stock rotation; keep containers closed when not in use. Recommended ambient storage, avoiding prolonged high humidity. |
| Shelf Life | Shelf life is 24 months from manufacture when stored unopened in original packaging under dry, cool conditions. |
For low-voltage terminal blocks and insulation displacement connectors molded on 100–160 t clamping-force injection lines, SABIC VALOX™ PBT+GF17%-FR DR48 is introduced as a ready-to-mold compound with the glass fiber loading fixed at 17 wt%; no downstream glass-fiber masterbatch is required, and the addition ratio for the pellet stream is 100 wt% neat compound unless a factory-managed regrind stream is validated. Compliance for this segment is anchored to IEC 60947-7-1:2009 for terminal blocks in low-voltage switchgear, IEC 60664-1:2020 for insulation coordination, UL 94 V-0 at 0.75 mm for flammability, and IEC 60112:2003 for comparative tracking index performance. The downstream process typically involves desiccant drying at 120 °C for 4 h to a residual moisture content below 0.02%, followed by injection molding with a melt temperature maintained between 245 °C and 260 °C and tool temperature controlled at 65–90 °C; barrel residence time above 6 min at melt temperature must be avoided to prevent decomposition of the flame-retardant system and resultant free-acid evolution, which lowers tracking resistance. The 17 wt% chopped glass reinforcement generates anisotropic shrinkage and weld-line weakness at terminal barrier geometry; therefore, gate placement is positioned to move knit lines away from the highest insertion-force locations. Terminal product types include DIN-rail terminal carriers, insulation displacement connection blocks, panel-mount barrier strips, and current transformer terminal housing elements where dimensional stability under screw-torque assembly is required.
The limiting variable in thin-walled solenoid bobbin production is not melt temperature alone but the interaction between glass-fiber orientation, weld-line formation around the core pin, and the resin's flame-retardant degradation window. Material feed is at 100 wt% of the SABIC compound; any addition of mold-release additive or pigment must be limited to ≤1.5 wt% total let-down to avoid diluting the flame-retardant package. Standards applying here include IEC 60335-1:2020 clause 30.2 glow-wire requirements, IEC 61558-1:2017 for transformer safeguards, and UL 1446 for insulation systems when the bobbin is part of a listed motor or transformer assembly. Downstream processing uses a reciprocating screw with 18:1–22:1 L/D, compression ratio between 2.4:1 and 2.8:1, and a shot size between 40% and 70% of rated barrel capacity. When the flow front splits around the core pin, the resulting knit line reduces local tensile strength by up to 40% relative to uninterrupted glass-fiber orientation as evaluated by ISO 527-2:2012 tensile specimens; this requires moving the gate to a ring or film gate configuration rather than a single side gate. Published data for this specific geometry and product combination is limited, so production-scale validation with 50-shot short-shot series establishes gate freeze time and weld-line position. Terminal parts include solenoid coil bobbins, control transformer bobbins, relay coil formers, and encapsulated coil shells for valve actuation.
Arc shields and barrier plates in miniature circuit breakers require retention of dimensional geometry after repeated high-temperature transients. The compound is not modified by the molder; it is processed at the supplied 17 wt% glass loading, with regrind addition generally restricted to 0–20 wt% and only after inspection for carbonized particles or copper dust contamination from switchgear factory environments. Relevant standards include IEC 60947-1:2020 for low-voltage switchgear and controlgear, IEC 60695-2-12:2021 and IEC 60695-2-13:2021 for glow-wire flammability index and ignition temperature, and UL 746B for polymeric materials with long-term thermal aging. The exact relative thermal index assigned to this grade remains the controlling value on the UL Yellow Card, not a value inferred from short-term heat deflection temperature measurements. The downstream process for arc-critical components often uses an injection profile with low-to-moderate injection velocity to avoid jetting and glass-fiber breakage, packing pressure sufficient to limit sink marks behind bosses, and a mold-temperature setpoint at the upper end of 80–90 °C to displace the crystallization onset and reduce post-mold shrinkage in the press. Thin-section shield ribs at 0.8–1.2 mm nominal wall require generous venting, typically 0.02–0.03 mm, to prevent burn marks and pressure-voltage breakdown from trapped gas. Terminal product types include arc chute side plates, arc runner supports, phase barriers, and mounting bases for air circuit breaker auxiliary contacts, where the UL 94 V-0 rating at 0.75 mm is a mandatory fire-containment boundary.
Across household-appliance control housings and sealed relay enclosures, the dominant compliance path is IEC 60335-1:2020 clause 30.2, which requires glow-wire ignition temperature and flame spread classification at end-product wall thickness. In these applications the pellet stream is 100 wt% VALOX DR48; if an in-house regrind stream is used for non-sealing covers, the maximum addition is typically 20 wt% of the shot mass, with virgin resin making up the remainder; seals and structural bosses remain virgin-compound-only to avoid contamination-induced tracking faults. Drying before molding uses a -30 °C dew-point desiccant bed at 120 °C for 4 h, because moisture levels above 0.02% accelerate hydrolysis of the PBT ester linkage during barrel residence and reduce tensile strength at the knit line. The downstream production process uses heated sprue bushings and valve-gated hot-runner nozzles where flow-length-to-thickness ratios exceed 150:1, with melt temperature held between 245 °C and 255 °C, and barrel hold-up time limited to 5–8 min. Terminal product types include washing-machine logic control housings, dishwasher electronic module covers, sealed relay bases, and motor-drive enclosures with snap-fit closures that require repeated assembly without stress cracking.
In corded power tool motor housings, the combination of 17 wt% glass fibers and brominated flame retardant produces a viscosity profile that is sensitive to shear heating in sequential valve-gated hot-runner systems, where the resin must remain below 265 °C to prevent thermal decomposition of the flame retardant. The material is charged as 100 wt% neat compound; any additional toughener or processing aid is not specified unless validated for UL listing retention. The relevant standards for this segment are IEC 62841-1:2014 for motor-operated hand-held tools, UL 94 V-0 at 0.75 mm, and ASTM D638-14 for tensile modulus measurements used to verify glass-fiber orientation in first-article testing. Production processing for this geometry requires droplet-free hot-runner needle sequencing, with valve pins opening only after the upstream flow front has established a frozen layer; this avoids filling-flow hesitation that creates visible flow lines at the junction between two gates. Injection speed is ramped from 40 mm/s to 90 mm/s during the fill phase, with packing pressure held for 8–12 s and mold temperature at 70–80 °C to maintain dimensional stability of bearing bores and brush-holder slots. Terminal product types include field-case liners, brush-holder plates, trigger housing components, and heat shields between motor and tool body.
In automotive fuse-box and relay-base platforms, the in-service requirement is not limited to initial flammability; terminal retention force after thermal cycling and underhood exposure determines whether the carrier remains functional after 100,000 km equivalent vibration and temperature cycles. The molding input is 100 wt% VALOX PBT+GF17%-FR DR48; regrind is typically excluded from safety-related interlock carriers and fuse bases unless the molder can demonstrate identical roving/glass length distribution and no cross-contamination with polyamide or polypropylene from other automotive lines. Standards governing this segment include ISO 6722-1:2011 for road-vehicle low-voltage cables with flame-propagation classification, LV 214 or OEM-specific terminal qualification for insertion/withdrawal force retention, and IEC 60068-2-14:2009 thermal shock testing for soldered terminal integrity. The production process often uses multi-cavity tools with sequential valve gates to prevent glass-fiber weld lines in the terminal latch region; fill analysis is run to maintain fill time between 1.5 s and 3.0 s to avoid premature gate freeze in long fuse-box frames, and hold pressure is set at 60–80% of injection pressure to limit post-mold warpage. Terminal product types include automotive relay bases, engine-compartment fuse-box brackets, connector position assurance frames, and glow-plug relay insulator carriers. Where published product-specific data for a given OEM validation protocol are unavailable, the molder should request batch-specific UL 94 and mechanical property data from the supplier before substituting regrind.
Competitive SABIC VALOX™ PBT+GF17%-FR DR48 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PBT+GF17%-FR DR48 is a flame-retarded, glass-fiber-reinforced polybutylene terephthalate injection-molding compound. The nominal glass-fiber content of 17% by weight positions the material between unfilled flame-retarded PBT and 30% glass-filled flame-retarded PBT in stiffness, melt viscosity, and molded-part flatness. Supplier documentation typically identifies the resin under the ISO designation PBT-GF17 FR, with the FR suffix indicating the flame-retardant modification. The grade is supplied in pellet form and is used for thin-wall electrical connectors, relay bases, switch housings, circuit-breaker components, low-voltage motor end caps, and appliance enclosures where dimensional repeatability, heat deflection, and flammability classification must be satisfied simultaneously. Before injection molding, desiccant-bed drying at 120 °C for 3–4 h is required to reduce moisture content to 0.02% or less by weight; a closed-loop dryer with −30 °C dew point or lower is necessary in plants where ambient relative humidity exceeds 60%. Residual moisture above the specified threshold promotes hydrolysis of the PBT ester linkages during plastication, causing measurable molecular-weight loss, surface splay, and reduced tensile strength. A hot-air tray dryer is generally insufficient because equilibrium moisture content remains above the target at typical molding-shop conditions.
Hydrolytic degradation is kinetically significant above 250 °C in the presence of moisture; the ester linkage scission rate increases with water concentration and residence time. A closed-loop desiccant dryer with a regeneration cycle capable of maintaining a dew point of −40 °C to −30 °C is preferred. If dried pellets are exposed to ambient air above 60% relative humidity for more than 30 min, they should be re-dried before processing. Melt strength at the nozzle may drop sharply when moisture content exceeds 0.03%, producing silver streaks and reduced tensile strength at weld lines. Hopper capacity should therefore be matched to consumption rate to avoid extended air contact.
Flame retardance is evaluated under UL 94 using IEC 60695-11-10 or ASTM D3801; the grade is normally listed as V-0 at 0.8 mm in the supplier’s published data. This thickness rating does not automatically confer 5VA or 5VB performance, because those classifications require plaque specimens of the end-use wall thickness with flame application of 500 W and a no burn-through criterion. For sections below 0.8 mm, published data for this specific configuration is limited; the actual molded thickness, gate location, glass-fiber orientation, and weld-line position influence flame performance and must be verified on the production tool. Comparative tracking index is determined under IEC 60112 with solution A; typical values reported for this grade fall in the 250–300 V band, which supports appliance and industrial-control insulation systems but does not by itself qualify for outdoor high-pollution tracking environments where 400 V or higher is specified. Volume resistivity is typically above 1 × 10^14 Ω·cm when conditioned and measured under IEC 62631-3-1; surface resistivity under IEC 62631-3-2 is typically above 1 × 10^15 Ω. Dielectric strength at 3.0 mm under IEC 60243-1 is generally reported in the 18–22 kV/mm range, with lower values expected at thinner sections or after moisture uptake.
| Property | Test method | Representative value |
|---|---|---|
| Flammability class | UL 94 / IEC 60695-11-10 | V-0 at 0.8 mm |
| Comparative tracking index | IEC 60112 | 250–300 V |
| Dielectric strength | IEC 60243-1 | 18–22 kV/mm at 3.0 mm |
| Volume resistivity | IEC 62631-3-1 | > 1 × 10^14 Ω·cm |
The mechanical response of the injection-molded grade is controlled by the 17% glass-fiber content and the crystallinity of the PBT matrix. Under ISO 527-2 at 5 mm/min, tensile stress at break is typically near 105 MPa, while elongation at break remains below 3%. Flexural modulus under ISO 178 is usually reported between 5500 MPa and 6500 MPa; this is lower than the 7500–8500 MPa range typical of 30% glass-reinforced flame-retarded PBT, but the lower glass loading reduces melt viscosity and transverse-flow shrinkage anisotropy. Notched Izod impact under ISO 180/1A at 23 °C is commonly in the 5–7 kJ/m² range, indicating moderate toughness and a need to avoid sharp internal corners, gate marks, and weld lines in load-bearing sections. Deflection temperature under load at 1.80 MPa, measured under ISO 75-2/Af, is approximately 200 °C; this supports short-term soldering or reflow profiles in connector assembly, but long-term heat-aging decisions must use the relative thermal index listed in the UL 746B yellow card rather than HDT alone. Linear thermal expansion parallel to flow is typically 4–6 × 10^−5 K^−1, with higher transverse values; the anisotropy produces differential shrinkage that must be compensated through mold cooling layout, gate position, and post-molding conditioning. Mold shrinkage values in supplier data are commonly 0.4–0.6% flow direction and 0.6–0.9% transverse. For insert-molded metallic contacts, the higher transverse shrinkage can create hoop stress around inserts; preheating the inserts to 120 °C and avoiding thick sections around the insert reduce the risk of delayed cracking.
Warpage is controlled less by absolute mold shrinkage than by differential shrinkage between flow and transverse directions. The 17% glass fiber reduces the difference compared with 30% glass-filled PBT but does not eliminate it; finite-element warpage analysis should use measured orthotropic shrinkage coefficients from a gate-specific mold-filling study. Cooling circuits with turbulent flow at 0.5–1.5 m/s coolant velocity and separate core/cavity temperature control are used to balance heat removal; mold temperature is normally maintained between 60 °C and 90 °C. Higher mold temperature improves crystallinity, reduces residual stress, and improves dimensional stability, but increases cycle time. For close-tolerance parts, post-molding annealing at 150 °C for 2 h may be performed to reduce molded-in stress and stabilize dimensions before assembly, although this operation changes crystallinity and can shift color slightly.
Processing is constrained simultaneously by flame-retardant dispersion and glass-fiber length retention. The recommended melt temperature is 240–265 °C, with a maximum of 270 °C; at higher melt temperatures the halogenated flame-retardant system can degrade and form acidic decomposition products. Injection speed for wall sections below 1.2 mm is typically set at 100–200 mm/s, and hold pressure is adjusted to maintain gate seal time of 3–5 s. Back pressure should remain below 0.5 MPa because higher back pressure raises residence time and produces additional fiber attrition; the resulting reduction in glass-fiber aspect ratio lowers flexural modulus after repeated molding cycles. A general-purpose screw with an L/D ratio of 20:1 to 22:1 and compression ratio of 2.2:1 to 2.8:1 is adequate for the melt viscosity at 250 °C and a shear rate of approximately 1000 s^−1. Shot size should be kept between 30% and 75% of barrel capacity to limit residence time; melt residence above 5 min at 265 °C can shift color and reduce flame-retardant efficacy. Regrind addition above 25–30% by weight introduces a measurable drop in melt viscosity because the recycled material contains shorter glass fibers; if the part relies on a UL 94 yellow card listing, the maximum regrind content in the recognition is commonly 30%, and higher levels require re-evaluation. Hot-runner systems should use externally heated manifolds with individual tip temperature control; a manifold temperature variation greater than ±5 °C across eight or more drops can create resin stagnation, streaking, and local flame-rating drift. Multi-cavity tools with cavity-to-cavity filling imbalance above 5% produce pack-pressure variation that shifts flame performance at thin ribs. Clamp force should be selected using 5–8 kN/cm² of projected part area; insufficient clamp force at high injection pressure creates flash that reduces effective wall thickness and can compromise parting-line flame performance.
Melt volume-flow rate under ISO 1133-1:2022 at 250 °C and 2.16 kg is typically reported in the 15–25 cm³/10 min range; this moderate flow provides adequate fill in thin walls but requires higher injection pressure than unfilled flame-retarded PBT. The nozzle temperature is usually maintained at 245 °C, while the first barrel zone from the hopper may be set at 220 °C to avoid bridging, with center zones at 250–260 °C. Screw rotation speed is typically 80–120 rpm for a screw diameter of 40 mm; higher speeds may generate excessive shear heat and degrade the flame-retardant additive.
For unattended appliance applications under IEC 60335-1, glow wire flammability index is tested under IEC 60695-2-12 and glow wire ignition temperature under IEC 60695-2-13. Typical PBT-GF17 FR compounds of this class exhibit glow wire ignition temperatures in the 750–775 °C band at 1.0 mm, but exact results depend on wall thickness, colorant chemistry, and moisture conditioning. Designers should verify that the listed glow wire ignition temperature exceeds the minimum specified in the end-product standard; if the requirement is 775 °C or higher, a thicker wall section or alternative grade may be required. The material also carries a UL 746A yellow card listing relative thermal index values for electrical, mechanical-with-impact, and mechanical-without-impact properties; these values are obtained from long-term oven-aging programs and should replace short-term HDT for continuous-use temperature assignment. Published data for this specific configuration is limited for some colorants and thicknesses, so production-machine plaques and molded parts should be tested when the application is safety-critical. The combination of moderate tracking resistance and flame retardance makes the grade appropriate for enclosed low-voltage compartments, but not for applications requiring simultaneous 400 V tracking resistance and 5VA flame classification without additional design margins.
Regulatory documentation is normally available through the supplier’s compliance portal. The grade is typically certified against RoHS Directive 2011/65/EU and REACH substance-of-very-high-concern restrictions, but certification must be confirmed by lot number because additive suppliers and colorants can vary. Electrical-contact applications may also require IEC 61249-2-21 or end-product IEC 60664-1 clearance and creepage verification; the comparative tracking index of 250–300 V supports material group II in many insulation-coordination calculations. For flow lengths above 100 mm at wall thickness below 1.0 mm, filling simulations with measured melt viscosity from capillary rheometry under ISO 11443 are preferable to spiral-flow approximations.
For snap-fit assembly, strain at the snap arm must remain below the lower-bound elongation of 3%; using insert tooling to produce radiused root details increases allowable deflection. Because the material has low ductility, assembly should occur at room temperature after moisture conditioning to equilibrium; cold parts below 10 °C show increased brittleness. The flammability rating and mechanical properties are affected by weld lines; under dynamic loading, weld-line strength is often 50–70% of the parent material strength, so gate placement should keep weld lines away from snap arms and sealing surfaces.
Relative to other SABIC VALOX materials, the 17% glass-fiber loading in DR48 defines a specific processing and property envelope. Unfilled flame-retarded PBT typically has flexural modulus below 3000 MPa and higher elongation, but its heat deflection temperature is lower and warpage in large flat parts can be more difficult to control. At the opposite end, 30% glass-reinforced flame-retarded PBT grades provide higher stiffness but raise melt viscosity, gate pressure, and transverse-flow shrinkage anisotropy; in multi-cavity connectors with long flow lengths, the lower glass content of DR48 improves fill balance and reduces core-pin deflection. The density of the reinforced grade is higher than unfilled PBT; the difference must be accounted for in part mass and screw recovery calculations. Because DR48 contains a halogenated flame-retardant system, processing equipment that also runs unhalogenated materials should be purged to prevent cross-contamination, and vent gases should be captured to avoid exposure to acidic decomposition products if the melt exceeds 270 °C. Chemical resistance follows general PBT behavior: aromatic hydrocarbons, alcohols, esters, and aliphatic hydrocarbons are usually compatible at room temperature, while hot water above 60 °C, strong acids, strong bases, and ketones can produce surface attack or hydrolysis. For alkaline cleaning solutions or long-term hot-water exposure, published data for this specific configuration is limited; immersion tests under ASTM D543 should be performed with the target fluid before specification. Compared with glass-reinforced polyamide, the grade offers faster crystallization, lower moisture absorption, and better dimensional stability in humid environments, but lower ultimate elongation and resistance to hot-water hydrolysis. The lower water absorption of PBT, typically below 0.1% at 23 °C and 50% relative humidity under ISO 62, means that electrical properties remain more stable than polyamide grades in humid applications; however, at temperatures above 60 °C and high humidity, PBT hydrolysis remains a limit. Since the glass reinforcement introduces notch sensitivity, stress concentrations at gate marks, weld lines, and ejector pins should be assessed by notched impact testing rather than smooth tensile data alone.