Sabic Valox Pbt Gf15 Non Cl Br Fr Enh4530

SABIC VALOX™ PBT+GF15% Non-Cl/Br FR ENH4530

    • Product Name: SABIC VALOX™ PBT+GF15% Non-Cl/Br FR ENH4530
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 860084
    Manufacturer SABIC
    Trade Name VALOX
    Grade ENH4530
    Polymer Type PBT
    Glass Fiber Content 15%
    Flame Retardant System Non-chlorinated/non-brominated
    Flammability Rating UL94 V-0
    Density 1.53 g/cm³
    Tensile Modulus 5500 MPa
    Tensile Stress At Break 100 MPa
    Tensile Strain At Break 2.5%
    Flexural Modulus 5500 MPa
    Flexural Strength 150 MPa
    Notched Charpy Impact Strength 5 kJ/m²
    Hdt At 1 8 Mpa 190 °C
    Hdt At 0 45 Mpa 200 °C
    Vicat Softening Temperature 210 °C
    Mold Shrinkage 0.3-0.6%
    Water Absorption 0.05%
    Processing Method Injection Molding

    As an accredited SABIC VALOX™ PBT+GF15% Non-Cl/Br FR ENH4530 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ ENH4530 is supplied in 25 kg moisture-proof bags, 40 bags per pallet (1,000 kg net), with labels and safety documentation.
    Container Loading (20′ FCL) 20′ FCL container loading for SABIC VALOX™ PBT+GF15% Non-Cl/Br FR ENH4530: palletized bags, secure stowage, compliant labeling, and moisture protection.
    Shipping Shipping description: Non-hazardous polymer resin pellets; not regulated as dangerous goods (no UN number, proper shipping name, hazard class, or packing group). Pack in sealed moisture-barrier bags/containers at ambient temperature, protected from moisture, contamination, direct sunlight, and excessive heat. Provide SDS with shipment and follow local regulations.
    Storage Store SABIC VALOX™ PBT+GF15% Non-Cl/Br FR ENH4530 in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and oxidizing materials. Keep in original sealed packaging, palletized, and protected from moisture, dust, and contamination. Avoid prolonged UV exposure. Observe good housekeeping and use appropriate PPE when handling. Maintain stable ambient temperature; rotate stock per supplier guidance.
    Shelf Life Store in a cool, dry place in original sealed packaging; typical shelf life is 12 months from date of manufacture.
    Application of SABIC VALOX™ PBT+GF15% Non-Cl/Br FR ENH4530

    VALOX™ ENH4530, a 15 wt% glass-fiber-reinforced PBT grade with a non-brominated/non-chlorinated phosphorus-based flame-retardant system, is conveyed from a desiccant-bed dryer set at 120°C for 3–4 h until the residual moisture measured by ISO 15512:2019 falls below 0.02 wt%; this threshold is maintained because the flame-retardant package hydrolyzes above this moisture concentration during plasticating, generating plate-out on cavity surfaces and reducing UL 94 V-0 performance at 1.5 mm. On hydraulic injection-molding machines with a 25 mm single-stage screw and 20:1 L/D ratio, the melt temperature is controlled at 250–270°C and the tool surface at 60–90°C; screw back pressure is set to 0.3–0.5 MPa and decompression is limited to 2–3 mm before melt recovery to prevent air entrapment and thermal yellowing. The formulation addition ratio for arc-chamber components and barriers is 100 wt% virgin VALOX ENH4530, while non-tracking terminal covers incorporate no more than 10 wt% regrind after three consecutive molding and granulation cycles; carbon-black masterbatch is metered at 0.5–0.8 wt%. Finished parts produced under this processing window include miniature circuit-breaker housings, arc shields, residual-current device base frames, and terminal covers. Conformity is assessed against IEC 60947-1, IEC 60898-1, UL 489, IEC 60695-2-11 at 850°C glow-wire exposure, and UL 94 V-0 at 1.5 mm; tracking performance is verified by IEC 60112, with creepage-distance calculation conducted under IEC 60664-1.

    Where Does IEC 62196-2 Contact Retention Meet Phosphorus-Based FR Thermal Decomposition?

    For alternating-current charging connector bodies and contact carriers, VALOX ENH4530 is processed in the upper melt-temperature range of 260–275°C to fill 0.8–1.0 mm wall sections around brass contact sleeves, with the hot-runner manifold held at 250–260°C and the mold at 70–90°C. The formulation addition ratio is 100 wt% virgin material for contact carriers that must retain spring-cage insertion force over 10,000 mating cycles under IEC 62196-2; regrind is permissible only in outer shell components at ≤15 wt% after the reground fraction has passed 200 h damp-heat exposure at 85°C/85% RH per IEC 60068-2-78 without loss of UL 94 V-0 rating at the specified 0.75 mm wall section, provided that thickness is covered by the grade's UL Yellow Card. Color masterbatch is added at 0.8–1.2 wt% using a carrier that does not reduce the IEC 60112 comparative tracking index used for creepage-distance calculation under IEC 60664-1. Processing on a valve-gated hot-runner system imposes a barrel residence-time limit of 5 min; prolonged exposure above 275°C accelerates decomposition of the non-halogen FR package, visible as gas bubbles at vent pins and plate-out on core pulls. Finished product types include wallbox plug housings, in-cable control box enclosures, contact carriers, locking sleeves, and charging-inlet mounting frames. Compliance is assessed under IEC 61851-1, IEC 62196-2, UL 2251, UL 94 V-0, IEC 60695-2-11 at 850°C, and dielectric withstand is verified by IEC 60243-1 at the minimum insulated wall thickness.

    Under-Hood Connector Retention, Hot-Oil Ageing and Dimensional Stability

    Under-hood connector housings produced from VALOX ENH4530 are insert-molded around 0.64 mm brass terminals on vertical or horizontal injection presses with 100–180 t clamp force; the melt temperature is controlled at 250–265°C and the tool at 80–100°C to maintain post-mold terminal-insertion retention force specified by USCAR-2. The formulation addition ratio for thin-wall engine-compartment parts is 100 wt% VALOX ENH4530, with in-line regrind limited to 20 wt% only after the reground fraction has been re-dried to below 0.02 wt% and validated after 1,000 h engine-oil immersion at 125°C according to ISO 16750-5; no additional glass fiber is compounded because raising the total glass content above the supplied 15 wt% reduces weld-line elongation at wall sections below 1.0 mm. The downstream molding process uses high-speed injection at 150–250 mm/s with cavity gas venting and a post-fill holding pressure of 60–100 MPa; uncontrolled fiber orientation at the weld line opposite pin gates reduces weld-line tensile strength relative to the gate area, requiring gate-position simulation before tool construction. Finished products include engine-control-unit connectors, camshaft-position sensor housings, intake-air temperature sensor shells, fuse-box brackets, and ignition coil bobbins. Conformity is assessed under USCAR-2, ISO 16750-5, and RoHS Directive 2011/65/EU Annex II; published data for long-term coolant exposure in glycol-based media at temperatures above 120°C for this specific non-halogen FR PBT configuration are limited, so coolant-contact applications require component-level approval.

    When relay bobbins are wound with 0.2–0.5 mm enameled copper wire and subsequently encapsulated, the molded VALOX ENH4530 surface must retain dielectric withstand after winding tension and epoxy potting; the pellets are dried at 120°C for 3–4 h to below 0.02 wt% moisture and molded at a melt temperature of 250–270°C with a tool temperature of 60–90°C. The formulation addition ratio for coil formers used in miniature PCB relays is 100 wt% virgin VALOX ENH4530, because regrind above 10 wt% has been associated with microcrack formation in the thin core wall after winding and solvent-based flux exposure; in non-wound motor end caps, regrind is permitted up to 20 wt% with 0.5–1.0 wt% carbon-black masterbatch for laser marking. Downstream processing uses multi-cavity tools with pinpoint gates and post-molding annealing at 120°C for 1 h to relieve molded-in stress before winding; cavity pressure is held at 80–110 MPa, and screw rotation is limited to 60–120 rpm to avoid fiber-length reduction that lowers flexural modulus below the value required for coil support. Terminal finished product types include PCB relay bobbins, contactor coil formers, solenoid coil shells, stepper-motor end caps, and electromagnetic valve coil bases. Compliance is assessed under IEC 61810-1, IEC 60730-1, UL 429, and thermal endurance classification according to UL 746A relative thermal index values assigned in the grade's UL file; electrical breakdown is verified by IEC 60243-1 at the minimum wall thickness after conditioning for 24 h at 23°C and 50% RH.

    DIN Rail Terminal Housings Demand a Narrow Back-Pressure Window

    DIN rail terminal bodies molded from VALOX ENH4530 are processed with a melt temperature of 250–270°C, a tool temperature of 70–90°C, and a screw back pressure of 0.3–0.5 MPa; back-pressure settings above 0.5 MPa produce excessive fiber breakage in the recirculation zone and reduce notched Izod impact strength measured by ISO 180/1A relative to the datasheet typical value. The formulation addition ratio for standard terminal housings is 100 wt% virgin material or a maximum 20 wt% of re-dried in-house regrind that has passed the same IEC 60112 tracking test as the virgin lot; terminal body sections requiring a comparative tracking index of ≥300 V under IEC 60664-1 are limited to 10 wt% regrind, and black masterbatch is metered at 0.5–1.0 wt%. Downstream production occurs in 16- to 64-cavity hot-runner tools with vent depths of 0.015–0.025 mm; insufficient venting at end-fill positions produces diesel ignition marks and local charring that are unacceptable under IEC 60695-2-11 at 850°C glow-wire testing. Finished products include feed-through terminal housings, fuse-terminal bodies, relay socket bases, sensor-actuator terminal blocks, and neutral disconnect terminal housings. Compliance is assessed under IEC 60947-7-1, UL 1059, IEC 60112, and IEC 60695-2-11; export documentation typically requires verification against RoHS Directive 2011/65/EU Annex II and REACH Regulation (EC) No 1907/2006.

    When Charger Housings Must Balance Impact Modification and Glow-Wire Compliance

    For power-tool charger enclosures and industrial adapter front panels, VALOX ENH4530 is injection-molded at a melt temperature of 250–270°C and a tool temperature of 60–80°C; the lower tool temperature is used when surface gloss variation must be limited on textured cavity surfaces, but this reduces melt flow at wall thicknesses below 1.2 mm and may require an increase in injection speed rather than melt temperature. The formulation addition ratio is 100 wt% virgin grade for thin-wall charger bases that must pass a 0.5 m drop test per IEC 60068-2-31; up to 20 wt% regrind is permitted only in thick-walled body shells where the notched Izod impact strength measured by ISO 180/1A remains above the value measured on virgin moldings after 500 h thermal ageing at 85°C. Color masterbatch is added at 0.8–1.2 wt%; increasing pigmentation above 2.0 wt% has been associated with inconsistent glow-wire results due to local changes in surface thermal conductivity. Downstream processing uses open-nozzle machines without hot-runner manifold dead spots to limit residence time to 4 min or less; after molding, parts are annealed at 100°C for 1 h where machining or ultrasonic welding is performed. Terminal finished products include power-tool charger housings, power-adapter enclosures, industrial battery-charger front panels, and cordless-tool battery-charger base plates. Compliance is tested under IEC 60335-1, IEC 60335-2-29, UL 1310, UL 94 V-0 at 1.5 mm, and IEC 60695-2-11 at 850°C; surface tracking is checked by IEC 60112.

    Free Quote

    Competitive SABIC VALOX™ PBT+GF15% Non-Cl/Br FR ENH4530 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ PBT+GF15% Non-Cl/Br FR ENH4530 is a reinforced polybutylene terephthalate injection-molding compound identified by the ENH4530 model designation. The matrix is semicrystalline PBT with a melting endotherm near 223°C to 225°C; reinforcement is introduced as 15% by weight glass fiber. The flame-retardant package is classified as non-chlorinated and non-brominated, meaning the active FR chemistry does not rely on chlorinated or brominated organic flame retardants. This distinguishes the grade from legacy PBT compounds using brominated diphenyl ethers, brominated polystyrene, or chlorinated phosphate packages. The product is deployed in electrical support components, relay bases, connector shells, switch housings, and appliance control enclosures where UL 94 flame-retardant behavior must coexist with evolving OEM restrictions on halogenated additives. Published datasheet values from SABIC place density at approximately 1.47 g/cm³ under ISO 1183-1 and tensile stress at break near 90 MPa under ISO 527-2; these central values assume dry-as-molded specimens and standardized conditioning. Actual molded-part performance is influenced by fiber orientation, weld-line formation, and moisture uptake, so lot-specific certificates of analysis should be used for critical dimensions.

    The product is not formulated for food-contact or medical use unless a specific SABIC compliance letter confirms the required regional status. Hydrolytic degradation is a known boundary for PBT matrices in hot-water or steam environments above approximately 80°C; end-use exposure should be validated using tensile retention after hydrothermal aging under ISO 22088-3 or equivalent. The compound should be kept in sealed moisture-barrier packaging until processing.

    What Melt-Temperature, Moisture, and Tooling Boundaries Govern the Processing Window?

    Because PBT crystallizes rapidly, melt-temperature control below 270°C is critical for the non-halogen FR package. Barrel profiles on a general-purpose single-flight screw of 20:1 L/D with a compression ratio of 2.2:1 to 2.8:1 are typically set from 240°C at the rear zone to 255°C at the front zone, with nozzle temperature held between 250°C and 265°C. Mold temperatures of 60°C to 100°C are required to manage crystallization and reduce post-mold shrinkage; lower mold temperatures may produce sink marks and anisotropic shrinkage in parts with wall-thickness transitions. Residual moisture before processing should not exceed 0.02 wt%. A desiccant dryer with a dew point of −40°C or lower and a hopper residence time of 3 h to 4 h at 120°C is standard. Opened lots should be re-dried after exposure to ambient conditions above 60% RH.

    In production-scale injection molding on machines with clamp force between 80 t and 250 t, gate dimensions for ENH4530 are governed by the viscosity of the glass-filled melt. Tunnel or submarine gates with diameter 0.8 mm to 1.5 mm are used for small electrical housings; edge gates require land length not exceeding 1.0 mm to avoid premature freeze-off. Vent slots should be cut to 0.015 mm to 0.025 mm depth and a width of 3 mm to 6 mm, with full-perimeter venting on the parting line adjacent to the fill end. Inadequate venting of PBT-GF15 FR compounds can lead to surface burning and yellowing in the melt-front region. Mold deposit formation on tool steel is a known maintenance variable for non-halogen FR systems; periodic cleaning is required, particularly on textured cavity surfaces and vent lands. Operating experience indicates hold pressure should be set to 60% to 80% of injection peak to avoid overpacking at the gate and to control glass-fiber orientation near the skin layer.

    Mechanical, Thermal, and Dimensional Data Cross-Referenced to ISO 527-2, ISO 178, ISO 75-2, and ASTM D648

    For short-term mechanical design, the grade is characterized by a tensile stress at break of approximately 90 MPa under ISO 527-2. The tensile modulus is generally reported near 6,000 MPa, while the flexural modulus under ISO 178 is typically 5,500 MPa. Elongation at break is on the order of 2.5%, reflecting the stiffening and embrittling effect of 15% glass-fiber reinforcement. Notched Izod impact values under ISO 180/A are relatively low, generally in the 3.0 kJ/m² to 4.5 kJ/m² range at 23°C, and should not be used for snap-fit designs without finite-element strain validation. Heat deflection temperature under 1.80 MPa load is approximately 200°C by ASTM D648; an ISO 75-2/Af value may be lower because of different specimen geometry and span. Mold shrinkage in the flow direction is commonly 0.4% to 0.6%, and transverse shrinkage may be 0.8% to 1.1%, depending on gate location. These values are not design limits but central datasheet observations.

    Electrical Insulation, Flame Propagation, and Global Regulatory Compliance Matrix

    The non-chlorinated/non-brominated FR package in ENH4530 is intended to support UL 94 V-0 compliance at a wall thickness of 1.5 mm. Some listings may extend to 0.8 mm or 3.0 mm, but the applicable thickness must be verified from the UL yellow card for the specific color and lot. Comparative tracking index under IEC 60112 is commonly reported at 250 V; surface contamination, mold release, and moisture can reduce operational tracking resistance in field use. The material is not typically used as a sole insulation barrier above 60 V DC without additional creepage and clearance analysis under IEC 60664-1. Volume resistivity and surface resistivity are characterized under IEC 62631-3-1 and IEC 62631-3-2; typical values exceed 1×10^13 Ω·m for volume resistivity at 500 V DC. The product does not provide electromagnetic shielding; conductive coatings or metal enclosures are required for EMC compliance.

    Standard/Regulation Clause or Method Data Point Status
    EU 2011/65/EU RoHS Annex II Lead 0.1%, mercury 0.1%, cadmium 0.01%, hexavalent chromium 0.1%, PBDE 0.1%, PBB 0.1% Compliant at homogeneous-material level based on SABIC declarations
    IEC 61249-2-21 Halogen-free definition Total chlorine <900 ppm, total bromine <900 ppm, total chlorine plus bromine <1500 ppm Requires assembly-level verification; non-Cl/Br FR chemistry addresses flame retardant only
    UL 94 Vertical burning test V-0 at 1.5 mm typical Verify final color and thickness against UL yellow card
    IEC 60112 Comparative tracking index 250 V or higher typical Testing on dry-as-molded plaques
    IEC 60664-1 Insulation coordination Clearance and creepage distances Design verification required

    From an industrial hygiene perspective, melt temperatures above 280°C can generate volatile degradation products from the PBT matrix and the non-halogen FR additives. Local exhaust ventilation is recommended over the mold open area and the nozzle zone. Purging of the barrel should be performed with a polyolefin or a dedicated purging compound having a throughput of at least 1.5 times barrel capacity. Residual ash from glass fiber and FR synergists can accumulate in hot-runner manifolds; the hot runner should be designed with no dead spots and a thermocouple sensitivity of ±2°C.

    When Dimensional Stability and Warpage Control Are the Primary Design Constraints

    Relative to unreinforced PBT, the 15% glass-fiber level shifts mold shrinkage from roughly 1.5% to 2.0% in the flow direction to 0.4% to 0.6%, which improves part-to-part dimensional repeatability in multi-cavity tools. The reinforcement also raises heat deflection temperature compared with unfilled PBT. However, 15% glass fiber creates anisotropic shrinkage and warpage risk in flat enclosure walls; rib-to-wall ratios should be kept below 0.6 to minimize sink. When high flatness is required, mold temperature uniformity of ±5°C across the cavity is necessary. The product is therefore specified for relay bases, terminal blocks, connector bodies, and small appliance housings where flame retardance and dimensional control are required but the stiffness of 30% glass-filled PBT is not needed. In living-hinge or high-impact applications, the low elongation and notched Izod values make ENH4530 unsuitable compared with unfilled PBT or polycarbonate blends.

    In comparison to brominated FR PBT-GF15 compounds of equivalent glass loading, ENH4530 generally offers a different balance of fire-retardant mechanism and smoke evolution. Brominated systems often rely on antimony trioxide synergists and generate higher smoke density during combustion; non-halogen packages in PBT typically use organophosphorus or nitrogen-based synergists and may exhibit lower smoke opacity under cone calorimeter testing, although published data for this specific configuration is limited. The absence of bromine and chlorine from the FR package can reduce corrosive gas release in poorly ventilated electrical fires, but it does not eliminate carbon monoxide or other combustion products. Mechanically, the non-halogen FR package may reduce notched Izod impact by 5% to 15% relative to a brominated FR control at equal glass content, depending on specimen thickness and fiber orientation. Designers should compare UL yellow card data, not only datasheet values.

    For applications requiring direct substitution from a brominated FR PBT-GF15, tooling modifications may be needed even when the shrinkage class appears similar. The non-halogen FR package can produce a narrower processing window, greater sensitivity to shear heating, and altered surface finish on polished cavities. Validation runs should include short-shot studies, pressure-drop analysis, and burn-risk assessment in hot-runner drops. Where published data for a specific ENH4530 configuration is not available, SABIC technical service should be contacted for lot-specific rheological and flammability data before tool release.

    Top