Sabic Valox Pbt Gf15 815

SABIC VALOX™ PBT+GF15% 815

    • Product Name: SABIC VALOX™ PBT+GF15% 815
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 586444
    Glass Fiber Content Percent 15
    Density G Cm3 1.39
    Tensile Modulus Mpa 6000
    Tensile Strength Mpa 100
    Elongation At Break Percent 2.5
    Flexural Modulus Mpa 5500
    Flexural Strength Mpa 150
    Notched Izod Impact J M 50
    Heat Deflection Temperature A C 200
    Melting Temperature C 225
    Molding Shrinkage Flow Percent 0.4-0.6
    Melt Temperature C 240-260
    Mold Temperature C 40-80

    As an accredited SABIC VALOX™ PBT+GF15% 815 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ PBT+GF15% 815 is packaged in 25 kg moisture-resistant foil-lined bags, 40 bags per pallet (1,000 kg pallet).
    Container Loading (20′ FCL) Standard 20′ FCL dry container loaded with palletized SABIC VALOX™ PBT+GF15% 815, securely strapped and shrink-wrapped for ocean shipment.
    Shipping SABIC VALOX™ PBT+GF15% 815 is shipped as non-hazardous thermoplastic resin pellets in moisture-barrier bags, boxes, or octabins. It is not regulated for transport under DOT/IMDG/IATA. Keep dry, avoid direct sunlight, and store at ambient temperature; no special shipping labels are required.
    Storage Store in original packaging, in a cool, dry, well-ventilated area away from direct sunlight, heat sources, moisture, and incompatible chemicals. Keep containers tightly closed to prevent contamination and moisture absorption. Avoid dust generation and static buildup; use appropriate grounding. Protect from physical damage. Follow the manufacturer’s SDS and local regulations; recommended storage is typically below 30°C and low humidity.
    Shelf Life Shelf life is typically 24 months from date of manufacture when stored dry, cool, and in original sealed packaging.
    Application of SABIC VALOX™ PBT+GF15% 815

    When Hot Ethylene Glycol and Transmission Fluid Contaminate Underhood Connector Housings

    In underhood wiring harness and sensor pod applications, SABIC VALOX™ PBT+GF15% 815 is injection-moulded into connector bodies that must preserve locking-latch geometry after thermal-chemical exposure and repeated harness service loads. Compliance anchors include USCAR-2 for automotive electrical connection system performance, SAE J1639 for vibration-and-temperature screening of assembled housings, and ISO 16750-5 for chemical load testing against engine oil, power steering fluid, battery acid, and 50/50 ethylene glycol/water. Material-level data are generated under ISO 527-2, ISO 178, and ISO 179/1eU, while flammability classification remains UL 94 HB as stated on the grade’s yellow card. The formulation addition ratio is fixed by the supplier: glass fibre loading is 15±1 wt% by ISO 3451-1 method A, and the material is normally fed at 100 wt% without let-down. Where a moulding operation blends this filled grade with unfilled PBT to adjust moulded shrinkage, the filled grade addition commonly falls between 20 wt% and 40 wt%, but published data for this specific diluted configuration is limited, and the resulting mechanical and chemical resistance envelope falls outside the single-grade processing window. Production-scale processing requires desiccant drying at 120°C for 3–4 h to reduce residual moisture below 0.02%; elevated moisture at barrel temperatures above 270°C accelerates hydrolytic molecular weight loss and produces silver streaking and pin-root weld line failures. Melt temperature is maintained at 250–270°C, mould temperature between 60°C and 90°C, and screw configuration typically uses 20:1–24:1 L/D with a compression ratio of 2.2:1–2.8:1. A 120 t toggle clamp machine running a 16-cavity connector body tool at 70 MPa injection pressure is a representative production configuration; glass fibre orientation around through-pins creates anisotropic shrinkage, with flow-direction shrinkage in the 0.3–0.5% range and cross-flow values up to 1.0–1.2% when measured by ISO 294-4. Finished components in this segment include underhood wiring harness connector bodies, camshaft sensor housings, ABS wheel-speed sensor shrouds, and electronic throttle control connector shells.

    What Limits Comparative Tracking Index and Glow-Wire Performance in Non-Halogenated PBT Terminal Blocks?

    Low-voltage terminal blocks, relay bases, and contactor coil bodies manufactured from SABIC VALOX™ PBT+GF15% 815 encounter insulation coordination requirements where tracking resistance, creepage, and glow-wire behaviour are evaluated together rather than independently. The grade contains no flame-retardant package, so its flammability classification is UL 94 HB; it is not a substitute for a V-0 grade in unsupervised circuits above 0.2 A where end-product glow-wire requirements invoke IEC 60695-2-11. The fixed formulation proportion is the as-supplied glass loading of 15 wt%; the material is processed at 100 wt% as pellets. If colour masterbatch is used, dosing at the hopper typically ranges from 2 wt% to 4 wt%, which reduces base resin proportion to 96–98 wt% and must be validated for tracking and glow-wire effects because colourant chemistry can alter surface conductivity. Regrind use should not exceed 20 wt% in thin-wall terminal bases; higher regrind ratios lower impact-modulated wall integrity around terminal retention windows. The downstream forming route is high-cavitation injection moulding with multi-pin tooling. Drying is performed at 120°C for 3–4 h to <0.02% moisture, melt temperature is capped at 270°C, and mould temperature is held at 80–90°C to reduce post-mould shrinkage anisotropy. A critical production limitation is weld-line integrity at the base of metal terminal retaining features; glass orientation around inserted pins creates local modulus variation, and excessive hold pressure beyond 80 MPa can increase moulded-in stress without improving weld strength. Where dimensional stability is required after termination, post-mould annealing at 120°C for 2 h is used to relax orientation stress, but the process must be balanced against embrittlement risk at sharp corners. Terminal products include DIN rail terminal block bodies, industrial relay base sockets, contactor coil former supports, and printed circuit board terminal housings.

    StandardTest or FunctionRelevance to PBT-GF15 Terminal BlocksApplication Note
    IEC 60947-7-1Terminal blocks for low-voltage switchgear and controlgearDimensional and thermal requirements for connection bodiesApplies to final terminal block assembly
    IEC 60664-1Insulation coordination for equipment within low-voltage systemsCreepage and clearance sizing based on tracking classTracking class may be lowered by glass filler
    IEC 60112Comparative tracking index testSurface tracking resistance of moulded insulationColour package can shift the index; verify per formulation
    UL 94Flammability classificationHB classification for the unfilled flame-retardant packageNot acceptable where V-0 is specified
    IEC 60695-2-11Glow-wire flammability test for end productsFinal product glow-wire ignition assessmentRequired when end-product standard invokes the test

    Appliance motor end caps, condenser fan hubs, and compressor mounting brackets made from SABIC VALOX™ PBT+GF15% 815 are governed by IEC 60335-1 for household appliance safety and by long-term thermal ageing data in UL 746B. The fixed glass addition ratio of 15 wt% is not adjusted at the press; the grade is used neat, and any attempt to dilute with unfilled resin below 80 wt% filled content compromises the stiffness required for shaft-bearing retention. Drying uses a desiccant hopper dryer at 120°C for 3 h minimum, with dew point maintained at -30°C or lower. Moulding on 8-cavity hot-runner tools requires externally heated manifolds rather than internal torpedo systems to avoid excess shear in the glass-filled melt; valve gating is preferred over open hot tips because 15 wt% glass fibre accelerates gate erosion. Mould temperature is held between 60°C and 80°C, and a slower fill profile reduces jetting at the hub centre where glass-rich skins can lift from unfilled core material. This scenario is well established and is not a deep process-conflict zone; the primary control points are moisture and gate maintenance. Finished parts include refrigerator compressor mounting brackets, outdoor condenser fan hubs, range hood motor mounts, and air purifier centrifugal fan hubs.

    Edison-base lampholder bodies and LED driver enclosures represent a regulatory path in which UL 496 and IEC 60838-1 control lampholder dimensional integrity, while IEC 61347-1 applies to lamp controlgear enclosures. The formulation addition ratio in this segment is base resin at 96–98 wt% with colour or UV masterbatch dosed at 2–4 wt%; glass fibre content remains 15 wt% in the compounded base pellet. Because the grade is not flame-retarded, it is specified only for socket and driver enclosure positions where end-product glow-wire testing does not require V-0, or where the luminaire standard uses current-carrying location exemptions. Moulding is performed on multi-cavity hot-runner tools with valve-gated drops; melt temperature is limited to 255–270°C, and mould temperature is held at 70–85°C to maintain socket thread diameter within UL 496 gauge limits. Injection speed is profiled with a fast initial fill into the thread zone followed by a reduced velocity across the body to prevent glass fibre read-through on the external surface. Drying before moulding is identical: 120°C for 3–4 h in a desiccant dryer to below 0.02% moisture. Terminal products include E12, E14, and E26 lampholder bodies, GU10 socket housings with copper insert retention, LED driver enclosures with snap-fit lids, and track lighting connector blocks. Use in fully enclosed luminaires requires verification that continuous socket temperature remains below the grade’s published relative thermal index.

    Pneumatic Valve Manifold Dimensional Control in Washed-Down Industrial Cabinets

    Pneumatic solenoid valve bases and flow-meter terminal housings produced from SABIC VALOX™ PBT+GF15% 815 must maintain port-to-port flatness after repeated pressure cycling and occasional wash-down exposure. Applicable compliance references include ISO 5599-1 for pneumatic valve mounting interfaces, IEC 60529 for enclosure sealing levels such as IP65, and IEC 60079-0 only where the final assembly is evaluated as non-sparking equipment; the plastic itself is not an explosion-protection barrier. The addition ratio is 100 wt% as supplied, with the 15 wt% glass reinforcement fixed by the manufacturer and verified by ISO 3451-1. Moulding uses desiccant-dried resin at 120°C for 3–4 h; melt temperature is kept at 250–265°C, and mould temperature is set at 70–80°C to stabilise flat sealing faces. Hold pressure is staged with a lower final segment to avoid overpacking thick manifold galleries where sink marks would violate sealing-surface flatness. Glass fibre accumulation around hot-runner corners can produce local flow marks, so runner diameter should not fall below 4 mm for 15 wt% filled PBT. Finished parts include pneumatic valve island manifold bases, flow-meter terminal boxes, pressure sensor enclosures, and industrial control panel mounting bases.

    Free Quote

    Competitive SABIC VALOX™ PBT+GF15% 815 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Designated as a semi-crystalline polyester injection-molding grade, SABIC VALOX™ PBT+GF15% 815 is a pelletized polybutylene terephthalate compound containing 15% glass-fiber reinforcement by mass. The product is positioned for components requiring higher stiffness and lower creep than unfilled PBT while retaining better melt flow and lower anisotropic shrinkage than 30% glass-reinforced PBT. In dry-as-molded condition, density is generally observed in the 1.40–1.45 g/cm³ range under ISO 1183-1; melt volume-flow rate at 250 °C and 5 kg falls approximately in the 10–25 cm³/10 min band when tested according to ISO 1133-1:2022. Because the polyester backbone is susceptible to hydrolytic chain scission, pellets must be dried to a residual moisture content below 0.02% before melt processing; typical regeneration parameters are 120 °C for 3–4 h in a dehumidifying dryer with air dew point at or below -30 °C. The compound is commonly used in multi-pin electrical connectors, relay bases, bobbins, motor brush holders, cooling fan blades, and small appliance housings where dimensional stability and moderate mechanical load capacity are required.

    How Does 15% Glass Reinforcement Shift the Mechanical Profile Relative to Unfilled PBT and 30% Glass PBT?

    The mechanical response is governed by fiber aspect ratio, glass-matrix adhesion, and fiber orientation through the thickness. Under ISO 527-2 tensile testing at 23 °C, unfilled PBT typically exhibits tensile stress at break between 40 MPa and 55 MPa; a 15% glass-filled grade such as VALOX 815 is generally reported in the 80–100 MPa range, whereas a 30% glass PBT commonly reaches 100–130 MPa. Flexural modulus measured by ISO 178 rises from 2.2–2.6 GPa for unfilled PBT to 4.5–5.5 GPa at 15% glass content, and to 7.5–9.0 GPa for 30% glass. Strain at break declines from double-digit unfilled values to roughly 2–4% for 15% reinforcement, reflecting the reduced ductility expected with rigid-fiber load transfer. Notched Izod impact data acquired under ISO 180/A are normally higher than unfilled PBT at room temperature, but the increase is less pronounced than in 30% glass compounds, placing VALOX 815 in a moderate-toughness band.

    Table 1. Class-typical mechanical and thermal profiles
    Property and test methodUnfilled PBTPBT+GF15 (VALOX 815 class)PBT+GF30
    Density, ISO 1183-11.30–1.32 g/cm³1.40–1.45 g/cm³1.50–1.55 g/cm³
    Tensile stress at break, ISO 527-240–55 MPa80–100 MPa100–130 MPa
    Flexural modulus, ISO 1782.2–2.6 GPa4.5–5.5 GPa7.5–9.0 GPa
    Notched Izod impact, ISO 180/A3–5 kJ/m²4–6 kJ/m²7–10 kJ/m²
    Deflection temperature at 1.8 MPa, ISO 75-2/Af50–60 °C175–195 °C200–215 °C
    Mold shrinkage flow direction, ISO 294-41.4–2.0%0.4–0.8%0.2–0.5%
    CLTE flow direction, ISO 11359-2100–120 µm/m/°C40–60 µm/m/°C20–35 µm/m/°C

    On production-scale injection lines, VALOX 815 is best processed with a general-purpose polyester or polyolefin screw having a low-to-moderate compression ratio, typically 2.0:1 to 2.5:1, and a shut-off nozzle to prevent drool from the low-melt-viscosity polyester. Barrel temperature settings from rear to front are normally set between 240 °C and 265 °C, with the nozzle set no higher than 270 °C. Melt residence time above 265 °C should be kept below 6 min; longer holdup accelerates hydrolytic and thermal degradation and produces surface streaks, brown discoloration, and molecular-weight loss. Mold temperature is maintained in the 60–100 °C window, with 80 °C used as a default for dimensional stability and sufficient crystallinity. Low mold temperatures below 60 °C reduce crystallization rate but may increase post-mold shrinkage and lower surface gloss; high mold temperatures above 100 °C can extend cycle time without proportional structural benefit. Injection speed should be moderate to high, with a fill time often falling in the 0.5–1.5 s range for parts of 2–3 mm nominal wall thickness. Gate diameters should not be less than 0.8 mm for unfilled grades and 1.0 mm for glass-reinforced PBT to limit shear-induced fiber breakage and surface jetting.

    Residual moisture control is not a secondary recommendation. At melt temperatures above 250 °C, water reacts with the ester linkage rapidly; a moisture content of 0.05% can lower melt viscosity by roughly 10–15% and reduce tensile strength after molding by 5–10% compared with dry material. On machines with long material feed lines, stainless steel tubes should be used instead of copper alloys, which can accelerate degradation of molten PBT. Hopper loaders should be cleaned to remove fines that hold moisture and produce splay. The dryer must be sized to the extruder throughput; a residence time of 3–4 h assumes a desiccant bed capable of maintaining dew point at -30 °C under full hopper load.

    Table 2. Representative processing window for VALOX 815
    ParameterSetpoint or rangeReference or equipment basis
    Drying temperature and time120 °C, 3–4 hDehumidifying dryer
    Drying air dew point-30 °C or lowerDew-point meter
    Maximum residual moisture0.02%ISO 15512 method B
    Melt temperature250–270 °CNozzle pyrometer
    Mold temperature60–100 °CThermolator
    Barrel setpoint range240–265 °CInjection machine zones
    Nozzle limit260–270 °CShut-off nozzle
    Hold pressure40–80 MPaMachine hydraulic pressure
    Fill time0.5–1.5 s2–3 mm wall thickness
    Screw cushion2–5 mmInjection molding machine
    Open hopper exposure at RH above 60%30 min maximumClosed feed system recommended

    When Thin-Wall Sections and Short Cycle Times Are Required, Processing Discipline Determines Part Quality

    Thin-wall molding with this class of PBT is constrained by freeze-off at the flow front because rapid crystallization induces a solidified skin layer. Tooling with generous venting, valve-gated hot runners, and direct edge gates minimizes pressure drop. For multi-cavity tools, fill balance should be within ±5% by mass to avoid cavity-to-cavity variation in fiber orientation and shrinkage; otherwise, warp and weld-line displacement occur in electrical connectors with pin pitches below 2.54 mm. Published data for this specific configuration is limited, but process capability studies on similar PBT+GF15 grades indicate that clamping-force requirements scale with projected area and are typically evaluated using a cavity-pressure transducer threshold of 30–50 MPa at transfer from velocity to pressure control. Decompression strokes longer than 3–5 mm should be avoided because air entrapment produces burn marks at the flow front. A cushion of 2–5 mm is adequate to maintain consistent hold pressure without degrading material in the compression zone.

    Thermal, Electrical, and Chemical Boundaries Governing Connector Reliability

    Because VALOX 815 is a non-flame-retardant glass-reinforced PBT, the UL rating is generally HB at thicknesses common to electrical enclosures; applications requiring V-0 at 0.8 mm or 1.6 mm should select a flame-retardant VALOX grade or verify the exact UL Yellow Card entry. Comparative tracking index values for glass-reinforced PBT typically fall in the 250–400 V interval under IEC 60112, although exact values depend on color formulations and test thickness. Continuous exposure to hot water above 60 °C is not advised because PBT undergoes hydrolytic degradation at ester linkages; brief contact with dilute acids and aliphatic hydrocarbons is tolerable, but strongly alkaline cleaners and amine-containing additives should be avoided. For outdoor use, UV stabilization is required and should be validated by accelerated weathering under ISO 4892-2 with a defined radiant exposure, not inferred from short-term property retention. Thermal aging under UL 746B should be reviewed for electrical insulating systems; the relative thermal index is application- and thickness-dependent and must not be assumed from heat deflection temperature alone.

    Drying at the molding machine should integrate a closed feed system when ambient relative humidity exceeds 60%; open hoppers are acceptable only if cumulative exposure is below 30 min. Hopper magnets and fine screens are recommended to capture tramp metal and fiber agglomerates before they reach the non-return valve. During long campaigns, purging with a high-viscosity polyolefin or commercial PBT purge compound reduces black specks and carbonized deposits in the screw. Tooling for glass-reinforced PBT requires wear-resistant steel, particularly at gates and runner intersections; hardened tool steel with surface hardness above 50 HRC is common for production runs exceeding 100,000 shots. Runner systems should be full-round or trapezoidal, and cold slug wells are required ahead of the cavity. Hot runners require internally heated torpedo or externally heated manifold systems with set temperatures no higher than 270 °C and thermal uniformity within ±5 °C to prevent local stagnation.

    Warpage, Weld-Line Strength, and Replacement Scope Against Polyamide and Higher-Glass PBT Grades

    Compared with a 30% glass-fiber PBT grade such as SABIC VALOX 420, VALOX 815 exhibits lower flow-direction flexural modulus and higher isotropic contraction during cooling, but also lower anisotropy between flow and transverse directions in flat plaques. Mold shrinkage differences of roughly 0.4–0.8% in flow and 0.8–1.2% transverse under ISO 294-4 mean that round-hole alignment in multi-pin connectors may require asymmetric tool dimensions rather than a simple global scale factor. The lower glass loading reduces abrasive wear on tooling and screw surfaces and produces less surface fiber blooming; it is therefore specified where snap-fit insertion force, hinge durability, or ultrasonic welding amplitude sensitivity require a balance of stiffness and limited embrittlement.

    Relative to glass-reinforced polyamide 66, PBT+GF15% 815 absorbs substantially less moisture at equilibrium; water absorption for PBT is generally reported at 0.3–0.5% by ISO 62 at 23 °C, whereas PA66 reaches 6–8%. The lower moisture uptake supports tighter dimensional stability in humid automotive cabin modules and electrical switch housings, but the continuous-use temperature ceiling of low-glass PBT is below that of heat-stabilized PA66. Components exposed to under-hood air temperatures above 130 °C should be evaluated against thermal-oxidative aging data, not only short-term heat deflection temperature. Against PBT+GF10, the 15% variant raises stiffness and reduces creep at moderate load; against PBT+GF30, it retains higher melt flow in thin ribs and lowers the risk of embrittlement at weld lines. A documented failure mode on production lines when weld-line strength is underestimated is cracking initiating at knit lines adjacent to pin inserts; this is mitigated by moving gates closer to thick sections, increasing mold temperature to 80 °C, and raising hold pressure within the 40–80 MPa range.

    Top