| HS Code | 199119 |
| Density | 1.53 g/cm3 |
| Glassfibercontent | 17% |
| Polymertype | PBT |
| Flameretardant | Yes |
| Tensilemodulus | 7000 MPa |
| Tensilestrength | 95 MPa |
| Elongationatbreak | 2.5% |
| Flexuralmodulus | 6200 MPa |
| Flexuralstrength | 145 MPa |
| Notchedizodimpactstrength | 50 J/m |
| Heatdeflectiontemperature 1 82mpa | 195 °C |
| Heatdeflectiontemperature 0 45mpa | 210 °C |
| Ul94flammabilityrating | V-0 |
| Waterabsorption | 0.07% |
| Moldingshrinkage | 0.3-0.6% |
| Dielectricstrength | 20 kV/mm |
| Volumeresistivity | 1E15 ohm·cm |
As an accredited SABIC VALOX™ PBT+GF17% 855 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT+GF17% 855 is packaged in 25 kg moisture-barrier bags, stacked on pallets for industrial shipment. |
| Container Loading (20′ FCL) | 20′ FCL loading of SABIC VALOX™ PBT+GF17% 855 in palletized packaging, securely stowed and braced for export shipment. |
| Shipping | SABIC VALOX™ PBT+GF17% 855 is shipped as dry resin pellets in sealed 25 kg bags, palletized and shrink-wrapped. Store/transport in a cool, dry, ventilated area away from direct sunlight, moisture, and heat. Avoid punctures and bag damage; keep containers closed. Handle according to SDS; normal industrial freight applies. |
| Storage | Store SABIC VALOX™ PBT+GF17% 855 in original, sealed containers in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, moisture, and incompatible materials such as strong oxidizers. Keep containers closed when not in use, avoid dust generation, use proper grounding, and follow the SDS and local regulations. Do not store near food or drinking water. |
| Shelf Life | SABIC VALOX™ PBT+GF17% 855 typically has a two-year shelf life when stored dry in original, unopened packaging under recommended conditions. |
Molded-case circuit breaker frames, terminal block housings, and relay bases processed from SABIC VALOX™ PBT+GF17% 855 exhibit a datasheet-rated flame performance of UL 94 V-0 at 0.75 mm, but the controlling regulatory boundary in end use is not the material listing alone; IEC 60898-1 and IEC 60695-2-11 impose additional glow-wire verification on the finished insulating part, with testing commonly required at 850°C for auxiliary circuits or at 960°C for current-carrying parts above 0.2 A in unattended equipment. The formulation addition ratio for these thin-wall insulating parts is held at 100 wt% virgin VALOX™ 855 when the part is molded at wall sections below 1.0 mm; regrind generated from sprue and runner systems is introduced only after passing a sieve with 2.0 mm mesh and is limited to 15 wt% of the total shot mass because repeated thermal histories fragment the glass-fiber length distribution and shift the UL 94 margin at the thinnest section. Downstream production uses a reciprocating-screw injection molding machine with a screw L/D ratio of 18:1 to 20:1, a compression ratio of 2.0:1 to 2.2:1, and a non-return ring clearance maintained below 0.05 mm to prevent stagnation of flame-retardant decomposition products. Pre-drying is executed at 120°C for 3–4 hours in a desiccant dryer with a dew point of -30°C or lower, targeting maximum residual moisture of 0.02 wt% before melt entry; moisture above this threshold produces surface splay and hydrolysis-induced molecular weight loss at the melt temperature of 245–260°C. Barrel temperature profiles should maintain the front zone no higher than 260°C, and total residence time should remain below 5 minutes, because the flame-retardant package will otherwise begin to release by-products that corrode hot-runner tips and produce visible silver streaks on black or dark-grey parts. Injection speed is set in the moderate range to fill 0.8–1.2 mm walls without jetting; packing pressure is held at 40–70 MPa for 1.5–3 seconds per mm of wall thickness, and mold temperature is maintained at 65–90°C to promote surface finish and dimensional accuracy. Terminal finished product types produced under these conditions include miniature circuit breaker internal partitions and arc-chute side plates, DIN-rail terminal block insulating bodies, relay base sockets, contactor arc covers, and current transformer coil formers. The main process conflict is the narrow window between freeze-off in thin ribs and thermal degradation in thick bosses; mold designs should avoid abrupt wall thickness transitions greater than 1.5:1 and should place gates at the greatest nominal wall section to permit continuous packing. Published data for glow-wire ignition temperature on VALOX™ 855 at specific wall thicknesses should be verified against the current SABIC UL Yellow Card because the result varies with color, glass content, and regrind level.
A 17% glass-fiber loading positions VALOX™ 855 between unreinforced PBT and 30% glass-reinforced PBT, which is significant for automotive electrical distribution because the lower fiber content reduces notch sensitivity and weld-line weakness in multi-pin connector bodies while retaining enough stiffness to prevent terminal retraction under lateral load. Industry compliance for engine-compartment connector housings, fuse boxes, and relay sockets is commonly anchored to USCAR-2 class 3 temperature and humidity cycling, ISO 6722-1 for 48 V board-net voltage classes, and OEM-specific LV214 contact-retention sequences; material acceptance usually requires a UL 94 V-0 at 0.75 mm listing and a UL 746B relative thermal index sufficient for continuous exposure at 125°C, although the exact RTI value must be confirmed against the current SABIC Yellow Card for the selected color. The formulation addition ratio in critical connector bodies remains 100 wt% virgin VALOX™ 855 because regrind shortens the fiber length distribution and lowers elongation at break, which directly influences terminal insertion and extraction forces; where regrind is permitted on non-sealed, non-current-carrying clips or brackets, the maximum documented addition is 10–15 wt% of shot weight, and only after melt-flow ratio verification per ISO 1133-1:2022 shows a shift of less than 10% from virgin material. The downstream production process for automotive connectors is dominated by multi-cavity hot-runner injection molding with valve-gate sequencing, requiring mold temperatures at the upper end of the recommended range, typically 80–90°C, to delay crystallization at the gate and reduce frozen-in orientation at the weld line. Pre-drying remains mandatory at 120°C for 3–4 hours to a moisture level below 0.02 wt%; after drying, material should be conveyed in closed loops because PBT reabsorbs moisture rapidly above 40% relative humidity. Barrel melt temperature is held between 245°C and 260°C, with the nozzle slightly below the front zone to avoid drooling; residence time in the hot runner should be below 10 minutes at start-up and below 5 minutes during production interruptions to preserve the flame-retardant package and prevent black specks from degraded material. Finished product types produced from this compound include automotive fuse and relay boxes underhood, battery management system connector housings, power distribution center insulators, ECU connector shields, and electric power steering sensor bodies. A documented process limitation arises in geometries with long finger-like terminal cavities: if the cavity wall drops below 0.6 mm, glass-fiber packing is insufficient to maintain terminal retention after thermal aging, and published data for this specific configuration is limited; flow simulation should be validated with short-shot trials before release.
In unattended appliance current-carrying insulating parts, IEC 60335-1 clause 30.2 transforms the material-level UL 94 V-0 listing into an end-product glow-wire requirement, usually 850°C for components that carry current above 0.2 A and are not supervised during operation, and 775°C for parts that merely retain connections. VALOX™ PBT+GF17% 855 enters this class of parts at 100 wt% virgin compound, with color masterbatch or titanium dioxide pigment concentrate limited to 1.0–2.0 wt% using a PBT carrier; higher pigment loadings dilute the flame-retardant package and reduce the glow-wire endurance, especially in white or light-colored molded bodies where the required end-product ignition time is more difficult to sustain. Downstream processing for appliance structural parts such as hair dryer inlet grilles, straightener internal frames, electric kettle base shells, coffee machine internal brackets, and fan shrouds uses conventional injection molding with mold temperatures between 70°C and 85°C to balance crystallization speed and surface gloss; textured cavity surfaces are preferred because the glass-fiber phase becomes visible on polished tools after only 2,000–5,000 cycles as tool wear increases. Pre-drying at 120°C for 3–4 hours to 0.02 wt% maximum moisture is required before molding, and any interruption longer than 30 minutes in humid environments above 50% RH should be followed by a re-drying step or a hopper blanketing system with dry air. The melt temperature should remain in the 245–260°C window; excursions above 270°C cause visible surface streaking on textured surfaces and leave deposits on cavity vents that increase maintenance frequency. Packing pressure, hold time, and gate freeze-off must be controlled together to avoid sink marks at rib intersections; thick bosses below the joint line are gated at the base and packed at 50–80 MPa, while thin grille ribs are filled fast at 80–120 mm/s ram speed to prevent premature glass-fiber freeze-off. The principal operational boundary is that VALOX™ 855 is not recommended for direct contact with exposed heating elements above its continuous-use temperature; applications such as hair dryer outlet grilles require an air-gap or metallic heat shield because the PBT matrix softens and loses structural modulus under continuous radiant load, even though the part does not ignite in a standard glow-wire test. Published data for mixed-color regrind effects on IEC 60335-1 glow-wire outcomes is limited; therefore process validation should use molded plaques at the lowest wall thickness of the final part before releasing regrind into current-carrying enclosure components.
When solenoid coil encapsulation and sensor-body molding require a flame-retardant PBT with a 17% glass-fiber skeleton, the addition ratio is held at 100 wt% virgin VALOX™ 855 for coils embedded in molded bodies because regrind variation in moisture absorption and volatile content creates dielectric voids and interfacial adhesion loss on copper windings. If regrind is allowed for non-encapsulated covers or mounting brackets, it is limited to 10 wt% of the shot mass and must be processed within 24 hours of drying to prevent moisture regain above 0.02 wt%. Industry compliance for these parts is anchored to IEC 61010-1 for measurement, control, and laboratory-use equipment, UL 429 for solenoid valves in specific markets, and IEC 60079-0 only for mechanically supported anti-static housings when the device is not the primary explosion-containment boundary. The downstream process is usually insert molding on a vertical injection machine with a shuttle or rotary table, where the operator fixture preheats copper wound inserts to 90–110°C before overmolding to prevent early freeze-off of thin walls around the copper surface and to reduce thermally induced wire breakage. Mold temperature is maintained at 75–90°C, and barrel temperature at 245–260°C, with a low-shear screw of 20:1 L/D and a reverse-tapered barrel design to minimize dead spots. Injection is profiled with a first-stage slow melt front to encapsulate the coil without displacing the winding, followed by a second-stage velocity increase to fill the outer shell; maximum injection pressure is typically held below 100 MPa to avoid insert deformation. Sensor-body production, including proximity sensor housings and fieldbus I/O module shells, often uses the same grade but without insert preheating; the mold is instead run at the higher end of the recommended range to permit fiber wet-out and to reduce visible glass-fiber lift on flat sealing surfaces. Terminal finished product types include solenoid coil encapsulated bodies for pneumatic and hydraulic valves, linear actuator end caps, industrial proximity sensor bodies, rotary encoder housings, and signal isolator enclosures. The process conflict documented on production lines is that shorter glass fibers fractured by regrind produce a measurable reduction in weld-line strength across the coil window, and the flame-retardant package can plate out on the mold surface when the barrel is kept hot during prolonged idle; if idle exceeds 5 minutes, the barrel temperature should be lowered to 230°C or the screw should be purged to avoid black speck contamination.
The outdoor enclosure candidate pool for photovoltaic junction boxes, combiner terminal brackets, and diode carrier plates includes VALOX™ PBT+GF17% 855 only when the selected black formulation carries a UL 746C f1 outdoor-suitability listing for ultraviolet exposure and water immersion, because the unfilled or lighter-color versions of PBT may fail to retain impact strength after sustained UV exposure. Industry compliance for the finished junction box is derived from IEC 62790 for box-level thermal, mechanical, and electrical tests, and from UL 746C f1 for the polymeric material itself; the material must also maintain a UL 94 V-0 at 0.75 mm rating and a comparative tracking index sufficient for the creepage distances designed into the enclosure, with the exact CTI value verified against the current UL Yellow Card because glass-reinforced flame-retardant PBT grades can sit near the boundary between CTI 175 V and 250 V. The formulation addition ratio is 100 wt% VALOX™ 855 with a carbon black masterbatch at 1.0–1.5 wt% using a PBT-compatible carrier; outdoor-stabilized UV additive packages are permissible but must not exceed 2.0 wt% total non-flame-retardant additive loading because every additional non-PBT phase dilutes the UL 94 flame and drip margin at the thinnest wall. Downstream processing for photovoltaic junction boxes uses a medium-size injection molding machine with a dry-air hopper, pre-drying at 110–120°C for 3–4 hours to 0.02 wt% moisture, and a melt temperature held between 240°C and 255°C to minimize thermal degradation of the outdoor stabilization package. Mold temperatures of 70–85°C produce the low-warpage top cover and base plate needed for gasket sealing; gate placement on the base plate should direct the melt flow away from screw bosses to avoid glass-fiber orientation that produces radial warpage and leaks at the gasket groove. The process restriction in outdoor enclosures is that the molded part must be produced without regrind unless the outdoor-suitability listing explicitly covers regrind content; if regrind is used at all, the maximum documented addition is 10 wt% and only for non-load-bearing internal brackets that are not exposed to direct UV. Terminal finished product types include IP65 photovoltaic junction box bases and lids, diode mounting plates, combiner box terminal brackets, microinverter housing covers, and quick-disconnect connector bodies for rooftop arrays. Published data for VALOX™ 855 under IEC 62790 combined damp-heat and thermal cycling is limited for custom formulations, so initial production trials should include a rib-thickness gradient plate to confirm post-aging dimensional stability before mold transfer.
| Standard | Designation / test | Release criterion |
|---|---|---|
| UL 94 | Flame class at 0.75 mm | V-0 |
| UL 746C | f1 outdoor suitability | Black formulation only |
| IEC 62790 | Junction box thermal cycling | No crack, no live part exposure |
| IEC 60695-2-11 | Glow-wire end product | Ignition temperature per product class |
Lighting ballast enclosures, creepage-path brackets, and GU10 socket bodies combine electrical insulating function with dimensional precision inside compact LED and fluorescent luminaires, and VALOX™ PBT+GF17% 855 provides a UL 94 V-0 at 0.75 mm baseline that is then verified in the finished luminaire assembly under IEC 60598-1 and UL 8750. Industry compliance for lampholder and ballast enclosure materials includes IEC 60695-2-11 glow-wire tests at 850°C for parts sustaining current, IEC 60112 tracking resistance to ensure creepage distances remain stable after dust and moisture accumulation, and IEC 61347-1 for lamp controlgear where the plastic is used as the outer non-live cover. The formulation addition ratio remains 100 wt% virgin VALOX™ 855 for thin-walled lamp socket bodies; regrind from the runner system is limited to 15 wt% for non-current-carrying mounting brackets and must be sorted to remove burnt material from hot-runner start-up. Downstream production uses injection molding with mold temperatures between 65°C and 80°C, depending on texture depth, because deep textures require higher mold temperature to reproduce the cavity detail while maintaining ejection without drag marks. Pre-drying follows the same 120°C for 3–4 hours sequence to 0.02 wt% moisture, and in humid production areas above 60% RH the machine hopper should be covered with a dry-air sweep or the material should be fed directly from the dryer through a closed tube. Melt temperature is held at 245–255°C to limit yellowing in natural or white variants; if the barrel temperature exceeds 265°C for more than 5 minutes, the melt begins to discolor and the molded part may exhibit reduced weld-line strength at pin-gate locations. Terminal finished product types produced from VALOX™ 855 in lighting include GU10 and GZ10 socket bodies, LED driver enclosure end caps, fluorescent ballast housings, terminal block covers within luminaires, and emergency power pack enclosures. The main operational boundary is the mating of shrink-fit metal shells and plastic socket bodies: the external metal shell should not be inserted while the plastic is above its glass transition, and post-mold annealing at 80–100°C for 1–2 hours is sometimes applied to stabilize dimensions before ultrasonic welding, though the published data for ultrasonic weld strength on this specific grade is limited and must be established by horn-frequency trials on the actual part.
Competitive SABIC VALOX™ PBT+GF17% 855 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Melt-phase integrity depends on temperature, residence time, and shear history. A melt-temperature setpoint below 245°C may leave partially unmelted fiber bundles and reduce packing at thin-wall sections, while a flat-temperature profile above 260°C accelerates chain scission through ester interchange and oxidative degradation. In hot-runner systems, the manifold temperature should not exceed 270°C, and the residence interval at melt temperature should be kept below 5 min. Start-up purging should use a thermally stable commercial purge compound rather than PVC or acetal-based materials, whose acidic decomposition products can attack the PBT ester linkage. Machine shutdown should not leave molten PBT in the barrel above 260°C for extended periods; barrel inventory should be purged or reduced before power-off.
Screw geometry for glass-filled PBT should use a low-compression, wear-resistant screw with an L/D ratio between 18:1 and 22:1. The non-return valve, barrel, and screw tip require hardened surfaces for glass-fiber service. Back pressure is typically set between 0.3 MPa and 0.7 MPa, while screw surface speed should remain within 0.1–0.3 m/s to limit fiber breakage. If pressure-limited injection occurs at thin sections, the gate should be widened or the pressure profile revised rather than raising melt temperature beyond the stated ceiling. Published data for spiral-flow length in this exact 17% glass-fiber configuration is limited; therefore flow behavior should be established on the intended tool with short shots rather than inferred from generic PBT-GF30 viscosity parameters.
A desiccant-bed or desiccant-wheel dryer with a supply dew point no higher than -40°C is the minimum practical system when ambient relative humidity exceeds 60%. PBT hydrolyzes at melt temperatures in the presence of free moisture; the reaction attacks ester bonds and lowers molar mass, producing surface splay, brittle gate regions, and reduced notched impact strength. Pre-drying at 120°C for 4 h in a properly sized hopper is the standard reference condition after open storage. Hopper configuration should provide mass-flow discharge, and pellet moisture should be verified with a Karl Fischer coulometer or an equivalent method aligned to ISO 15512; hopper probes that measure air dew point do not measure pellet moisture. Regrind addition changes particle-size distribution and can reintroduce moisture. If regrind is used, it should be limited to 30 wt%, derived from clean dried runner systems, and blended consistently to avoid feed segregation.Shrinkage in glass-reinforced PBT is anisotropic because fiber orientation develops along the melt-flow direction during injection. Mold-shrinkage specimens evaluated under ISO 294-4 typically show lower shrinkage parallel to flow and higher shrinkage transverse to flow. For a 17 wt% glass-fiber PBT class, the difference between flow-direction and cross-flow shrinkage can fall between 0.3% and 0.8%, depending on gate geometry and packing pressure. This differential produces warpage in flat plates unless gate location, wall thickness, and hold-pressure profile are balanced. Weld lines are a controlling limitation in multi-gate tools: fiber orientation at the weld line is perpendicular to the fill front, so local tensile and notched impact strength may decrease by 30–50% relative to a continuous fiber-oriented ligament. Moving the weld line to a low-stress region with valve-gated hot runners or sequential valve timing is more effective than increasing packing pressure after the melt fronts meet.
Mold temperature should be held between 60°C and 90°C to control crystallinity and reduce post-mold dimensional drift. Because semicrystalline PBT continues to crystallize after demolding, dimensional inspection is preferably delayed for 24–48 h after molding. For applications with tight flatness tolerances, tooling should include gate-balancing simulations and pilot-run shrinkage verification rather than relying on generic PBT mold-shrinkage tables.
The 17 wt% glass-fiber level occupies an intermediate position in the property envelope. Relative to unfilled PBT, the grade has higher density, higher tensile and flexural modulus, lower elongation at break, and higher heat deflection temperature at 1.8 MPa. Relative to a 30 wt% glass-filled PBT grade such as VALOX 420SEO, the present compound has lower melt viscosity, better thin-wall fill, lower density, and less severe screw and tool wear, but also lower tensile and flexural modulus and lower notched impact strength. The 17% fiber fraction reduces anisotropy compared with 30% fiber loading while retaining sufficient stiffness for semi-structural parts. The grade is not a direct substitute for flame-retarded VALOX grades if the application requires UL 94 V-0 at the same thickness; this grade is normally classified as UL 94 HB unless a specific lot is certified otherwise.
The table below provides behavioral ranges documented in public technical literature for dry-as-molded commercial grades; the ranges are not certified lot limits for any single SABIC production batch.
| Parameter | Unfilled PBT | PBT+GF17% class | PBT+GF30% class | Test method |
|---|---|---|---|---|
| Density (g/cm³) | 1.30–1.32 | 1.40–1.44 | 1.51–1.56 | ISO 1183-1 |
| Tensile modulus (GPa) | 2.4–2.8 | 5.2–6.5 | 8.5–10.0 | ISO 527-2 |
| Notched Charpy impact (kJ/m²) | 3.0–5.0 | 4.0–6.0 | 6.0–9.0 | ISO 179-1/1eA |
| HDT/A at 1.8 MPa (°C) | 50–60 | 170–190 | 200–215 | ISO 75-2 |
| Mold shrinkage flow/cross-flow (%) | 1.6–2.0 / 1.8–2.2 | 0.3–0.5 / 0.6–1.0 | 0.2–0.4 / 0.4–0.7 | ISO 294-4 |
Compliance statements should be anchored to the following methods and designations:
| Requirement | Method / designation |
|---|---|
| Material identification | ISO 1043-1 / PBT-GF17 |
| Density | ISO 1183-1 |
| Tensile properties | ISO 527-2 / ASTM D638-14 Type I |
| Flexural properties | ISO 178 |
| Notched impact | ISO 179-1/1eA / ASTM D256 |
| Heat deflection temperature | ISO 75-2 method A / ASTM D648-18 |
| Melt-volume rate | ISO 1133-1 |
| Mold shrinkage | ISO 294-4 |
| Flammability classification | UL 94 at specified thickness |
| Long-term thermal aging | UL 746B / ISO 2578 |
| Moisture content verification | ISO 15512 method A |