| HS Code | 968969 |
| Polymer Base | PBT |
| Ul94 Flame Rating | V-0 at 0.8 mm |
| Volume Resistivity Ohm Cm | >1E15 |
| Mold Shrinkage Percent | 0.3-0.8 |
As an accredited SABIC VALOX™ PBT+GF15% 830 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT+GF15% 830 is supplied in sealed 25 kg moisture-barrier bags, palletized for industrial handling. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): SABIC VALOX™ PBT+GF15% 830 loaded in a 20′ FCL, palletized, secured, and prepared for ocean freight. |
| Shipping | SABIC VALOX™ PBT+GF15% 830 is a glass-fiber-reinforced PBT resin supplied as pellets. Ship in sealed moisture-barrier packaging under dry, ambient conditions, away from heat and direct sunlight. It is typically non-hazardous and not regulated for transport; follow the SDS and local regulations. |
| Storage | Store SABIC VALOX™ PBT+GF15% 830 in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and oxidizing materials. Keep original packages closed and protected from moisture, dust, and contamination. Use pallets, avoid prolonged high humidity, do not stack excessively, rotate stock, and follow the SDS and local storage regulations. |
| Shelf Life | SABIC VALOX™ PBT+GF15% 830 has a shelf life of 2 years when stored dry, cool, and in original unopened packaging. |
Injection molding of VALOX 830 for underhood connector housings starts with desiccant drying at 120 °C for 4 h, with dryer air dew point at or below −40 °C. Karl Fischer titration per ISO 15512:2019 must show residual moisture below 0.02 wt%; higher moisture hydrolyzes the ester backbone during plastication, causing a measurable drop in melt viscosity and a reduction in weld-line strength. Plastication is carried out on a general-purpose screw with 20:1 to 22:1 L/D ratio and a free-flow check ring; compression ratio is set between 2.5:1 and 3.0:1 to limit glass fiber breakage. Barrel temperatures are set with the rear zone at 230 °C, the center zones between 240 °C and 255 °C, and the nozzle between 250 °C and 270 °C. Hot runner manifolds must not exceed 265 °C, and total residence time at processing temperature should stay below 6 min to limit tetrahydrofuran formation from β-hydrogen transfer during thermal degradation. Mold temperature is held between 80 °C and 100 °C using pressurized-water temperature control units; this range accelerates PBT crystallization and stabilizes the connector locking-tab dimensions after ejection. Pack-and-hold pressure is set between 60 MPa and 80 MPa on the part surface, with hold time adjusted until gate freeze is confirmed by part weight stabilization, typically between 3 s and 6 s for wall sections from 1.2 mm to 2.5 mm.
Short-glass fiber orientation creates anisotropic mold shrinkage. Flow-direction shrinkage is typically 0.2 % to 0.4 %, while transverse shrinkage reaches 0.9 % to 1.2 % when measured after 48 h at 23 °C per ISO 294-4:2018. Tool offsets for connector pin pitches must compensate for this anisotropy; a 0.10 mm mismatch across a four-pin array can exceed terminal retention tolerance when the housing is assembled to a PCB header. The 15 wt% glass reinforcement reduces creep under connector contact preload but also creates weld lines with tensile strength 40 % to 50 % below unwelded values when tested per ISO 527-2:2012. Gas or air entrapment at the end of fill is controlled by placing vent channels 0.01 mm to 0.03 mm deep along the parting line and by reducing injection velocity in the final 20 % of stroke. Underhood exposure should be limited to locations where continuous air temperature remains below 120 °C and oil mist temperature below 100 °C; prolonged contact with hot ethylene glycol coolant above 110 °C should be avoided because polyester hydrolysis accelerates under basic pH. Automotive validation for terminal position assurance and connector latch cycling references USCAR-2, and sealed housings are checked under IEC 60529 IP67 when a soft TPE gasket is overmolded.
Miniature relay bobbin tools produce wall sections between 0.35 mm and 0.80 mm around crimped coil terminals. At mold temperatures below 80 °C, the polymer skin solidifies before the core reaches full crystallization, leaving an under-crystallized layer that post-shrinks when the relay coil is baked at 120 °C for winding varnish cure. This post-mold distortion changes coil-winding OD and can shift the air gap between the bobbin flange and the armature by 0.05 mm to 0.10 mm, altering relay pull-in voltage. The mold temperature is therefore held between 85 °C and 100 °C with turbulent water flow at 6 L/min to 10 L/min per circuit. Nozzle melt temperature is kept between 245 °C and 260 °C; higher temperatures shorten glass fiber length after plastication, which reduces flexural modulus measured by ISO 178:2019 and lowers the bobbin flange stiffness that resists winding tension.
Because glass reinforcement reduces comparative tracking index relative to unfilled PBT, the relay bobbin must be tested per IEC 60112 at the specified voltage; creepage and clearance distances are assigned under IEC 60664-1. For reinforced PBT, CTI values commonly fall between 250 V and 300 V, but grade-specific datasheets control whether the bobbin can be used in a pollution degree 2 circuit. Dielectric strength is thickness-dependent and is verified by IEC 60243-1; a 0.5 mm wall may show breakdown strength near 20 kV/mm, but voids around glass fibers can create local field enhancement. The gate is normally a subgate or film gate 0.8 mm to 1.0 mm thick placed on an outside flange, never on the core surface where gate vestige would disturb armature movement. Valve-gate sequencing in four-cavity tools must be tuned to prevent imbalanced filling; cavity-to-cavity fill imbalance above 5 % leads to uneven packing, visible as sink marks on flange radii and inconsistent coil-winding profiles. UL 1446 insulation-system recognition applies to the complete coil assembly, not the bobbin material alone, so the molder must verify that the selected VALOX 830 grade is listed in the insulation system file before substituting from unfilled PBT or PA66.
| Downstream segment | Nozzle melt temperature | Mold temperature | Residual moisture | Mold shrinkage flow/transverse | Hold pressure |
|---|---|---|---|---|---|
| Automotive underhood connector housing | 250–270 °C | 80–100 °C | ≤0.02 wt% | 0.2–0.4 % / 0.8–1.2 % | 60–80 MPa |
| Miniature relay bobbin | 245–260 °C | 85–100 °C | ≤0.02 wt% | 0.3–0.5 % / 0.9–1.1 % | 50–70 MPa |
| Low-voltage terminal block | 240–260 °C | 60–85 °C | ≤0.03 wt% | 0.2–0.4 % / 1.0–1.3 % | 55–75 MPa |
| Power tool clamshell housing | 245–270 °C | 70–95 °C | ≤0.02 wt% | 0.2–0.5 % / 0.9–1.2 % | 60–85 MPa |
Because PBT crystallization is rapid, low-voltage terminal blocks molded in multi-cavity tools reach ejection temperature sooner than equivalent PA66 parts, but the glass fiber network generates non-uniform thermal conductivity across the melt front. The result is a thickness-dependent skin-core orientation that changes the position of weld lines between terminal holes. In a 2.5 mm wall terminal block, the core remains molten long enough for glass fibers to orient through the thickness, while the 0.15 mm to 0.25 mm outer skin freezes almost immediately. This dual morphology increases bending stiffness but creates a shear plane between the skin and core that can delaminate when a self-tapping screw is overtorqued above 0.6 N·m in the terminal pocket. The boss is therefore designed with a minimum outer diameter of 7.0 mm for an M3 screw, and the gate location is selected to place the weld line behind the terminal area, not along the screw axis.
Compliance for terminal blocks in unattended household appliances is evaluated by glow-wire testing under IEC 60695-2-11; the glass-filled PBT part must be tested at final wall thickness and color because ignition resistance changes with pigment metal oxides and glass content. Tracking index per IEC 60112 and ball pressure per IEC 60695-10-2 are also specified in appliance standards. Creep under terminal screw load is assessed by ISO 899-2 at 23 °C and 80 °C; the 15 wt% glass fiber lowers creep strain compared with unfilled PBT, but the clamp should not exceed 20 MPa long-term compression on the insulating body. When the terminal strip is molded with metal inserts, insert temperature should be above 85 °C to prevent premature skin crystallization and improve insert-matrix adhesion. After molding, parts are annealed at 100 °C for 2 h to relax orientation stresses before electrical testing; this reduces hole-pitch drift by approximately 0.05 % relative to as-molded values.
Dimensional control in appliance motor brackets becomes critical when the part is heat-staked or screw-fastened onto a steel lamination stack. At an external motor-case temperature of 85 °C, an unfilled PBT bracket can lose clamp load because amorphous regions continue to densify. The 15 wt% short-glass filler in VALOX 830 lowers the proportion of free amorphous phase and raises the heat deflection temperature under 1.8 MPa load above 175 °C when measured per ISO 75-2:2013, which supports bracket flatness after 1,000 h at 85 °C. The appliance molder should set mold temperature at the upper end of the 80–100 °C window and apply a post-mold annealing step at 100 °C for 2 h; without annealing, residual stress from fiber orientation can warp the bracket after the first heat cycle in a dishwasher or oven-cooling motor.
Water absorption is the primary advantage over PA66 in this application. At 23 °C and 50 % relative humidity, PBT absorbs 0.07 wt% to 0.10 wt% moisture per ISO 62, while PA66 absorbs 1.5 wt% to 2.5 wt%. In a humid laundry-room environment, a PA66 motor bracket swells and shifts the rotor-stator air gap, whereas the VALOX 830 bracket remains within a narrower tolerance band. Continuous contact with hot alkaline detergent solutions above 60 °C must be avoided because ester hydrolysis weakens the glass-matrix interface. When heat-staking is used, the stake punch temperature is set between 180 °C and 210 °C, and the post is conditioned for 30 s to 60 s at 80 °C to reduce brittle fracture at the glass-fiber-rich base.
In low-moisture assembly environments, PA66 power tool housings exhibit dimensional variation due to moisture uptake of 1.5 wt% to 2.5 wt% at 50 % relative humidity. VALOX 830 can replace PA66 when the tool operates in dry indoor air and the housing does not see repeated impact against concrete. The design must address the lower notched Izod impact toughness of PBT GF15 relative to conditioned PA66 measured by ISO 180:2019; ribs and screw bosses should be thickened by 10 % to 15 % compared with the PA66 original, and snap-fit engagement should not exceed 1.5 mm to limit flexural strain at the glass-fiber-rich hinge. Injection molding of a large clamshell housing uses sequential valve gating with opening delays of 0.5 s to 1.5 s between nozzles, allowing the melt front to merge before the first gate freezes. Clamp force is calculated from projected cavity area using a peak cavity pressure of 35 MPa to 50 MPa; a 400 cm² projected area tool therefore requires 140 t to 200 t clamp tonnage.
Gas-assisted injection is not recommended for this glass-filled PBT because the gas channel can displace glass fibers into the gas-nominated area and create a resin-rich skin with reduced stiffness; structural foam and water-assisted injection are also avoided due to ester hydrolysis risk and poor surface finish. The tool should be hardened to 48 HRC minimum because glass fiber abrasion at the gate wears P20 inserts faster than unfilled PBT. Draft angles are increased to 1° minimum, and gate lands are fabricated from H13 steel to resist erosion. For motor housings, a post-mold cooling fixture holds the part for 30 s to 60 s at 23 °C to prevent inward bowing of split-line surfaces. The assembled housing must meet the mechanical strength requirements of IEC 62841-1; published data for this specific power-tool configuration is limited, so drop-test pass criteria should be confirmed on a production-grade tool rather than a prototype sample.
Thermal isolation in double-insulated LED drivers depends on creepage distance and comparative tracking index. A 15 wt% glass-reinforced PBT enclosure can be molded in two snap-fit halves, but the material’s CTI under IEC 60112 must be checked at the final color because dark pigments and glass content affect surface tracking. For driver circuits operating at 230 V AC in a pollution degree 2 environment, the minimum creepage distance is derived from IEC 60664-1 tables; if CTI falls below 250 V, the design must shift to larger spacing or add a ribbed barrier. PBT GF15 exhibits a relative permittivity between 3.5 and 4.0 at 1 MHz per IEC 62631-3-1, which reduces dielectric heating compared with mineral-filled grades. The enclosure is molded with mold temperature between 80 °C and 95 °C to produce a highly crystalline skin that resists silicone potting adhesion loss when the driver is potted with a two-part pour-in silicone.
UL Yellow Card recognition under UL 746B must be confirmed for the exact wall thickness and color used in the driver. Long-term thermal aging data for PBT GF15 typically show electrical relative thermal index values in the 130 °C to 140 °C range, but published data for this specific configuration is limited and the converter should verify current UL file information before specifying hot spots above 105 °C at the LED module interface. The snap-fit design should limit insertion force so that the glass-filled PBT does not fracture at the undercut; a 0.4 mm to 0.6 mm undercut with a 1.2 mm nominal wall and a 0.5 mm root radius is typical. The final driver enclosure must pass the ball pressure test at 125 °C under IEC 60695-10-2, glow-wire testing at the end-product level, and dielectric strength testing per IEC 60243-1 at 1,000 V AC plus twice the rated voltage.
Competitive SABIC VALOX™ PBT+GF15% 830 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The SABIC VALOX™ PBT+GF15% 830 material is a 15 wt% glass-fibre-reinforced polybutylene terephthalate injection-moulding grade supplied as cylindrical pellets. It is classified as PBT-GF15 under ISO 1043. Published typical values include density of 1.45 g/cm³ by ISO 1183-1, tensile stress at break between 95 MPa and 105 MPa by ISO 527-2/5, flexural modulus between 5.5 GPa and 6.5 GPa by ISO 178, and heat deflection temperature under 1.8 MPa between 195 °C and 205 °C by ISO 75-2/Af. These figures are supplier-published typical ranges, not lot-specific specification limits. The suffix 830 identifies the non-flame-retardant, medium-stiffness product within the VALOX portfolio.
The glass content is commonly verified by ash content using ISO 3451-1. Because the fibre loading is intermediate, the material is selected when unfilled PBT lacks sufficient flexural modulus at elevated temperature but a 30 wt% glass product would increase density, surface roughness, and machine wear beyond the acceptable range. The following sections describe the property shift, processing boundaries, application-specific constraints, and documentation status.
The 15 wt% compound occupies an intermediate stiffness design envelope. Flexural modulus rises from approximately 2.5 GPa for unfilled PBT to 5.5–6.5 GPa for this grade, while the notched Izod impact value remains closer to unfilled PBT than to the 30 wt% compound. The improvement in heat deflection temperature is significant: unfilled PBT can fall below dimensional requirements above 60 °C under 1.8 MPa, whereas the glass-reinforced grade maintains resistance to deformation to approximately 200 °C. Compared with 30 wt% glass PBT, the lower fibre content reduces density from roughly 1.53 g/cm³ to 1.45 g/cm³ and lowers gate-area warpage, but the compound sacrifices part of the flexural modulus and HDT/A margin available from higher fibre loadings.
| Property | Test method | Unfilled PBT | PBT+GF15 | PBT+GF30 |
|---|---|---|---|---|
| Density | ISO 1183-1 | 1.31 g/cm³ | 1.45 g/cm³ | 1.53 g/cm³ |
| Flexural modulus | ISO 178 | 2.5 GPa | 5.5–6.5 GPa | 8.5–9.5 GPa |
| Tensile stress at break | ISO 527-2/5 | 45–60 MPa | 90–110 MPa | 110–135 MPa |
| HDT/A at 1.8 MPa | ISO 75-2/Af | 50–60 °C | 195–205 °C | 200–215 °C |
| Notched Izod impact | ISO 180/A | 3–5 kJ/m² | 4–7 kJ/m² | 7–10 kJ/m² |
| Mould shrinkage, flow direction | ISO 294-4 | 1.8–2.2 % | 0.4–0.6 % | 0.2–0.4 % |
Selection should account for weld-line sensitivity. The 15 wt% glass grade shows higher notch sensitivity at moulded-in stress concentrators than unfilled PBT even where the published Izod value appears similar. Sharp internal corners, press-fit inserts, and poorly positioned gates create fibre-aligned planes that can propagate cracks under impact. Compared with 30 wt% compounds, the lower fibre concentration reduces this effect slightly, but it remains operationally important in connector snap-fits and terminal-block retaining features.
The product is not an impact-modified compound. Applications requiring low-temperature ductility below −30 °C should not rely solely on the published room-temperature notched Izod value; low-temperature impact testing according to ISO 179-1/1eA or ISO 180/A should be performed on moulded plaques. Published data for this specific formulation below −30 °C is limited.
In automotive under-hood connector shells and sensor mounts, the grade is moulded with melt temperature 250–270 °C and mould temperature 60–90 °C. Hydraulic or electric moulding machines of 80–150 t clamp force are commonly used for multicavity tools; cavity pressure should be held at 35–50 MPa during packing. Published data for this specific configuration is limited; therefore, production validation should include moulded weld-line plaques according to ISO 527-2 and notched impact specimens cut from the part according to ISO 180/A. Dimensional audit should be performed no earlier than 24 h after moulding, preferably after 48 h at 23 °C and 50 % relative humidity, because anisotropic post-mould shrinkage continues after ejection.
Rheological measurement according to ISO 11443 is recommended before hot-runner layout. Glass-reinforced PBT at 260 °C typically shear-thins to a viscosity of 80–160 Pa·s at 1000 s⁻¹; the exact curve should be obtained from the current SABIC datasheet or capillary rheometry on dried pellets. Unfilled PBT viscosity data are not suitable for hot-runner pressure-drop simulation because the fibre phase increases entrance pressure loss, especially at contraction ratios above 4:1.
The polyester chain is hydrolytically unstable at melt temperature. If pellet moisture exceeds 0.02 wt% by Karl Fischer or calibrated moisture analysis, exposure above 250 °C produces chain scission, terminal carboxyl end-group increase, surface splay, and reduced notched impact strength. Moulding without drying is not acceptable for this grade. Predrying in a desiccant dryer with air inlet temperature 120–130 °C, dew point −40 °C or lower, and pellet residence time of 4–6 h reduces moisture to the required level. If sacks have been opened at relative humidity above 60 % for more than 4 h, drying should be extended to 8 h because the glass-fibre interface is not immune to moisture uptake and surface moisture adsorption is rapid.
Hopper dryers operating with ambient air cannot achieve the required dew point. Desiccant wheel dryers must be sized so that the bed temperature remains at 120 °C or higher throughout the residence time; cold spots in hopper cones allow wet pellets to bypass drying. The return air temperature, airflow, and desiccant rotor performance should be checked at process start-up. A moisture analyser reading above 0.02 wt% after drying indicates inadequate dryer capacity or leakage in the intake filter.
After drying, pellets should be conveyed with dry air and held in a heated hopper at 80 °C for no longer than 24 h. Re-exposure to plant air beyond this period requires re-drying.
Processing on a general-purpose screw with an L/D ratio of at least 20:1 and compression ratio 2.5:1 is typical. A low-shear mixing section is acceptable, but high-shear barriers or aggressive Maddock sections may reduce glass-fibre length and notched impact strength. Barrel zones from rear to nozzle are typically set as 230–240 °C, 240–250 °C, 250–260 °C, and 250–265 °C. Melt temperature at the nozzle should not exceed 270 °C. Total barrel residence time should remain below 5 min; longer residence times discolour the resin and accelerate hydrolytic chain scission even in pre-dried material.
Mould surface temperature controls crystallinity. A surface temperature below 40 °C yields low crystallinity, greater post-mould shrinkage, and flow-line defects, whereas 60–90 °C is preferred for dimensionally stabilised housings. For walls below 1.5 mm, high injection speed is required to avoid gate freeze-off. For walls above 3 mm, reduced injection speed with extended hold pressure prevents sink marks and internal voids. Hold pressure should be applied until gate sealing; gate diameters of 0.8–1.2 mm are common depending on part mass, and gate-depth to wall-thickness ratios below 0.6 reduce packing efficiency. Valve-gated hot-runner systems should limit gate shear rate to below 50 000 s⁻¹ to avoid fibre attrition and surface roughness.
Reground sprues and runners may be blended with virgin material up to 20 % by weight for non-safety enclosures if the regrind is clean and dry. Each heat history reduces glass-fibre length; load-bearing or impact-sensitive parts should be re-qualified using ISO 527-2, ISO 178, and ISO 180/A before any increase in regrind ratio. Because 15 wt% glass is abrasive, screws with hard coatings or bimetallic barrels are recommended for extended campaigns. Screw and check-ring wear produces gradual loss of melt cushion control and can shift plastication time; batch-to-batch variance on a worn screw often appears as inconsistent shot weight and dimensional scatter rather than immediate visual defects. Production-scale failure modes observed with glass-filled PBT include gate blush, fibre-rich surface patches at high shear, weld-line cracking in snap-fits, and dimensional warp due to unbalanced fibre orientation.
In low-voltage switchgear terminal blocks and appliance control-panel frames, the intermediate stiffness of the 15 wt% glass product supports creep-resistant screw bosses and thin wall sections at service temperatures below the deflection limit. The flammability classification is UL 94 HB at 1.5 mm; it is not suitable for equipment requiring UL 94 V-0, V-2, or 5VA ratings unless an additional flame-retardant system is validated on the finished assembly. This limitation is significant because unfilled PBT and some glass-filled PBT variants may carry different flame ratings even within the same supplier portfolio.
For outdoor telecommunications enclosures, additional UV stabilisation may be necessary because standard PBT can undergo surface chalking and embrittlement under extended ultraviolet exposure. The 15 wt% glass reinforcement does not mitigate that degradation mechanism. If outdoor installation is required, a UV-stabilised grade or a secondary protective coating should be included in the application validation plan.
For metal-insert moulding, brass or copper alloy inserts should be preheated to 120–180 °C to reduce differential thermal contraction around the PBT matrix. Cracking at sharp insert knurls or hexagonal edges may be evaluated by dye penetrant inspection or sectioning after thermal cycling from −40 °C to 85 °C. Alkaline mould-release sprays containing sodium hydroxide or potassium hydroxide should not be applied to cavity surfaces because alkaline residues attack the polyester at the gate and induce delamination.
The regulatory status of the grade is documented through supplier declarations rather than a single universal certificate. The material is supplied under a standard compounding quality system; it is not a food-contact grade unless specifically listed for the application. Compliance claims for production parts should be verified against the current SABIC product stewardship bulletin and the raw-material composition letter.
| Requirement | Standard or regulation | Typical documentation status |
|---|---|---|
| RoHS restricted substances | Directive 2011/65/EU with amendments | Supplier declaration of conformity available |
| REACH SVHC content | Regulation (EC) No 1907/2006 | No SVHC above 0.1 wt% by supplier declaration |
| Flammability classification | UL 94 | HB at 1.5 mm |
| Food contact | FDA 21 CFR 177.1660 or regional equivalent | Not generally listed; consult product stewardship |
In chemical exposure applications such as automotive coolant sensors or low-pressure hydraulic components, continuous immersion in hot alkaline fluids above 80 °C should be avoided because PBT hydrolyses. Compatibility screening should follow ASTM D543 or ISO 22088-3 on moulded plaques at the intended maximum service temperature. Additive packages containing primary or secondary amines should be avoided in masterbatch dilution because amine transesterification can reduce molecular weight at processing temperatures. Published data for this specific formulation under continuous hot glycol-water immersion is limited; therefore, no safety factor can be assumed without part-level testing.