| HS Code | 797923 |
| Base Polymer | Polybutylene terephthalate (PBT) |
| Glass Fiber Content | 15% |
| Flow Characteristic | High flow |
| Density | 1.46 g/cm³ |
| Tensile Modulus | 6000 MPa |
| Tensile Strength At Break | 100 MPa |
| Elongation At Break | 2.5% |
| Flexural Modulus | 5500 MPa |
| Notched Izod Impact Strength | 60 J/m |
| Hdt At 1 8 Mpa | 195 °C |
| Hdt At 0 45 Mpa | 215 °C |
| Vicat Softening Temperature | 210 °C |
| Mold Shrinkage Flow | 0.4% |
| Water Absorption | 0.1% |
| Melt Temperature Range | 250-270 °C |
| Mold Temperature Range | 60-100 °C |
| Ul94 Flame Rating | HB |
As an accredited SABIC VALOX™ PBT+GF15%-HF SHF4330 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT+GF15%-HF SHF4330 is supplied in 25 kg moisture-resistant bags, palletized for safe industrial storage and handling. |
| Container Loading (20′ FCL) | 20′ FCL container loading of SABIC VALOX™ PBT+GF15%-HF SHF4330, palletized bags securely stowed and protected for ocean freight. |
| Shipping | SABIC VALOX™ PBT+GF15%-HF SHF4330 is a glass-fiber-reinforced PBT resin supplied as pellets in moisture-barrier bags, boxes, or octabins. Ship dry, ventilated, away from heat and moisture; follow SDS and applicable transport regulations. Verify hazard classification before shipment. |
| Storage | Store SABIC VALOX™ PBT+GF15%-HF SHF4330 in a cool, dry, well-ventilated warehouse, protected from direct sunlight, heat, moisture, and contamination. Keep original containers sealed when not in use, minimize dust generation, and avoid ignition sources or incompatible chemicals such as oxidizers. Follow first-in, first-out stock rotation, observe shelf life, and dry pellets as recommended before processing. |
| Shelf Life | Shelf life is typically 24 months from date of manufacture when stored unopened in dry conditions at recommended temperatures. |
At wall sections below 0.5 mm, the high-flow glass-reinforced PBT grade SHF4330 is processed on fully electric injection moulding machines with screw diameters of 18–25 mm to limit melt residence time. The pellet bed is predried at 120 °C for 4–6 h in a desiccant dryer with an inlet dew point of −40 °C or lower. Residual moisture is verified by Karl Fischer titration at ≤ 0.02 % before plastication. On a 24-cavity hot-runner connector housing tool with 0.4 mm terminal retention walls, the nozzle melt temperature is controlled at 255–265 °C. The manifold is held at 250–260 °C, and the cavity inserts are maintained at 90–105 °C using a water-oil thermolator with a flow rate of 12–18 L/min per circuit. Injection velocity is ramped from 180 mm/s to 300 mm/s over the first 60 % of stroke to prevent free-jet formation; after pack switchover, hold pressure is set to 65–85 MPa. This produces a gate seal time of 1.8–2.3 s in cold sprue gate inserts with spherical radius of 0.8 mm. At this wall thickness, the flow-length-to-thickness ratio exceeds 350:1 and is limited more by frozen-layer growth than by total shot displacement. Cavity pressure sensors mounted behind the terminal retention core show an integral pressure of 420–480 bar·s during the packing stage; when the integral falls below 380 bar·s, the terminal insertion force after assembly rises by 6–10 N because the surround wall collapses inward by 0.02–0.04 mm. The high-flow resin reduces peak cavity pressure compared with a standard-flow glass-filled PBT by approximately 18–25 % in this tool; the advantage is consumed only in sections thinner than 0.35 mm, where glass-fibre orientation anisotropy dominates. After demoulding, dimensional stabilisation is tracked over 48 h at 23 °C and 50 % RH. Differential shrinkage between the flow and transverse directions of 0.12–0.18 % is observed in linear connector bodies, which is lower than unreinforced PBT but still sufficient to require a straightening fixture when terminal pitch tolerance is ±0.05 mm. Splay in gate areas is caused almost exclusively by moisture remaining above 0.04 % at the hopper outlet; raising the melt temperature above 275 °C increases the likelihood of formaldehyde odour and surface deposits on the cavity steel. This condition is not merely cosmetic: carboxylic acid end groups generated during ester hydrolysis shift the viscosity downward and reduce the relative molecular weight of the melt, resulting in batch-to-batch holding pressure drift of 4–6 MPa for the same cavity pressure target. The processing window table below summarises the starting conditions; all values are adjusted against lot-specific melt volume-flow rate and glass content data from the certificate of analysis.
| Processing variable | Operating band for thin-wall applications | Measurement or reference point |
|---|---|---|
| Drying air dew point | ≤ −40 °C | Drying hopper inlet |
| Pellet bed temperature | 120 °C | Hopper outlet thermocouple |
| Drying time | 4–6 h | From cold start |
| Residual moisture | ≤ 0.02 % | Karl Fischer titration |
| Melt temperature at nozzle | 250–270 °C | Immersion probe |
| Mould temperature | 80–110 °C | Thermocouple at cavity insert |
| Injection velocity | 180–320 mm/s | Screw translational velocity |
| Holding pressure | 60–90 MPa | Hydraulic pressure corrected by intensification ratio |
| Back pressure | 0.5–1.5 MPa | Screw return stage |
| Screw peripheral speed | 0.10–0.25 m/s | For 20–25 mm bore |
Continuous current rating in a mated connector is not mainly a function of the polymer melt flow. It is governed by the temperature rise at the terminal contact interface, the retention pressure of the metal terminal against the polymer wall, and the long-term thermal ageing of the insulation material under load. For high-flow PBT reinforced with 15 % glass fibre, the relevant thermal index is established by long-term ageing tests such as UL 746B; published data for this specific grade under continuous load may be limited, and the designer must separate the lot-specific relative thermal index from the generic value assigned to the PBT-GF family. In automotive electrical distribution boxes operating at 23 °C ambient, intermittent loads of 5–10 A per circuit produce local contact temperatures of 70–95 °C. At a continuous 25 A circuit load, the terminal body temperature can reach 120–135 °C in a sealed engine-side box, which exceeds the continuous-use temperature region where unreinforced PBT retains more than 80 % of initial tensile strength after 5,000 h. For SHF4330, the glass fibre raises the heat distortion temperature under 1.8 MPa to approximately 190–205 °C in the standard test, but the practical electrical service temperature is set lower by oxidation and by creep under the spring force of the metal terminal. The retention force of a 0.64 mm gate terminal inserted into a 0.7 mm wall socket is measured by axial extraction at a crosshead speed of 25 mm/min; retention force below 35 N after 1,000 thermal cycles from −40 °C to 125 °C indicates that the polymer wall has stress-crazed around the lance retention window. Because high-flow grades contain shorter glass fibres after plastication in small screw machines, the crack propagation resistance along the fibre-matrix interface is poorer than standard-flow counterparts when moulded at a melt temperature above 270 °C and a residence time longer than 5 min. For this reason, connector bodies that must carry continuous current above 20 A should either use thicker terminal flank sections, metal retainers, or a higher-viscosity PBT grade; otherwise the electrical compliance tests of IEC 60664-1 for creepage and clearance through insulation interfaces may pass initially but not after thermal ageing. The material can be processed with copper alloy terminals, but direct contact with bare aluminium terminals should be avoided because the formation of bimetallic corrosion products under condensed moisture can deposit conductive salts on the polymer surface. Comparative tracking index tested under IEC 60112 is generally in the 175–250 V band for glass-filled PBT classes; exact CTI data for SHF4330 must be taken from the colour-specific UL yellow card or SABIC technical datasheet. No performance claim should be transferred from a natural grade to a carbon-black-loaded automotive grey without re-testing, because carbon masterbatch reduces tracking resistance by forming conductive pathways at the surface under wet contamination.
Because copper magnet wire with a polyamide-imide enamel is wound at a tension of 0.15–0.30 N onto solenoid bobbin cores, the overmoulding grade must fill 0.3–0.6 mm channels around the wire pack without causing enamel displacement. The high-flow SHF4330 grade is processed with a mould temperature of 80–95 °C, a nozzle melt temperature of 255–265 °C, and a low back pressure of 0.5–1.0 MPa to prevent fibre-glass separation in the screw assembly. In a four-cavity valve-gated bobbin tool, the holding pressure is limited to 55–70 MPa because higher pressure collapses the wound wire layers and produces shorted turns in the finished coil. The injection speed is set to 140–220 mm/s through the gate, and the gate is placed on the outer flange away from the wire terminations. The insulation system is tested after overmoulding according to IEC 60085 thermal class; PBT-GF15-HF is not suitable for class F or class H windings that exceed 155 °C continuously, but it is used in class B and class E systems where the hot-spot temperature remains below 130 °C. The main failure mode in production is not thermal softening: it is the formation of micro-flashes at the winding exit slots. These flashes are 20–35 μm thick and are caused by the low shear viscosity of the high-flow resin. When clamping force exceeds 1,000 kN on a four-cavity tool, the flash risk becomes unacceptable; the preferred clamp is 800–950 kN for a projected cavity area of 80–100 cm². After moulding, the coil form is annealed at 120 °C for 2 h to relax moulded-in stress and to verify that no terminal displacement occurs during the shrink-back of the glass-fibre network. Dimensional measurements are taken under ISO 294-4; the total linear shrinkage is generally 0.5–0.7 % after 48 h, and the roundness of the bore is held to ±0.03 mm only when the gate is centrally located and the packing time is controlled. The material must be dried below 0.02 % residual moisture before use in any coil body, because moisture above that level reduces molecular weight during plastication and produces acetic acid-like volatiles that attack copper wire enamel during the injection cycle.
Conventional glass-filled PA6 has higher notched impact strength and lower unpainted surface hardness than PBT; in a half-shell power tool housing, this conversion is driven by the need for lower post-mould moisture growth and better dimensional stability at low humidity. The draft angle on visual side surfaces is increased from 0.5° to 1.0° because PBT-GF15-HF produces a stiffer, harder surface with a lower elongation at break; ejection drag is more visible. Rib-to-wall ratios are reduced from 0.7:1 to 0.6:1 because the high-flow glass-filled PBT has a higher mould shrinkage anisotropy and is more prone to sink at the root of a thick rib. The nominal wall of the PA6 part is often 2.5–3.0 mm; for PBT-GF15-HF the same structural stiffness can be achieved at 2.0–2.3 mm with a tensile modulus of 4,500–5,500 MPa under ISO 527-2. However, the impact of the conversion is not uniform: PBT-GF15-HF shows a notched Izod impact of 4–6 kJ/m² under ISO 180/A, which is lower than PA6-GF30 by a factor of two or more. If the tool retains the deep snap-fit undercuts designed for polyamide, the PBT version must be re-evaluated with insertion and withdrawal force testing at 23 °C and −10 °C. The material is processed at a lower mould temperature than PA6 but requires a similar thermal balance; the polymer does not absorb significant post-mould moisture, so final dimensions stabilise within 48–72 h instead of weeks. Screw bosses used for self-tapping screws must be designed with an outside diameter 2.4 times the screw pitch and a pilot hole diameter 0.8 times the thread root diameter; otherwise the brittle root cracks at the boss base due to glass-fibre orientation. Unlike PA6, which softens at high humidity, the PBT part retains its dimensions in sweaty-hand contact, but it is less tolerant of impact at low temperatures. The conversion is therefore appropriate only when the housing is not a primary drop-load path and when the clamping screws are located in reinforced bosses. It is not appropriate for air-tool components continuously exposed to −20 °C with impact loading perpendicular to the glass-fibre orientation.
Photovoltaic junction boxes of the type referenced in IEC 62790 are injection-moulded from flame-retarded, glass-reinforced PBT at wall sections of 1.2–2.0 mm. In damp-heat preconditioning at 85 °C and 85 % relative humidity for 1,000 h, the ester linkage in PBT undergoes hydrolysis. The diffusion front advances from the exposed surface; for a 1.5 mm thick specimen, a measurable reduction in tensile strength under ISO 527-2 can occur after 500 h if the material is not stabilised. The 15 % glass fibre reduces the absolute moisture uptake and restricts the post-hydrolysis dimensional growth to approximately 0.15–0.30 % after 1,000 h. The mould must therefore avoid weld lines at the sealing channel, because the weld zone has a different fibre orientation and swells differently in damp heat. Leakage current across the busbar mounting surface is measured under 1,000 V DC after the damp-heat cycle; sustained moisture films combined with the tracking residues from the junction box potting compound can produce creepage failure at a clearance below 3.0 mm. The grade should be used with a room-temperature-vulcanizing silicone sealant that does not release amine or ketoxime by-products; amine-based adhesion promoters are explicitly incompatible because they accelerate PBT surface hydrolysis. Moulded-in metal inserts must be post-cured and pass a salt-mist test under IEC 60068-2-52; edge cracking around the inserts after 96 h indicates that the insert preheat was below the polymer melt temperature or that the glass fibre packing pressure was too low in the insert boss. For terminal blocks and busbars, the usual practice is to insert short brass M4 pins with preheat at 110 °C before moulding; after 1,000 h of damp heat, pull-out force retention above 80 % is expected for a well-packed boss. Published data for SHF4330 in full 85/85 photovoltaic qualification is limited; ageing curves must be generated for the actual colourant and flame retardant system used on the production line. This is one of the deep-dive zones because a processing window of ±5 °C at the nozzle determines whether the glass fibres remain bonded to the matrix near the sealing lip.
In proximity sensor bodies exposed to cutting fluids and glycol-water heat transfer media at 95 °C, the polymer undergoes ester hydrolysis at a rate proportional to the concentration of amine-based corrosion inhibitors. The high-flow PBT-GF15-HF grade is moulded into cylindrical shells with a wall thickness of 0.8–1.5 mm and glass lens retention grooves. Mould core and cavity inserts are made from hardened H13 steel with a draft angle of 0.5°. The resin is dried to below 0.02 % residual moisture and processed with a melt cushion of 3–5 mm; no open vent is used because fibre-rich melt escaping from worn vents produces flash. In chemical exposure tests under ISO 22088-3, the sample is immersed in a 50:50 water-glycol mixture with 1 % corrosion inhibitor for 30 days at 95 °C. After immersion, the outer shell stiffness is measured by a compression test to 5 % strain. A retention of 85 % of the initial compressive modulus is considered the lower limit for sensor function; below that value the housing can crack at the retaining lip during insertion into a steel barrel. The material is not resistant to strong alkaline cleaners above pH 10, and continuous immersion in hot water above 90 °C at high pressure will degrade the glass-fibre sizing. In hygienic washdown environments, the sensor body is usually protected by a stainless steel or fluoropolymer sheathing because the PBT-GF surface roughening after multiple 90 °C wash cycles releases micro-particles and reduces the fibre-matrix bond.
Terminal blocks in building switchgear are tested under IEC 60695-2-11 with a glow-wire tip temperature of 960 °C for 30 s or 650 °C for 30 s depending the product standard and the end-use current. PBT-GF15-HF can be formulated with halogenated or halogen-free flame retardant systems, but the final classification is colour-specific and thickness-specific. In a 16-cavity valve-gated terminal body tool, the gate is placed at the bottom of the terminal well, not on the visible sidewall. The sequencing controller opens the outer cavities first and the inner cavities after a delay of 0.2–0.5 s; this reduces gas trap and improves the packing of the terminal retention ribs. The mould temperature is maintained at 85–100 °C; lower temperature causes insufficient crystallisation at the surface, reducing resistance to glow-wire ignition. After the glow-wire test, the sample is observed for flame persistence; a 1.0 mm thick black PBT-GF15-HF part may pass at 850 °C when the carbon black masterbatch loading is below 0.5 %, but above this level the surface ignites earlier. For uninsulated live parts, the required comparative tracking index under IEC 60112 is specified by the insulation coordination standard in the product-specific series; typical minimum values are 250 V for pollution degree 2. The high-flow grade with glass fibre is not inherently tracking-resistant; if the application calls for CTI above 400 V, a specialized tracking-resistant PBT formulation may be required. The compliance matrix below is used when quoting this grade for switchgear; it is not a substitute for UL component recognition data. The processing condition that most influences glow-wire results is the presence of surface defects and weld lines: a weld line at a terminal separation barrier reduces the ignition threshold by 50–75 °C in some thick sections, and the tool should be flow-simulated with short-shot trials to relocate the gate accordingly.
| Regulatory or test context | Standard designation | Measured property or condition | Comments for PBT-GF15-HF |
|---|---|---|---|
| Glow-wire flammability | IEC 60695-2-11 | 750 °C, 850 °C, 960 °C tip temperature | Material thickness and structure determine pass/fail; published data for this specific grade are limited. |
| Tracking resistance | IEC 60112 | Comparative tracking index at 60 drops | Typical high-flow PBT-GF15 grades are in the 175–250 V band; lot-specific certificate governs. |
| Flammability | UL 94 | V-0 at 0.75 mm | Subject to specific colour and processing conditions. |
| Moisture absorption | ISO 62 | 23 °C water saturation | Typically ≤ 0.2 % for glass-filled PBT; conditioning under 85 °C / 85 % RH changes diffusivity. |
| Tensile property retention after heat ageing | ISO 527-2 / ISO 188 | 150 °C air oven | Reported values depend on stabilizer package and specimen thickness. |
Fuse covers for industrial switchgear are small, thin parts with wall thicknesses of 0.6–1.0 mm and lateral clip arms. They are produced in high-cavitation tools, often 32 or 48 cavities, where the runner system must be balanced to within 2 % of fill time across all cavities. The high-flow SHF4330 resin permits lower melt temperature and shorter filling time, but the low-viscosity melt increases the risk of screw slip and fibre breakage if the screw speed is too high. The screw is a low-compression, three-zone design with a compression ratio of 2.0:1 and a check ring free-flow clearance of 0.03–0.05 mm. Screw speed is maintained at 50–100 min⁻¹ for a 25 mm bore; at 150 min⁻¹ the glass fibre length number-average drops below 120 μm and the tensile elongation at break measured on a fan-gate plaque under ISO 527-2 declines by 0.3–0.5 percentage points. Total melt residence time is kept below 5 min; in a 48-cavity tool running a cycle time of 5.5 s, the shot size is matched to the screw recovery so that no stagnant melt remains in the barrel. The gate geometry for fuse covers is a submarine gate with a diameter of 0.8–1.0 mm and a land length of 1.0 mm, which freezes after 1.2–1.6 s. If the gate remains open longer, the transparent cover section shows subsurface flow marks from oscillating check ring leakage. The clip arms are moulded from the same material but the glass fibres align along the arm axis; the flexural fatigue limit is therefore anisotropic. In use, the fuse cover is changed under repeated opening cycles; clip retention force after 5,000 cycles at 23 °C is often 12–18 % lower than the as-moulded value, so the clip arm is designed with an initial interference of 0.25–0.35 mm rather than the 0.15 mm used for unfilled PBT. High-flow grades permit avoiding the need for excessive pack pressure, which would orient fibres too strongly and produce warpage in the transparent web. Published data for long-term clip retention in SHF4330 is limited; lot-specific testing is required when the moulder changes colourant or regrind level.
Competitive SABIC VALOX™ PBT+GF15%-HF SHF4330 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PBT+GF15%-HF SHF4330 is a 15% glass-fibre-reinforced polybutylene terephthalate injection-moulding resin positioned in the high-flow segment of the VALOX thermoplastic polyester portfolio. The compound combines a semicrystalline PBT matrix with chopped glass fibre at a nominal 15% by weight and a flow-modified architecture that depresses melt viscosity relative to standard-flow PBT-GF15 grades of equivalent filler loading. The HF/SHF designation signals the intended conversion route: thin-wall, multi-cavity injection moulding in which conventional glass-reinforced PBT grades may exceed available injection-pressure margins or fail to pack terminal cavities. Property verification for the grade is performed under ISO 1183-1, ISO 527-1/-2, ISO 178, ISO 180/1A, and ISO 75-2/Af. Because glass-fibre compounds are sensitive to fibre length distribution, coupling chemistry, and moulding history, the current SABIC technical data sheet and certificate of analysis remain the controlling references; values extracted from secondary material databases are not accepted as tooling-release evidence.
In high-volume electrical and electronic component production, the material is assigned to connector bodies, relay bases, sensor housings, power-distribution brackets, and appliance control modules that require rigidity, dimensional repeatability, and short-time heat resistance under load. The 15% glass-fibre addition reduces mould shrinkage relative to unfilled PBT, but the reduction is anisotropic because fibre orientation creates separate flow-direction and transverse-direction shrinkage responses. Mould-filling analysis for multi-gate connector tooling therefore requires anisotropic shrinkage input rather than a single isotropic coefficient. Production-scale evaluation is typically carried out on injection-moulding machines with clamping force between 500 kN and 1500 kN, general-purpose screws of 18:1 to 22:1 L/D ratio, and pressure-controlled switchover from injection to holding phase. In multi-cavity layouts exceeding 8 cavities, valve-gated hot-runner drops are frequently used because the high-flow matrix reduces runner-pressure loss, though gate-freeze-off behaviour in thin ribs and latch features is not eliminated by the flow modification alone.
The processing boundaries for this grade are defined by moisture-induced hydrolysis, thermal degradation, glass-fibre attrition, and crystallinity control. PBT is an ester-linked thermoplastic; if residual moisture exceeds approximately 0.02% by weight at the feed throat, hydrolysis during plastication causes chain scission and a measurable decline in melt viscosity, weld-line strength, and retention of impact properties. Desiccant drying at 120 °C for 3 h to 4 h is the standard pre-processing condition, with a dryer dew point below -40 °C. In plants operating above 60% relative humidity, hopper residence time is commonly extended to 4 h to 6 h because surface moisture uptake at the granule-bed boundary is rapid. Karl Fischer titration according to ISO 15512:2019 is the accepted verification method for residual moisture; a hopper-mounted hygrometer reading alone does not provide lot-acceptance certainty.
Melt-temperature control is the second boundary. The practical barrel-and-nozzle band for glass-reinforced PBT is normally 240 °C to 270 °C. Below 240 °C, incomplete homogenization and wetting of glass fibres can produce flow lines and weak knit regions. Above 270 °C, thermal decomposition accelerates and volatile species can appear as nozzle drool or tool deposit. The high-flow character of SHF4330 does not raise the thermal-stability limit. Because the lower melt viscosity generates less shear heating than a standard-flow PBT-GF15, there can be an operational temptation to elevate barrel temperatures to maintain screw recovery speed. This adjustment is not advisable at melt temperatures above 270 °C when total residence time exceeds 5 min; black speck formation and loss of impact performance become increasingly likely. Melt temperature should be checked at the nozzle with a needle pyrometer, and the screw buffer should be managed so that the oldest melt does not remain in the barrel longer than 5 min.
Crystallinity development is governed by mould temperature. PBT crystallizes rapidly, but a mould wall below 60 °C produces an amorphous skin with lower hot-dry dimensional stability and reduced short-time heat resistance. Mould temperatures between 60 °C and 100 °C are used for thin-wall connectors: the lower portion of the range is selected when cycle-time targets dominate, and the upper portion is selected when maximum heat deflection and weld-line strength are required. For high-flow PBT-GF15, elevated mould temperature can improve knit-line integrity because it delays front freezing at the meeting surface. The flow-modified matrix reduces the pressure required to fill a cavity, but it does not remove the need for holding pressure adequate to compensate PBT’s volumetric shrinkage. Holding-pressure settings should be derived from gate-seal studies on the production tool, not from generic datasheet tables.
Glass-fibre attrition during plastication is a further variable. In standard-flow PBT-GF15, glass fibres undergo shear-induced breakage in the screw compression zone. The lower-viscosity matrix of SHF4330 may reduce viscous drag on fibre bundles, but back pressures above 1 MPa and screw peripheral speeds above 0.3 m/s can still increase fibre breakage and shift the effective reinforcement length lower. When mechanical-property outliers are observed between cavities, fibre-length distribution after moulding should be measured by ashing followed by image analysis. Published data for this specific configuration is limited; production trials on the intended tool are required to establish the optimum screw profile, back pressure, and injection velocity envelope.
The property envelope in Table 1 is assembled from publicly reported ranges for 15% glass-fibre-reinforced high-flow PBT injection-moulding grades. It is supplied as a first-pass screening reference and does not replace the current SABIC VALOX SHF4330 data sheet. Specimen preparation for mechanical testing normally follows ISO 294-1, ISO 294-3, and ISO 294-5; conditioning before testing follows ISO 291 at 23 °C and 50% relative humidity unless the data sheet specifies otherwise.
| Property | Test method | Typical range | Unit |
|---|---|---|---|
| Density | ISO 1183-1 | 1.40–1.43 | g/cm³ |
| Tensile stress at break | ISO 527-2/5 | 85–105 | MPa |
| Tensile strain at break | ISO 527-2/5 | 1.8–3.5 | % |
| Flexural modulus | ISO 178 | 4200–5200 | MPa |
| Flexural strength | ISO 178 | 120–150 | MPa |
| Notched Izod impact, 23 °C | ISO 180/1A | 3.5–6.0 | kJ/m² |
| Heat deflection temperature, 1.80 MPa | ISO 75-2/Af | 190–205 | °C |
| Water absorption, 24 h immersion | ISO 62 | 0.05–0.10 | % |
For lot acceptance, the certificate of analysis should be reviewed for the actual melt volume-flow rate and mechanical values measured on the same batch. Melt flow characterisation is reported under ISO 1133-1:2022, normally at 250 °C and 2.16 kg or at a grade-specific condition indicated in the supplier data sheet. Mould shrinkage data are generated on defined plaque dimensions and thickness, with flow and cross-flow values listed separately; using an averaged shrinkage figure understates warpage risk in elongated connector bodies and asymmetrically gated housings.
For electrical and electronic screening, surface tracking resistance is measured under IEC 60112, and volume resistivity is characterised under IEC 62631-3-1. Glass reinforcement and flow-modifying additives can affect surface tracking behaviour, so electrical values are specific to the exact grade and test thickness. Flammability claims must be confirmed against the supplier’s current UL Yellow Card under UL 746A and UL 746B protocols because minimum thickness and colour dependence can change the classification. Compliance statements for REACH Regulation EC No 1907/2006 and RoHS Directive 2011/65/EU should be obtained from SABIC product stewardship documentation rather than inferred from the generic PBT material class.
The decision to use SHF4330 instead of a standard-flow 15% glass-fibre PBT is usually controlled by mould-fill pressure and thin-wall filling capability. A standard-flow PBT-GF15 forces the processor toward higher melt temperature, higher injection velocity, or larger clamp force to fill long ribs, latch arms, and thin connector walls. SHF4330 reduces screw-tip pressure demand for an equivalent flow path. The trade-off is assessed in the mechanical domain: high-flow PBT formulations are designed to retain tensile and flexural properties close to standard-flow PBT-GF15, but the molecular-architecture shift and additive package can reduce weld-line elongation and low-temperature notched impact. A connector with well-positioned gates and no impact-critical knit line may transfer to SHF4330 without measurable functional loss; an enclosure boss adjacent to a knit line requires weld-line tensile and impact testing before approval.
Against a 30% glass-fibre PBT such as VALOX 420SEO, SHF4330 has lower filler content, lower density, and lower melt viscosity. The 30% glass-fibre grade provides higher tensile modulus and higher heat deflection resistance, but it also raises melt viscosity and injection-pressure demand. In thin-wall parts where the controlling variable is fill pressure rather than flexural modulus, the 15% high-flow grade is preferred. A 30% glass-fibre PBT typically exhibits flexural modulus in the range of 7000 MPa to 9000 MPa, while the 15% glass-fibre high-flow envelope is lower. If the application imposes a minimum flexural modulus above 6000 MPa, SHF4330 is not the default candidate; a PBT-GF30 or a PBT/PET blend should be evaluated.
Compared with unfilled PBT, SHF4330 provides higher tensile modulus, higher heat deflection temperature, and lower mould shrinkage. Unfilled PBT retains high elongation at break but low stiffness, with isotropic mould shrinkage commonly in the range of 1.5% to 2.0%. A 15% glass-fibre PBT can show flow-direction shrinkage values closer to 0.3% to 0.6% depending on part thickness, gate position, and fibre orientation. The high-flow version should not be assumed to have identical shrinkage to a standard-flow PBT-GF15 because flow modification can alter crystallization and fibre-orientation patterns. Shrinkage must be measured on the production part or a geometrically representative plaque before tooling steel revision.
In multi-cavity automotive connector tooling with wall thickness below 0.8 mm and flow length above 80 mm, the high-flow characteristic of SHF4330 is verified by measuring cavity-pressure transfer at the last cavity to fill. A cavity pressure below 30 MPa at the end of fill indicates insufficient packing and a high probability of sink marks despite the low melt viscosity. The material therefore cannot be specified by melt-flow value alone; the processing response is defined by the interaction of melt viscosity, gate freeze-off time, and holding-pressure profile. Production sign-off is based on dimensional capability studies, short-shot progression, and weld-line mechanical testing under the intended end-use thermal load.